High-voltage thermal breakdown has great potential application in permeability enhancement of coal seam. The characteristics of the breakdown channel, coal element, porosity and microscopic coal petrography of coal un...High-voltage thermal breakdown has great potential application in permeability enhancement of coal seam. The characteristics of the breakdown channel, coal element, porosity and microscopic coal petrography of coal under high-voltage electric load were experimentally studied. The coal interior left apparent tracks due to electric current burning with high temperature. The percentage of C, O, Al, Fe, and Si had slightly decreased, while the content of element N increased obviously. Low-pressure nitrogen gas adsorption(LP-N_2GA) and mercury intrusion analysis showed that coal porosity increased. The increases of micropores and mesopores are beneficial to promotion of the ability of gas storage, and the increase of macropores could enhance the gas seepage and migration. The results of scanning electron microscope(SEM) show that there are many exogenous fractures in coal, which is also beneficial to gas seepage and migration. The results lay a theoretical foundation for application of high-voltage thermal breakdown in coal mines.展开更多
In order to study the influence of three-grid assembly thermal deformation caused by heat accumulation on breakdown times and an ion extraction process,a hot gap test and a breakdown time test are carried out to obtai...In order to study the influence of three-grid assembly thermal deformation caused by heat accumulation on breakdown times and an ion extraction process,a hot gap test and a breakdown time test are carried out to obtain thermal deformation of the grids when the thruster is in 5 k W operation mode.Meanwhile,the fluid simulation method and particle-in-cell-Monte Carlo collision(PICMCC) method are adopted to simulate the ion extraction process according to the previous test results.The numerical calculation results are verified by the ion thruster performance test.The results show that after about 1.2 h operation,the hot gap between the screen grid and the accelerator grid reduce to 0.25–0.3 mm,while the hot gap between the accelerator grid and the decelerator grid increase from 1 mm to about 1.4 mm when the grids reach thermal equilibrium,and the hot gap is almost unchanged.In addition,the breakdown times experiment shows that 0.26 mm is the minimal safe hot gap for the grid assembly as the breakdown times improves significantly when the gap is smaller than this value.Fluid simulation results show that the plasma density of the screen grid is in the range 6?×10^(17)–6?×?10^(18) m^(13) and displays a parabolic characteristic,while the electron temperature gradually increases along the axial direction.The PIC-MCC results show that the current falling of an ion beam through a single aperture is significant.Meanwhile,the intercepted current of the accelerator grid and the decelerator grid both increase with the change in the hot gap.The ion beam current has optimal perveance status without thermal deformation,and the intercepted current of the accelerator grid and the decelerator grid are 3.65 m A and 6.26 m A,respectively.Furthermore,under the effect of thermal deformation,the ion beam current has over-perveance status,and the intercepted current of the accelerator grid and the decelerator grid are 10.46 m A and 18.24 m A,respectively.Performance test results indicate that the breakdown times increase obviously.The intercepted current of the accelerator grid and the decelerator grid increases to 13 m A and 16.5 m A,respectively,due to the change in the hot gap after 1.5 h operation.The numerical calculation results are well consistent with performance test results,and the error comes mainly from the test uncertainty of the hot gap.展开更多
The carbon nanotube (CNT)-based materials can be used as vacuum device cathodes. Owing to the excellent field emission properties of CNT, it has great potentials in the applications of an explosive field emission ca...The carbon nanotube (CNT)-based materials can be used as vacuum device cathodes. Owing to the excellent field emission properties of CNT, it has great potentials in the applications of an explosive field emission cathode. The falling off of CNT from the substrate, which frequently appears in experiments, restricts its application. In addition, the onset time of vacuum breakdown limits the performance of the high-power explosive-emission-cathode-based diode. In this paper, the characteristics of the CNT, electric field strength, contact resistance and the kind of substrate material are varied to study the parameter effects on the onset time of vacuum breakdown and failure mechanism of the CNT by using the finite element method.展开更多
A significant number of fire-induced power disruptions are observed in several countries every year. The faults are normally phase-to-phase short circuiting or conductor-to-ground discharges at mid-span region of the ...A significant number of fire-induced power disruptions are observed in several countries every year. The faults are normally phase-to-phase short circuiting or conductor-to-ground discharges at mid-span region of the high-voltage transmission system. In any case, the wildfire plumes provide a conductive path. The electrical conductivity is due to intense heat in combustion zone of the fire which creates ion and electrons from flame inherent particulates. Increase in the ion concentration increases the electrical conductivity of the fire plume. The main purpose of this study was to measure dielectric breakdown electric field for vegetation and hydrocarbon flames. The experimental data is needed for validation of simulation schemes which are necessary for evaluation of power grid systems reliability under extreme wildfire weather conditions. In this study, hydrocarbon and vegetation fuels were ignited in a cylindrically shaped steel burner which was fitted with type-K thermocouples to measure flame temperature. The fuels consisted of dried weeping wattle (Peltophorum africanum) litter, butane gas and candle wax. Two pinned copper electrodes supported by retort stands were mounted to the burner and energized to a high voltage. This generated a strong electric field sufficient to initiate dielectric breakdown in the flames. Breakdown electric field strength (Ecrit) obtained from the experiment decreased from 10.5 to 6.9 kV/cm for the flames with temperature range of 1003 to 1410 K, respectively.展开更多
The purpose of this work is to determine the impact of thermal aging on the dielectric and physicochemical properties of the oil/paper mixed insulation. We performed a comparative analysis of dielectric paper dipped i...The purpose of this work is to determine the impact of thermal aging on the dielectric and physicochemical properties of the oil/paper mixed insulation. We performed a comparative analysis of dielectric paper dipped in two cooling fluids: palm kernel oil methyl ester (MEPKO) and mineral oil (MO). Two types of dielectric paper were used: Thermally Upgraded Kraft paper (TUK) and Nomex-910 paper (NP-910). An accelerated aging test was realized at 110<span style="white-space:nowrap;">°</span>C during a total of 96 hours. Samples of oil and paper were collected after 0, 48, 72 and 96 hours for analyses purposes. The analyses performed included the measurement of the Breakdown voltage (BDV) of the dielectric papers, the Total Acid Number (TAN) and the Decay Dissolved Products (DDP) of the liquid dielectrics. The BDV of NP-910 is greater than the BDV of TUK. Concerning the type of oil, the BDV of dielectric papers impregnated with MEPKO is greater than the BDV of similar papers impregnated with MO, indicating a better preservation of paper when dipped in methyl esters. The analyses of TAN and DDP revealed that Nomex-910 improves the oxidation stability of MO, but reduces the oxidation stability of MEPKO. These results prove that methyl esters can be used as a substitute to replace mineral oils in power transformers. Furthermore, they show that NP can be used mainly in areas of transformer where solid insulation is subjected to high thermal and electrical stress, and TUK other places where solid insulation is required. Such combination could assure money savings and a better preservation of the oil viscosity.展开更多
基金provided by the Scientific Research Foundation of the State Key Lab.of Coal Mine Disaster Dynamics and Control(No.2011DA105287-FW201509)the National Natural Science Foundation of China(No.51474211)the Innovation Team of CUMT(No.2014QN001)
文摘High-voltage thermal breakdown has great potential application in permeability enhancement of coal seam. The characteristics of the breakdown channel, coal element, porosity and microscopic coal petrography of coal under high-voltage electric load were experimentally studied. The coal interior left apparent tracks due to electric current burning with high temperature. The percentage of C, O, Al, Fe, and Si had slightly decreased, while the content of element N increased obviously. Low-pressure nitrogen gas adsorption(LP-N_2GA) and mercury intrusion analysis showed that coal porosity increased. The increases of micropores and mesopores are beneficial to promotion of the ability of gas storage, and the increase of macropores could enhance the gas seepage and migration. The results of scanning electron microscope(SEM) show that there are many exogenous fractures in coal, which is also beneficial to gas seepage and migration. The results lay a theoretical foundation for application of high-voltage thermal breakdown in coal mines.
基金supported by the National Key Laboratory Fund of Science and Technology on Vacuum Technology & Physics (Grant No.6142207030103)National Natural Science Foundation of China (Grant No.11702123)
文摘In order to study the influence of three-grid assembly thermal deformation caused by heat accumulation on breakdown times and an ion extraction process,a hot gap test and a breakdown time test are carried out to obtain thermal deformation of the grids when the thruster is in 5 k W operation mode.Meanwhile,the fluid simulation method and particle-in-cell-Monte Carlo collision(PICMCC) method are adopted to simulate the ion extraction process according to the previous test results.The numerical calculation results are verified by the ion thruster performance test.The results show that after about 1.2 h operation,the hot gap between the screen grid and the accelerator grid reduce to 0.25–0.3 mm,while the hot gap between the accelerator grid and the decelerator grid increase from 1 mm to about 1.4 mm when the grids reach thermal equilibrium,and the hot gap is almost unchanged.In addition,the breakdown times experiment shows that 0.26 mm is the minimal safe hot gap for the grid assembly as the breakdown times improves significantly when the gap is smaller than this value.Fluid simulation results show that the plasma density of the screen grid is in the range 6?×10^(17)–6?×?10^(18) m^(13) and displays a parabolic characteristic,while the electron temperature gradually increases along the axial direction.The PIC-MCC results show that the current falling of an ion beam through a single aperture is significant.Meanwhile,the intercepted current of the accelerator grid and the decelerator grid both increase with the change in the hot gap.The ion beam current has optimal perveance status without thermal deformation,and the intercepted current of the accelerator grid and the decelerator grid are 3.65 m A and 6.26 m A,respectively.Furthermore,under the effect of thermal deformation,the ion beam current has over-perveance status,and the intercepted current of the accelerator grid and the decelerator grid are 10.46 m A and 18.24 m A,respectively.Performance test results indicate that the breakdown times increase obviously.The intercepted current of the accelerator grid and the decelerator grid increases to 13 m A and 16.5 m A,respectively,due to the change in the hot gap after 1.5 h operation.The numerical calculation results are well consistent with performance test results,and the error comes mainly from the test uncertainty of the hot gap.
基金supported by the National Natural Science Foundation of China(Grant Nos.11305263 and 61401484)
文摘The carbon nanotube (CNT)-based materials can be used as vacuum device cathodes. Owing to the excellent field emission properties of CNT, it has great potentials in the applications of an explosive field emission cathode. The falling off of CNT from the substrate, which frequently appears in experiments, restricts its application. In addition, the onset time of vacuum breakdown limits the performance of the high-power explosive-emission-cathode-based diode. In this paper, the characteristics of the CNT, electric field strength, contact resistance and the kind of substrate material are varied to study the parameter effects on the onset time of vacuum breakdown and failure mechanism of the CNT by using the finite element method.
文摘A significant number of fire-induced power disruptions are observed in several countries every year. The faults are normally phase-to-phase short circuiting or conductor-to-ground discharges at mid-span region of the high-voltage transmission system. In any case, the wildfire plumes provide a conductive path. The electrical conductivity is due to intense heat in combustion zone of the fire which creates ion and electrons from flame inherent particulates. Increase in the ion concentration increases the electrical conductivity of the fire plume. The main purpose of this study was to measure dielectric breakdown electric field for vegetation and hydrocarbon flames. The experimental data is needed for validation of simulation schemes which are necessary for evaluation of power grid systems reliability under extreme wildfire weather conditions. In this study, hydrocarbon and vegetation fuels were ignited in a cylindrically shaped steel burner which was fitted with type-K thermocouples to measure flame temperature. The fuels consisted of dried weeping wattle (Peltophorum africanum) litter, butane gas and candle wax. Two pinned copper electrodes supported by retort stands were mounted to the burner and energized to a high voltage. This generated a strong electric field sufficient to initiate dielectric breakdown in the flames. Breakdown electric field strength (Ecrit) obtained from the experiment decreased from 10.5 to 6.9 kV/cm for the flames with temperature range of 1003 to 1410 K, respectively.
文摘The purpose of this work is to determine the impact of thermal aging on the dielectric and physicochemical properties of the oil/paper mixed insulation. We performed a comparative analysis of dielectric paper dipped in two cooling fluids: palm kernel oil methyl ester (MEPKO) and mineral oil (MO). Two types of dielectric paper were used: Thermally Upgraded Kraft paper (TUK) and Nomex-910 paper (NP-910). An accelerated aging test was realized at 110<span style="white-space:nowrap;">°</span>C during a total of 96 hours. Samples of oil and paper were collected after 0, 48, 72 and 96 hours for analyses purposes. The analyses performed included the measurement of the Breakdown voltage (BDV) of the dielectric papers, the Total Acid Number (TAN) and the Decay Dissolved Products (DDP) of the liquid dielectrics. The BDV of NP-910 is greater than the BDV of TUK. Concerning the type of oil, the BDV of dielectric papers impregnated with MEPKO is greater than the BDV of similar papers impregnated with MO, indicating a better preservation of paper when dipped in methyl esters. The analyses of TAN and DDP revealed that Nomex-910 improves the oxidation stability of MO, but reduces the oxidation stability of MEPKO. These results prove that methyl esters can be used as a substitute to replace mineral oils in power transformers. Furthermore, they show that NP can be used mainly in areas of transformer where solid insulation is subjected to high thermal and electrical stress, and TUK other places where solid insulation is required. Such combination could assure money savings and a better preservation of the oil viscosity.