The mixer-settler is a core device of solvent extraction for separating rare earth elements. There are some adverse effects like high rare earth accumulation and poor production efficiency during industrial production...The mixer-settler is a core device of solvent extraction for separating rare earth elements. There are some adverse effects like high rare earth accumulation and poor production efficiency during industrial production. Current researches usually focus on changing the structure of the mixer-settler without making a breakthrough towards gravity clarification. In this paper, in order to improve the efficiency of clarification, a mixer-settler with double stirring mode was designed and manufactured by adding a stirring device in the settler after reducing the volume of the settler. The innovation of this research involves adopting the ultraviolet-visible spectrophotometer to investigate the quantity of aqueous phase entrainment at the settler outlet in order to measure the clarification degree. Experimental results show that the clarification effect with stirring is better than that without stirring. The clarification effect is ameliorated as the stirring speed increases. Generally, the clarification effect shows a best condition when the offset distance is 12.5 cm, making the phase entrainment reduced to less than 0.1%. When the clearance over the tank bottom is 7 cm and 10 cm, respectively, the quantity of aqueous phase entrainment is better than the case with a clearance of 4 cm. The results show that the stirring paddle close to the mixed phase zone can better promote the two-phase separation.展开更多
In order to solve the problem that the vulcanizing agent utilization rate is low and the dilution effect of copper slag is poor,the vortex stirring dilution method was used to improve the conditions of the dilution ki...In order to solve the problem that the vulcanizing agent utilization rate is low and the dilution effect of copper slag is poor,the vortex stirring dilution method was used to improve the conditions of the dilution kinetics and copper recovery.The water model was used to simulate the effect of copper slag dilution.Under the premise of keeping the Reynolds number consistent,silicone oil and glass beads were used instead of copper slag and vulcanizing agent.Based on the relationship between voltage and concentration,the PC6D dual-channel particle concentration measuring instrument was used to study the stirring speed and the insertion depth of the stirring paddle in model experiments,and the suitable conditions were speed 250 rpm and insertion depth 70 mm.The fire dilution of copper slag was done under the conditions.After stirring and sedimentation,the Fe_(3)O_(4) in slag decreased from 22.58% to 4.65%,and the copper content of the slag decreased from 2.94% to 0.34%.The copper recovery was 88.44%.展开更多
基金supported by Hi-Tech Research and Development Program(863)of China(2010AA03A405)the National Natural Science Foundation of China(No.50974035,No.51004033)
文摘The mixer-settler is a core device of solvent extraction for separating rare earth elements. There are some adverse effects like high rare earth accumulation and poor production efficiency during industrial production. Current researches usually focus on changing the structure of the mixer-settler without making a breakthrough towards gravity clarification. In this paper, in order to improve the efficiency of clarification, a mixer-settler with double stirring mode was designed and manufactured by adding a stirring device in the settler after reducing the volume of the settler. The innovation of this research involves adopting the ultraviolet-visible spectrophotometer to investigate the quantity of aqueous phase entrainment at the settler outlet in order to measure the clarification degree. Experimental results show that the clarification effect with stirring is better than that without stirring. The clarification effect is ameliorated as the stirring speed increases. Generally, the clarification effect shows a best condition when the offset distance is 12.5 cm, making the phase entrainment reduced to less than 0.1%. When the clearance over the tank bottom is 7 cm and 10 cm, respectively, the quantity of aqueous phase entrainment is better than the case with a clearance of 4 cm. The results show that the stirring paddle close to the mixed phase zone can better promote the two-phase separation.
基金Funded by the National Natural Science Foundation of China(52004284)the Fundamental Research Funds from the Central University of the Ministry of Education of China(2020QN55)the China Postdoctoral Science Foundation(2019M661979)。
文摘In order to solve the problem that the vulcanizing agent utilization rate is low and the dilution effect of copper slag is poor,the vortex stirring dilution method was used to improve the conditions of the dilution kinetics and copper recovery.The water model was used to simulate the effect of copper slag dilution.Under the premise of keeping the Reynolds number consistent,silicone oil and glass beads were used instead of copper slag and vulcanizing agent.Based on the relationship between voltage and concentration,the PC6D dual-channel particle concentration measuring instrument was used to study the stirring speed and the insertion depth of the stirring paddle in model experiments,and the suitable conditions were speed 250 rpm and insertion depth 70 mm.The fire dilution of copper slag was done under the conditions.After stirring and sedimentation,the Fe_(3)O_(4) in slag decreased from 22.58% to 4.65%,and the copper content of the slag decreased from 2.94% to 0.34%.The copper recovery was 88.44%.
基金National Natural Science Foundation of China (U1908225, U1702253)Fundamental Research Funds for the Central Universities (N182515007,N170908001, N2025004)
基金Fundamental Research Funds for the Central Universities(N182504018)National Natural Science Foundation of China(51874078)Fund of Liaoning S&T Project(20180551008)。