Li元素对Bi_(0.5)Na_(0.5)TiO_3基无铅压电陶瓷压电性能的影响
1
作者 答元 白岗 《西安工业大学学报》 CAS 2009年第5期417-420,共4页
针对无铅压电陶瓷的压电常数d33偏小的情况,采用传统的固相反应烧结方法制备得到了高压电性能的Bi0.5Na0.5TiO3基无铅压电陶瓷Bi0.5(Na0.7K0.3-xLix)0.5TiO3(x=0.04,0.08,0.12,0.16,0.20).研究了Li元素的添加量对陶瓷的烧结温度以及压... 针对无铅压电陶瓷的压电常数d33偏小的情况,采用传统的固相反应烧结方法制备得到了高压电性能的Bi0.5Na0.5TiO3基无铅压电陶瓷Bi0.5(Na0.7K0.3-xLix)0.5TiO3(x=0.04,0.08,0.12,0.16,0.20).研究了Li元素的添加量对陶瓷的烧结温度以及压电性能的影响.研究结果表明,Li元素对K的替代可以降低陶瓷的烧结温度,提高样品致密度,适量的Li可以大幅度提高陶瓷的压电性能.陶瓷样品的压电常数d33和平面机电耦合系数kp随着Li含量的增加先增大后减小.在1 090℃的烧结温度下,Li含量x=0.08时的陶瓷样品表现出最佳的压电性能,压电常数d33=212 pC/N,平面机电耦合系数kp=33%. 展开更多
关键词 无铅 压电陶瓷 bi0.5(na0.7k0.3-xlix)0.5tio3 烧结温度 压电性能
下载PDF
脉冲激光沉积Bi0.5(Na0.7K0.1Li0.2)0.5TiO3无铅压电薄膜的研究 被引量:1
2
作者 陆雷 肖定全 +2 位作者 赁敦敏 张永彬 朱建国 《功能材料》 EI CAS CSCD 北大核心 2008年第6期915-918,共4页
采用脉冲激光沉积制备了新型无铅压电Bi0.5(Na0.7K0.1Li0.2)0.5TiO3陶瓷薄膜,分别利用X射线衍射仪、X射线光电子谱、俄歇电子能谱、原子力显微镜及扫描电镜研究了该薄膜的晶体结构、组成成分及表面形貌。结果表明,薄膜基体温度和工作气... 采用脉冲激光沉积制备了新型无铅压电Bi0.5(Na0.7K0.1Li0.2)0.5TiO3陶瓷薄膜,分别利用X射线衍射仪、X射线光电子谱、俄歇电子能谱、原子力显微镜及扫描电镜研究了该薄膜的晶体结构、组成成分及表面形貌。结果表明,薄膜基体温度和工作气压对所生长的薄膜影响较大;在SiO2/Si基片上制备Bi0.5(Na0.7K0.1Li0.2)0.5TiO3薄膜的最佳温度和氧气压力分别为600℃和13Pa;利用脉冲激光沉积的薄膜具有精细的表面结构。 展开更多
关键词 脉冲激光沉积 bi0.5(na0.7k0.1Li0.2)0.5tio3 薄膜
下载PDF
P-E hysteresis loop going slim in Ba0.3Sr0.7TiO3-modified Bi0.5Na0.5TiO3 ceramics for energy storage applications 被引量:13
3
作者 Dongxu LI Zong-Yang SHEN +5 位作者 Zhipeng LI Wenqin LUO Xingcai WANG Zhumei WANG Fusheng SONG Yueming LI 《Journal of Advanced Ceramics》 SCIE CSCD 2020年第2期183-192,共10页
(Ba0.3Sr0.7)x(Bi0.5Na0.5)1-xTiO3(BSxBNT,x=0.3–V0.8)ceramics were prepared to investigate their structure,dielectric and ferroelectric properties.BSxBNT ceramics possess pure perovskite structure accompanied from a te... (Ba0.3Sr0.7)x(Bi0.5Na0.5)1-xTiO3(BSxBNT,x=0.3–V0.8)ceramics were prepared to investigate their structure,dielectric and ferroelectric properties.BSxBNT ceramics possess pure perovskite structure accompanied from a tetragonal symmetry to pseudo-cubic one with the increase of x value,being confirmed by X-ray diffraction(XRD)and Raman results.The Tm corresponding to a temperature in the vicinity of maximum dielectric constant gradually decreases from 110℃(x=0.3)to-45℃(x=0.8),across Tm=36℃(x=0.5)with a maximum dielectric constant(ɛr=5920@1 kHz)around room temperature.The saturated polarization Ps gradually while the remnant polarization Pr sharply decreases with the increase of x value,making the P-E hysteresis loop of BSxBNT ceramics goes slim.A maximum difference between Ps and Pr(Ps-Pr)is obtained for BSxBNT ceramics with x=0.5,at which a high recoverable energy density(Wrec=1.04 J/cm3)is achieved under an applied electric field of 100 kV/cm with an efficiency ofη=77%.Meanwhile,the varied temperature P-E loops,fatigue measurements,and electric breakdown characteristics for the sample with x=0.5 indicate that it is promising for pulsed power energy storage capacitor candidate materials. 展开更多
关键词 energy storage ceramics Ba0.3Sr0.7tio3(BST) bi0.5na0.5tio3(BNT) relaxor ferroelectrics pulsed power capacitor
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部