ZrO_(2) toughened Al_(2)O_(3)(Al_(2)O_(3)/ZrO_(2))ceramic layers with required thickness were prepared by electrophoretic deposition(EPD)method using ethanol suspensions with stabilizing agent of polyethyleneimine(PEI...ZrO_(2) toughened Al_(2)O_(3)(Al_(2)O_(3)/ZrO_(2))ceramic layers with required thickness were prepared by electrophoretic deposition(EPD)method using ethanol suspensions with stabilizing agent of polyethyleneimine(PEI)under constant-voltage mode in this paper.The deposition of Al_(2)O_(3)/ZrO_(2) ceramic powders occurred on the titanium alloy cathode.A stable suspension with 1wt% PEI in ethanol at pH 5 was prepared in terms of the zeta potential and sedimentation of the suspension.The effects of the suspension concentration,applied voltage,deposition time and processing method of titanium alloy cathode on the coating thickness and morphology were investigated.The deposition layers on titanium alloys with smooth surfaces and thickness of 0.35–1.2 mm could be obtained by adjusting the aforementioned parameters.In addition,after being sintered at 1500℃ for 3 h in air atmosphere,ZrO_(2) toughened Al_(2)O_(3) ceramic layers became smooth and dense.展开更多
基金This work was supported by the National Natural Science Foundation of China(Grant Nos.60871062 and 50873066)Distinguished Young Scholars of Sichuan Province(08ZQ026-007)The supports from Sichuan Province through a Science Fund for Key Technologies Research and Development Program of Sichuan Province(2008SZ0021 and 2006Z08-001-1)are also acknowledged with gratitude.
文摘ZrO_(2) toughened Al_(2)O_(3)(Al_(2)O_(3)/ZrO_(2))ceramic layers with required thickness were prepared by electrophoretic deposition(EPD)method using ethanol suspensions with stabilizing agent of polyethyleneimine(PEI)under constant-voltage mode in this paper.The deposition of Al_(2)O_(3)/ZrO_(2) ceramic powders occurred on the titanium alloy cathode.A stable suspension with 1wt% PEI in ethanol at pH 5 was prepared in terms of the zeta potential and sedimentation of the suspension.The effects of the suspension concentration,applied voltage,deposition time and processing method of titanium alloy cathode on the coating thickness and morphology were investigated.The deposition layers on titanium alloys with smooth surfaces and thickness of 0.35–1.2 mm could be obtained by adjusting the aforementioned parameters.In addition,after being sintered at 1500℃ for 3 h in air atmosphere,ZrO_(2) toughened Al_(2)O_(3) ceramic layers became smooth and dense.