Microstructure and mechanical properties of cast Mg-15Al-xNd alloy by permanent mold 被引量:2
1
作者 Zhou Kangkang Wang Hongxia +2 位作者 Liang Wei Zhang Jinshan Zhang Hongxia 《China Foundry》 SCIE CAS 2013年第5期315-320,共6页
To improve the comprehensive mechanical properties of Mg-15Al magnesium alloy,different amounts(from 0 to 4.0wt.%)of Nd were added to the alloy and six Mg-15Al-xNd alloys were prepared by metal mould casting.The effec... To improve the comprehensive mechanical properties of Mg-15Al magnesium alloy,different amounts(from 0 to 4.0wt.%)of Nd were added to the alloy and six Mg-15Al-xNd alloys were prepared by metal mould casting.The effect of Nd content on microstructure of the alloys was investigated by means of OM,SEM,EDS,TEM,and XRD.The tensile properties were tested at room temperature(RT)and high temperature(473 K).The results indicate that the primaryα-Mg dendrite is significantly refined with the addition of Nd.The best refinement is reached at 1.0wt.%Nd content and the average dendrite arm spacing decreases from 80-100μm(without Nd addition)to^20μm.A further increase in Nd content leads to the coarsening of the primaryα-Mg dendrite.The addition of Nd improves the tensile properties of Mg-15Al both at RT and 473 K.The Mg-15Al alloy containing 1.0wt.%Nd exhibits the best tensile properties.Compared with the alloy without Nd,the yield and ultimate tensile strength of the Mg-15Al-1.0Nd alloy at RT increase from 132.3 to 148.6 MPa and 152.3 to 189.6MPa,increase by 12.3%and 24.5%,respectively;and the elongation at RT increases from 0.05%to 1.24%.The yield and tensile strength of the alloy at 473 K increase from 97.9 to 115.3 MPa and 121.6 to 140.1 MPa,increase by 15.2%and 20%,respectively.Further increment of Nd content to 1.5wt.%degrades the tensile properties,which is ascribed to grain coarsening and growth of the Al-Nd phase. 展开更多
关键词 mg-15al magnesium alloy MICROSTRUCTURE mechanical properties
下载PDF
Mg-(6~8)A1-0.7Si合金的组织和力学性能分析 被引量:3
2
作者 白亮 潘复生 杨明波 《重庆大学学报(自然科学版)》 EI CAS CSCD 北大核心 2006年第10期96-99,共4页
通过金相观察、扫描电镜、X衍射分析和拉伸实验等方法,研究了Mg-(6~8)Al-0.7Si合金的铸态组织和力学性能.研究结果表明:添加了少量Sb和RE的Mg-(6~8)Al-0.7%Si的铸态组织主要由α—Mg基体、Mg17Al12相、Mg2Si相、Mg3Sb2相和... 通过金相观察、扫描电镜、X衍射分析和拉伸实验等方法,研究了Mg-(6~8)Al-0.7Si合金的铸态组织和力学性能.研究结果表明:添加了少量Sb和RE的Mg-(6~8)Al-0.7%Si的铸态组织主要由α—Mg基体、Mg17Al12相、Mg2Si相、Mg3Sb2相和少量针状Al4Si2Mn2Y相组成,并且随着Al含量的增加,试验合金组织中的Mg17Al12相增多,共晶析出物变得更加连续.同时,力学性能的测试结果表明:Al含量变化对于试验合金抗拉强度、屈服强度和延伸率的影响呈现出不同的变化规律. 展开更多