Cationic ring-opening polymerization of 3,3-bis(chloromethyl)oxacyclobutane in ionic liquids 被引量:1
1
作者 Yuan Yuan Wang Wei Li Li Yi Dai 《Chinese Chemical Letters》 SCIE CAS CSCD 2007年第10期1187-1190,共4页
Cationic ring-opening polymerization of 3,3-bis(chloromethyl)oxacyclobutane catalyzed by BF3.OEt2 was carded out in ionic liquids [bmim]BF4 and [bmim]PF6. The influences of BCMO concentration and molar ratio of BCMO... Cationic ring-opening polymerization of 3,3-bis(chloromethyl)oxacyclobutane catalyzed by BF3.OEt2 was carded out in ionic liquids [bmim]BF4 and [bmim]PF6. The influences of BCMO concentration and molar ratio of BCMO/BF3.OEt2 on the molecular weights and yield of PBCMO were investigated. The polymerization in ionic liquids proceed to high conversions, although molecular weights are limited, similar to polymerization in organic solvent such as CH2Cl2. Follow a viewpoint of green chemistry, we feel ionic liquid [bmim]BF4 is superior to [bmim]PF6. Extracting [bmim]PF6 from the product using organic solvent as extractant limits its advantage as a green reaction media. 展开更多
关键词 Ionic hquid 3 3-Bis(chloromethyl)oxacyclobutane cationic ring-opening polymerization CHARACTERIZATION
下载PDF
SYNTHESIS AND CATIONIC RING-OPENING POLYMERIZATION OF 1, 4-ANHYDRO-2, 3-DI-O-(P-AZIDOBENZYL)-α-D-RIBOPYRANOSE
2
作者 Toshiyuki Uryu 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 1999年第2期123-128,共6页
New highly stereoregular 2, 3 -di- O-(p-azidobenzyl )-(1 →5 ) - α-D -ribofuranan was synthesized byselective ring-opening polymerization of 1, 4-anhydro-2, 3 - di-O -(p-azidobenzyl )-α-D -ribopyranose(ADABR) using ... New highly stereoregular 2, 3 -di- O-(p-azidobenzyl )-(1 →5 ) - α-D -ribofuranan was synthesized byselective ring-opening polymerization of 1, 4-anhydro-2, 3 - di-O -(p-azidobenzyl )-α-D -ribopyranose(ADABR) using phosphorus pentafluoride or tin tetrachloride as catalyst at low temperature indichloromethane. The monomer was obtained by the reaction of p - bromomethyl -phenyleneazide with 1, 4 -anhydro-α-D-ribose in DMF. The structure of poly(ADANR) was identified by specific rotation and ^(13)C-NMR spectroscopy. Acid chloride-AgCl_4 complex catalyst such as CH_2=C(CH_3)C^+OClO_4^- used in thepolymerization resulted in polymers with mixed structures, i.e. (1→5)-α-D-ribofuranosidic and (1→4)-β-D-ribopyranosidic units. However, with C_6H_5C^+OClO_4^- as catalyst, pure (1→5)-α-D-ribofuranan was obtained.The effects of catalyst, polymerization temperature and time on polymer stereoregularity were examined, andthe mechanism of the ring-opening polymerization was discussed. 展开更多
关键词 cationic ring-opening polymerization Azido-containing polysaccharide Lewis acid catalysts 1 4-anhydro-2 3-di-O-(p-azidobenzyl)-α-D-ribopyranose STEREOREGULARITY
下载PDF
Real-time Monitoring of Living Cationic Ring-opening Polymerization of THF and Direct Prediction of Equilibrium Molecular Weight of Poly THF 被引量:4
3
作者 An-ru Guo Fan Yang +1 位作者 Rui Yu 吴一弦 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2015年第1期23-35,共13页
A convenient real-time monitoring of monomer concentration during living cationic ring-opening polymerizations of tetrahydrofuran(THF) initiated with methyl triflate(Me OTf) has been developed for kinetic investig... A convenient real-time monitoring of monomer concentration during living cationic ring-opening polymerizations of tetrahydrofuran(THF) initiated with methyl triflate(Me OTf) has been developed for kinetic investigation and determination of equilibrium monomer concentration([M]e) via in situ FTIR spectroscopy in combination with a diamond tipped attenuated total reflectance(ATR) immersion probe. The polymerization rate was first order with respect to monomer concentration and initiator concentration from the linear slope of ln([M]0-[M]e)/([M]-[M]e) versus polymerization time at different temperatures in various solvents. [M]e decreased linearly with initial monomer concentration while increased exponentially with increasing polymerization temperature. The equilibrium also strongly depends on solvent polarity and its interaction with monomer. The equilibrium polymerization time(te) decreased with increasing solvent polarity and decreased linearly with increasing [M]0 in three solvents with different slopes to the same point of bulk polymerization in the absence of solvent. Equation of Mn,e = 72.1/(0.14–0.04[M]e) has been established to provide a simple and effective approach for the prediction for the number-average molecular weight of poly THFs at equilibrium state(Mn,e) in the equilibrium living cationic ring-opening polymerization of THF at 0 °C. 展开更多
关键词 cationic ring-opening polymerization Living polymerization Tetrahydrofuran Equilibrium Kinetics.
原文传递
STUDY ON CATIONIC RING-OPENING COPOLYMERIZATION OF 1,4-ANHYDRO-2,3-DI-O-BENZYL-α-D-RIBOPYRANOSE WITH 1,4-ANHYDRO-2,3-O-ISOPROPYLIDENE-α-D-RIBOPYRANOSE
4
作者 吴承佩 潘才元 瓜生敏之 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 1997年第3期282-288,共7页
Cationic ring-opening copolymerization of 1, 4-anhydro-2, 3-O-isopropylidene-α-D-ribo-pyranose (AIRP) with 1,4-anhydro-2,3-di-O-benzyl-α-D-ribopyranose (ADBR) preparedfrom D-ribose was studied. Copolymerization usin... Cationic ring-opening copolymerization of 1, 4-anhydro-2, 3-O-isopropylidene-α-D-ribo-pyranose (AIRP) with 1,4-anhydro-2,3-di-O-benzyl-α-D-ribopyranose (ADBR) preparedfrom D-ribose was studied. Copolymerization using SbCl_5 or BF_3 OEt_2 as catalyst atlow temperature gave stereoregular (1→4)β-D-ribofuranan (C-1 and C-4 ring cleavagesee Scheme 1) or (1→5) α-D-ribofuranan (C-1 and C-5 ring cleavage) respectively. Theeffects of catalysts, reaction time and temperatures on yield and stereoregularity of the ob-tained polymers were studied. Polymers were characterized by molecular weight, ~1HNMR,^(13)CNMR and optical rotation. 展开更多
关键词 1 4-Anhydroribose derivatives cationic ring-opening copolymerization Specific rotation Lewis acid catalysts
下载PDF
CATIONIC POLYMERIZATION OF ISOBUTYLENE COINITIATED BY AICI_3 IN THE PRESENCE OF ETHYL BENZOATE 被引量:4
5
作者 吴一弦 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2010年第1期55-62,共8页
The cationic polymerizations of isobutylene (IB) coinitiated by AlCl3 were carried out in solvent mixture of nhexane/methylene dichloride (n-hex/CH2Cl2) of 60/40 V/V in the presence of ethyl benzoate (EB) at var... The cationic polymerizations of isobutylene (IB) coinitiated by AlCl3 were carried out in solvent mixture of nhexane/methylene dichloride (n-hex/CH2Cl2) of 60/40 V/V in the presence of ethyl benzoate (EB) at various temperatures range from -80℃ to -30℃. The effects of EB concentration ([EB]) and polymerization temperature on monomer conversion, weight-average molecular weight (Mw) and molecular weight distribution (MWD, Mw/Mn) of polyisobutylene (PIB) products were investigated. The rate of polymerization decreased while Mw of PIB products increased with increasing [EB]. The polymers with high molecular weight could be prepared in the presence of a suitable amount of EB. Significantly, the polymers with high Mw of 80.2 × 10^4 and 65.4 × 10^4 could be produced at -80℃ and -70℃ at [EB] = 0.24 × 10^3 mol/L respectively, which were much higher than that (Mw = 57.9 × 10^4) of PIB prepared at -100℃ in the absence ofEB. A simple but effective method for preparing the high molecular weight polyisobutylenes was developed in this work. It has been also found that the activation energy for propagation (Ep) depended on the polymerization temperature range in the presence of EB. An obvious inflection of the linear plots of lnXn versus 1/Tp occurred at the temperature range from -60℃ to -50℃ at four different concentrations of EB from 0.19 × 10^3 mol/L to 0.33× 10^3 tool/L, and thus the inflection temperature (Tinf) was in the range of -60℃ to -50℃. When [EB] was in the range of 0.24 × 10^3 mol/L to 0.33× 10^3 mol/L, Ep was determined to be around -12 kJ/mol when the polymerization was carried out at temperatures from -80℃ to Tinf and to be around -28 kJ/mol at temperatures from Tinf to -15℃ respectively. 展开更多
关键词 Electron donor cationic polymerization ISOBUTYLENE Polyisobutylene.
下载PDF
Cationic Ring Opening Polymerization of Octamethylcyclotetrasiloxane Initiated by Acid Treated Bentonite 被引量:5
6
作者 陈碧 詹晓力 +1 位作者 易玲敏 陈丰秋 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2007年第5期661-665,共5页
Cationic ring opening polymerization of octamethylcyclotetrasiloxane (Da) initiated by acid treated bentonite was investigated. The experimental conditions were chosen on the basis of preliminary experiments.Higher ... Cationic ring opening polymerization of octamethylcyclotetrasiloxane (Da) initiated by acid treated bentonite was investigated. The experimental conditions were chosen on the basis of preliminary experiments.Higher temperature was found beneficial for the reaction process while stirring intensity beyond a certain level showed no obvious effect on the reaction rate. Polymers were characterized by Fourier transform infrared, proton nuclear magnetic resonance (IH-NMR) and gel perneation chromotography. The width of molecular mass distribution was found ranging between 1.2 and 1.4, which is extraordinarlly narrow compared with that of cationic polymerizations reported elsewhere (〉 1.9). The results were believed due to the absence of free proton and counter ion which simplifies the polymerization process and the huge steric hindrance provided by bentonite particles which keeps the propagation of polysiloxane onto the surface of bentonite particles in a much more regular way. A feasible mechanism is proposed and seems to be supported well by experiments. Additionally, from the results of α, ω-dihydrogen terminated polysiloxanes prepared, the possibility of applying this potential environmentally friendly heterogeneous catalyst in industrial polymerization of cyclosiloxanes is anticipated. 展开更多
关键词 OCTAMETHYLCYCLOTETRASILOXANE cationic polymerization POLYSILOXANE
下载PDF
RING-OPENING POLYMERIZATION OF TRIMETHYLENE CARBONATE CATALYZED BY NOVEL SINGLE COMPONENT RARE EARTH CALIXARENE COMPLEXES 被引量:3
7
作者 沈之荃 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2005年第4期407-410,共4页
In this paper,ring-opening polymerization of trimethylene carbonate(TMC)with rare earth(Nd,Y,La)ρ-tert- butylcalix[n]arene(n=4,6,and 8)complexes as catalysts has been studied.Poly(trimethylene carbonate)(PTMC)with M_... In this paper,ring-opening polymerization of trimethylene carbonate(TMC)with rare earth(Nd,Y,La)ρ-tert- butylcalix[n]arene(n=4,6,and 8)complexes as catalysts has been studied.Poly(trimethylene carbonate)(PTMC)with M_v of 21,400 was produced by bulk polymerization under the conditions as follows:[TMC]_0/[Nd](molar ratio)=1000,80℃, 8 h.Mechanism study reveals that the polymerization proceeds via a coordination mechanism. 展开更多
关键词 ring-opening polymerization Trimethylene carbonate CALIXARENE Rare earth complex
下载PDF
Ring-opening Polymerization ofε-Caprolactone Using Lanthanide Tris(4-tert-butylphenolate)s as a Single-component Initiator 被引量:4
8
作者 Cui Ping YU, Li Fang ZHANG, Zhi Quan SHEN Institute of Polymer Science, Zhejiang University, Hangzhou 310027 《Chinese Chemical Letters》 SCIE CAS CSCD 2003年第10期1021-1023,共3页
The ring-opening polymerization of e-caprolactone (CL) initiated by novel single lanthanide tris(4-tert-butylphenolate)s [Ln(OTBP)3] is reported. Single-component La(OTBP)3 can effectively prepare polycaprolactone (PC... The ring-opening polymerization of e-caprolactone (CL) initiated by novel single lanthanide tris(4-tert-butylphenolate)s [Ln(OTBP)3] is reported. Single-component La(OTBP)3 can effectively prepare polycaprolactone (PCL) with over 90% yield and viscosity average molecular weight about 60 x 10 under quite mild conditions: molar ratio of CL to initiator is 1000, 60 C, 2 h in toluene. Mechanism study indicates that the monomer inserts into the growing chain via the break of acyl-oxygen bond of CL. 展开更多
关键词 Lanthanide tris(4-tert-butylphenolate)s e-caprolactone ring-opening polymerization.
下载PDF
SYNTHESIS OF POLYISOBUTYLENE WITH SEC-ARYLAMINO TERMINAL GROUP BY COMBINATION OF CATIONIC POLYMERIZATION WITH ALKYLATION 被引量:1
9
作者 吴一弦 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2009年第4期551-559,共9页
The highly reactive polyisobutylenes(PIBs) withα-double bonds(87.5 mol%) or tert-chloro(tert-Cl) groups(95 mol%) could be prepared via the cationic polymerization of isobutylene(IB) coinitiated by BF_3 or TiCl_4 resp... The highly reactive polyisobutylenes(PIBs) withα-double bonds(87.5 mol%) or tert-chloro(tert-Cl) groups(95 mol%) could be prepared via the cationic polymerization of isobutylene(IB) coinitiated by BF_3 or TiCl_4 respectively.The Friedel-Crafts alkylation of diphenylamine(DPA) with the highly reactive PIB withα-double bonds was further conducted under different conditions,such as at different alkylation temperature,in the mixed solvents of CH_2Cl_2/n-hexane with different solvent polarity and at DPA concentr... 展开更多
关键词 POLYISOBUTYLENE cationic polymerization DIPHENYLAMINE ALKYLATION
下载PDF
RING-OPENING POLYMERIZATION OFε-CAPROLACTONE USING LANTHANIDE TRIS(N-PHENYL-3,5-DI-T-BUTYLSALICYLALDIMINATO)S AS SINGLE COMPONENT CATALYST 被引量:2
10
作者 沈之荃 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2007年第5期541-544,共4页
Ring-opening polymerization of ε-caprolactone has been carried out by using rare earth Schiff base complexes: lanthanide tris(N-phenyl-3,5-di-t-butylsalicylaldiminato)s [Ln(OPBS)3] as single component catalyst f... Ring-opening polymerization of ε-caprolactone has been carried out by using rare earth Schiff base complexes: lanthanide tris(N-phenyl-3,5-di-t-butylsalicylaldiminato)s [Ln(OPBS)3] as single component catalyst for the first time. The influences of different rare earth elements, monomer and catalyst concentration as well as reaction time on the polymerization were investigated. Mechanism studies showed that monomer inserts into the active site with the acyl-oxygen bond scission rather than the break of alkyl-oxygen bond. 展开更多
关键词 ring-opening polymerization Ε-CAPROLACTONE Lanthanide Schiff base complex.
下载PDF
SYNTHESIS, CHARACTERIZATION AND RING-OPENING POLYMERIZATION OF CYCLIC (ARYLENE PHOSPHONATE) OLIGOMERS 被引量:2
11
作者 陈天禄 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2004年第1期83-89,共7页
A series of cyclic (arylene phosphonate) oligomers were prepared by reaction of phenylphosphonic dichloride (PPD) with various bisphenols under pseudo-high dilution conditions via interfacial polycondensation. The yie... A series of cyclic (arylene phosphonate) oligomers were prepared by reaction of phenylphosphonic dichloride (PPD) with various bisphenols under pseudo-high dilution conditions via interfacial polycondensation. The yield of cyclic (arylene phosphonate) oligomers is over 85% by using hexadecyltrimethylammoniun bromide as phase transfer catalyst (PTC) at 0 'C . The structures of the cyclic oligomers were confirmed by a combination of matrix-assisted laser desorption/ionization time-of-flight mass spectrometry (MALDI-TOF-MS) and IR analysis. These cyclic oligomers undergo facile ring-opening polymerization in the melt by using potassium 4,4'-biphenoxide as the initiator to give linear polyphosphonate. Free-radical ring-opening polymerization of cyclic(arylene phosphonate) oligomers containing sulfur linkages was also performed in the melt using 2,2'-dithiobis(benzothiazole) (DTB) as the initiator at 270 °C and the resulting polymer had a Mw, of 8 × 103 with a molecular weight distribution of 4. Ring-opening copolymerization of these cyclic oligomers with cyclic carbonate oligomers was also achieved. The average molecular weight of the resulting copolymer is higher than the corresponding homopolymer and the thermal stability of the copolymer is better than the corresponding homopolymer. 展开更多
关键词 Cyclic(arylene phosphonate) oligomer ring-opening polymerization COpolymer
下载PDF
SYNTHESIS OF POLY(5,5-DIMETHYL-1,3-DIOXAN-2-ONE)BY LIPASE-CATALYZED RING-OPENING POLYMERIZATION 被引量:1
12
作者 贺枫 卓仁禧 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2003年第1期5-8,共4页
Porcine pancreas lipase (PPL) and PPL immobilized on narrow distributed micron-sized glass beads wereemployed successfully for the ring-opening polymerization of 5, 5-dimethyl-1, 3-dioxan-2-one (DTC) for the first tim... Porcine pancreas lipase (PPL) and PPL immobilized on narrow distributed micron-sized glass beads wereemployed successfully for the ring-opening polymerization of 5, 5-dimethyl-1, 3-dioxan-2-one (DTC) for the first time.Different polymerization conditions such as enzyme concentration and reaction temperature were studied. Immobilized PPLexhibits higher activity than native PPL. Along wth the increasing enzyme concentration, the molecular weigh of resultingPDTC decreases. PPL immobilized on narrow distributed micron-sized glass beads has outstanding recyclability. For thethird recycle time, immobilized PPL exhibits the highest catalytic activity and with high activity even after the fifth recyletime for the synthesis of PDTC. The ~1H-NMR spectra indicate that decarboxylation does not occur during the ring-openingpolymerization. 展开更多
关键词 Enzymatic polymerization Immobilized enzyme ring-opening polymerization POLYCARBONATES
下载PDF
Calcium chloride doped zinc-cobalt metal-cyanide complex:Unexpected highly activity towards ring-opening polymerization of propylene oxide 被引量:1
13
作者 Yi Jun Huang Xing Hong Zhang +1 位作者 Zheng Jiang Hua Guo Rong Qi 《Chinese Chemical Letters》 SCIE CAS CSCD 2010年第8期897-901,共5页
Highly active calcium chloride(CaCl2) doped Zn-Co^Ⅲdouble metal-cyanide(Ca-DMC) catalysts were firstly reported.Ca-DMCs presented a very higher polymer yield(54 kg polymer/g catalyst) at relative low temperatur... Highly active calcium chloride(CaCl2) doped Zn-Co^Ⅲdouble metal-cyanide(Ca-DMC) catalysts were firstly reported.Ca-DMCs presented a very higher polymer yield(54 kg polymer/g catalyst) at relative low temperature(80-115℃) toward ringopening polymerization(ROP) of propylene oxide(PO) than did DMC catalysts without modification. 展开更多
关键词 Catalysts POLYETHERS ring-opening polymerization Metal-cyanide complex
下载PDF
A Series of Rare Earth Phenolates Substituted by Alkyl Groups for D,L-Lactide Ring-Opening Polymerization 被引量:1
14
作者 王艳 张丽芳 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2011年第5期939-944,共6页
Single component rare earth phenolates substituted by various alkyl groups have been prepared and the correlation between the aryloxides' structure and catalytic activity in the ring-opening polymerization of D,L-lac... Single component rare earth phenolates substituted by various alkyl groups have been prepared and the correlation between the aryloxides' structure and catalytic activity in the ring-opening polymerization of D,L-lactide has also been investigated.The catalytic activity of all rare earth aryloxides,characteristics of the ring-opening polymerization as well as polymerization kinetics and mechanism were investigated.The results showed that both phenolates' catalytic activities and polymerization characteristics changed regularly,keeping in good concordance with variations in substitutents' number on phenol and structure of aryloxide ligands.The stronger ability of electron-donation of alkyl groups,the higher catalytic activity.Moreover,the more numbers of substituted alkyl on phenyl ring,the higher catalytic activity.The analyses of polymer ends revealed that the polymerization proceeded via a coordination-acyl-oxygen bond cleavage-insertion mechanism. 展开更多
关键词 ring-opening polymerization D L-LACTIDE rare earth phenolates
下载PDF
Tetrahydrosalen backboned gadolinium complex as initiator for the ring-opening polymerization of ε-caprolactone 被引量:1
15
作者 Guang Ming Wu Xu Feng Ni Wei Lin Sun Zhi Quan Shen 《Chinese Chemical Letters》 SCIE CAS CSCD 2008年第6期681-684,共4页
Tetrahydrosalen ligand was employed in the synthesis of gadolinium complex. The ligand was deprotoned by LiBu, and the afforded lithium salt was reacted with anhydrous GdCl3 to produce the gadolinium complex through s... Tetrahydrosalen ligand was employed in the synthesis of gadolinium complex. The ligand was deprotoned by LiBu, and the afforded lithium salt was reacted with anhydrous GdCl3 to produce the gadolinium complex through salt metathesis. This complex was successfully used to initiate the ring-opening polymerization of ε-caprolactone. The initiation conditions in different temperature, monomer-to-initiator ratio and time were investigated. Under the condition: [ε-caprolactone]:[catalyst] = 600, 56 ℃, toluene: 2 ml, poly(ε-caprolactone) (PCL) with Mw = 11,2782 and PDI = 1.96 was achieved. 展开更多
关键词 Tetrahydrosalen complex Rare earth catalyst Ε-CAPROLACTONE ring-opening polymerization
下载PDF
RING-OPENING POLYMERIZATION OF TRIMETHYLENE CARBONATE BY CALIX[8]ARENE-NEODYMIUM 被引量:1
16
作者 Ling Ge Zhi-quan Shen +1 位作者 Yi-feng Zhang Qiao-hong Huang Department of Polymer Science and Engineering, Zhejiang University, Hangzhou 310027, China 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2000年第1期77-80,共4页
Ring-opening polymerization of trimethylene carbonate (TMC) with a rare earth calixarene compound as catalyst has been studied for the first time. The effect of TMC/Nd (molar ratio) and polymerization conditions were ... Ring-opening polymerization of trimethylene carbonate (TMC) with a rare earth calixarene compound as catalyst has been studied for the first time. The effect of TMC/Nd (molar ratio) and polymerization conditions were investigated in detail. It was found that calix[8]arene-neodymium is a highly effective catalyst for the bulk polymerization of TMC and gives high molecular weight (M-v = 60,000) polymer. The optimum conditions of TMC polymerization were found to be as follows:TMC/Nd (molar ratio) = 2,000, 80 degrees C, 16 h. The polymers were characterized by NMR, GPC and DSC. Studying the mechanism by NMR showed that the polymerization of TMC catalyzed by calix[8]arene-neodymium proceeds via a cationic mechanism. 展开更多
关键词 ring-opening polymerization trimethylene carbonate arene-neodymium
下载PDF
SYNTHESIS OF NOVEL BI-FUNCTIONAL COPOLYMER BEARING STERICALLY HINDERED PHENOL AND HINDERED AMINE GROUPS VIA RING-OPENING METATHESIS POLYMERIZATION 被引量:1
17
作者 Bo-yong Xue Kenichi Ogata Akinori Toyota 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2008年第5期525-531,共7页
Norbornene derivatives exo,endo-2-[2-(3,5-di-tert-butyl-4-hydroxyphenoxy)-acetoxy]methyl-5-norbornene(M1) and 3,3,5,5-tetramethyl-4-piperidinyl 5-norbornene-exo,endo-2-carboxylate(M2)were synthesized and polymerized b... Norbornene derivatives exo,endo-2-[2-(3,5-di-tert-butyl-4-hydroxyphenoxy)-acetoxy]methyl-5-norbornene(M1) and 3,3,5,5-tetramethyl-4-piperidinyl 5-norbornene-exo,endo-2-carboxylate(M2)were synthesized and polymerized by RuCl_2(=CHPh)(PCy_3)_2 to prepare a novel kind of bi-functional polymer bearing sterically hindered phenol(SHP)and hindered amine(HLAS)groups via ring-opening metathesis polymerization(ROMP).The resulting copolymers were characterized by gel permeation chromatography(GPC),~1H-NMR and differen... 展开更多
关键词 Sterically hindered phenol Hindered amine ring-opening metathesis polymerization(ROMP)
下载PDF
Novel Single-component Rare Earth Phenolate Catalyst for Ring-opening Polymerization of ε-Caprolactone 被引量:1
18
作者 FAN Ling ZHANG Li-fang SHEN Zhi-quan 《Chemical Research in Chinese Universities》 SCIE CAS CSCD 2003年第4期516-517,共2页
关键词 Lanthanide tris(2 4 6-trimethylphenolate) ring-opening polymerization ε -Caprolactone
下载PDF
RING-OPENING POLYMERIZATION OF l,4-DIOXAN-2-ONE INITIATED BY LANTHANUM TRIS(2,6-DI-TERT-BUTYL-4-METHYLPHENOLATE) 被引量:1
19
作者 沈之荃 郑豪 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2007年第4期427-430,共4页
The ring-opening polymerization of 1,4-dioxan-2-one (PDO) was carried out by lanthanum tris(2,6-di-tert-butyl-4- methylphenolate) (La(OAr)3) as novel single component initiaLor. The influences of polymerizatio... The ring-opening polymerization of 1,4-dioxan-2-one (PDO) was carried out by lanthanum tris(2,6-di-tert-butyl-4- methylphenolate) (La(OAr)3) as novel single component initiaLor. The influences of polymerization reaction temperature and the molar ratio of monomer to initiator on the monomer conversion and molecular weight of poly(1,4-dioxan-2-one) (PPDO) were explored. PPDO with high viscosity average molecular weight of 1.95×10^5 can be prepared at 40℃ when [PDO]/ [La(OAr)3] molar ratio was 800. Mechanism investigation shows that the polymerization proceeds through a "coordination- insertion" mechanism with selective rupture of acyl-oxygen be,nd of PDO. 展开更多
关键词 Lanthanum tris(2 6-di-tert-butyl-4-methylphenolate) 1 4-dioxan-2-one ring-opening polymerization.
下载PDF
Mononuclear and Dinuclear Yttrium Complexes Supported by Pyrrolide Ligands: Syntheses, Structures and Catalytic Behaviors towards the Ring-opening Polymerization of ε-Caprolactone 被引量:1
20
作者 裴浩 陆宁 +5 位作者 刘玮 陈砚美 吴冰 李海燕 李亚红 李武 《Chinese Journal of Structural Chemistry》 SCIE CAS CSCD 2016年第7期1085-1092,共8页
The syntheses, structures and catalytic activities of two yttrium complexes supported by pyrrolide ligands are reported. Treatment of Y(N(Si Me3)2)3 with one equivalent of H3bptd(H3bptd = 1,9-bis(2-pyrrolyl)-2,... The syntheses, structures and catalytic activities of two yttrium complexes supported by pyrrolide ligands are reported. Treatment of Y(N(Si Me3)2)3 with one equivalent of H3bptd(H3bptd = 1,9-bis(2-pyrrolyl)-2,5,8-triazanona-1,8-diene) in THF gave a complex of composition [Y(bptd)(THF)]2(1). Reaction of Y(N(Si Me3)2)3 with one equivalent of H3tpa(H3tpa = tris(pyrrolyl-α-methyl)amine) in THF generated [Y(tpa)(THF)3](2) in good yield. Complexes 1and 2 have been characterized by single-crystal X-ray diffraction, elemental analyses and NMR spectroscopy. Complex 1 is dinuclear. The two metal centers are doubly bridged by two amine nitrogen atoms to form a Y–N–Y–N four-membered rhombus ring. The geometries of Y^3+ ions in 1and 2 are well described as pentagonal bipyramid and capped octahedron, respectively. The ring-opening polymerization reactions of ε-caprolactone initiated by 1 and 2, respectively, were investigated. They both exhibited good catalytic activity for the polymerization of ε-caprolactone. All of the obtained polymers have high molecular weights and relatively narrower PDIs. The polymers generated by 2 possessed polydispersity close to 1.1. The good catalytic activities of 1 and 2 reveal their potential applications in polymer industry. 展开更多
关键词 yttrium pyrrolide ligand synthesis crystal structure ring-opening polymerization