Mg处理Nb-Ti微合金钢中非金属夹杂物演变机理研究
1
作者 朱吴杰 王德永 +2 位作者 孙群 温荣宇 屈天鹏 《炼钢》 CAS 北大核心 2024年第4期40-51,共12页
在工业生产条件下,对Nb-Ti微合金钢进行Mg处理试验,分析了Mg处理条件下,微合金钢中非金属夹杂物的演变规律。结果表明,微合金钢经过铝脱氧产物主要为Al_(2)O_(3)夹杂,进行Ca处理后,Al_(2)O_(3)夹杂减少,转变为CaO-Al_(2)O_(3)夹杂,且部... 在工业生产条件下,对Nb-Ti微合金钢进行Mg处理试验,分析了Mg处理条件下,微合金钢中非金属夹杂物的演变规律。结果表明,微合金钢经过铝脱氧产物主要为Al_(2)O_(3)夹杂,进行Ca处理后,Al_(2)O_(3)夹杂减少,转变为CaO-Al_(2)O_(3)夹杂,且部分MnS夹杂转变为CaS夹杂;精炼阶段将Ca处理改为Mg处理后,可将铝脱氧产物Al_(2)O_(3)夹杂变性为MgO-Al_(2)O_(3)夹杂。Mg处理前,夹杂物在LF主要是Al_(2)O_(3)夹杂,进行Mg处理和Ti合金化后,钢中主要夹杂物变为MgO-Al_(2)O_(3)夹杂、MgO夹杂和TiN夹杂,最终在铸坯中的夹杂物为MgO-Al_(2)O_(3)外包裹CaS/MnS和(Nb、Ti)N复合夹杂。对Ca处理和Mg处理的夹杂物尺寸进行对比,夹杂物尺寸主要分布在5μm以内,Mg处理形成的2μm以内的夹杂物占比高于Ca处理工艺,表明镁处理可以较好地细化夹杂物,形成大量弥散分布的细小夹杂,有助于提升钢的综合力学性能。 展开更多
关键词 Mg处理 nb-ti微合金钢 非金属夹杂物 热力学分析
下载PDF
Review of Sc microalloying effects in Al-Cu alloys
2
作者 Shenghua Wu Chong Yang +7 位作者 Peng Zhang Hang Xue Yihan Gao Yuqing Wang Ruihong Wang Jinyu Zhang Gang Liu Jun Sun 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第5期1098-1114,共17页
Artificially controlling the solid-state precipitation in aluminum (Al) alloys is an efficient way to achieve well-performed properties,and the microalloying strategy is the most frequently adopted method for such a p... Artificially controlling the solid-state precipitation in aluminum (Al) alloys is an efficient way to achieve well-performed properties,and the microalloying strategy is the most frequently adopted method for such a purpose.In this paper,recent advances in lengthscale-dependent scandium (Sc) microalloying effects in Al-Cu model alloys are reviewed.In coarse-grained Al-Cu alloys,the Sc-aided Cu/Sc/vacancies complexes that act as heterogeneous nuclei and Sc segregation at the θ′-Al_(2)Cu/matrix interface that reduces interfacial energy contribute significantly to θ′precipitation.By grain size refinement to the fine/ultrafine-grained scale,the strongly bonded Cu/Sc/vacancies complexes inhibit Cu and vacancy diffusing toward grain boundaries,promoting the desired intragranular θ′precipitation.At nanocrystalline scale,the applied high strain producing high-density vacancies results in the formation of a large quantity of (Cu Sc,vacancy)-rich atomic complexes with high thermal stability,outstandingly improving the strength/ductility synergy and preventing the intractable low-temperature precipitation.This review recommends the use of microalloying technology to modify the precipitation behaviors toward better combined mechanical properties and thermal stability in Al alloys. 展开更多
关键词 aluminum alloy microalloying effect length-scale dependence PRECIPITATION mechanical properties
下载PDF
Development in oxide metallurgy for improving the weldability of high -strength low-alloy steel-Combined deoxidizers and microalloying elements
3
作者 Tingting Li Jian Yang 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第6期1263-1284,共22页
The mechanisms of oxide metallurgy include inducing the formation of intragranular acicular ferrite(IAF)using micron-sized inclusions and restricting the growth of prior austenite grains(PAGs)by nanosized particles du... The mechanisms of oxide metallurgy include inducing the formation of intragranular acicular ferrite(IAF)using micron-sized inclusions and restricting the growth of prior austenite grains(PAGs)by nanosized particles during welding.The chaotically oriented IAF and refined PAGs inhibit crack initiation and propagation in the steel,resulting in high impact toughness.This work summarizes the com-bined effect of deoxidizers and alloying elements,with the aim to provide a new perspective for the research and practice related to im-proving the impact toughness of the heat affected zone(HAZ)during the high heat input welding.Ti complex deoxidation with other strong deoxidants,such as Mg,Ca,Zr,and rare earth metals(REMs),can improve the toughness of the heat-affected zone(HAZ)by re-fining PAGs or increasing IAF contents.However,it is difficult to identify the specific phase responsible for IAF nucleation because ef-fective inclusions formed by complex deoxidation are usually multiphase.Increasing alloying elements,such as C,Si,Al,Nb,or Cr,con-tents can impair HAZ toughness.A high C content typically increases the number of coarse carbides and decreases the potency of IAF formation.Si,Cr,or Al addition leads to the formation of undesirable microstructures.Nb reduces the high-temperature stability of the precipitates.Mo,V,and B can enhance HAZ toughness.Mo-containing precipitates present good thermal stability.VN or V(C,N)is ef-fective in promoting IAF nucleation due to its good coherent crystallographic relationship with ferrite.The formation of the B-depleted zone around the inclusion promotes IAF formation.The interactions between alloying elements are complex,and the effect of adding dif-ferent alloying elements remains to be evaluated.In the future,the interactions between various alloying elements and their effects on ox-ide metallurgy,as well as the calculation of the nucleation effects of effective inclusions using first principles calculations will become the focus of oxide metallurgy. 展开更多
关键词 oxide metallurgy technology heat affected zone high-strength low-alloy steel intragranular acicular ferrite microalloying element
下载PDF
变形工艺参数对Nb-Ti微合金钢再结晶的影响 被引量:1
4
作者 张琦 王晓南 +1 位作者 朱国辉 敬和民 《热加工工艺》 北大核心 2023年第3期25-30,共6页
通过热压缩实验研究了应变量及加热温度对Nb-Ti微合金钢的再结晶行为及变形后相变产物的影响。结果表明:当加热温度为1100℃时,奥氏体晶粒尺寸不均匀,导致压缩过程中各晶粒的应变累积不均匀,当总应变量为0.380时即发生了动态再结晶;奥... 通过热压缩实验研究了应变量及加热温度对Nb-Ti微合金钢的再结晶行为及变形后相变产物的影响。结果表明:当加热温度为1100℃时,奥氏体晶粒尺寸不均匀,导致压缩过程中各晶粒的应变累积不均匀,当总应变量为0.380时即发生了动态再结晶;奥氏体加热温度为1050和1000℃时,动态再结晶的临界应变量分别为0.668和0.552;当变形温度为850℃,应变量超过0.552时,试样在道次间隔发生静态再结晶;奥氏体化1100℃保温后压缩样品的冷却相变显微组织为贝氏体和准多边形铁素体,而1050℃和1000℃奥氏体化保温后压缩样品冷却相变后显微组织均为多边形铁素体,1000℃奥氏体化保温后压缩样品冷却相变后多边形铁素体晶粒尺寸更细小(2~5μm)。 展开更多
关键词 nb-ti微合金钢 动态再结晶 静态再结晶 相变
下载PDF
Effects of Rare-earth and Microalloying Elements on the Microstructure Characteristics of Hypereutectoid Rails
5
作者 戴宇恒 ZHAO Wenqian +1 位作者 包喜荣 陈林 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2023年第3期682-688,共7页
We performed thermal simulation experiments of double-pass deformation of hypereutectoid rails with different microalloying elements at a cooling rate of 1℃/s and deformation of 80%to explore the influence of rare-ea... We performed thermal simulation experiments of double-pass deformation of hypereutectoid rails with different microalloying elements at a cooling rate of 1℃/s and deformation of 80%to explore the influence of rare-earth and microalloying elements on the structure of hypereutectoid rails and optimize the composition design of hypereutectoid rails.Scanning electron microscopy,transmission electron microscopy,X-ray diffraction,and other characterization techniques were employed to quantitatively analyzed the effects of different microalloying elements,including rare-earth elements,on pearlite lamellar spacing,cementite characteristics,and dislocation density.It was found that the lamellar spacing was reduced by adding various microalloying elements.Cementite lamellar thickness decreased with the refinement of pearlite lamellar spacing while the cementite content per unit volume increased.Local cementite spheroidization,dispersed in the ferrite matrix in granular form and thus playing the role of dispersion strengthening,was observed upon adding cerium(Ce).The contributions of dislocation density to the alloy strength of four steel sheet samples with and without the addition of nickel,Ce,and Ce–copper(Cu)composite were 26,27,32,and 37 MPa,respectively,indicating that the Ce–Cu composite had the highest dislocation strengthening effect.The Ce–Cu composite has played a meaningful role in the cementite characteristics and dislocation strengthening,which provides a theoretical basis for optimizing the composition design of hypereutectoid rails in actual production conditions. 展开更多
关键词 microalloying elements rare earth hypereutectoid rail CEMENTITE DISLOCATION
下载PDF
Enhancing corrosion resistance of ZK60 magnesium alloys via Ca microalloying: The impact of nanoscale precipitates
6
作者 Wei Fu Hejie Yang +7 位作者 Tianshu Li Jiapeng Sun Shengwu Guo Daqing Fang Weichao Qin Xiangdong Ding Yimin Gao Jun Sun 《Journal of Magnesium and Alloys》 SCIE EI CAS CSCD 2023年第9期3214-3230,共17页
Enhancing corrosion resistance of Mg-Zn alloys with high strength and low cost was critical for broadening their large-scale practical applications. Here we prepared solutionized, peak-and over-aged ZK60 alloys with a... Enhancing corrosion resistance of Mg-Zn alloys with high strength and low cost was critical for broadening their large-scale practical applications. Here we prepared solutionized, peak-and over-aged ZK60 alloys with and without microalloying Ca(0.26 wt.%) to explore the effects of nanoscale precipitates on their corrosion behavior in detail via experimental analyses and theoretical calculations. The results suggested the peak-aged ZK60 alloy with Ca addition showed improved corrosion resistance in comparison with the alloys without Ca,owing to the contribution of Ca on the refinement of precipitates and increase in their number density. Although the precipitates and Mg matrix formed micro-galvanic couples leading to dissolution, the fine and dense precipitates could generate “in-situ pinning” effect on the corrosion products, forming a spider-web-like structure and improving the corrosion inhibition ability accordingly. The pinning effect was closely related to the size and number density of precipitates. This study provided important insight into the design and development of advanced corrosion resistant Mg alloys. 展开更多
关键词 MAGNESIUM PRECIPITATES microalloying Electrochemical test Pinning effect Calculation
下载PDF
微量Ca对ZE22镁合金显微组织及加工硬化行为的影响
7
作者 张莉 曾敏 《兵器材料科学与工程》 CAS CSCD 北大核心 2024年第4期71-76,共6页
为改善ZE系列镁合金延展性及加工性能,以ZE22为基础合金,通过Ca微合金化改善其加工硬化能力。进行EBSD及室温拉伸试验,研究微量Ca对ZE22镁合金显微组织及加工硬化行为的影响。结果表明:微量Ca的加入可细化晶粒,使平均晶粒尺寸为6.38~8.4... 为改善ZE系列镁合金延展性及加工性能,以ZE22为基础合金,通过Ca微合金化改善其加工硬化能力。进行EBSD及室温拉伸试验,研究微量Ca对ZE22镁合金显微组织及加工硬化行为的影响。结果表明:微量Ca的加入可细化晶粒,使平均晶粒尺寸为6.38~8.44μm,并引起基面织构弱化,织构极强度从22.3降至19.2,提高了基面滑移系的施密特因子。微观分析发现,加工硬化的弱化是晶粒尺寸和织构双重作用的结果。微量Ca的加入使合金加工硬化能力和应变率敏感系数降低,ZEG220合金的强塑性匹配更佳。研究结果为微合金化调控镁合金的加工硬化能力提供了理论基础和指导。 展开更多
关键词 镁合金 显微组织 加工硬化 力学性能 微合金化
下载PDF
不同孕育剂随流孕育对微合金化球墨铸铁组织和性能的影响
8
作者 李蒙 任莎歌 +1 位作者 李贵胜 祝庆 《兵器材料科学与工程》 CAS CSCD 北大核心 2024年第2期77-83,共7页
为探究硫氧孕育剂随流孕育对微合金化球墨铸铁组织和性能的影响,在相同铸造条件下,用树脂砂型分别浇注75Si Fe孕育剂和硫氧孕育剂随流孕育处理的球墨铸铁试样。通过组织观察、室温拉伸试验、布氏硬度试验等分析了两种不同孕育剂随流孕... 为探究硫氧孕育剂随流孕育对微合金化球墨铸铁组织和性能的影响,在相同铸造条件下,用树脂砂型分别浇注75Si Fe孕育剂和硫氧孕育剂随流孕育处理的球墨铸铁试样。通过组织观察、室温拉伸试验、布氏硬度试验等分析了两种不同孕育剂随流孕育对微合金化球墨铸铁的显微组织、力学性能和拉伸断口的影响,探寻硫氧孕育剂随流孕育与球墨铸铁组织和性能的联系。结果表明:两种试样均由大量的珠光体、少量的铁素体、大量的石墨球组成,其中用75Si Fe孕育剂进行随流孕育,石墨球易畸变,圆整度不好,石墨球数量少,尺寸较大,平均球化率为84%,平均石墨球数为137个/mm^(2);而用硫氧孕育剂进行随流孕育,石墨形态改善明显,石墨球径更细小,分布更均匀,石墨球数量大幅增加,平均球化率为91%,平均石墨球数为297个/mm^(2)。硫氧孕育剂试样的抗拉强度和断后伸长率均高于75Si Fe孕育剂,分别为874 MPa和6.4%。硫氧孕育剂随流孕育球墨铸铁试样断裂模式为伴有少量塑性变形的准解理断裂。综合认为,用硫氧孕育剂随流孕育可获得较高的综合力学性能。 展开更多
关键词 微合金化球墨铸铁 硫氧孕育剂 随流孕育 显微组织 力学性能
下载PDF
白云鄂博矿稀土在钢中的传承与作用
9
作者 任慧平 计云萍 +3 位作者 高雪云 瞿伟 刘香军 金自力 《包钢科技》 2024年第4期27-36,共10页
白云鄂博矿是世界上最大的稀土资源储量共生矿,搞清稀土在钢中的传承规律,清晰认识稀土在钢中的作用及机理,是有效利用稀土资源的关键。文章总结作者团队多年的研究成果,围绕白云鄂博矿稀土在钢中的传承、稀土对钢冶金质量的影响和稀土... 白云鄂博矿是世界上最大的稀土资源储量共生矿,搞清稀土在钢中的传承规律,清晰认识稀土在钢中的作用及机理,是有效利用稀土资源的关键。文章总结作者团队多年的研究成果,围绕白云鄂博矿稀土在钢中的传承、稀土对钢冶金质量的影响和稀土在钢中的微合金化作用进行了综述。相关基础研究工作,能够丰富稀土在钢中作用的认识,也能够为白云鄂博矿稀土资源在钢中的高质高效利用提供理论和技术支撑。 展开更多
关键词 白云鄂博矿 稀土 传承 冶金质量 微合金化
下载PDF
Ti和Nb微合金化对CuZr基相变增韧非晶复合材料组织性能的影响
10
作者 赵燕春 姚文博 +5 位作者 董杰 吕志超 黄燕 张艺波 马东 杨铭 《有色金属工程》 CAS 北大核心 2024年第10期25-30,共6页
以典型B2相增韧非晶复合材料形成合金Zr_(48)Cu_(48)Al_(4)为基础,分别研究了Ti、Nb微合金化添加对其凝固组织和性能的影响规律。研究发现,与基础合金相比,微合金化显著改变了B2相的组织形貌(包括大小、数量、形状),其中Ti微合金化降低... 以典型B2相增韧非晶复合材料形成合金Zr_(48)Cu_(48)Al_(4)为基础,分别研究了Ti、Nb微合金化添加对其凝固组织和性能的影响规律。研究发现,与基础合金相比,微合金化显著改变了B2相的组织形貌(包括大小、数量、形状),其中Ti微合金化降低了B2晶体相的形核能力,提高了非晶和非晶复合材料的形成能力;而Nb微合金化则提高了B2相的稳定性,并大幅提高了非晶相与B2相的硬度以及非晶复合材料的强度和压缩塑性(分别达到了1470 MPa和21.5%)。本研究为非晶复合材料的成分设计与制备提供了实验依据,对开发高性能相变增韧非晶复合材料具有参考价值。 展开更多
关键词 非晶复合材料 微合金化 非晶形成能力 相变诱导塑性
下载PDF
Ti微合金化热轧高强钢带性能试验研究
11
作者 张保忠 杨锁兵 +3 位作者 葛允宗 张博睿 孙国敏 唐辉 《宽厚板》 2024年第1期17-20,共4页
针对Ti微合金化高强钢带力学性能波动的问题,进行炼钢生产工艺优化,开展不同工艺对低合金高强钢热轧钢带力学性能影响的研究。原炼钢工艺为先将钢水在氩站进行钛合金化,然后直接送连铸机浇铸。为了进一步提高钢水洁净度、改善产品质量... 针对Ti微合金化高强钢带力学性能波动的问题,进行炼钢生产工艺优化,开展不同工艺对低合金高强钢热轧钢带力学性能影响的研究。原炼钢工艺为先将钢水在氩站进行钛合金化,然后直接送连铸机浇铸。为了进一步提高钢水洁净度、改善产品质量、增强力学性能稳定性,在原炼钢工艺中增加LF精炼工序,并进行新工艺试验。结果表明:钢水经过LF精炼处理,钢中硫含量从0.010%左右降低到0.005%左右,TiN夹杂物颗粒尺寸减小到10μm以内,能够使Ti微合金化高强钢热轧钢带的纵向冲击功提高43 J、横向冲击功提高38.9 J,并且具有良好的0℃低温冲击性能,保持产品力学性能稳定。 展开更多
关键词 TI微合金化 低合金高强度 脱硫 冲击功 TIN
下载PDF
钛微合金化螺纹钢筋的生产试验
12
作者 温斌 李娜 《河南冶金》 2024年第2期12-15,50,共5页
介绍了钛微合金化螺纹钢筋的生产工艺,以及不同的钛含量对螺纹钢组织性能的影响。试验表明:随着钛含量的增加,螺纹钢筋的强度得到显著提高,但是钛含量过高时,拉伸曲线会出现无屈服平台的现象,其原因是钛的加入降低了贝氏体临界转变速度... 介绍了钛微合金化螺纹钢筋的生产工艺,以及不同的钛含量对螺纹钢组织性能的影响。试验表明:随着钛含量的增加,螺纹钢筋的强度得到显著提高,但是钛含量过高时,拉伸曲线会出现无屈服平台的现象,其原因是钛的加入降低了贝氏体临界转变速度,发生贝氏体转变,组织中的贝氏体比例较高,导致拉伸曲线无屈服平台。 展开更多
关键词 钛微合金化 屈服现象 贝氏体
下载PDF
含Nb-Ti低碳微合金钢双道次高温压缩软化行为 被引量:13
13
作者 朱松鹤 戴兵 +2 位作者 张梅 卫品官 张恒华 《材料热处理学报》 EI CAS CSCD 北大核心 2010年第10期53-57,共5页
利用Gleeble-3500热力模拟实验机对含Nb-Ti低碳微合金钢双道次高温压缩软化行为进行了模拟研究。研究了各种变形参数对该钢软化行为的影响,建立了该钢软化行为的动力学方程。结果表明,随着道次间停留时间的延长、变形温度、变形量以及... 利用Gleeble-3500热力模拟实验机对含Nb-Ti低碳微合金钢双道次高温压缩软化行为进行了模拟研究。研究了各种变形参数对该钢软化行为的影响,建立了该钢软化行为的动力学方程。结果表明,随着道次间停留时间的延长、变形温度、变形量以及应变速率的增大,再结晶率随之增大。变形温度对奥氏体晶粒尺寸有着显著的影响,变形温度的降低将使奥氏体晶粒尺寸明显粗化;奥氏体晶粒尺寸随着道次间停留时间的延长而增大,随着变形量以及应变速率的增大而减小。 展开更多
关键词 nb-ti低碳微合金钢 双道次热压缩 软化
下载PDF
Nb-Ti微合金化超低碳低合金高强度钢中第二相的析出行为 被引量:37
14
作者 陈颜堂 郭爱民 李平和 《金属热处理》 EI CAS CSCD 北大核心 2007年第9期51-54,共4页
研究了Nb-Ti微合金化超低碳低合金高强钢在控轧控冷及回火过程中含Nb和Ti相的析出行为及其与硬度的关系。结果表明,Nb-Ti微合金化超低碳低合金高强钢在控轧控冷驰豫过程及随后的回火过程中均有第二相析出,在变形过程中Nb(CxNy)相析出颗... 研究了Nb-Ti微合金化超低碳低合金高强钢在控轧控冷及回火过程中含Nb和Ti相的析出行为及其与硬度的关系。结果表明,Nb-Ti微合金化超低碳低合金高强钢在控轧控冷驰豫过程及随后的回火过程中均有第二相析出,在变形过程中Nb(CxNy)相析出颗粒更为细小,在回火过程中Nb(CxNy)依附于TiN形核长大,600℃回火2 h后其硬度高于其它温度回火后的硬度。 展开更多
关键词 nb-ti微合金化 低合金高强度钢 控轧控冷 析出相
下载PDF
一种Nb-Ti微合金钢微合金碳氮化物析出行为的研究 被引量:30
15
作者 陆匠心 王国栋 《钢铁》 CAS CSCD 北大核心 2005年第9期69-72,共4页
利用热模拟和TEM技术研究了Nb-Ti微合金钢中微合金碳氮化物的析出行为,研究结果表明,高温奥氏体区析出的微合金碳氮化物数量随变形量的增大而增加,尺寸随着变形温度的升高稍有增大。铁素体区析出的微合金碳氮化物尺寸比在形变奥氏体中... 利用热模拟和TEM技术研究了Nb-Ti微合金钢中微合金碳氮化物的析出行为,研究结果表明,高温奥氏体区析出的微合金碳氮化物数量随变形量的增大而增加,尺寸随着变形温度的升高稍有增大。铁素体区析出的微合金碳氮化物尺寸比在形变奥氏体中析出的更为细小,数量随着保温时间的增加而增多,但尺寸变化不大;当温度较低的时候,微合金碳氮化物主要在位错线等晶内缺陷处析出。 展开更多
关键词 nb-ti微合金钢 氮化物 形变诱导析出 热模拟 TEM
下载PDF
Nb-Ti微合金钢中第二相析出的热力学计算 被引量:13
16
作者 赵素 张立 +1 位作者 徐国栋 李金富 《宝钢技术》 CAS 2012年第2期19-25,共7页
分析了Nb-Ti微合金钢在液相、凝固过程、奥氏体以及铁素体相中氮化物、碳化物和碳氮化物等第二相析出的热力学条件,计算了钛和铌的碳化物和氮化物在不同温度下的溶度积,由此得出微合金钢在不同相阶段的析出规律。计算结果表明,在该微合... 分析了Nb-Ti微合金钢在液相、凝固过程、奥氏体以及铁素体相中氮化物、碳化物和碳氮化物等第二相析出的热力学条件,计算了钛和铌的碳化物和氮化物在不同温度下的溶度积,由此得出微合金钢在不同相阶段的析出规律。计算结果表明,在该微合金钢中,氮化物、碳化物和碳氮化物不可能在液相中析出;TiC0.03N0.97和TiN在凝固过程中具备析出的热力学条件;在奥氏体相中,随着温度的降低,氮化物、碳化物及碳氮化物的析出顺序为:NbC0.75N0.25、NbC、TiC、NbN。 展开更多
关键词 nb-ti微合金钢 热力学计算 析出 氮化物 碳化物 碳氮化物
下载PDF
热轧冷却工艺对Nb-Ti微合金双相钢组织和性能的影响 被引量:6
17
作者 陈连生 那顺桑 +5 位作者 狄国标 张洪波 王月香 刘振宇 刘相华 何舒星 《特殊钢》 北大核心 2007年第3期10-12,共3页
研究了热轧后空冷(800-850℃→750℃)+水冷(750℃→300~180℃)的两段式和水冷(782℃→760℃)+空冷(760℃→713℃)+水冷(713℃→414℃)三段式冷却方式对双相钢(%:0.08C、1.02Mn、0.22Si、0.02Nb、0.01Ti)组织和机械性能的影响。结果表... 研究了热轧后空冷(800-850℃→750℃)+水冷(750℃→300~180℃)的两段式和水冷(782℃→760℃)+空冷(760℃→713℃)+水冷(713℃→414℃)三段式冷却方式对双相钢(%:0.08C、1.02Mn、0.22Si、0.02Nb、0.01Ti)组织和机械性能的影响。结果表明,采用两段式冷却方式可得到铁素体+分散的板条马氏体组织,并使铁素体尺寸达5.5μm,钢的屈服强度为345~365 MPa,抗拉强度为565~575 MPa、屈强比为0.60~0.65,优于三段式冷却方式轧制的双相钢。 展开更多
关键词 nb-ti微合金化 热轧双相钢 控制冷却 组织 力学性能
下载PDF
Nb-Ti微合金化钢QStE380TM汽车大梁用热轧钢板的研制 被引量:6
18
作者 王宝峰 丁国 +2 位作者 赵丽萍 王雪莲 李德刚 《特殊钢》 北大核心 2006年第2期49-51,共3页
采用铁水预处理-210t顶底复吹转炉-LF精炼-2流立弯型CSP铸机(65mm厚铸坯)-6机架SMS轧机控轧控冷工艺试制了成分(%)为:0.04~0.08C,0.20~0.35Si,1.20~1.35Mn,≤0.015P,≤0.010S,0.015~0.025Nb,0.005~0.015Ti Q... 采用铁水预处理-210t顶底复吹转炉-LF精炼-2流立弯型CSP铸机(65mm厚铸坯)-6机架SMS轧机控轧控冷工艺试制了成分(%)为:0.04~0.08C,0.20~0.35Si,1.20~1.35Mn,≤0.015P,≤0.010S,0.015~0.025Nb,0.005~0.015Ti QStE380TM汽车大梁用6~12mm热轧钢板。检验结果表明,钢板组织为铁素体+少量珠光体,晶粒尺寸4~7μm,其机械性能均符合标准要求,钢板不同方向屈服强度最大差值为30Mpa,抗拉强度最大差值20Mpa,大多数钢板常温冲击功为140~180J。 展开更多
关键词 nb-ti微合金化 CSP工艺 汽车大粱用钢
下载PDF
Nb-Ti微合金化热轧多相钢的组织和性能 被引量:4
19
作者 郑东升 朱伏先 +1 位作者 张明亚 李艳梅 《东北大学学报(自然科学版)》 EI CAS CSCD 北大核心 2010年第6期803-807,共5页
通过两阶段控轧和随后的三段冷却,获得了14mm厚的Nb-Ti微合金化热轧多相钢板.利用光学显微镜、扫描电镜、透射电镜、X射线衍射(XRD)、电子背散射衍射(EBSD)和力学性能测试等手段对其组织和性能进行了研究.结果表明,试验钢的显微组织由... 通过两阶段控轧和随后的三段冷却,获得了14mm厚的Nb-Ti微合金化热轧多相钢板.利用光学显微镜、扫描电镜、透射电镜、X射线衍射(XRD)、电子背散射衍射(EBSD)和力学性能测试等手段对其组织和性能进行了研究.结果表明,试验钢的显微组织由铁素体、贝氏体和少量马氏体组成;其平均屈服强度为518MPa,抗拉强度为616MPa,延伸率高达41%;组织中大量的铁素体大角度晶界、近似等轴状铁素体晶粒和较小尺寸贝氏体束的存在,大大提高了试验钢的塑性;铁素体和贝氏体组织的细化,细小的(Nb,Ti)C粒子以及铁素体晶粒和贝氏体板条内的位错提高了试验钢的强度. 展开更多
关键词 nb-ti微合金钢 热轧多相钢 控轧控冷 显微组织 力学性能
下载PDF
低碳结构用Nb-V和Nb-Ti复合微合金钢性能的比较 被引量:4
20
作者 韩安昌 林大为 邱昱斌 《上海金属》 CAS 2004年第5期34-37,共4页
简述低碳结构钢微合金系的发展,重点介绍NbV和NbTi微合金钢在强度、韧塑性、织构及焊接性能方面的差异。
关键词 Nb-V nb-ti 复合微合金钢 机械性能 韧塑性 强度 焊接性能
下载PDF