Fluid Flow and Solidification Simulation in Beam Blank Continuous Casting Process With 3D Coupled Model 被引量:14
1
作者 YANG Jian-wei DU Yan-ping +1 位作者 SHI Rong CUI Xiao-chao 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2006年第4期17-21,共5页
Based on turbulent theory, a 3D coupled model of fluid flow and solidification was built using finite difference method and used to study the influence of superheating degree and casting speed on fluid flow and solidi... Based on turbulent theory, a 3D coupled model of fluid flow and solidification was built using finite difference method and used to study the influence of superheating degree and casting speed on fluid flow and solidification, analyze the interaction between shell and molten steel, and compare the temperature distribution under different technological conditions. The results indicate that high superheating degree can lengthen the liquid-core depth and make the crack and breakout possible, so suitable superheating should be controlled within 35℃ according to the simulation results. Casting speed which is one of the most important technological parameters of improving production rate, should be controlled between 0. 85 m/min and 1.05 m/min and the caster has great potential in the improvement of blank quality. 展开更多
关键词 beam blank continuous casting flow field temperature distribution coupled model SOLIDIFICATION
下载PDF
NUMERICAL SIMULATION OF THE THERMO-MECHANICAL PROCESS FOR BEAM BLANK CONTINUOUS CASTING 被引量:8
2
作者 W. Chen Y.Z. Zhang +4 位作者 C.J. Zhang L.G. Zhu B.X. Wang W.G. Lu J.H. Ma 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2007年第4期241-250,共10页
The aim of this study was to simulate the solidification process of beam blank continuous casting, and then find the reasons for the typical defects of the beam blank. A two-dimensional transient coupled finite elemen... The aim of this study was to simulate the solidification process of beam blank continuous casting, and then find the reasons for the typical defects of the beam blank. A two-dimensional transient coupled finite element model has been developed to compute the temperature and stress profile in beam blank continuous casting. The enthalpy method was used in the heat conduction equation. The thermo-mechanical property in the mushy zone was taken into consideration in this calculation. It is shown that at the mold exit the thickness of the shell had its maximum value at the flange tip and its minimum value at the fillet. The temperature had a great fluctuation on the surface of the beam blank in the secondary cooling zone. At the unbending point, the surface temperature of the web was in the brittleness temperature range under the present condition. To ensure the quality, it is necessary to weaken the intensity of secondary cooling. At the mold exit the equivalent stress and strain have higher values at the flange tip and at the web. From the spray 1 to the unbending point, the maximum values of stress and strain gradually moved to the internal section of the flange tip and the web. However, whenever, there were bigger stress and strain values near the flange tip and the web than in the other parts, it must be very easy to generate cracks at those positions. Now, online verification of this simulation has been developed, which has proved to be very useful and efficient to instruct the practical production of beam blank continuous casting. 展开更多
关键词 beam blank continuous basting thermo-mechanical process SIMULATION
下载PDF
EFFECT OF SUBMERGED ENTRY NOZZLE (SEN) PARAMETERS AND SHAPE ON 3-D FLUID FLOW IN MOULD FOR BEAM BLANK CONTINUOUS CASTING
3
作者 Y.P.Du J.W.Yang +1 位作者 R.Shi X.C.Cui 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2004年第5期705-712,共8页
According to turbulent theory and characteristics of beam blank continuous casting, 3-D model to represent the flow of beam blank mould is established. The predicted results indicate that the exit obliquity of up 15&#... According to turbulent theory and characteristics of beam blank continuous casting, 3-D model to represent the flow of beam blank mould is established. The predicted results indicate that the exit obliquity of up 15°(+15°) should be adopted, which will benefit the floatation of non-metallic inclusion and purification of the molten steel. When the nozzle angle is 120°, the flow pattern is reasonable. Proper nozzle depth can be 200mm. Turbulent kinetic of meniscus can be reduced by adopting the square nozzle and suitable area of side outlet when casting speed increases. The results are consistent with those of water model experiment, so the model is exact and reasonable. The model can provide important information for design of SEN and defining of immersion depth. 展开更多
关键词 SEN parameter SEN shape beam blank continuous casting 3-D flow distribution turbulent kinetic energy
下载PDF
Analysis of Thermal Behavior for Beam Blank Continuous Casting Mold 被引量:3
4
作者 XU Hai-lun WEN Guang-hua +2 位作者 SUN Wei WANG Kai-zhong YAN Bo 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2010年第12期17-22,共6页
Finite element models of steady heat conduction for cross section of beam blank mold were developed by using ABAQUS software. The effect of mold grinding thickness, cooling water velocity, diameter of restrietor rods ... Finite element models of steady heat conduction for cross section of beam blank mold were developed by using ABAQUS software. The effect of mold grinding thickness, cooling water velocity, diameter of restrietor rods and water channel design on hot face temperature was analyzed in detail. Attention was focused on the peak temperature and temperature uniformity along hot face. The results showed that the peak temperature of existing mold, about 337.2 ℃, is located in the fillet, and two valleys of hot face temperature are found in flange corner and junction of wide face and narrow face, respectively. Decreasing mold thickness, increasing cooling water velocity and increasing diameter of restrictor rods can all reduce peak temperature and improve temperature uniformity along hot race at the expense of lower overall temperature. Redesigning the water channel can decrease peak temperature and thermal gradient of mold without lowering overall temperature of hot face. In particular, the small hole design can improve temperature uniformity across hot face and obtain the best advantage. 展开更多
关键词 beam blank continuous casting mold thermal behavior temperature distribution
原文传递
基于异形坯钢种低成本脱氧的实践与研究
5
作者 冯振亮 孙丰硕 +2 位作者 李宗一 姜成 安中超 《南方金属》 CAS 2024年第1期36-39,共4页
基于现场实际生产模型,结合工业工程手法,对异形坯生产过程中的脱氧剂进行研究。发现生产过程中降低出钢氧,同时调整脱氧剂结构,能够有效降低脱氧剂成本,实现低成本脱氧的目的。
关键词 异形坯 低成本 脱氧
下载PDF
重型异形坯铸坯表面横裂纹的成因分析与控制
6
作者 胡林梅 沈昶 王猛 《冶金动力》 2024年第1期86-89,共4页
针对国内某钢厂生产Q355级和Q420级异形坯低合金钢时产生铸坯表面横裂纹的现状,解析了连铸坯翼缘顶端横裂纹产生的机理和主要影响因素之间的对应关系,以降低重型异形坯铸坯横裂纹的发生率。研究结果表明铸坯表面横裂纹沿粗大的奥氏体晶... 针对国内某钢厂生产Q355级和Q420级异形坯低合金钢时产生铸坯表面横裂纹的现状,解析了连铸坯翼缘顶端横裂纹产生的机理和主要影响因素之间的对应关系,以降低重型异形坯铸坯横裂纹的发生率。研究结果表明铸坯表面横裂纹沿粗大的奥氏体晶粒开裂,Q355级钢低塑性区的温度范围为600~620℃和740~920℃,Q420级钢低塑性区的温度范围为600~950℃,通过提高铸机拉速、降低冷却水强度、降低钢种铝含量等工艺措施能有效控制重型异形坯铸坯翼缘表面横裂纹的产生。 展开更多
关键词 重异连铸坯 翼缘顶端 横裂纹
下载PDF
异型坯连铸机断面改造与生产实践
7
作者 吴旭鹏 高志滨 +2 位作者 侯光达 刘文凭 刘忠建 《山东冶金》 CAS 2024年第5期8-10,共3页
为适应异型坯的市场增长需求,在异型坯连铸机原有BB1断面尺寸555 mm×440 mm×90 mm基础上,升级改造为575 mm×450 mm×110 mm。通过对结晶器、扇形段、引锭杆、拉矫机等设备的升级改造和工艺参数的优化,成功进行了连... 为适应异型坯的市场增长需求,在异型坯连铸机原有BB1断面尺寸555 mm×440 mm×90 mm基础上,升级改造为575 mm×450 mm×110 mm。通过对结晶器、扇形段、引锭杆、拉矫机等设备的升级改造和工艺参数的优化,成功进行了连铸机正常生产,跟踪铸坯轧材质量及性能均满足现场使用需求,提高了整个工序的生产能力。 展开更多
关键词 异型坯 连铸机 断面 结晶器
下载PDF
异型坯连铸机黏结漏钢的原因分析及控制措施
8
作者 吴旭鹏 侯光达 +2 位作者 高志滨 刘文凭 刘忠建 《山东冶金》 CAS 2024年第4期24-26,共3页
对异型坯连铸机黏结漏钢的原因进行了分析,导致异型坯黏结的主要原因与保护渣的理化性能、钢种、异常操作、浸入式水口偏斜、钢水温度、结晶器液面波动、结晶器铜板使用寿命等方面有关。在这些方面制定了相关控制措施,有效降低了连铸机... 对异型坯连铸机黏结漏钢的原因进行了分析,导致异型坯黏结的主要原因与保护渣的理化性能、钢种、异常操作、浸入式水口偏斜、钢水温度、结晶器液面波动、结晶器铜板使用寿命等方面有关。在这些方面制定了相关控制措施,有效降低了连铸机黏结漏钢概率。 展开更多
关键词 异型坯连铸机 保护渣 漏钢事故 结晶器
下载PDF
铌微合金化异形坯翼缘横裂纹成因分析
9
作者 王猛 胡春林 +1 位作者 吴坚 杨应东 《安徽冶金科技职业学院学报》 2024年第3期7-8,14,共3页
针对铌微合金化异形坯表面横裂纹在翼缘顶端和翼缘内侧发生率较高的问题,通过对异形坯的夹杂物、高温热塑性、表面温度分布、等效应力进行系统研究,揭示了异形坯铌微合金化钢在翼缘顶端和翼缘内侧的横裂纹的产生原因。通过优化工艺和提... 针对铌微合金化异形坯表面横裂纹在翼缘顶端和翼缘内侧发生率较高的问题,通过对异形坯的夹杂物、高温热塑性、表面温度分布、等效应力进行系统研究,揭示了异形坯铌微合金化钢在翼缘顶端和翼缘内侧的横裂纹的产生原因。通过优化工艺和提高设备精度,有效地控制了异形坯横裂纹的产生,异形坯轧后裂纹修磨率下降了13%。 展开更多
关键词 异形坯 表面横裂纹 高温热塑性 应力集中
下载PDF
单水口浇注Q420NQR1异型坯表面纵裂纹控制
10
作者 张凯 彭治强 +4 位作者 卢雄慧 赵宏志 崔弘 侯自兵 唐萍 《包钢科技》 2023年第6期7-12,共6页
针对亚包晶钢Q420NQR1连铸坯及轧材的表面纵裂纹缺陷分析了纵裂纹成因并提出了控制措施。结果表明,轧材的纵裂纹缺陷源于铸坯表面纵裂纹,铸坯表面纵裂纹绝大部分位于异型坯远离水口位置的腹板。通过物理模拟对结晶器内部流场进行研究,... 针对亚包晶钢Q420NQR1连铸坯及轧材的表面纵裂纹缺陷分析了纵裂纹成因并提出了控制措施。结果表明,轧材的纵裂纹缺陷源于铸坯表面纵裂纹,铸坯表面纵裂纹绝大部分位于异型坯远离水口位置的腹板。通过物理模拟对结晶器内部流场进行研究,发现结晶器内腹板位置存在单循环流,这直接导致远离水口位置的保护渣液渣层较薄,在该位置下难以实现有效控热。通过适当增加水口插入深度可以降低钢液表面流速并促进液渣均匀分布;同时结合保护渣非均匀布料方式可有效改善铸坯及轧材质量,铸坯及轧材纵裂纹率分别降低30%和34%。 展开更多
关键词 Q420NQR1异型坯 纵裂纹 物理模拟 插入深度 非均匀布料
下载PDF
连铸异形坯结晶器开口度检测解决方案
11
作者 孟强 闫炯 孙胜勇 《包头职业技术学院学报》 2023年第4期63-66,共4页
结晶器是炼钢厂连铸生产过程中的核心设备,又称连铸机的“心脏”主要作用是把液态钢水快速、连续不断地凝固。结晶器的工作性能直接影响铸坯的质量、生产效率、安全生产等方面,其中结晶器的锥度参数是影响其性能最重要的指标。本文针对... 结晶器是炼钢厂连铸生产过程中的核心设备,又称连铸机的“心脏”主要作用是把液态钢水快速、连续不断地凝固。结晶器的工作性能直接影响铸坯的质量、生产效率、安全生产等方面,其中结晶器的锥度参数是影响其性能最重要的指标。本文针对异形坯结晶器在实际生产过程中关键尺寸参数检测较困难或精度不高的情况,提出合理化解决方案,对企业安全生产、提高生产效率、保证产品质量、提高经济效益具有重要的指导意义。 展开更多
关键词 异形坯 开口度 结构设计 变形
下载PDF
窄断面异型坯工艺参数分析及改进研究
12
作者 贾敬伟 杨鹏辉 毛伟龙 《山西冶金》 CAS 2023年第10期66-69,共4页
根据异型坯窄断面和宽断面生产实践中表面质量差异对比,结合两个断面结晶器流场和温度场耦合数值模拟和连铸坯凝固特性、异型坯应力分析,深入分析不同工艺参数下窄断面异型坯结晶器流场和温度场情况,为后续异型坯表面质量控制指导方向。
关键词 异型坯 裂纹 流场 温度场 分析
下载PDF
日钢异型坯结晶器液面波动机理分析
13
作者 毛伟龙 杨鹏辉 贾敬伟 《山西冶金》 CAS 2023年第9期249-251,共3页
针对日钢异型坯出现的结晶器液面波动问题,研究其产生机理并进行了系统地理论分析。通过一系列的试验调整和效果跟踪,最终实现对结晶器液面的稳定控制,解决异型坯拉速再提升的瓶颈问题。
关键词 异型坯 结晶器液面 波动 拉速
下载PDF
异形坯连铸过程流场与温度场耦合三维数值模拟 被引量:12
14
作者 杨建伟 杜艳平 +2 位作者 崔小朝 史荣 刘才 《金属学报》 SCIE EI CAS CSCD 北大核心 2001年第7期767-771,共5页
建立了异形坯内流体流动与凝固传热的三维耦合模型,充分考虑了对流换热对凝固过程的影响,分析了铸坯与钢液之间的相互作用,并对不同工艺条件下的温度场进行了比较.运用此模型可预报铸坯的温度场、坯壳厚度及液芯长度等,便于现场调... 建立了异形坯内流体流动与凝固传热的三维耦合模型,充分考虑了对流换热对凝固过程的影响,分析了铸坯与钢液之间的相互作用,并对不同工艺条件下的温度场进行了比较.运用此模型可预报铸坯的温度场、坯壳厚度及液芯长度等,便于现场调整工艺参数. 展开更多
关键词 异形坯连铸 数值模拟 流场 温度场 耦合
下载PDF
异型坯结晶器与铸坯热力耦合数值模拟 被引量:9
15
作者 罗伟 严波 +2 位作者 熊跃兴 文光华 徐海伦 《材料科学与工艺》 EI CAS CSCD 北大核心 2012年第1期31-37,43,共8页
为研究异型坯连铸结晶器内铸坯凝固和变形过程,采用ABAQUS软件建立了异型坯连铸结晶器和铸坯的二维瞬态热力耦合有限元模型,编制ABAQUS用户自定义子程序GAPCON实现结晶器内壁和铸坯之间的传热模拟.计算模型中考虑了铸坯的凝固和热变形... 为研究异型坯连铸结晶器内铸坯凝固和变形过程,采用ABAQUS软件建立了异型坯连铸结晶器和铸坯的二维瞬态热力耦合有限元模型,编制ABAQUS用户自定义子程序GAPCON实现结晶器内壁和铸坯之间的传热模拟.计算模型中考虑了铸坯的凝固和热变形、气隙对传热的影响以及铸坯与结晶器之间的接触应力.分别对2种不同水缝设计结晶器进行了数值模拟,数值分析结果表明,小孔水缝设计的结晶器温度峰值较低、热面温度分布更均匀,因而比大孔水缝设计结晶器具有更长的使用寿命和更优的铸坯质量,这一结论与现场试验结果一致. 展开更多
关键词 异型坯 结晶器 热力耦合 水缝 有限元方法
下载PDF
近终形连铸异型坯的质量问题及对策 被引量:13
16
作者 茆勇 鲁怀敏 汪开忠 《钢铁》 CAS CSCD 北大核心 2001年第6期21-23,9,共4页
连铸异型坯质量的波动直接影响到 H型钢实物质量。结合出口美国 H型钢 (MA34 5 )的生产 ,对影响连铸异型坯质量的工艺和设备因素进行了分析总结 。
关键词 异型坯 连铸 H型钢 近终形连铸 表面质量
下载PDF
异形坯连铸结晶器内三维流场的数值模拟 被引量:6
17
作者 杨建伟 杜艳平 +2 位作者 史荣 崔小朝 刘才 《中国有色金属学报》 EI CAS CSCD 北大核心 2001年第z2期248-252,共5页
根据湍流理论及异形坯连铸的特点 ,建立了异形坯结晶器三维流场数学模型 ,对不同条件下的流场进行了数值模拟 ,分析了水口结构和工艺参数变化时异形坯结晶器内涡心深度的变化规律及液面湍动能的分布状态。结果表明 :采用上倾式水口 ,水... 根据湍流理论及异形坯连铸的特点 ,建立了异形坯结晶器三维流场数学模型 ,对不同条件下的流场进行了数值模拟 ,分析了水口结构和工艺参数变化时异形坯结晶器内涡心深度的变化规律及液面湍动能的分布状态。结果表明 :采用上倾式水口 ,水口夹角为 12 0°,拉速为 0 .9m/s时 ,结晶器内流场分布较为合理 ,液面较稳定。模拟结果与水模实验结果吻合较好。该模型可对连铸过程进行离线分析 ,确定最佳参数 ,并可作为在线控制模型的基础。 展开更多
关键词 异形坯连铸 结晶器 湍动能 涡心深度
下载PDF
连铸工字形异型坯腹板中心裂纹研究 被引量:7
18
作者 汤寅波 汪开忠 杜松林 《钢铁》 CAS CSCD 北大核心 2003年第10期19-20,34,共3页
通过现场调研和工艺参数统计 ,分析了 Mn/ S、S、P、拉速、连铸二冷设备等对异型坯腹板中心裂纹的影响 。
关键词 异型坯 连铸 中心裂纹 工艺参数 拉速 二冷设备
下载PDF
异型坯连铸液固温耦合计算机仿真 被引量:5
19
作者 杜艳平 史荣 +2 位作者 杜建新 刘才 崔小朝 《矿冶工程》 CAS CSCD 北大核心 2000年第4期75-77,共3页
在建立连铸过程液固温耦合分析数学模型的基础上 ,开发了异型坯液固区的流场、温度场及鼓肚变形耦合分析软件 ,为异型坯连铸生产过程工艺参数设定与优化提供了理论依据。
关键词 异型坯连铸 计算机模拟 固液耦合 钢液流动
下载PDF
异型坯连铸结晶器内流场 被引量:11
20
作者 周俐 沈昶 王建军 《北京科技大学学报》 EI CAS CSCD 北大核心 2000年第5期431-434,共4页
经过数模和水模研究得到:影响异型坯结晶器内流场,结晶器腹板处上、下回流区的大小及结晶器液面波动的因素有:水口开孔的夹角、水口的出口倾角、铸坯拉速及水口浸入深度.在工作拉速时,采用120°夹角、出口倾角为9°、浸入... 经过数模和水模研究得到:影响异型坯结晶器内流场,结晶器腹板处上、下回流区的大小及结晶器液面波动的因素有:水口开孔的夹角、水口的出口倾角、铸坯拉速及水口浸入深度.在工作拉速时,采用120°夹角、出口倾角为9°、浸入深度为75mm(换算到原型为150mm)的水口,结晶器内的流体的流动状态较为合理. 展开更多
关键词 异型坯结晶器 流场 连续铸钢