Magnetic Properties and Workability of 6.5% Si Steel Sheet Manufactured by Siliconizing Process 被引量:2
1
作者 Koichiro Fujita, Misao Namikawa and Yoshikazu Takada (Materials and Processing Research Center NKK Corp., 1-1 Minamiwatarida-cho, Kawasaki-ku Kawasaki-shi, 210-0855 Japan) 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2000年第2期137-140,共4页
A siliconizing process to manufacture 6.5% Si steel sheet has been developed. Electric components, such as transformers and reactors are made easily from 6.5% Si steel sheet. However, improved workability is desirable... A siliconizing process to manufacture 6.5% Si steel sheet has been developed. Electric components, such as transformers and reactors are made easily from 6.5% Si steel sheet. However, improved workability is desirable to increase the applications. Therefore the improvement of workability of 6.5% Si steel sheet was investigated, and the results were obtained as follows: (a) workability of 6.5% Si steel sheet is deteriorated by grain boundary oxidization, (b) grain boundary oxidization can be restrained by the addition of C. Workability and magnetic properties of 6.5% Si steel sheet with C addition are discussed. Furthermore, it was found that the workability of high Si steel sheet was improved remarkably by varying the Si content gradient along the thickness without deterioration of high frequency magnetic properties. This newly developed magnetic gradient high Si steel sheet is also discussed. 展开更多
关键词 si steel sheet Manufactured by siliconizing Process Magnetic Properties and Workability of 6.5 St
下载PDF
Microstructure & texture evolution and magnetic properties of high magnetic-induction 6.5% Si electrical steel thin sheet fabricated by a specially designed rolling route
2
作者 李昊泽 刘海涛 +6 位作者 刘振宇 王项龙 骆忠汉 张凤泉 陈圣林 黄景文 王国栋 《Journal of Central South University》 SCIE EI CAS CSCD 2016年第3期523-528,共6页
Electrical steel sheets with 6.5%(mas fraction) Si with good shapes and superior magnetic inductions were successfully produced by a specially designed processing route including ingot casting, hot rolling and warm ro... Electrical steel sheets with 6.5%(mas fraction) Si with good shapes and superior magnetic inductions were successfully produced by a specially designed processing route including ingot casting, hot rolling and warm rolling both with interpass thermal treatment, and final annealing. The sheets were of 0.2 mm and 0.3 mm thick over 140 mm width. A detailed study of the microstructural and textural evolutions from the hot rolling to annealing was carried out by optical microscopy, X-ray diffraction and electron backscattered diffraction. The hot rolled sheet characterized by near-equiaxed grains was dominated by the mixture of <001>//ND fiber(λ-fiber), <110>//RD fiber(α-fiber) and <111>//ND fiber(γ-fiber) textures owing to the partial recrystallization and strain induced boundary migration(SIBM) during the hot rolling interpass thermal treatment. The static recovery and SIBM during the warm rolling interpass thermal treatment result in large and elongated warm rolling grains. The warm rolling texture is dominated by obvious λ, Goss and strong γ-fiber textures. The application of the interpass thermal treatment during hot and warm rolling significantly enhances the impact of SIBM during annealing, which is responsible for the formation of the moderate λ-fiber, some near-λ fiber texture components and the obviously weakened γ-fiber texture in the annealed sheet, leading to a higher magnetic induction compared to the commercially produced 6.5% Si steel by chemical vapor deposition(CVD). 展开更多
关键词 6.5% si electrical steel MICROSTRUCTURE texture magnetic property
下载PDF
粉末轧制法制备Fe-6.5%Si硅钢片的研究 被引量:19
3
作者 员文杰 沈强 张联盟 《粉末冶金技术》 EI CAS CSCD 北大核心 2007年第1期32-34,共3页
采用粉末轧制法制备了Fe-6.5%(质量分数)Si硅钢片,并对其密度、物相组成和磁性能进行了测试分析。研究表明:在一定的轧制成形和烧结条件下,所制备的Fe-6.5%Si硅钢片的饱和磁感应强度Bs为1.8T;高频铁损W2/10k为69W/kg。
关键词 粉末轧制 Fe-6.5%si 硅钢片 铁损 磁感应强度
下载PDF
Fe-6.5%Si硅钢片交流磁性能的研究 被引量:2
4
作者 员文杰 邓承继 +2 位作者 祝洪喜 沈强 张联盟 《武汉科技大学学报》 CAS 2010年第5期548-552,共5页
对分别采用粉末轧制法和化学气相沉积法制备的Fe-6.5%Si硅钢片在交流磁场(Bm=0.2~1.0 T,f=50~5 000 Hz)下的铁损、矫顽力和振幅磁导率进行了研究,采用幂函数对测试数据进行拟合,比较其交流磁性能随磁感应强度和频率的变化趋势。结果表... 对分别采用粉末轧制法和化学气相沉积法制备的Fe-6.5%Si硅钢片在交流磁场(Bm=0.2~1.0 T,f=50~5 000 Hz)下的铁损、矫顽力和振幅磁导率进行了研究,采用幂函数对测试数据进行拟合,比较其交流磁性能随磁感应强度和频率的变化趋势。结果表明,试样的矫顽力和铁损与磁感应强度的相关性均大于其与频率的相关性;Fe-6.5%Si硅钢片的交流磁化过程和性能与其本征特性密切相关;两类试样初始磁化过程的差异随着频率的提高而增大。 展开更多
关键词 Fe-6.5%si硅钢片 铁损 矫顽力 振幅磁导率
下载PDF
PCVD法制备Fe-6.5%Si高硅钢片的工艺研究 被引量:5
5
作者 周磊 潘应君 +2 位作者 徐超 彭骏松 张改璐 《表面技术》 EI CAS CSCD 北大核心 2013年第3期88-90,共3页
为制备Fe-6.5%Si高硅钢片,先利用PCVD技术在0.2 mm厚的纯铁片表面沉积硅,再进行高温扩散。通过正交实验分析了沉积硅的工艺参数对表层硅含量的影响,并研究了扩散参数对截面硅含量分布的影响。结果表明:以10%SiH4+90%Ar作为渗源气,在500... 为制备Fe-6.5%Si高硅钢片,先利用PCVD技术在0.2 mm厚的纯铁片表面沉积硅,再进行高温扩散。通过正交实验分析了沉积硅的工艺参数对表层硅含量的影响,并研究了扩散参数对截面硅含量分布的影响。结果表明:以10%SiH4+90%Ar作为渗源气,在500℃下沉积20 min,所得样品的表层硅含量高达40.5%;然后在工业纯氢气的保护下,于1050℃保温60 min,可获得满足要求的Fe-6.5%Si高硅钢片。 展开更多
关键词 PCVD 6 5%si硅钢片 渗硅 扩散处理
下载PDF
化学气相沉积法制备6.5%Si高硅钢的研究 被引量:2
6
作者 王爱华 刘畅 《新技术新工艺》 2011年第12期80-82,共3页
采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高... 采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 展开更多
关键词 化学气相沉积(CVD) 渗硅 6.5%si高硅钢片 磁性能
下载PDF
薄规格6.5%Si高硅钢片的激光切割技术研究
7
作者 刘念 陈子宏 +1 位作者 吕超 冯大军 《河北冶金》 2015年第7期34-37,共4页
针对薄规格6.5%Si高硅钢片脆性大,难加工的特点,采用激光切割的方法对其进行成型切割加工。专门设计了一套方便快速定位的夹具,摸索出适合高硅钢片的激光切割工艺参数和最佳的切割路径。试验结果表明,该方法能快速高效地切割出断面质量... 针对薄规格6.5%Si高硅钢片脆性大,难加工的特点,采用激光切割的方法对其进行成型切割加工。专门设计了一套方便快速定位的夹具,摸索出适合高硅钢片的激光切割工艺参数和最佳的切割路径。试验结果表明,该方法能快速高效地切割出断面质量好、尺寸精度高、满足使用要求的薄规格高硅钢片。 展开更多
关键词 6.5%si高硅钢 加工 激光切割
下载PDF
6.5%Si硅钢片制备技术的进展 被引量:14
8
作者 李慧 李运刚 梁精龙 《特殊钢》 北大核心 2008年第6期23-25,共3页
6.5%Si硅钢片具有良好的电磁性能,是实现电磁设备高效化、节能化、轻便化的理想材料。介绍了6.5%Si硅钢的研究历史,评述了冷轧轧制、快速凝固、薄膜生产工艺、CVD法、粉末轧制法、PCVD法和熔盐电沉积法等制备工艺,以及目前所做的研究工... 6.5%Si硅钢片具有良好的电磁性能,是实现电磁设备高效化、节能化、轻便化的理想材料。介绍了6.5%Si硅钢的研究历史,评述了冷轧轧制、快速凝固、薄膜生产工艺、CVD法、粉末轧制法、PCVD法和熔盐电沉积法等制备工艺,以及目前所做的研究工作,指出当前最重要的是研究开发经济高效的制备工艺。 展开更多
关键词 6.5%si 硅钢片 制备工艺
下载PDF
高硅电工钢超薄带冷轧过程中的织构演变 被引量:2
9
作者 柳金龙 沙玉辉 +1 位作者 邵光帅 左良 《东北大学学报(自然科学版)》 EI CAS CSCD 北大核心 2017年第5期645-649,654,共6页
采用轧制工艺制备了0.10 mm厚的6.5%Si高硅电工钢超薄带,并用X射线衍射技术对冷轧过程中的形变织构演变规律进行了研究,进而提出了分别有利于λ(<100>//ND,ND为轧面法线方向)和η(<100>//RD,RD为轧向)再结晶织构优化的形变... 采用轧制工艺制备了0.10 mm厚的6.5%Si高硅电工钢超薄带,并用X射线衍射技术对冷轧过程中的形变织构演变规律进行了研究,进而提出了分别有利于λ(<100>//ND,ND为轧面法线方向)和η(<100>//RD,RD为轧向)再结晶织构优化的形变织构控制方法.研究表明,50%~70%压下率有利于η再结晶织构优化,易于促进S=0.5层强η再结晶织构的形成.小于30%压下率和91%~97%压下率均有利于λ再结晶织构优化,其中30%的压下率更适合于二次冷轧法制备高硅钢超薄带时λ再结晶织构控制. 展开更多
关键词 Fe-6.5%si 高硅钢 薄带 冷轧 织构
下载PDF