Study on wear resistant cast B-containing 1Cr18Ni9Ti stainless steel 被引量:5
1
作者 Kuang Jiacai Jiang Zhiqiang +2 位作者 Zhang Shiyin Ye Chang Liu Qicheng 《China Foundry》 SCIE CAS 2009年第1期32-36,共5页
The developed 1Cr18Ni9Ti austenitic stainless steel containing 1.63 wt.%B have been characterized by X-ray diffraction(XRD),electron probe microanalyzer(EPMA),optical microscopy(OM),scanning electron microscopy(SEM),e... The developed 1Cr18Ni9Ti austenitic stainless steel containing 1.63 wt.%B have been characterized by X-ray diffraction(XRD),electron probe microanalyzer(EPMA),optical microscopy(OM),scanning electron microscopy(SEM),energy dispersive X-ray spectroscopy(EDS)and Vickers microhardness measurement.The microstructural evolution and property of high boron stainless steel after solution treatment at the temperature of 1050℃are also investigated.The results show that the main compositions of borides are Fe,Cr and B,and with small amount of Ni,Mn and C elements.Silicon is insoluble in the borides.The hardness of borides is over 1,500 HV.It has been found that borides do not decompose during solution treatment,but part of borides dissolves into the matrix. The effect of increasing the solubility of boron element in the austenitic matrix favours the hardness enhancement by 8.54%.High boron stainless steel has excellent wear resistance in corrosive environment.Lifetime of transfer pipe made of high boron-containing stainless steel is 1.5-1.8 times longer than that of boron-free 1Cr18Ni9Ti stainless steel. 展开更多
关键词 1cr18ni9ti austenitic stainless steel BORON BORIDE corrosive wear
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部