Effects of continuous casting mould fluxes on reducing longitudinal and star cracks on a slab surface 被引量:1
1
作者 WANGQian WANGYu +4 位作者 CHIJinghao XIEBing HEYuming zhubing CHENWenman 《Journal of Chongqing University》 CAS 2004年第1期65-68,共4页
In the continuous casting production of medium carbon steel (whose mass fraction of carbon is 0.09 % to 0.16 %) and high strength low alloy steel (whose mass fraction of Mn is 0.90 % to 1.40 %), flecks occurring the m... In the continuous casting production of medium carbon steel (whose mass fraction of carbon is 0.09 % to 0.16 %) and high strength low alloy steel (whose mass fraction of Mn is 0.90 % to 1.40 %), flecks occurring the most often are usually longitudinal and star cracks. In additional to the employment of a galvanized plate mould, two kinds of fluxes with special properties were studied and used to harmonize the conflicts between the function of heat transfer and lubrication. An industrial application revealed that the crystallizing temperature (Tc) and crystal ratio (R) of fluxes have a crucible effect on impeding the occurrence of above defects on a slab surface. In the case of slab section (180 to 240) mm(1000 to 1400) mm and casting speed Vc of (0.7 to 1.2) m/min, the optimized parameters of fluxes are Tc of (1170 to 1190) ℃, R of 80 % to 95 % for medium carbon steel, and Tc of (1100 to 1150) ℃, plus R of 40 % to 60 % for high strength low alloy steel. 展开更多
关键词 continuous casting mould flux star crack longitudinal crack
下载PDF
Cecropin B gene transformed rice(Oryza sativa L.) plants show improved resistance to rice bacterial diseases
2
作者 HUANGDanian zhubing +4 位作者 YANGWei XUERui XIAOHan LILiangcai TIANWenzhong 《Chinese Rice Research Newsletter》 1995年第2期2-2,共1页
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部