A novel, reactive amide-bridged ladder polyvinylsiloxane (abbr. LP) with Mn= 2.4×10^4 was synthesized for the first time by means of aryl amide H-bonding self-assembled template. The regularity of LP was charac...A novel, reactive amide-bridged ladder polyvinylsiloxane (abbr. LP) with Mn= 2.4×10^4 was synthesized for the first time by means of aryl amide H-bonding self-assembled template. The regularity of LP was characterized by the XRD, ^29Si NMR and DSC methods. XRD analysis demonstrated the ladder width w = 9.09A and the ladder thickness t = 3.89A, respectively, which are approximately consistent with the molecular simulation-calculated ones: w'= 10.60A and t'= 3.06A. ^29Si NMR displayed a resonance peak with small half peak width, △1/2 - 4 ppm, for the moiety [=Si(Vi)O2/2-]n of LP. Besides, as a collateral evidence, DSC measurement revealed a high glass transition temperature Tg = 225℃, suggesting high stiffness of the ladder main chain of LP.展开更多
文摘A novel, reactive amide-bridged ladder polyvinylsiloxane (abbr. LP) with Mn= 2.4×10^4 was synthesized for the first time by means of aryl amide H-bonding self-assembled template. The regularity of LP was characterized by the XRD, ^29Si NMR and DSC methods. XRD analysis demonstrated the ladder width w = 9.09A and the ladder thickness t = 3.89A, respectively, which are approximately consistent with the molecular simulation-calculated ones: w'= 10.60A and t'= 3.06A. ^29Si NMR displayed a resonance peak with small half peak width, △1/2 - 4 ppm, for the moiety [=Si(Vi)O2/2-]n of LP. Besides, as a collateral evidence, DSC measurement revealed a high glass transition temperature Tg = 225℃, suggesting high stiffness of the ladder main chain of LP.