INFLUENCE OF MnO ON REDUCTION OF TiO_2 IN BLAST FURNACE TYPE SLAG
1
作者 DU Hegui ZOU Anhua, Northeast University of Technology, Shenyang, China Du Hegui, Professor, Department of Ferrous Metallurgy, Northeast University of Technology, Shenyang 110006, China 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1992年第7期1-7,共7页
A study was carried out on the formation of Ti(C,N) during smelting vanadium-bearing titanomagnetite in blast furnace and the influence of MnO content on reduction of TiO_2 in the slag containing high titania. The red... A study was carried out on the formation of Ti(C,N) during smelting vanadium-bearing titanomagnetite in blast furnace and the influence of MnO content on reduction of TiO_2 in the slag containing high titania. The reduction of TiO_2 is restricted by MnOpredominantly at the slag-metal interface and no more at the slag-coke one. The formation of Ti(C,N) is remarkably restricted by MnO in the slag when the MnO content is about 4% and the basicity from 0.6 to 1.2 in the slag. MnO may also retards the reduction of SiO_2 and accelerates the desulphidation under certain condition. 展开更多
关键词 blast furnace smelting TiO_2 REDUCTION SLAG MNO
下载PDF
Effect of Coke Reaction Index on Reduction and Permeability of Ore Layer in Blast Furnace Lumpy Zone Under Non-Isothermal Condition 被引量:4
2
作者 ZHAO Hong-bo BAI Yong-qiang CHENG Shu-sen 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2013年第4期6-10,共5页
Reasonable control on CRI(coke reaction index)is one of the key factors for BF(blast furnace)low-carbon smelting.However,there are contrary opinions.One is increasing CRI to improve reaction efficiency in BF and t... Reasonable control on CRI(coke reaction index)is one of the key factors for BF(blast furnace)low-carbon smelting.However,there are contrary opinions.One is increasing CRI to improve reaction efficiency in BF and the other is decreasing CRI to suppress coke degradation in furnace.Different methods are adopted to realize effective catalysis(increasing CRI)and passivation(decreasing CRI)of coke.Simulation tests of coke in BF lumpy zone under gradual temperature rising have been done.Effect of CRI on gas composition,ore reduction,burden column permeability and heat reserve zone′s temperature under non-isothermal condition are studied.Then combined with iron making calculations,a novel BF operation suggestion is proposed as coke nut with small size be catalyzed and mixed with ore while skeletal coke with large size be passivated and separately charged into BF. 展开更多
关键词 blast furnace low carbon smelting resistance loss coke reaction index
原文传递
Development of Intensified Technologies of Vanadium-Bearing Titanomagnetite Smelting 被引量:28
3
作者 FU Wei-guo WEN Yong-cai XIE Hong-en 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2011年第4期7-10,18,共5页
It was very difficult for the smelting of vanadium-bearing titanomagnetite by blast furnace because the content of TiO2 of blast furnace slag could amount to 20%-25%.After long term development and continuous improvem... It was very difficult for the smelting of vanadium-bearing titanomagnetite by blast furnace because the content of TiO2 of blast furnace slag could amount to 20%-25%.After long term development and continuous improvement,special intensified smelting technologies for vanadium-bearing titanomagnetite by blast furnace were obtained and improved gradually.With the improvement of beneficiated material level and equipment level,smelting intensity has been increased gradually and the highest comprehensive smelting intensity reached 1.45 t/(m3·d).Technical-economic indexes of blast furnace have also been increased remarkably.The highest utilization coefficient exceeded 2.7 t/(m3·d)on the condition that the burden grade was only about 50%. 展开更多
关键词 vanadium-bearing titanomagnetite blast furnace smelting intensified technology