The flow stress of spray formed 70Si30Al alloy was studied by hot compression on a Gleeble- 1500 test machine. The experimental results indicated that the flow stress depends on the strain rate and the deformation tem... The flow stress of spray formed 70Si30Al alloy was studied by hot compression on a Gleeble- 1500 test machine. The experimental results indicated that the flow stress depends on the strain rate and the deformation temperature. The flow stress increases with an increase in strain rate at a given deformation temperature. The flow stress decreases with the deformation temperature increasing at a given strain rate. The relational expression among the flow stress, the swain rate, and the deformation temperature satisfies the Arrhenius equation. The deformation activation energy of 70Si30Al alloy during hot deformation is 866.27 kJ/mol from the Arrhenius equation. 展开更多
关键词 70si30al alloy spray forming flow stress hot compression An'henius equation
下载PDF
Effect of P/M value on the preforms and microstructures of spray formed 70Si30Al alloy 被引量:2
2
作者 Yanguang Wei Baiqing Xiong Yongan Zhang Hongwei Liu Feng Wang Baohong Zhu 《Journal of University of Science and Technology Beijing》 CSCD 2007年第2期141-145,共5页
A novel 70Si30Al alloy was prepared by the spray forming process for electronic packaging materials. The effect of the ratio of atomization pressure to metal melt mass flux rate (P/M) on the preforms and microstruct... A novel 70Si30Al alloy was prepared by the spray forming process for electronic packaging materials. The effect of the ratio of atomization pressure to metal melt mass flux rate (P/M) on the preforms and microstructures of the spray-deposited 70Si30Al alloy was studied. The results indicate that the PIM value has a considerable influence on the formation of the preforms and the optimal value is in the range of 0.209-0.231 MPa/(kg.min^-1). The microstructure of the spray formed 70Si30AI alloy is fine and homogenous. The primary silicon phases distributing in the aluminum matrix evenly are fine and irregular. The aluminum matrix is divided into two groups: supersaturated α-Al phase or α-Al phase and Al-Si pseudoeutectic phase or Al-Si eutectic phase. 展开更多
关键词 70si30al alloy spray forming atomization pressure mass flux rate microstructure
下载PDF
Deformation mechanism of the spray formed 70Si30Al alloy during hot compression 被引量:1
3
作者 WEI Yanguang XIONG Baiqing ZHANG Yong'an LIU Hongwei WANG Feng ZHU Baohong 《Rare Metals》 SCIE EI CAS CSCD 2007年第1期56-61,共6页
The deformation mechanism of the spray formed 70Si30Al alloy was studied by hot compression on a Gleeble-1500 test machine. It is shown that hot deformation of the spray formed 70Si30Al alloy is achieved by liquid flo... The deformation mechanism of the spray formed 70Si30Al alloy was studied by hot compression on a Gleeble-1500 test machine. It is shown that hot deformation of the spray formed 70Si30Al alloy is achieved by liquid flow due to isostatic pressure and movement of solid particles due to shear force. Deformation condition depends on the nucleation rate and closure rate of the cavities. The flow stress slightly varies when the difference between the nucleation rate and closure rate of the cavities is small; however, it decreases when the nucleation rate of the cavities is greater than the closure rate of the cavities. 展开更多