Synthesis and Characterization of Chitosan-g-poly- (D, L-lactic acid) Copolymer 被引量:2
1
作者 HuaYANG ShaoBingZHOU XianMoDENG 《Chinese Chemical Letters》 SCIE CAS CSCD 2005年第1期123-126,共4页
Biodegradable chitosan-g-poly (D, L-lactic acid) copolymers were prepared via two methods. (1) The lactide was grafted onto hydroxyl groups of chitosan by using macromolecular initiator sodium of trimethylsilyl-chit... Biodegradable chitosan-g-poly (D, L-lactic acid) copolymers were prepared via two methods. (1) The lactide was grafted onto hydroxyl groups of chitosan by using macromolecular initiator sodium of trimethylsilyl-chitosan, (2) poly (D,L-lactic acid)(PLA) with low molecular weight can be linked to the amino group by coupling activated PLA to trimethylsilyl-chitosan. Two graft copolymers had hydrophilic-hydrophobic character and can be applied as carriers for drug delivery. 展开更多
关键词 poly (d L-lactic acid) CHITOSAN graft copolymer coupling macromolecular initiator.
下载PDF
Preparation and characterization of biodegradable nanoparticles from methoxy poly(ethylene glycol)-poly(D,L-lactide)block copolymers as novel drug carriers
2
作者 姜维 王运东 +5 位作者 张建铮 甘泉 张汉威 贝建中 赵秀文 费维扬 《化工学报》 EI CAS CSCD 北大核心 2006年第2期461-464,共4页
Methoxy poly(ethylene glycol)-poly(D,L-lactide) block copolymers (PEG-PLA) were prepared through ring-opening polymerization.The oil in water suspension method was used to prepare block copolymer micelles. The critica... Methoxy poly(ethylene glycol)-poly(D,L-lactide) block copolymers (PEG-PLA) were prepared through ring-opening polymerization.The oil in water suspension method was used to prepare block copolymer micelles. The critical micelle concentration (CMC) by fluorescence spectroscopy was 0.0056 mg·ml -1 . The physical state of the inner core region of micelles was characterized with 1HNMR. The size of indomethacin (IMC) loaded micelles measured by dynamic light scattering (DLS) showed narrow monodisperse size distribution and the average diameters were less than 50 nm. In addition, the nanoparticles with relatively high drug loading content (DLC) were obtained. 展开更多
关键词 药物载体 聚乙醇-聚丙交酯 载药颗粒 制备 表征 胶囊 共聚体
下载PDF
Co-delivery of resveratrol and docetaxel via polymeric micelles to improve the treatment of drug-resistant tumors 被引量:4
3
作者 Xiong Guo Zhiyue Zhao +5 位作者 Dawei Chen Mingxi Qiao Feng Wan Dongmei Cun Yi Sun Mingshi Yang 《Asian Journal of Pharmaceutical Sciences》 SCIE 2019年第1期78-85,共8页
Co-delivery of anti-cancer drugs is promising to improve the efficacy of cancer treatment.This study was aiming to investigate the potential of concurrent delivery of resveratrol(RES)and docetaxel(DTX)via polymeric na... Co-delivery of anti-cancer drugs is promising to improve the efficacy of cancer treatment.This study was aiming to investigate the potential of concurrent delivery of resveratrol(RES)and docetaxel(DTX)via polymeric nanocarriers to treat breast cancer.To this end,methoxyl poly(ethylene glycol)-poly(D,L-lactide)copolymer(mPEG-PDLA)was prepared and characterized using FTIR and 1H NMR,and their molecular weights were determined by GPC.Isobologram analysis and combination index calculation were performed to find the optimal ratio between RES and DTX to against human breast adenocarcinoma cell line(MCF-7 cells).Subsequently,RES and DTX were loaded in the mPEG-PDLA micelles simultaneously,and the morphology,particle size distribution,in vitro release,pharmacokinetic profiles,as well as cytotoxicity to the MCF-7 cells were characterized.IC50 of RES and DTX in MCF-7 cells were determined to be 23.0μg/ml and 10.4μg/ml,respectively,while a lower IC50 of 4.8μg/ml of the combination of RES and DTX was obtained.The combination of RES and DTX at a ratio of 1:1(w/w)generated stronger synergistic effect than other ratios in the MCF-7 cells.RES and DTX loaded mPEG-PDLA micelles exhibited prolonged release profiles,and enhanced cytotoxicity in vitro against MCF-7 cells.The AUC(0→t)of DTX and RES in mPEG-PDLA micelles after i.v.administration to rats were 3.0-fold and 1.6-fold higher than that of i.v.injections of the individual drugs.These findings indicated that the co-delivery of RES and DTX using mPEG-PDLA micelles could have better treatment of tumors. 展开更多
关键词 RESVERATROL dOCETAXEL Methoxyl poly(ethylene glycol)-poly(d l-lactide)copolymer (mPEG-PdLA) Micelles drug resistance tumor
下载PDF
聚乙二醇单甲醚一聚(D,L-乳酸)嵌段共聚物的研究 被引量:5
4
作者 邓联东 姚芳莲 +2 位作者 孙多先 姚春梅 董岸杰 《中国生物医学工程学报》 EI CAS CSCD 北大核心 2005年第6期736-739,共4页
采用熔融缩聚反应合成一系列聚(D,L-乳酸)(PDLLA)/聚乙二醇单甲醚(mPEG)两亲性二嵌段共聚物(PEDLLA),采用IR、1H-NMR、DSC、WAXD和TEM等手段分析和研究PEDLLA的结构与性能。实验结果表明,PEDLLA的结构和组成与设计相一致,结晶度和熔点... 采用熔融缩聚反应合成一系列聚(D,L-乳酸)(PDLLA)/聚乙二醇单甲醚(mPEG)两亲性二嵌段共聚物(PEDLLA),采用IR、1H-NMR、DSC、WAXD和TEM等手段分析和研究PEDLLA的结构与性能。实验结果表明,PEDLLA的结构和组成与设计相一致,结晶度和熔点均低于均聚物,且随着PEDLLA中PDLLA含量的增加,mPEG嵌段熔点降低,随着PDLLA嵌段相对分子质量的增大,PEDLLA降解速率增大。载药纳米粒呈核壳结构,载药量达30%。 展开更多
关键词 聚(d L-乳酸) 聚乙二醇单甲醚 聚乙二醇单甲醚-b-聚(d L-乳酸) 两亲性共聚物 嵌段共聚物
下载PDF
PDLA-PBS-PDLA三嵌段共聚物的合成及性能 被引量:7
5
作者 马丽莉 邵俊 +2 位作者 杨晨光 汤朝晖 陈学思 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2015年第11期2329-2334,共6页
合成了末端均为羟基的聚丁二酸丁二醇酯(PBS)预聚物,再以PBS的端羟基引发D-丙交酯(D—LA)开环聚合,得到聚右旋乳酸(PDLA)与PBS的三嵌段共聚物(PDLA—PBS—PDLA).通过凝胶渗透色谱和核磁共振氢谱进行了结构表征.随着m(D—L... 合成了末端均为羟基的聚丁二酸丁二醇酯(PBS)预聚物,再以PBS的端羟基引发D-丙交酯(D—LA)开环聚合,得到聚右旋乳酸(PDLA)与PBS的三嵌段共聚物(PDLA—PBS—PDLA).通过凝胶渗透色谱和核磁共振氢谱进行了结构表征.随着m(D—LA):m(PBS)由0.51:1逐渐增加至2.60:1,PDLA—PDS.PDLA中PDLA链段的长度逐渐增加.随着PDLA嵌段长度的增加,PDLA嵌段对PBS嵌段的限制作用增强,并导致PBS嵌段结晶温度下降,结晶焓降低.当m(D—LA):m(PBS)=2.60:1时,PBS嵌段不再能形成结晶.而m(D—LA):m(PBS)在0.51:1~3.04:1范围内,PDLA嵌段均可形成结晶,PDLA嵌段的熔点随其在嵌段共聚物中含量的增加而逐渐升高,但PDLA嵌段的熔融焓呈现先增加后降低的趋势.在部分嵌段共聚物中,PBS和PDLA嵌段可各自形成结晶,且PBS和PDLA的结晶结构不随组分的变化而发生改变,表明该嵌段共聚物中PDLA嵌段和PBS嵌段呈微相分离结构. 展开更多
关键词 聚丁二酸丁二醇酯 右旋聚乳酸 PdLA—PBS—PdLA三嵌段共聚物
下载PDF
聚乙二醇甲醚聚(D,L-乳酸)嵌段共聚物纳米胶束的制备 被引量:5
6
作者 邓联东 孙多先 +2 位作者 姚芳莲 霍建中 董岸杰 《应用化学》 CAS CSCD 北大核心 2004年第3期247-250,共4页
采用熔融缩聚反应合成了一系列聚 (D ,L 乳酸 ) (PDLLA) /聚乙二醇单甲醚 (mPEG)两亲性二嵌段共聚物 (PEDLLA) ,采用纳米沉淀技术制备PEDLLA纳米胶束 ,运用动态光散射法、氢核磁光谱法、芘荧光探针技术、紫外光谱法研究了PEDLLA纳米胶... 采用熔融缩聚反应合成了一系列聚 (D ,L 乳酸 ) (PDLLA) /聚乙二醇单甲醚 (mPEG)两亲性二嵌段共聚物 (PEDLLA) ,采用纳米沉淀技术制备PEDLLA纳米胶束 ,运用动态光散射法、氢核磁光谱法、芘荧光探针技术、紫外光谱法研究了PEDLLA纳米胶束。结果表明 ,胶束呈核壳结构 ,粒径为纳米级 ,受PDLLA链段相对分子质量和有机相中共聚物浓度的影响 ,PEDLLA的临界胶束浓度 (CMC)小于 2 4 3× 10 -6mol/L ,且随着PDLLA链段相对分子质量的增大而减小。 展开更多
关键词 聚(d L-乳酸) 聚乙二醇单甲醚 两亲性二嵌段共聚物 纳米沉淀技术 胶束
下载PDF
四臂星形嵌段共聚物s-PDLLA-b-PEG的合成 被引量:3
7
作者 魏芬芬 林雅铃 +2 位作者 张安强 陈秀云 王炼石 《合成化学》 CAS CSCD 北大核心 2010年第1期90-93,共4页
季戊四醇与D,L-丙交酯开环聚合制得末端为羟基的四臂星形聚乳酸(s-PDLLA);s-PDLLA与羧基封端的聚乙二醇单甲醚(CT-mPEG)完成酯化反应,合成了以季戊四醇为核,以聚乳酸为内部嵌段、聚乙二醇为外部嵌段的四臂星形聚(D,L-乳酸)-聚乙二醇嵌... 季戊四醇与D,L-丙交酯开环聚合制得末端为羟基的四臂星形聚乳酸(s-PDLLA);s-PDLLA与羧基封端的聚乙二醇单甲醚(CT-mPEG)完成酯化反应,合成了以季戊四醇为核,以聚乳酸为内部嵌段、聚乙二醇为外部嵌段的四臂星形聚(D,L-乳酸)-聚乙二醇嵌段共聚物(s-PDLLA-b-PEG),其结构经1H NMR,IR和GPC表征。 展开更多
关键词 四臂星形嵌段共聚物 季戊四醇 聚乳酸 聚乙二醇 合成
下载PDF
Preparation, Release-control and Cell Apoptosis of C_6 Glioma Cells in PEG-PLGA-Rg3 Nanoparticles
8
作者 BIE Li YUAN Hong-yan +2 位作者 WANG Xin ZHAO Gang LIU Xing-ji 《Chemical Research in Chinese Universities》 SCIE CAS CSCD 2010年第5期780-784,共5页
With biodegradable material poly(ethylene glycol)-poly(lactide-co-glycolide) (PEG-PLGA) as substrate, the size distribution of Rg3-NPs was approved by the scanning electron microscopy. MTT assay was used to dete... With biodegradable material poly(ethylene glycol)-poly(lactide-co-glycolide) (PEG-PLGA) as substrate, the size distribution of Rg3-NPs was approved by the scanning electron microscopy. MTT assay was used to detect the effects of Rg3-NPs on the growth rate of C6 cells at various concentrations and flow cytometry(FCM) was applied to assay the cell cycle and cell apoptosis of C6 glioma cells. Western blot analysis was used to measure the protein level of PCNA. The results show that Rg3-NPs are slick and uniformity, the average diameter of the nanoparticles is about 75-90 nm, entrapment efficiency is (89.7±1.7)%. MTT assay shows the growth of C6 Glioma Cells can be significantly inhibited by Rg3-NPs in a dose-dependence manner. FCM and Western blot analysis show Rg3 can be released from the conjugated nanoparticles to function in the cell nuclei so as to lead to the changes in the growth cycle of the cells, which results in the arrest of G0-G1 cell cycle and induces the apoptosis of C6 cells. Therefore, Rg3-NPs may be used for the auxiliary therapy of brain glioma. 展开更多
关键词 Ginsenoside Rg3 poly(d l-lactide-co-glycolide) Characteristics of physical chemistry C6 glioma cell APOTOSIS
下载PDF
壳聚糖聚乳酸接枝共聚物作为DNA递送载体 被引量:1
9
作者 曾荣胤 苏均乐 谢德明 《暨南大学学报(自然科学与医学版)》 CAS CSCD 北大核心 2011年第3期294-299,303,共7页
以硅烷基保护壳聚糖分子中-NH2和部分羟基,与D,L-丙交酯接枝聚合,制备壳聚糖与聚乳酸接枝共聚物(CS-g-PDLLA).利用CS-g-PDLLA作为DNA载体,复合pEGFP-N1质粒,分别采用动态激光散射及原子力显微镜(AFM)分析复合物粒子的粒径分布及形态,凝... 以硅烷基保护壳聚糖分子中-NH2和部分羟基,与D,L-丙交酯接枝聚合,制备壳聚糖与聚乳酸接枝共聚物(CS-g-PDLLA).利用CS-g-PDLLA作为DNA载体,复合pEGFP-N1质粒,分别采用动态激光散射及原子力显微镜(AFM)分析复合物粒子的粒径分布及形态,凝胶电泳试验考察载体与质粒DNA的结合情况,人体胃癌细胞培养进行细胞毒性评估.测试表明CS-g-PDLLA/DNA复合物平均粒径为91.59~234.56 nm,AFM结果显示,在D,L-丙交酯与壳聚糖单元的摩尔比等于3,N/P等于3所形成的壳聚糖聚乳酸共聚物/pEGFP-N1复合物粒径小于100 nm.提高载体材料的PDLLA比例及复合物N/P比,复合物对DNase I显示高稳定性,并且具有较好的DNA缓释效果.细胞培养显示载体良好的生物相容性.结果表明壳聚糖与聚乳酸共聚物可作为一种新型的非病毒型基因载体. 展开更多
关键词 壳聚糖聚乳酸共聚物 载体 基因递送
下载PDF
Biologically Inspired Self-assembling Synthesis of Bone-like Nano-hydroxyapatite/PLGA-(PEG-ASP)_n Composite: A New Biomimetic Bone Tissue Engineering Scaffold Material 被引量:13
10
作者 郭晓东 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2005年第B12期234-237,共4页
A new biomimetic bone tissue engineering scaffold material, nano-HAI PLGA-( PEG-Asp )n composite, was synthesized by a biologically inspired self-assembling approach. A novel biodegradable PLGA- ( PEG-Asp )n cop... A new biomimetic bone tissue engineering scaffold material, nano-HAI PLGA-( PEG-Asp )n composite, was synthesized by a biologically inspired self-assembling approach. A novel biodegradable PLGA- ( PEG-Asp )n copolymer with pendant amine functional groups and enhanced hydrophilicity woo synthesized by bulk ring-opening copolymerization by DL-lactide( DLLA) and glycolide( GA ) with Aspartic acid ( Asp )-Polyethylene glycol(PEG) alt-prepolymer. A Three-dimensional, porous scaffold of the PLGA-( PEG- Asp)n copolymer was fabricated by a solvent casting , particulate leaching process. The scaffold woo then incubated in modified simulated body fluid (naSBF). Growth of HA nanocrystals on the inner pore surfaces of the porous scaffold is confirmed by calcium ion binding analyses, SEM , mass increooe meoourements and quantification of phosphate content within scaffolds. SEM analysis demonstrated the nucleation and growth of a continuous bonelike, low crystalline carbonated HA nanocrystals on the inner pore surfaces of the PLGA- ( PEG-Asp )n scaffolds. The amount of calcium binding, total mass and the mass of phosphate on experimental PLGA- ( PEG-Asp ) n scaffolds at different incubation times in mSBF was significantly greater than that of control PLGA scaffolds. This nano-HA/ PLGA-( PEG- Asp )n composite stunts some features of natural bone both in main composition and hierarchical microstrueture. The Asp- PEG alt-prepolymer modified PleA copolymer provide a controllable high surface density and distribution of anionic functional groups which would enhance nucleation and growth of bonelike mineral following exposure to mSBF. This biomimetic treatment provides a simple method for surface functionalization and sabsequent mineral nucleation and self-oosembling on bodegradable polymer scaffolds for tissue engineering. 展开更多
关键词 bone tissue engineering biomimetic material BIOMINERALIZATION self-asserrdaling poly d l-lactide-co-glycolide hydroxyapatite
下载PDF
羟基保护法制备聚(D-乳酸-葡萄糖)共聚物及其性能研究
11
作者 朱前进 祁俐燕 +2 位作者 曹丹 刘婷婷 高勤卫 《生物质化学工程》 CAS 2021年第2期1-8,共8页
以α-D-葡萄糖为原料,采用羟基保护法制备1,2∶5,6-双-O-异丙叉基-α-D-呋喃葡萄糖(ODG),并与聚D-乳酸(PDLA)熔融共聚合成聚(D-乳酸-1,2∶5,6-双-O-异丙叉基-α-D-呋喃葡萄糖)共聚物(PDLAODG),然后水解脱羟基制备聚(D-乳酸-葡萄糖)共聚... 以α-D-葡萄糖为原料,采用羟基保护法制备1,2∶5,6-双-O-异丙叉基-α-D-呋喃葡萄糖(ODG),并与聚D-乳酸(PDLA)熔融共聚合成聚(D-乳酸-1,2∶5,6-双-O-异丙叉基-α-D-呋喃葡萄糖)共聚物(PDLAODG),然后水解脱羟基制备聚(D-乳酸-葡萄糖)共聚物(PDLAG)。采用核磁共振氢谱、傅里叶变换红外光谱、热重法、差示扫描量热法、X射线衍射、接触角与吸水率等方法测定结构与性能。结果表明:通过葡萄糖羟基保护法和熔融共聚法可以合成PDLAODG和PDLAG,且共聚物中葡萄糖基团接枝的PDLA链段的数量受到n(ODG)/n(PDLA)的调控,当n(ODG)/n(PDLA)≥5时,共聚物中只含有1条D-乳酸链段。PDLAODG与PDLAG的PDLA链段均形成α-型结晶。随着葡萄糖基团含量的增加,PDLAODG的熔点从151.5℃降至147.9℃、结晶度从58.2%降至42.1%、水接触角从78.1°降至71.5°,而PDLAG的熔点从156.8℃降至149.4℃、结晶度从61.9%降至50.0%、水接触角从70.1°降至64.4°。PDLAODG与PDLAG的亲水性均高于纯PDLA,且在葡萄糖基团含量相同时PDLAG的结晶度、熔点和亲水性均高于PDLAODG,即其热稳定性、结晶性和亲水性增加。 展开更多
关键词 葡萄糖 聚乳酸 聚(d-乳酸-葡萄糖)共聚物 亲水性
下载PDF
微波辅助壳聚糖接枝聚乳酸共聚物的合成及表征 被引量:9
12
作者 何柱国 罗丙红 +3 位作者 周长忍 程松 张奕 钟翠红 《应用化学》 CAS CSCD 北大核心 2009年第10期1134-1138,共5页
在微波辅助下,以辛酸亚锡为催化剂、壳聚糖(CS)为大分子引发剂引发消旋丙交酯(D,L-LA)本体开环聚合制备了壳聚糖接枝聚乳酸共聚物。通过正交试验确定了最佳合成条件:微波功率10W,反应温度120℃,反应时间15min,催化剂用量:n(丙交酯)∶n(... 在微波辅助下,以辛酸亚锡为催化剂、壳聚糖(CS)为大分子引发剂引发消旋丙交酯(D,L-LA)本体开环聚合制备了壳聚糖接枝聚乳酸共聚物。通过正交试验确定了最佳合成条件:微波功率10W,反应温度120℃,反应时间15min,催化剂用量:n(丙交酯)∶n(辛酸亚锡)=1000∶1。通过红外光谱、元素分析、核磁共振氢谱、X射线衍射和热分析测试技术对接枝共聚物的结构与性能进行了表征和测试。结果表明,在微波条件下,能快速、有效地合成壳聚糖接枝聚乳酸共聚物,单位糖环上聚乳酸支链的平均乳酰单元数大于17.46;聚乳酸支链的引入有效削弱了壳聚糖分子间和分子内较强的氢键作用,与壳聚糖相比较,共聚物的结晶性能下降,热分解发生在246℃,低于壳聚糖的253℃;随n(D,L-LA)/n(CS糖环数)值增大,共聚物中平均乳酰单元数逐渐增大,共聚物的结晶性能、起始分解温度逐渐下降。 展开更多
关键词 微波合成 壳聚糖 聚乳酸 接枝共聚物
下载PDF
羟乙基壳聚糖接枝聚乳酸的合成与表征 被引量:8
13
作者 程松 钟翠红 +2 位作者 周长忍 焦延鹏 罗丙红 《功能材料》 EI CAS CSCD 北大核心 2010年第4期666-670,共5页
首先采用壳聚糖(CS)与2-氯乙醇反应制备了羟乙基壳聚糖(HECS),然后通过本体开环聚合法,以辛酸亚锡为催化剂,CS和HECS为大分子引发剂引发消旋-丙交酯开环聚合制备了一系列CS-g-PDL-LA和HECS-g-PDLLA共聚物,用FTIR、1HNMR、XRD、TG和溶解... 首先采用壳聚糖(CS)与2-氯乙醇反应制备了羟乙基壳聚糖(HECS),然后通过本体开环聚合法,以辛酸亚锡为催化剂,CS和HECS为大分子引发剂引发消旋-丙交酯开环聚合制备了一系列CS-g-PDL-LA和HECS-g-PDLLA共聚物,用FTIR、1HNMR、XRD、TG和溶解实验对产物的结构与性能进行了分析表征。结果表明,与CS相比,HECS明显具有较高的反应活性,当n(D,L-LA):n(aminoglucoside)投料比从10:1增大到40:1,对应CS-g-PDLLA和HECS-g-PDLLA共聚物的接枝率分别从24.01%和77.42%上升到114.85%和380.51%,而两者中的聚乳酸侧链上的平均乳酰单元数也相应从0.61和2.51分别上升到2.48和12.31。另外,原料投料比对共聚物的组成与性能有显著影响,随n(D,L-LA):n(ami-noglucoside)值增大,共聚物的接枝率和聚乳酸侧链上的平均乳酰单元数也逐渐增大,共聚物的结晶性能下降,起始热分解温度有所降低。与CS-g-PDLLA相比,HECS-g-PDLLA在常用有机溶剂中的溶解性能有所改善。 展开更多
关键词 壳聚糖 羟乙基壳聚糖 聚乳酸 接枝共聚物 本体聚合
下载PDF
壳聚糖修饰PLGA阳离子型纳米微球的制备与表征 被引量:9
14
作者 官习鹏 全大萍 +1 位作者 廖凯荣 麦堪成 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2006年第10期1965-1968,共4页
采用单乳化-溶剂(O/W)挥发技术制备表面带正电荷的壳聚糖(CHS)修饰聚乙/丙交酯(PLGA)纳米微球(PLGA/CHS),通过正交试验优化了纳米微球的制备条件.结果表明,微球粒径可控制在150~200nm内,在pH=4时,纳米微球表面电位最高为55mV.影响微球... 采用单乳化-溶剂(O/W)挥发技术制备表面带正电荷的壳聚糖(CHS)修饰聚乙/丙交酯(PLGA)纳米微球(PLGA/CHS),通过正交试验优化了纳米微球的制备条件.结果表明,微球粒径可控制在150~200nm内,在pH=4时,纳米微球表面电位最高为55mV.影响微球粒径的主要因素是聚合物的浓度,CHS的分子量和浓度以及介质的pH值对微球表面电位也有明显影响.制备粒径较小而表面电位较高的PLGA/CHS纳米微球条件为:ρ(CHS)=3mg/mL,ρ(PLGA)=10mg/mL,Vo/Va=1/4.SEM图像显示经CHS修饰的PLGA的纳米微球形状规整,荧光显微观察和XPS分析结果证实CHS包覆于微球表面. 展开更多
关键词 阳离子纳米微球 丙交酯-乙交酯共聚物 壳聚糖
下载PDF
聚乳酸/聚乙二醇-聚乳酸新型亲水支架的制备与研究 被引量:8
15
作者 孙蕊 潘高峰 +2 位作者 张丽芳 杜建 熊成东 《生物医学工程学杂志》 EI CAS CSCD 北大核心 2007年第1期91-96,共6页
利用热致相分离/粒子沥滤结合法,制备了聚乳酸(PDLLA)以及聚乳酸与聚乙二醇-聚乳酸共聚物(PELA)复合的PDLLA/PELA组织工程支架。讨论了聚乙二醇(PEG)分子量、PELA含量及组成比对于支架内部结构、力学性能、降解行为和细胞毒性... 利用热致相分离/粒子沥滤结合法,制备了聚乳酸(PDLLA)以及聚乳酸与聚乙二醇-聚乳酸共聚物(PELA)复合的PDLLA/PELA组织工程支架。讨论了聚乙二醇(PEG)分子量、PELA含量及组成比对于支架内部结构、力学性能、降解行为和细胞毒性的影响。结果表明,热致相分离/粒子沥滤结合法制备的支架,具有100~250μm大孔与5~40μm小孔兼备的特殊内部结构,PEG含量愈高、PEG分子量愈小,支架的孔隙率愈大。PDLLA/PELA比率的减小,PEG/PLA比率的增大会引起支架力学性能的下降和降解的加速。材料无细胞毒性。当支架中PDLLA/PELA为3:1,PEG5000/PLA为25:75时,其内部孔形态最为理想。 展开更多
关键词 聚乳酸 聚乙二醇-聚乳酸共聚物 热致相分离
下载PDF
聚环氧乙烷-聚丙交酯嵌段共聚物的合成 被引量:4
16
作者 王玉东 张孝彦 +3 位作者 刘晓琼 付鹏 刘民英 赵清香 《郑州大学学报(工学版)》 CAS 北大核心 2011年第2期26-28,共3页
以自制一缩二乙二醇单甲醚钾为引发剂,利用阴离子聚合原理,进行了环氧乙烷的开环聚合,得到了分子量为2 000,分子量分布为1.07和一端是甲氧基一端是羟基的窄分布聚环氧乙烷(mPEO),然后利用得到的mPEO作为大分子引发剂,在Sn(Oct)2催化作用... 以自制一缩二乙二醇单甲醚钾为引发剂,利用阴离子聚合原理,进行了环氧乙烷的开环聚合,得到了分子量为2 000,分子量分布为1.07和一端是甲氧基一端是羟基的窄分布聚环氧乙烷(mPEO),然后利用得到的mPEO作为大分子引发剂,在Sn(Oct)2催化作用下,引发D,L-丙交酯开环聚合,得到两亲性mPEO-b-PLA嵌段共聚物,其分子量分别为5 250,14 070,23 360和44 300,分子量分布分别为1.45,1.47,1.53和1.59.对目标产物和中间产物进行了表征,分子量与设计结果吻合,聚合是可控的. 展开更多
关键词 聚环氧乙烷 聚丙交酯 嵌段共聚物 活性阴离子聚合 配位-插入开环聚合
下载PDF
可生物降解PLA/PCL、PELA/PECL共混体系的研究 被引量:4
17
作者 张连来 熊成东 邓先模 《高分子材料科学与工程》 EI CAS CSCD 北大核心 1993年第2期70-74,共5页
本工作以DSC研究了聚d,l-乳酸/聚ε-己内酯(PLA/PCL)、聚d,l-乳酸-聚乙二醇嵌段共聚物/聚ε-己内酯-聚乙二醇嵌段共聚物(PELA/PECL)共混体系的相容性,发现PLA/PCL体系是不相容的,随PLA含量的增大,PCL结晶度增大。而PELA/PECL共混体系中... 本工作以DSC研究了聚d,l-乳酸/聚ε-己内酯(PLA/PCL)、聚d,l-乳酸-聚乙二醇嵌段共聚物/聚ε-己内酯-聚乙二醇嵌段共聚物(PELA/PECL)共混体系的相容性,发现PLA/PCL体系是不相容的,随PLA含量的增大,PCL结晶度增大。而PELA/PECL共混体系中,由于PEG链段的“内增容作用”,使二组分有较好的相容性。随PELA含量的增加,PECL的熔点、结晶度降低。 展开更多
关键词 高聚物 生物降解 相容性 共混体系
下载PDF
mPEG表面修饰的PLGA嵌段共聚物的血液相容性评价 被引量:9
18
作者 聂宇 段友容 张志荣 《生物医学工程学杂志》 EI CAS CSCD 北大核心 2007年第2期336-339,共4页
本实验室设计合成了三种不同LA/GA比例的mPEG修饰PLGA(PELGA,含15%mPEG),为了评价它们的血液相容性,我们以硅化玻璃试管为阴性对照,未硅化的试管为阳性对照,参照国际标准(ISO10993)和《中华人民共和国国家标准GB/T 16886医疗器械生... 本实验室设计合成了三种不同LA/GA比例的mPEG修饰PLGA(PELGA,含15%mPEG),为了评价它们的血液相容性,我们以硅化玻璃试管为阴性对照,未硅化的试管为阳性对照,参照国际标准(ISO10993)和《中华人民共和国国家标准GB/T 16886医疗器械生物学评价》方法进行了体外评价实验。试验包括溶血率实验,血小板黏附实验,动态凝血时间实验,凝血时间实验,血浆复钙时间实验和凝血酶原时间实验等综合评价指标。结果表明,合成材料具有优良的血液相容性,材料制成的纳米粒有望应用于静脉注射。 展开更多
关键词 聚乙交酯丙交酯 聚乙烯醇 嵌段共聚物 血液相容性 静脉注射
下载PDF
生物降解材料胆酸-乳酸共聚物的热性能研究 被引量:2
19
作者 王群芳 汪朝阳 +2 位作者 赵海军 侯晓娜 罗玉芬 《广州化学》 CAS 2008年第4期1-6,共6页
通过直接熔融共聚法合成了系列的不同乳酸/胆酸组成比(LA/CA)的胆酸-乳酸共聚物,用DSC、TG等手段研究生物降解材料胆酸-乳酸共聚物的热性能。结果表明,共聚物的热性能与其组成、结构有关。LA/CA小的多核共聚物无明显熔融峰,热失重分两... 通过直接熔融共聚法合成了系列的不同乳酸/胆酸组成比(LA/CA)的胆酸-乳酸共聚物,用DSC、TG等手段研究生物降解材料胆酸-乳酸共聚物的热性能。结果表明,共聚物的热性能与其组成、结构有关。LA/CA小的多核共聚物无明显熔融峰,热失重分两步进行;LA/CA大的单核共聚物出现明显双头熔融峰,其热失重一步进行,其Tg随着LA/CA增加而升高。 展开更多
关键词 生物降解材料 胆酸-乳酸共聚物 热性能 dSC TG
下载PDF
可生物降解的PELA微球优化工艺的研究 被引量:4
20
作者 雷永 陆彬 《华西药学杂志》 CAS CSCD 北大核心 1994年第4期215-217,共3页
本文报道了可生物降解的PELA微球的优化工艺,制得平均球径为32.5μm,平均包封率为75%以上,临界相对湿度约78%以及流动性好的白色球形粉末。体外释放药物符合零级释放规律,达到了肌内注射用的缓释微球的要求。