Effect of electric field,stress and environment on delayed fracture of a PZT-5 ferroelectric ceramic 被引量:2
1
作者 WANG Yi, SU Yanjing, CHU Wuyang & QIAO Lijie Department of Material Physics, University of Science and Technology Beijing, Beijing 100083, China School of Mechanic and Electric Control Engineering, Beijing Jiaotong University, Beijing 100044, China 《Science China(Physics,Mechanics & Astronomy)》 SCIE EI CAS 2005年第1期89-100,共12页
The combined effect of electric and mechanical loading on fracture of a PZT-5 ferroelectric ceramic in silicone oil has been investigated using a single edge notched specimen. The results show that the fracture toughn... The combined effect of electric and mechanical loading on fracture of a PZT-5 ferroelectric ceramic in silicone oil has been investigated using a single edge notched specimen. The results show that the fracture toughness and the threshold stress intensity factor of delayed fracture in silicone oil, i.e. stress corrosion cracking, decrease linearly with the increasing applied electric field, either positive or negative. For the PZT-5 ferroelectric ceramics, delayed fracture in silicone oil under sustained positive or negative field can occur, and the threshold field for delayed fracture under sustained positive or negative field decreases linearly with applied stress intensity factor. The combined effect of electric and mechanical loading on delayed fracture in silicone oil includes fieldenhancing delayed fracture under sustained load and stress-enhancing delayed fracture in silicone oil under sustained field. 展开更多
关键词 pzt-5 ferroelectric ceramics FRACTURE toughness DELAYED FRACTURE under SUSTAINED load delayedfracture under SUSTAINED electric field.
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部