Temperature dependence of elastic moduli , , and the latter for the piezo-active and non-piezo-active versions, have been measured in the interval of 4 - 180 K at 28 - 262 MHz in a CdSe: Cr2+ crystal. Anomalies below ...Temperature dependence of elastic moduli , , and the latter for the piezo-active and non-piezo-active versions, have been measured in the interval of 4 - 180 K at 28 - 262 MHz in a CdSe: Cr2+ crystal. Anomalies below 40 K have been found for all the moduli, except . The interpretation of the results has been carried out involving the Jahn-Teller effect and relaxation between the equivalent distortions of the tetrahedral CrSe4 centers.展开更多
文摘Temperature dependence of elastic moduli , , and the latter for the piezo-active and non-piezo-active versions, have been measured in the interval of 4 - 180 K at 28 - 262 MHz in a CdSe: Cr2+ crystal. Anomalies below 40 K have been found for all the moduli, except . The interpretation of the results has been carried out involving the Jahn-Teller effect and relaxation between the equivalent distortions of the tetrahedral CrSe4 centers.