作者 Z. Li y.l. yand +1 位作者 J.K Xi J.X. Qu and H. S. Shao (Department of Materials Engineering, Luoyang institute of Technology, Luoyang 471039, China)(Beijing Graduate School, China University of Mining and Technology, Beijing 100083, China) 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1996年第5期355-360,共6页
Annealing treatment has a strong effect on mechanical Properties of cold worked tungsten-nickel-iron heavy alloys. A 93W-4.5Ni-2.5Fe alloy swaged 15% was annealed from 500 to 1350℃ to investigate the changes in micro... Annealing treatment has a strong effect on mechanical Properties of cold worked tungsten-nickel-iron heavy alloys. A 93W-4.5Ni-2.5Fe alloy swaged 15% was annealed from 500 to 1350℃ to investigate the changes in microstructure and their effects on mechanical properties. Recrystallization of W particles takes place during annealing treatments above 800℃ and the microhardnesses reduces rapidly. High density of dislocations in the, matrix phase after annealing treatment at 1350℃ suggests that recrystallization of the matrix phase has not taken place. A small decrease in microhardness of the matrix phase is caused by recovery during the annealing treatments.The changes in mechanical properties of swaged and annealed 93W-4.5 Ni-2.SFe alloy are mainly due to the changes in microstructure of W particles because of their recrystallization. 展开更多
关键词 W-4.5 Ni-2. 5 Fe alloy RECRYSTALLIZATION DISLOCATION
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部