Application of Vacuum Drying to Silica Sol Ceramic Mold 被引量:1
1
作者 Ming ZENG Xinqiang YUAN +1 位作者 Baoluo SHEN Yunqiu ZHENG 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2008年第2期233-235,共3页
Silica sol ceramic mold was made at room temperature with JN-30 silica sol, silica powder and NH4Cl. It is found that the harden time of silica sol ceramic mold is only 0.5 to 1.5 h under the amount of NH4Cl solution ... Silica sol ceramic mold was made at room temperature with JN-30 silica sol, silica powder and NH4Cl. It is found that the harden time of silica sol ceramic mold is only 0.5 to 1.5 h under the amount of NH4Cl solution of 7% to 8% with 15% concentration, and less surface cracks occur by using vacuum drying. The proper vacuum drying process parameters: vacuum drying temperature is 80 to 100℃, drying time is 5 h and vacuum is 0.06 to 0.07MPa. The harden mechanics, vacuum drying mechanics and the reason of less surface cracks of silica sol ceramic mold by vacuum drying: were also analyzed in this paper. 展开更多
关键词 Silica sol Ceramic mold Vacuum drying nh4cl solution
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部