A comparative evaluation of DQP, OQP and CEH bleaching of non-wood fibres has revealed that wheat straw, reed, bagasse and bamboo pulps can be bleached to brightness levels of just above 80% ISO, when applying an OQP ...A comparative evaluation of DQP, OQP and CEH bleaching of non-wood fibres has revealed that wheat straw, reed, bagasse and bamboo pulps can be bleached to brightness levels of just above 80% ISO, when applying an OQP bleaching sequence and to brightness levels of about 85% ISO when applying the DQP sequence using 10 - 15 kg/tp of ClO2 (aCl.), 15 - 20 kg/tp of H2O2 together with 1 - 2 kg/tp of EDTA. The P.C. numbers of the DQP and OQP bleached pulps are much lower and the viscosity much higher than those of the CEH bleached pulps. Compared with CEH pulps, both the DQP and OQP pulps had better strength properties, particularly Tear Index. In spite of their higher final brightness levels, the DQP pulps show similar or better strength properties than the OQP pulps. A comparison of the CEH and DQP effluents showed that the DQP bleaching could reduce the pollution load (CODCr, BOD5, SS) by 35 to 60% without the need for recirculation of any effluent streams. The AOX levels could be reduced by 87 to 93%.展开更多
The influences on the brightness, viscosity and Kappa of the straw pulp under the different oxygen-alkali bleaching conditions have been studied in this paper.
文摘A comparative evaluation of DQP, OQP and CEH bleaching of non-wood fibres has revealed that wheat straw, reed, bagasse and bamboo pulps can be bleached to brightness levels of just above 80% ISO, when applying an OQP bleaching sequence and to brightness levels of about 85% ISO when applying the DQP sequence using 10 - 15 kg/tp of ClO2 (aCl.), 15 - 20 kg/tp of H2O2 together with 1 - 2 kg/tp of EDTA. The P.C. numbers of the DQP and OQP bleached pulps are much lower and the viscosity much higher than those of the CEH bleached pulps. Compared with CEH pulps, both the DQP and OQP pulps had better strength properties, particularly Tear Index. In spite of their higher final brightness levels, the DQP pulps show similar or better strength properties than the OQP pulps. A comparison of the CEH and DQP effluents showed that the DQP bleaching could reduce the pollution load (CODCr, BOD5, SS) by 35 to 60% without the need for recirculation of any effluent streams. The AOX levels could be reduced by 87 to 93%.
文摘The influences on the brightness, viscosity and Kappa of the straw pulp under the different oxygen-alkali bleaching conditions have been studied in this paper.