S_2O_8^(2-)/ZrO_2-Al_2O_3固体超强酸催化剂的研制与应用 被引量:46
1
作者 但悠梦 米远祝 田大听 《应用化学》 CAS CSCD 北大核心 2001年第10期840-842,共3页
A S 2O 2- 8/ZrO 2 Al 2O 3 type solid superacid catalyst was prepared from ZrOCl 2·8H 2O, AlCl 3· 6H 2O and (NH 4) 2S 2O 8 by coprecipitation, maceration and calcination processes. Their crystal structures an... A S 2O 2- 8/ZrO 2 Al 2O 3 type solid superacid catalyst was prepared from ZrOCl 2·8H 2O, AlCl 3· 6H 2O and (NH 4) 2S 2O 8 by coprecipitation, maceration and calcination processes. Their crystal structures and acidities were determined by XRD and Hammett method, respectively. The activity of the catalyst was studied as function of Al 2O 3 content, calcination temperature and time in the esterification of acetic acid with butanol, and a conversion of 96 5% was obtained. The catalyst gave also higher yields in syntheses of ketals and acetals: cyclohexanone ethylene ketal(86 2%), acetophenone ethylene ketal(78 5%), acetylacetic ester ketal(88 5%), benzaldehyde glycol acetal(76 3%). The chemical structures of the products were confirmed by IR spectra. 展开更多
关键词 s2o8^2-/Zro2-al2o3 固体超强酸催化剂 酯化 缩酮化 缩醛化 制备 应用 氧化锆 氧化铝 硫酸 催化活性
下载PDF
La改性固体超强酸S_2O_8^(2-)/ZrO_2-Al_2O_3的制备及催化性能研究 被引量:13
2
作者 马惠琴 王卫 马媛媛 《材料导报》 EI CAS CSCD 北大核心 2014年第6期48-52,64,共6页
采用共沉淀-浸渍法制备了固体超强酸S2O82-/ZrO2-Al2O3催化剂,并加入La对催化剂进行改性。以柠檬酸三丁酯的合成为探针反应评价催化剂的活性,并通过红外光谱、X射线衍射、NH3程序升温脱附等方法对催化剂进行表征,考察制备条件及La的引... 采用共沉淀-浸渍法制备了固体超强酸S2O82-/ZrO2-Al2O3催化剂,并加入La对催化剂进行改性。以柠檬酸三丁酯的合成为探针反应评价催化剂的活性,并通过红外光谱、X射线衍射、NH3程序升温脱附等方法对催化剂进行表征,考察制备条件及La的引入对催化剂结构和性能的影响。结果表明:(NH4)2S2O8溶液浸渍浓度为0.5mol/L,锆铝氧化物物质的量比为1∶1,600℃焙烧4h后于1%(质量分数)的La(NO3)3溶液浸渍所得的催化剂活性较好,柠檬酸的转化率可达93.69%。La的引入可以提高催化剂对S2O82-的结合能力,抑制活性组分的分解,增加催化剂的酸强度和酸总量,提高催化剂的活性。 展开更多
关键词 稀土 固体超强酸 s2o82- ZRo2-al2o3 柠檬酸三丁酯
下载PDF
微乳液法制备Pt-S_2O_8^(2-)/ZrO_2-Al_2O_3型固体超强酸催化剂及其异构化性能 被引量:4
3
作者 宋华 石洋 宋华林 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2012年第9期2061-2066,共6页
采用微乳液法负载Pt制备了Pt-S2O28-/ZrO2-Al2O3(Pt-SZA-M)固体超强酸催化剂,以正戊烷异构化反应为探针,对比了微乳液法和浸渍法负载Pt制备的催化剂(Pt-SZA)的异构化性能,并采用XRD,FTIR,BET,TG-DTA,TPR和TEM对催化剂进行了表征.结果表... 采用微乳液法负载Pt制备了Pt-S2O28-/ZrO2-Al2O3(Pt-SZA-M)固体超强酸催化剂,以正戊烷异构化反应为探针,对比了微乳液法和浸渍法负载Pt制备的催化剂(Pt-SZA)的异构化性能,并采用XRD,FTIR,BET,TG-DTA,TPR和TEM对催化剂进行了表征.结果表明,与Pt-SZA催化剂相比,Pt-SZA-M催化剂中Pt粒子的粒径更小(4.5 nm)且尺寸更均一;Pt-SZA-M催化剂的比表面积(109.6 m2/g)比Pt-SZA催化剂(95.0m2/g)增加了15.4%.Pt-SZA-M催化剂的初始还原温度比Pt-SZA催化剂降低了10~20℃,表明微乳液法负载Pt可以提高催化剂的氧化活性,提高氢分子在催化剂上的吸附解离能力.异构化活性实验结果表明,与Pt-SZA催化剂相比,Pt-SZA-M催化剂的低温活性得到明显改善,在反应压力为2.0 MPa、氢烃摩尔比为4∶1、质量空速为1.0 h-1的条件下,Pt-SZA-M催化剂在反应温度为230℃时活性达到60.8%,在100 h内异戊烷的收率可稳定在58.0%左右,选择性在95.0%以上. 展开更多
关键词 固体超强酸 微乳液法 异构化 PT s2o28- ZRo2-al2o3
下载PDF
浸渍法制备高选择性1-丁烯齐聚催化剂Fe_2O_3·SO_4^(2-)/γ-Al_2O_3 被引量:2
4
作者 肖林久 陈家欢 +2 位作者 盛永刚 李文泽 王金豹 《石油学报(石油加工)》 EI CAS CSCD 北大核心 2016年第4期695-702,共8页
通过分步浸渍法制备Fe_2O_3·SO_4^(2-)/γ-Al_2O_3催化剂,并用于催化1-丁烯齐聚反应,考察了催化剂制备条件和反应条件对催化性能的影响,并与Fe_2(SO_4)_3/γ-Al_2O_3催化剂进行性能比较。结果表明,在0.96 MPa、60℃、液时空速为5h-... 通过分步浸渍法制备Fe_2O_3·SO_4^(2-)/γ-Al_2O_3催化剂,并用于催化1-丁烯齐聚反应,考察了催化剂制备条件和反应条件对催化性能的影响,并与Fe_2(SO_4)_3/γ-Al_2O_3催化剂进行性能比较。结果表明,在0.96 MPa、60℃、液时空速为5h-1的反应条件下,采用Fe负载量为6%、SO_4^(2-)负载量为1.2 mmol/g(γ-Al_2O_3)的Fe_2O_3·SO_4^(2-)/γ-Al_2O_3催化剂,1-丁烯齐聚反应的转化率达到68.0%,二聚物选择性为95.0%。α-Fe_2O_3是催化1-丁烯齐聚反应的活性组分,并能提高二聚体选择性;此外,α-Fe_2O_3晶相与SO2-4的相互作用对其催化1-丁烯齐聚反应的活性有重要影响,γ-Al_2O_3与SO_4^(2-)的相互作用也对催化活性有一定的影响。Fe负载量为6%的Fe_2O_3·SO_4^(2-)/γ-Al_2O_3催化活性最高,此时NH_3-TPD结果显示,催化剂只存在较弱的酸中心和适中的酸量。 展开更多
关键词 1-丁烯齐聚 催化剂 fe2oso42--al2o3 硫酸铁
下载PDF
复合固体超强酸S_2O_8^(2-)/Fe_2O_3CoO催化合成乙酸正丁酯 被引量:9
5
作者 朱学文 张应军 王军 《郑州轻工业学院学报(自然科学版)》 CAS 2004年第3期16-18,共3页
采用沉淀-浸渍法制备了复合固体超强酸S2O2-8/Fe2O3 CoO,并以S2O2-8/Fe2O3 CoO为催化剂,冰醋酸和正丁醇为原料合成乙酸正丁酯.结果表明:S2O2-8/Fe2O3 CoO的催化活性大于S2O2-8/Fe2O3和S2O2-8/Fe2O3 ZnO,CoO的存在对超强酸性有调变作用,... 采用沉淀-浸渍法制备了复合固体超强酸S2O2-8/Fe2O3 CoO,并以S2O2-8/Fe2O3 CoO为催化剂,冰醋酸和正丁醇为原料合成乙酸正丁酯.结果表明:S2O2-8/Fe2O3 CoO的催化活性大于S2O2-8/Fe2O3和S2O2-8/Fe2O3 ZnO,CoO的存在对超强酸性有调变作用,当V(正丁醇)∶V(乙酸)=3∶1,m(催化剂)∶m(乙酸)=0 8∶100,反应时间为2 5h时,乙酸正丁酯转化率≥98%,催化剂可重复使用4次以上. 展开更多
关键词 复合固体超强酸 s2o8^2-/fe2o3—Coo 催化合成 乙酸正丁酯 沉淀—浸渍法 催化活性
下载PDF
S_2O_8^(2-)/ZrO_2-Al_2O_3的制备、表征及其催化合成富马酸二甲酯 被引量:5
6
作者 李文戈 金华峰 《精细石油化工》 CAS CSCD 北大核心 2008年第1期10-15,共6页
采用浸渍-沉淀法制备出纳米固体超强酸催化剂S_2O_8^(2-)/ZrO_2-Al_2O_3,通过正交实验得到最佳制备条件:Al_2O_3质量分数2.0%,-15℃陈化24 h,浸渍液(NH_4)_2 S_2O_8浓度0.8 mol/L,焙烧温度650℃,焙烧时间3 h。用XRD、TEM、BET、TG-DTG... 采用浸渍-沉淀法制备出纳米固体超强酸催化剂S_2O_8^(2-)/ZrO_2-Al_2O_3,通过正交实验得到最佳制备条件:Al_2O_3质量分数2.0%,-15℃陈化24 h,浸渍液(NH_4)_2 S_2O_8浓度0.8 mol/L,焙烧温度650℃,焙烧时间3 h。用XRD、TEM、BET、TG-DTG和化学分析手段分析了S_2O_8^(2-)/ZrO_2~Al_2O_3的晶化过程、比表面积、含硫量和热稳定性。结果表明,在焙烧温度为500~650℃时制备的催化剂属纳米材料(粒径<41 nm),有较大比表面积和较好的热稳定性;富马酸二甲酯的最佳合成条件为:n(甲醇):n(富马酸)=6.0:1.0,S_2O_8^(2-)/ZrO_2- Al_2O_3用量1.5%,带水剂苯用量10 mL,反应时间4.0 h,催化剂重复使用6次,酯化率大于90%。 展开更多
关键词 纳米复合固体超强酸 s2o8^2-/Zro2-al2o3 催化酯化 富马酸二甲酯
下载PDF
固体超强酸催化剂S_2O_8^(2-)/Fe_2O_3-Al_2O_3的制备及其酯化性能 被引量:6
7
作者 占华端 陈晓晖 魏可镁 《工业催化》 CAS 2010年第8期23-29,共7页
以硝酸铁为铁源、硝酸铝为铝源,通过共沉淀法制备固体超强酸催化剂S_2O_8^(2-)/Fe_2O_3-Al_2O_3。通过催化剂样品的FT-IR谱图、不同焙烧温度催化剂样品的XRD谱图、不同陈化温度的N_2吸附-脱附曲线以及催化剂样品的SEM照片,研究了其晶体... 以硝酸铁为铁源、硝酸铝为铝源,通过共沉淀法制备固体超强酸催化剂S_2O_8^(2-)/Fe_2O_3-Al_2O_3。通过催化剂样品的FT-IR谱图、不同焙烧温度催化剂样品的XRD谱图、不同陈化温度的N_2吸附-脱附曲线以及催化剂样品的SEM照片,研究了其晶体的形成过程。催化剂样品红外谱图表明,催化剂中的S=O有较强的共价双键特征,诱导催化剂形成超强酸性;在XRD谱图中既无Al_2O_3的晶相峰,也无Fe_2(SO_4)_3晶相峰,说明Al_2O_3与Fe_2O_3在催化剂样品的表面形成了Al_2O_3-Fe_2O_3共价键的复杂结构。采用BET方程和BJH模型计算催化剂样品的比表面积和孔径分布,经冰水陈化的催化剂样品平均孔径为9.1 nm,最可几孔径为7.5 nm,比表面积为78.9 m^2·g^(-1),孔容0.149 cm^3·g^(-1)。研究了催化剂的铁与铝物质的量比、(NH_4)_2S_2O_8浸渍浓度和不同焙烧温度对硬脂酸正丁酯酯化率的影响。在反应温度85℃、催化剂用量0.2 g(为反应物总质量的2%)和回流反应150 min的条件下,酯化率可达84.5%。 展开更多
关键词 催化化学 过硫酸铵 共沉淀法 s_2o_8~2-/fe_2o_3-al_2o_3固体超强酸 硬脂酸正丁酯
下载PDF
H_2O对Cu^+/S_2O_8^(2-)/γ-Al_2O_3催化剂合成碳酸二甲酯性能的影响 被引量:1
8
作者 郑华艳 刘媛媛 +2 位作者 董睿敏 孟凡会 李忠 《燃料化学学报》 EI CAS CSCD 北大核心 2013年第1期110-115,共6页
反应温度120℃、压力3.0 MPa的条件下,考察了H2O对浆态床DMC合成催化剂Cu+/S2O28-/γ-Al2O3活性的影响。结果表明,外界H2O的引入加剧了催化剂的失活速率。对引入H2O后回收催化剂进行了元素分析、XRD、DTG、Py-FT-IR和NH3-TPD等表征,结... 反应温度120℃、压力3.0 MPa的条件下,考察了H2O对浆态床DMC合成催化剂Cu+/S2O28-/γ-Al2O3活性的影响。结果表明,外界H2O的引入加剧了催化剂的失活速率。对引入H2O后回收催化剂进行了元素分析、XRD、DTG、Py-FT-IR和NH3-TPD等表征,结果表明,H2O的引入加速了催化剂中活性组分Cu的流失速率,生成更多没有催化甲醇氧化羰基化活性的Cu2(OH)3Cl晶体,加剧了催化剂的失活。 展开更多
关键词 失活 Cu%PLUs%/s2o82--al2o3 浆态床 DMC
下载PDF
纳米复合固体超强酸S_2O_8^(2-)/ZrO_2-Al_2O_3的制备及其催化合成乙酸苄酯 被引量:4
9
作者 金华峰 李文戈 《化学世界》 CAS CSCD 北大核心 2008年第3期133-138,共6页
采用改性技术和浸渍—沉淀法制备出纳米固体超强酸催化剂S2O82-/ZrO2-Al2O3。通过正交试验获得了催化剂制备的最佳条件。用XRD、TEM、BET、TG-DTG和化学分析等手段分析了S2O82-/ZrO2-Al2O3的晶化过程、比表面积、含硫量和热稳定性,分析... 采用改性技术和浸渍—沉淀法制备出纳米固体超强酸催化剂S2O82-/ZrO2-Al2O3。通过正交试验获得了催化剂制备的最佳条件。用XRD、TEM、BET、TG-DTG和化学分析等手段分析了S2O82-/ZrO2-Al2O3的晶化过程、比表面积、含硫量和热稳定性,分析结果表明这四个方面对催化剂的酸性有较大影响。500~650°C焙烧温度下制备的催化剂属纳米材料(<41 nm),有较大比表面积和较好的热稳定性。以优化的催化剂S2O82-/ZrO2-Al2O3通过正交试验得到合成乙酸苄酯的最佳条件为∶n(苄醇)∶n(乙酸)=1.3∶1.0,催化剂用量为0.8 g(以0.2 mol乙酸为准),带水剂苯用量为14 mL,反应时间为2.5 h,催化剂重复使用7次酯化率在90%以上,该催化剂具有催化活性高、不污染环境、可重复使用等特点。 展开更多
关键词 纳米复合固体超强酸 s2o8^2-/Zro2-al2o3 催化酯化 乙酸苄酯
下载PDF
Fe_2(SO_4)_3/γ-Al_2O_3固体超强酸的Mssbauer谱研究 被引量:1
10
作者 吴勇 马刚 +4 位作者 胡玉海 张庆 董林 胡征 陈懿 《无机化学学报》 SCIE CAS CSCD 北大核心 2001年第6期859-864,共6页
采用浸渍法制备了一系列Fe2SO43/γAl2O3型固体超强酸样品用Mssbauer谱和XRD研究了不同温度处理对样品中铁组分的存在状态及稳定性的影响结果表明随Fe2SO43含量的变化铁组分可以在γAl2O3表面以单层分散和无定形形式存在当温度≥600℃... 采用浸渍法制备了一系列Fe2SO43/γAl2O3型固体超强酸样品用Mssbauer谱和XRD研究了不同温度处理对样品中铁组分的存在状态及稳定性的影响结果表明随Fe2SO43含量的变化铁组分可以在γAl2O3表面以单层分散和无定形形式存在当温度≥600℃时无定形状态的Fe2SO43又生成晶态的Fe2SO43而形成的晶态Fe2SO43即使在700℃时也不分解。 展开更多
关键词 Moessbauer谱 固体超强酸 fe2(so4)3/ Γ-al2o3 浸渍法 负载型催化剂 γ-三氧化二铝 硫酸铁
下载PDF
固体强酸催化剂S_2O_8^(2-)/ZrO_2-Al_2O_3-M_2O_3(M=Cr,Ce,La)的制备 被引量:14
11
作者 但悠梦 《应用化学》 CAS CSCD 北大核心 2002年第11期1106-1108,共3页
Three kinds of new type solid strong acid catalysts S2O 2-8/ZrO2-Al2O3-M2O3(M=Cr,Ce,La) were prepared. Their crystal structure, surface area, acid strength and sulfur content were determined by means of XRD, BET, fl... Three kinds of new type solid strong acid catalysts S2O 2-8/ZrO2-Al2O3-M2O3(M=Cr,Ce,La) were prepared. Their crystal structure, surface area, acid strength and sulfur content were determined by means of XRD, BET, flow Hammett indicator method and chemical analysis. Their catalytic activities in esterification reaction of acetic acid with n-butanol were studied. The results showed that ZrO2 in the catalysts mainly in tetragonal phase and few in monoclinic phase. The tetragonal phase of ZrO2 and S2O 2-8 are the key factors that guarantee the catalytic activity. Incorporation of appropriate amounts of metallic oxides(Cr2O3,Ce2O3,La2O3) into the catalyst favors the stabilization of sulfur species and surface area, which increase the activity sites on the catalyst. The experimental results showed that three catalysts S2O 2-8/ZrO2-Al2O3(2%)-M2O3(1%)(M=Cr,Ce,La) had higher catalytic activity in mentioned esterification, with the conversion of acetic acid reached 96.8%, 95.7% and 96.1%, respectively. The preparation condition of the catalysts showed great influence on the catalytic activity. 展开更多
关键词 固体强酸催化剂 s2o^2-8/Zro2-al2o3-M2o3 制备 二氧化铬 氧化铝 氧化锰 酯化反应 催化活性
下载PDF
纳米固体酸S_2O_8^(2-)/Fe_2O_3催化合成马来酸二己酯 被引量:2
12
作者 华平 张海军 《精细石油化工》 CAS CSCD 北大核心 2004年第1期21-25,共5页
用S2 O2 -8 浸渍Fe2 O3 并焙烧制得了比SO2 -4/Fe2 O3 催化活性更强的固体超强酸S2 O2 -8/Fe2 O3 。通过马来酐与正己醇的酯化反应考察了催化剂的活性 ,对所合成的催化剂的结构用XRD和TEM进行了表征。结果表明 :S2 O2 -8/Fe2 O3 的催化... 用S2 O2 -8 浸渍Fe2 O3 并焙烧制得了比SO2 -4/Fe2 O3 催化活性更强的固体超强酸S2 O2 -8/Fe2 O3 。通过马来酐与正己醇的酯化反应考察了催化剂的活性 ,对所合成的催化剂的结构用XRD和TEM进行了表征。结果表明 :S2 O2 -8/Fe2 O3 的催化作用明显高于SO2 -4/Fe2 O3 ;对于给定的反应 ,用NH3 ·H2 O作Fe2 O3 沉淀剂、用0 .2 5mol/L的 (NH4) 2 S2 O8浸渍Fe2 O3 15min ,在 5 5 0℃焙烧 3h时可制得较高活性的纳米级催化剂S2 O2 -8/Fe2 O3 ;其晶形为α Fe2 O3 ;有较好的重复使用性 ;它能代替硫酸、对甲苯磺酸用于催化马来酐和正己醇的酯化反应 。 展开更多
关键词 纳米固体酸 s2o8^2-/fe2o3 催化合成工艺 马来酸二己酯 酯化反应
下载PDF
Pt-S_2O_(8-)~2/ZrO_2-Al_2O_3催化剂的制备及其催化正戊烷异构化性能 被引量:2
13
作者 宋华 张旭 《大庆石油学院学报》 CAS 北大核心 2010年第5期96-100,170,共6页
制备固体超强酸Pt-S2O82-/ZrO2-Al2O3催化剂,采用XRD、SEM、TG-DTA、FTIR、ICP等对催化剂进行表征;以正戊烷异构化为模型反应,在高压微反-色谱联合装置上,评价催化剂的活性,考察质量空速、反应温度、反应压力及氢与正戊烷物质的量比(n(... 制备固体超强酸Pt-S2O82-/ZrO2-Al2O3催化剂,采用XRD、SEM、TG-DTA、FTIR、ICP等对催化剂进行表征;以正戊烷异构化为模型反应,在高压微反-色谱联合装置上,评价催化剂的活性,考察质量空速、反应温度、反应压力及氢与正戊烷物质的量比(n(氢)∶n(正戊烷))对正戊烷异构化反应的影响.结果表明:当反应温度为220℃、压力为2.0MPa、n(氢)∶n(正戊烷)=4∶1、质量空速为1.5h-1时,正戊烷转化率为76.7%,异戊烷产率为72.5%,异戊烷选择性为94.5%,液收率为96.5%. 展开更多
关键词 固体超强酸 s2o28- 异构化 PT ZRo2-al2o3 正戊烷
下载PDF
Fe掺杂对Pt-Sn-K/γ-Al_2O_3异丁烷脱氢催化剂性能的影响 被引量:2
14
作者 荣欣 时宇 +3 位作者 李先如 顾彬 于杨 孙承林 《工业催化》 CAS 2016年第4期48-54,共7页
采用共沉淀法制备不同Fe含量的Fe(x)-γ-Al_2O_3复合氧化物载体,并采用真空浸渍法制备了Pt-Sn-K/Fe(x)-γ-Al_2O_3催化剂。对制备的催化剂进行XRD、N_2物理吸附-脱附和NH_3-TPD表征,研究Fe的掺杂对Pt-Sn-K/Fe(x)-γ-Al_2O_3催化剂的结... 采用共沉淀法制备不同Fe含量的Fe(x)-γ-Al_2O_3复合氧化物载体,并采用真空浸渍法制备了Pt-Sn-K/Fe(x)-γ-Al_2O_3催化剂。对制备的催化剂进行XRD、N_2物理吸附-脱附和NH_3-TPD表征,研究Fe的掺杂对Pt-Sn-K/Fe(x)-γ-Al_2O_3催化剂的结构及其催化异丁烷脱氢反应性能的影响。结果表明,Fe的引入可以改变催化剂的反应活性和产物选择性,当Fe_2O_3掺杂质量分数为4%时,催化剂具有最高的异丁烯收率,50 h的平均收率达到42.9%。 展开更多
关键词 催化化学 fe掺杂 Pt—sn—K/fe(x)-γ-al2o3催化剂 共沉淀 异丁烷脱氢
下载PDF
铁系固体超强酸Fe_2O_3/S_2O_8^(2-)的制备及丁酸异戊酯的合成 被引量:4
15
作者 李家贵 朱万仁 陈渊 《化工时刊》 CAS 2002年第12期37-39,共3页
Fe_2O_3/S_2O_8^(2-)超强酸是直接由Fe_2O_3制备而成。本文研究了焙烧温度对催化活性的影响,探索了催化酯化反应的最佳条件。实验结果表明:Fe_2O_3/S_2O_8^(2-)超强酸催化剂是一种性能良好的酯化催化剂,制备简单,能够循环使用,无三废污... Fe_2O_3/S_2O_8^(2-)超强酸是直接由Fe_2O_3制备而成。本文研究了焙烧温度对催化活性的影响,探索了催化酯化反应的最佳条件。实验结果表明:Fe_2O_3/S_2O_8^(2-)超强酸催化剂是一种性能良好的酯化催化剂,制备简单,能够循环使用,无三废污染,催化效率高,对丁酸异戊酯酯化产率可高达96.02%。 展开更多
关键词 铁系 固体超强酸 fe2o3/s2o8^2- 制备 丁酸异戊酯 合成
下载PDF
Cu/ZrO_2/S_2O_8^(2-)/γ-Al_2O_3固体酸催化剂制备与催化选择还原NO性能 被引量:1
16
作者 郭锡坤 王小明 《环境科学》 EI CAS CSCD 北大核心 2008年第6期1737-1742,共6页
以拟薄水铝石焙烧得到的γ-Al2O3为载体,分步浸渍负载(NH4)2S2O8、ZrOCl2和Cu(NO3)2,制成Cu/ZrO2/S2O28-/γ-Al2O3固体酸催化剂.考察了Cu/ZrO2/S2O82-/γ-Al2O3在富氧条件下对C3H6选择还原NO的催化性能,并借助SEM、XRD、Py-IR和TPR等表... 以拟薄水铝石焙烧得到的γ-Al2O3为载体,分步浸渍负载(NH4)2S2O8、ZrOCl2和Cu(NO3)2,制成Cu/ZrO2/S2O28-/γ-Al2O3固体酸催化剂.考察了Cu/ZrO2/S2O82-/γ-Al2O3在富氧条件下对C3H6选择还原NO的催化性能,并借助SEM、XRD、Py-IR和TPR等表征方法研究了它的结构和性能的关系.性能的实验结果表明,Cu/ZrO2/S2O28-/γ-Al2O3在无水条件下能使NO的最大转化率达到82.9%,在有10%水蒸气存在条件下仍能使NO的最大转化率达到80.2%.表征测试的结果表明,S2O82-和ZrO2能够抑制γ-Al2O3颗粒之间的烧结及CuAl2O4尖晶石相的生成,同时促使催化剂表面新酸性中心(B酸)的形成及总酸量的增加,另外ZrO2还能提高Cu物种的还原性,从而有效地改善了催化剂的催化活性和水热稳定性. 展开更多
关键词 Cu/Zro2/s2o8^2--al2o3 固体酸 选择还原 No
下载PDF
SO_4^(-2)/Fe_2O_3-Al_2O_3纳米固体酸的红外光谱研究 被引量:6
17
作者 尤秀丽 林德娟 +1 位作者 陈彰旭 卢双春 《光谱实验室》 CAS CSCD 2003年第2期228-230,共3页
用 IR光谱研究了 SO2 -4 / Fe2 O3- Al2 O3纳米固体酸在不同焙烧温度下表面结构与酸性的变化 ,结果表明 ,当焙烧温度在 4 5 0— 5 0 0℃时 ,双齿螯合配位结构特征谱带齐全 ,酸性强 ,小于 4 5 0℃时 ,双齿螯合配位特征谱带不齐全 ,酸性不... 用 IR光谱研究了 SO2 -4 / Fe2 O3- Al2 O3纳米固体酸在不同焙烧温度下表面结构与酸性的变化 ,结果表明 ,当焙烧温度在 4 5 0— 5 0 0℃时 ,双齿螯合配位结构特征谱带齐全 ,酸性强 ,小于 4 5 0℃时 ,双齿螯合配位特征谱带不齐全 ,酸性不强 ,而大于 5 0 0℃时 ,随着温度的升高 ,特征谱带区域宽化 ,特征峰消失 ,酸性变弱。此外 ,从 Fe- O纳米颗粒的特征振动带显示可得知 ,样品的粒径小于 30 nm。 展开更多
关键词 红外光谱 so4^2-/fe2o3-al2o3 纳米固体酸 双齿螯合配位 催化剂
下载PDF
固体超强酸S_2O^(2-)_8ZrO_2-Al_2O_3催化合成丙酸苄酯的研究 被引量:7
18
作者 但悠梦 《湖北民族学院学报(自然科学版)》 CAS 2002年第3期46-48,共3页
用固体超强酸S2 O2 -8 ZrO2 -Al2 O3催化苯甲醇与丙酸的酯化反应合成了丙酸苄酯 .实验结果表明 :S2 O2 -8 ZrO2 -Al2 O3具有较高的催化活性 .考察了苯甲醇与丙酸摩尔比、催化剂用量、反应温度、反应时间、带水剂环己烷用量对酯收率的影... 用固体超强酸S2 O2 -8 ZrO2 -Al2 O3催化苯甲醇与丙酸的酯化反应合成了丙酸苄酯 .实验结果表明 :S2 O2 -8 ZrO2 -Al2 O3具有较高的催化活性 .考察了苯甲醇与丙酸摩尔比、催化剂用量、反应温度、反应时间、带水剂环己烷用量对酯收率的影响 .在典型反应条件下 (苯甲醇与丙酸摩尔比 =1.2∶1,1.0g催化剂 0 .33mol丙酸 ,反应温度 16 0℃ ,反应时间 3.0h和 10ml环己烷 ) ,丙酸苄酯的收率可以达到 86 .6 % .该催化剂易于回收且可重复使用 。 展开更多
关键词 固体超强酸催化剂 s2o8^2-/Zro2-al2o3 催化活性 酯化反应 丙酸苄酸 酯类香料
下载PDF
La添加对S_2O_8^(2-)/ZrO_2-Al_2O_3固体超强酸催化剂性能的影响 被引量:1
19
作者 马惠琴 王卫 马媛媛 《石河子大学学报(自然科学版)》 CAS 2014年第3期360-365,共6页
柠檬酸三丁酯(TBC)是绿色环保无毒的增塑剂,其传统合成工艺采用浓硫酸作催化剂,设备腐蚀、三废问题严重,开发高效、绿色的替代催化剂是当前研究的重点。本文采用共沉淀-浸渍法向S2O82-/ZrO2-Al2O3催化剂中引入适量的La元素,制备出具有... 柠檬酸三丁酯(TBC)是绿色环保无毒的增塑剂,其传统合成工艺采用浓硫酸作催化剂,设备腐蚀、三废问题严重,开发高效、绿色的替代催化剂是当前研究的重点。本文采用共沉淀-浸渍法向S2O82-/ZrO2-Al2O3催化剂中引入适量的La元素,制备出具有较高催化活性和稳定性的固体超强酸催化剂;以柠檬酸三丁酯的合成为探针反应评价催化剂的活性,并通过红外光谱、X射线衍射、NH3程序升温脱附,吡啶红外光谱等表征方法考察了La的添加对催化剂结构和性能的影响,结果表明:La的加入能够阻止催化剂中过硫酸根的分解,增强S和O之间的相互作用;少量的La不仅能增加催化剂的比表面积、酸强度和酸量,且能提高催化剂的活性和稳定性,当La的加载量为1%时,制得的催化剂活性最高,柠檬酸的转化率达到93.69%。这表明La的引入可提高固体超强酸催化剂的活性和稳定性,所制备的催化剂可用于传统催化剂浓硫酸的替代品,并有效降低设备的损耗,提高产品TBC的品质,优化TBC合成工艺,具有良好的经济价值。 展开更多
关键词 固体超强酸 s2o8^2-/Zro2-al2o3 柠檬酸三丁酯
下载PDF
S_2O_8^(2-)/ZrO_2-Al_2O_3-TiO_2固体超强酸的制备及催化活性研究 被引量:3
20
作者 王占领 《化学工程师》 CAS 2010年第9期13-15,共3页
本文采用单因素实验法,研究了固体超强酸催化剂S2O82-/ZrO2-Al2O3-TiO2的制备工艺。结果表明,S2O28-/ZrO2-Al2O3-TiO2的最佳制备条件为:n(Zr)∶n(Al)∶n(Ti)=1∶3∶1,(NH4)2S2O8浸渍液浓度0.5mo.lL-1,浸渍时间2h,焙烧温度300℃,焙烧时... 本文采用单因素实验法,研究了固体超强酸催化剂S2O82-/ZrO2-Al2O3-TiO2的制备工艺。结果表明,S2O28-/ZrO2-Al2O3-TiO2的最佳制备条件为:n(Zr)∶n(Al)∶n(Ti)=1∶3∶1,(NH4)2S2O8浸渍液浓度0.5mo.lL-1,浸渍时间2h,焙烧温度300℃,焙烧时间6h。此外,用红外光谱对固体酸进行了结构表征,以乙酸正丁酯的酯化反应对其酸催化活性进行了初步研究。 展开更多
关键词 s2o82-/Zro2-al2o3-Tio2固体超强酸 红外光谱 酯化反应
下载PDF
上一页 1 2 3 下一页 到第
使用帮助 返回顶部