In this paper the critical cooling rate, Rc, for the glass formation of Fe80P13C7 alloy has been determined using both Uhlmann's and Barandiaran-Colmenero's method. In Uhlmann's method, all kinds of the expres-sion...In this paper the critical cooling rate, Rc, for the glass formation of Fe80P13C7 alloy has been determined using both Uhlmann's and Barandiaran-Colmenero's method. In Uhlmann's method, all kinds of the expres-sions of △G^l-s (T) and η/(T) determined using the different modes and methods had been investigated. It is indicated that the Rc for the glass formation of FesoP13C7 alloy can be estimated to be 349 K/s by Uhlmann's method based on the appropriate expressions of △G^l-s(T) and η/(T). The calculated result accords with our experimental result. The Rc for the glass formation of Fe80P13C7 alloy has also been determined to be 0.49 K/s using Barandiaran-Colmenero's method. This resultant Rc is unreasonable low and it indicates that Barandiaran-Colmenero's method does not suit to Fe-based alloy.展开更多
基金supported by the National Natural Science Foundation of China (No. 50861007)the Project of Supporting Xinjiang Uyghur Autonomous Region by Science and Technology (No. 201191203)the Opening Subject from State Key Laboratory of Powder Metallurgy in Central South University
文摘In this paper the critical cooling rate, Rc, for the glass formation of Fe80P13C7 alloy has been determined using both Uhlmann's and Barandiaran-Colmenero's method. In Uhlmann's method, all kinds of the expres-sions of △G^l-s (T) and η/(T) determined using the different modes and methods had been investigated. It is indicated that the Rc for the glass formation of FesoP13C7 alloy can be estimated to be 349 K/s by Uhlmann's method based on the appropriate expressions of △G^l-s(T) and η/(T). The calculated result accords with our experimental result. The Rc for the glass formation of Fe80P13C7 alloy has also been determined to be 0.49 K/s using Barandiaran-Colmenero's method. This resultant Rc is unreasonable low and it indicates that Barandiaran-Colmenero's method does not suit to Fe-based alloy.