Integrated Equipment Health Prognosis Considering Crack Initiation Time Uncertainty and Random Shock 被引量:2
1
作者 Fu-Qiong Zhao Ming-Jiang Xie +1 位作者 Zhi-Gang Tian Yong Zeng 《Chinese Journal of Mechanical Engineering》 SCIE EI CAS CSCD 2017年第6期1383-1395,共13页
With integrated equipment health prognosis, both physical models and condition monitoring data are utilized to achieve more accurate prediction of equipment remaining useful life (RUL). In this paper, an integrated ... With integrated equipment health prognosis, both physical models and condition monitoring data are utilized to achieve more accurate prediction of equipment remaining useful life (RUL). In this paper, an integrated prognostics method is proposed to account for two important factors which were not considered before, the uncertainty in crack initiation time (CIT) and the shock in the degradation. Prognostics tools are used for RUL pre- diction starting from the CIT. However, there is uncertainty in CIT due to the limited capability of existing fault detection tools, and such uncertainty has not been explic- itly considered in the literature for integrated prognosis. A shock causes a sudden damage increase and creates a jump in the degradation path, which shortens the total lifetime, and it has not been considered before in the integrated prognostics framework either. In the proposed integrated prognostics method, CIT is considered as an uncertain parameter, which is updated using condition monitoring data. To deal with the sudden damage increase and reduction of total lifetime, a virtual gradual degradation path with an earlier CIT is introduced in the proposed method. In this way, the effect of shock is captured through identifying an appropriate CIT. Examples of gear prog- nostics are given to demonstrate the effectiveness of the proposed method. 展开更多
关键词 crack initiation time Shock Uncertaintyquantification Integrated prognostics Failure timeprediction Bayesian inference GEARS Fatigue crack
下载PDF
Simultaneously measuring initiation toughness of pure mode Ⅰ and mode Ⅱ cracks subjected to impact loads
2
作者 LANG Lin ZHU Zhe-ming +3 位作者 ZHOU Chang-lin ZHOU Lei WANG Meng WANG Lu 《Journal of Central South University》 SCIE EI CAS CSCD 2022年第11期3720-3731,共12页
In order to simultaneously measure the initiation toughness of pure mode Ⅰ and mode Ⅱ cracks in one specimen,a large-size double-cracked concave-convex plate(DCCP)specimen configuration was proposed.Impacting tests ... In order to simultaneously measure the initiation toughness of pure mode Ⅰ and mode Ⅱ cracks in one specimen,a large-size double-cracked concave-convex plate(DCCP)specimen configuration was proposed.Impacting tests were implemented in the drop plate impact device.Strain gauges were employed to measure impact loads and crack initiation time.The corresponding numerical model was established by using the dynamic finite difference program AUTODYN,and the experimental-numerical method and ABAQUS code were utilized to obtain the initial fracture toughness of the crack.Using experiments and numerical research,we concluded that the DCCP specimen is suitable for measuring the initial fracture toughness of pure mode Ⅰ and mode Ⅱ cracks at the same time;the dynamic initiation toughness increases with the increase of loading rate and the crack initiation time decreases with increasing loading rate;the initiation toughness of mode Ⅱ crack is 0.5 times that of mode Ⅰ crack when subjected to the same loading rate.For the pre-crack in the vicinity of the bottom of a sample,when its length increases from 20 to 100 mm,the dynamic initiation toughness of the pure mode Ⅰ crack gradually decreases,and the longer the lower crack length is,the easier the crack would initiate,but the dynamic initiation toughness of pure mode Ⅱ crack varies little. 展开更多
关键词 initiation toughness crack initiation time mode crack mode crack impact loads
下载PDF
飞机典型结构当量初始缺陷尺寸分布模型研究
3
作者 冯浩凌 许希武 +1 位作者 古兴瑾 俞晓楠 《南京航空航天大学学报》 CAS CSCD 北大核心 2024年第3期438-446,共9页
利用结构耐久性分析技术可以在保证飞机结构可靠性的同时,有效提高飞机结构的经济性。应用结构耐久性分析技术,对某型飞机飞行载荷谱作用下一种7B04-T651高强铝合金典型疲劳结构的原始疲劳质量(Initial fatigue qualit,IFQ)进行了研究... 利用结构耐久性分析技术可以在保证飞机结构可靠性的同时,有效提高飞机结构的经济性。应用结构耐久性分析技术,对某型飞机飞行载荷谱作用下一种7B04-T651高强铝合金典型疲劳结构的原始疲劳质量(Initial fatigue qualit,IFQ)进行了研究。开展了3级不同应力水平下的飞行载荷谱疲劳试验研究;利用极大似然估计法处理基于三参数Weibull分布的裂纹萌生时间分布的参数估计问题,利用蒙特卡罗法对比验证了该方法的正确性,提出使用对数样本矩处理当量初始缺陷尺寸(Equivalent initial flaw size,EIFS)分布以获取通用当量初始缺陷尺寸分布模型;建立描述该典型结构的原始疲劳质量模型,验证其当量初始缺陷尺寸小于许用规定的0.125mm;最后通过对该典型结构的原始疲劳质量分析,验证了通用化方法的正确性和实用性,并且建立了结构在不同应力区、不同指定裂纹尺寸和不同可靠度下的寿命估计模型。 展开更多
关键词 原始疲劳质量 裂纹萌生时间 当量初始缺陷尺寸 极大似然估计 铝合金
下载PDF
含埋藏裂纹结构的拘束效应和蠕变裂纹孕育期研究
4
作者 李宇鹏 李文彭 +3 位作者 李顶河 邬栋权 王宇峰 郑宇翔 《机械强度》 CAS CSCD 北大核心 2024年第2期461-467,共7页
以含埋藏椭圆形裂纹的高温试样结构为研究对象,基于延性耗散模型,用三维(3D)有限元方法对其拘束效应和蠕变裂纹孕育期进行了研究。结果表明,对于裂尖前沿拘束水平,拘束参量Q的最大值总是分布在椭圆形裂纹的长轴端点处,且随着裂纹横向长... 以含埋藏椭圆形裂纹的高温试样结构为研究对象,基于延性耗散模型,用三维(3D)有限元方法对其拘束效应和蠕变裂纹孕育期进行了研究。结果表明,对于裂尖前沿拘束水平,拘束参量Q的最大值总是分布在椭圆形裂纹的长轴端点处,且随着裂纹横向长度c和纵向长度a的增加,拘束参量Q越大,意味着应力集中越严重,该处位置更为危险;对于蠕变裂纹孕育期,椭圆形裂纹深度比a/t越大或长度比a/c越小,或者载荷越大,则蠕变裂纹损伤率越高,结构发生蠕变裂纹萌生的孕育期越短,结构越危险。此外,建立了拘束参量和蠕变裂纹孕育期的预测公式和工程计算方法,并验证了蠕变裂纹孕育期工程计算模型的有效性。 展开更多
关键词 埋藏裂纹 蠕变孕育期 延性耗散模型 蠕变损伤 拘束效应
下载PDF
Analytical study of subcritical crack growth under mode I loading to estimate the roof durability in underground excavation 被引量:3
5
作者 Songtao Ji Zeng Wang Jurij Karlovšek 《International Journal of Mining Science and Technology》 SCIE EI CAS CSCD 2022年第2期375-385,共11页
The long-term stability of the roof is particularly important in designing underground rock structures.To estimate the durability of roof strata in underground excavation,a computation scheme of subcritical crack grow... The long-term stability of the roof is particularly important in designing underground rock structures.To estimate the durability of roof strata in underground excavation,a computation scheme of subcritical crack growth is proposed in this study.By adopting the proposed method,the potential collapse location of strata is derivable in accordance with a static model,the durability of roof strata can be estimated,a dynamic time step control strategy is achieved to balance the accuracy and speed of computing,and the initial crack size of rock can be estimated.In addition to the above,a mechanical model of underground excavation with non-uniformly distributed loads and partially yielded foundation is presented as the prototypical case.A set of case studies is carried out that showcase a power correlation between applied stress and roof durability.The allowable applied tensile stress for a 100-year life cycle is about 76%of the tensile strength.By using the proposed subcritical crack growth computation scheme,the roof stability in an underground excavation can be identified not only from the spatial view but also from the temporal perspective. 展开更多
关键词 Roof durability Analytical model Subcritical crack growth Stress intensity factor initial crack size Dynamic time step
下载PDF
Shrinkage and Cracking Sensitivity of Cement Mortar Containing Fly Ash, Granulated Blast-furnace Slag and Silica Fume
6
作者 胡利民 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2006年第z1期136-139,共4页
A laboratory study was undertaken to investigate drying shrinkage and cracking sensitivity subjected to restrained shrinkage of mortar containing fly ash (FA), granulated blast-furnace slag (GBFS) and silica fume (SF)... A laboratory study was undertaken to investigate drying shrinkage and cracking sensitivity subjected to restrained shrinkage of mortar containing fly ash (FA), granulated blast-furnace slag (GBFS) and silica fume (SF). Six mortar mixtures including control Portland cement (PC) and FA, GBFS and SF mortar mixtures were prepared. FA replaced the cement on mass basis at the replacement ratios of 20% and 35%, GBFS replaced the cement at the replacement ratios of 40%, SF replaced the cement at the replacement ratios of 8% and the blended mixtures with 20% FA, 20% GBFS and 8% SF. Water-cementitious materials ratio and sand-cementitious materials ratio were 0.4 and 2.0 for all mixtures, respectively. The mixtures were cured at 65% relative humidity and 20℃. The drying shrinkage value, initial cracking time and cracking width of the mortar samples were measured. The results show that all the mortar mixture containing FA exhibited the decrease of drying shrinkage. Moreover, initial cracking time was markedly delayed, and the crack width of the initial crack was reduced. However, the incorporations of various ratios of GBFS and SF led to an increase of drying shrinkage, initial cracking time and cracking width as compared to control mixture. 展开更多
关键词 drying shrinkage cracking sensitivity cement mortar initial cracking time crack width
下载PDF
国产P92钢的蠕变裂纹扩展行为研究 被引量:1
7
作者 侍克献 田根起 +2 位作者 张作贵 谈建平 刘长军 《压力容器》 北大核心 2023年第6期1-6,14,共7页
对国产P92钢开展了600℃蠕变试验,得到了蠕变变形曲线、蠕变指数和蠕变延性等,再在600℃进行蠕变裂纹扩展行为试验研究,得到了蠕变裂纹萌生时间和蠕变裂纹扩展速率与蠕变断裂力学参量C^(*)的关系,将国产P92钢的性能与BS 7910数据进行比... 对国产P92钢开展了600℃蠕变试验,得到了蠕变变形曲线、蠕变指数和蠕变延性等,再在600℃进行蠕变裂纹扩展行为试验研究,得到了蠕变裂纹萌生时间和蠕变裂纹扩展速率与蠕变断裂力学参量C^(*)的关系,将国产P92钢的性能与BS 7910数据进行比较,评估NSW模型的预测效果,计算得到材料的蠕变断裂韧性。结果表明,蠕变裂纹萌生时间和蠕变裂纹扩展速率与蠕变断裂力学参量C^(*)之间有较好的双对数线性相关性。国产P92钢的蠕变裂纹扩展性能优于BS 7910中9%Cr钢的平均性能,NSW模型的平面应力预测结果与试验数据接近,材料的蠕变断裂韧性随着服役时间的增大逐渐降低。该研究结果可以用于评估长期服役高温结构的安全性。 展开更多
关键词 P92钢 蠕变裂纹萌生时间 蠕变裂纹扩展 NSW模型 蠕变断裂韧性
下载PDF
矿渣微粉掺量对混凝土收缩开裂的影响 被引量:37
8
作者 梁文泉 王信刚 +3 位作者 何真 马保国 叶群山 彭卫兵 《武汉大学学报(工学版)》 CAS CSCD 北大核心 2004年第1期77-81,共5页
收缩开裂是现代混凝土劣化的重要原因.采用改进的椭圆环收缩开裂试验、自由收缩和抗折强度试验,以及不同养护条件下混凝土抗压强度对比试验来综合评价矿渣微粉掺量对混凝土收缩开裂的影响.结果表明,矿渣微粉掺量为40%~50%时,胶砂初始... 收缩开裂是现代混凝土劣化的重要原因.采用改进的椭圆环收缩开裂试验、自由收缩和抗折强度试验,以及不同养护条件下混凝土抗压强度对比试验来综合评价矿渣微粉掺量对混凝土收缩开裂的影响.结果表明,矿渣微粉掺量为40%~50%时,胶砂初始开裂时间明显增长,混凝土自由收缩减小,混凝土早期收缩开裂性能显著改善,混凝土抗压强度达到最高;标准养护条件比干燥养护条件对矿渣微粉混凝土强度的发展更有利. 展开更多
关键词 矿渣微粉 初始开裂时间 收缩开裂 自由收缩 养护条件
下载PDF
矿渣、粉煤灰掺量对混凝土收缩、开裂性能的研究 被引量:23
9
作者 乔艳静 费治华 +1 位作者 田倩 刘加平 《长江科学院院报》 CSCD 北大核心 2008年第4期90-92,96,共4页
收缩、开裂是影响现代混凝土耐久性的主要因素,为评价掺合料对混凝土收缩、开裂的影响,通过圆环开裂试验、收缩试验来评定矿物掺和料对混凝土收缩开裂的性能。圆环开裂试验主要表征混凝土试件在约束条件下抵抗干燥收缩应力的能力,收缩... 收缩、开裂是影响现代混凝土耐久性的主要因素,为评价掺合料对混凝土收缩、开裂的影响,通过圆环开裂试验、收缩试验来评定矿物掺和料对混凝土收缩开裂的性能。圆环开裂试验主要表征混凝土试件在约束条件下抵抗干燥收缩应力的能力,收缩试验则表征试件的体积变形,收缩是开裂的原因,也是影响开裂的最重要因素。结果表明矿渣掺量在一定范围内时可抑制混凝土的开裂,混凝土的自收缩随矿渣掺量的增大而增大,干缩随矿渣掺量的增大而减小。粉煤灰可有效抑制混凝土的开裂,随掺量的增大抑制作用越显著;粉煤灰掺量越大对自收缩的抑制作用越明显,混凝土的干缩略有增大。总的来看,粉煤灰较矿渣可更好地抑制混凝土的收缩与开裂。 展开更多
关键词 粉煤灰 矿渣微粉 初始开裂时间 自收缩 裂缝宽度 干缩
下载PDF
掺高效减水剂水泥砂浆的早期开裂研究 被引量:23
10
作者 马保国 王信刚 +3 位作者 梁文泉 李相国 何真 叶群山 《建筑材料学报》 EI CAS CSCD 2005年第6期593-598,共6页
采用多通道椭圆环收缩开裂试验、自由收缩试验和强度试验综合评价了萘系(UNF)、聚羧酸类(PC)高效减水剂对水泥砂浆体积稳定性及早期开裂的影响.结果表明,高效减水剂的掺入延长了水泥砂浆的初始开裂时间,从而降低了水泥砂浆的开裂敏感性... 采用多通道椭圆环收缩开裂试验、自由收缩试验和强度试验综合评价了萘系(UNF)、聚羧酸类(PC)高效减水剂对水泥砂浆体积稳定性及早期开裂的影响.结果表明,高效减水剂的掺入延长了水泥砂浆的初始开裂时间,从而降低了水泥砂浆的开裂敏感性.高效减水剂降低水泥砂浆开裂敏感性的效果为:聚羧酸类>高浓型萘系>普通型萘系.掺高效减水剂均增大了水泥砂浆的自由收缩值,且水泥砂浆自由收缩值随着高效减水剂掺量的增加而增大.高效减水剂控制水泥砂浆体积稳定性的效果为:聚羧酸类>普通型萘系>高浓型萘系.聚羧酸类高效减水剂的掺入减小了水泥砂浆的最大裂纹宽度,而萘系高效减水剂的掺入则加快了水泥砂浆最大裂纹宽度的发展速度.在干燥养护条件下,掺聚羧酸类高效减水剂比掺萘系高效减水剂更能有效地提高水泥砂浆28 d的强度. 展开更多
关键词 高效减水剂 早期开裂 体积稳定性 初始开裂时间
下载PDF
单轴压缩作用下内置裂隙扩展的CT扫描试验 被引量:72
11
作者 李术才 李廷春 +1 位作者 王刚 白世伟 《岩石力学与工程学报》 EI CAS CSCD 北大核心 2007年第3期484-492,共9页
精选出一种与岩石较为接近的相似材料制作标准试件,并在其内部预置单币状裂隙,进行加载过程中的CT实时扫描试验。通过分析CT扫描图像,初步判定试件的破坏是由裂隙的损伤演化造成的。采用多种区域划分的方法,通过CT数及CT方差的对比分析... 精选出一种与岩石较为接近的相似材料制作标准试件,并在其内部预置单币状裂隙,进行加载过程中的CT实时扫描试验。通过分析CT扫描图像,初步判定试件的破坏是由裂隙的损伤演化造成的。采用多种区域划分的方法,通过CT数及CT方差的对比分析,获得随载荷的不断增加裂隙被压密、自相似扩展、翼裂纹扩展、微裂纹扩展、裂纹汇合贯通以及裂纹加速扩展、试件崩裂的损伤演化过程;同时,也得到初裂强度、翼裂纹扩展长度和自相似扩展长度等一些重要参数;将试件破坏前的应力、应变过程曲线分为4段,说明预置裂隙的损伤演化过程。 展开更多
关键词 岩石力学 内置裂隙 扩展规律 CT实时试验
下载PDF
分布式光纤传感器裂缝传感模型试验(英文) 被引量:5
12
作者 丁睿 刘浩吾 +1 位作者 罗凤林 牟廷敏 《四川大学学报(工程科学版)》 EI CAS CSCD 2004年第3期24-27,共4页
基于光时域反射技术及瑞利散射,构建全自动控制的高精度力-光耦合试验系统,进行了分布式光纤传感器裂缝传感模型试验,研究了混凝土模型力-光本构关系,试验中组合传感光纤初始感知缝宽达0.1mm,光纤传感动态范围达5.3mm,定位精度达到0.2m... 基于光时域反射技术及瑞利散射,构建全自动控制的高精度力-光耦合试验系统,进行了分布式光纤传感器裂缝传感模型试验,研究了混凝土模型力-光本构关系,试验中组合传感光纤初始感知缝宽达0.1mm,光纤传感动态范围达5.3mm,定位精度达到0.2m,并根据试验数据拟合出半经验公式。 展开更多
关键词 分布式光纤传感器 光时域反射技术 瑞利散射 衰减
下载PDF
减缩剂对水泥基材料早期水化及收缩变形性能的影响 被引量:19
13
作者 陈美祝 周明凯 +1 位作者 吴少鹏 何真 《武汉大学学报(工学版)》 CAS CSCD 北大核心 2007年第1期78-82,共5页
采用非接触式电阻率测定仪和半绝热实验方法分别研究了减缩剂对常温和半绝热条件下的水泥浆体早期水化的电阻率和温升的影响,对比研究了减缩剂对水泥砂浆在干燥条件和常温水中养护时的线性长度变化与强度发展情况的影响,应用五路裂缝测... 采用非接触式电阻率测定仪和半绝热实验方法分别研究了减缩剂对常温和半绝热条件下的水泥浆体早期水化的电阻率和温升的影响,对比研究了减缩剂对水泥砂浆在干燥条件和常温水中养护时的线性长度变化与强度发展情况的影响,应用五路裂缝测定仪研究了减缩剂在水泥砂浆中的抗裂效果.结果表明:在常温条件下减缩剂会延缓水泥早期水化,而在半绝热条件下则会加速水泥早期水化;减缩剂主要提高干燥环境下的水泥砂浆的抗裂性能,降低其线性收缩值与强度增长,推迟其约束收缩初始开裂时间,而对水中养护的砂浆无补偿收缩效应,因此不利于控制热裂缝.分析表明,减缩剂在水泥基材料中应用时不仅具有物理作用,而且具有化学作用. 展开更多
关键词 水泥基材料 减缩剂 早期水化 自由收缩 初始开裂时间
下载PDF
减水剂对砂浆早期开裂行为的影响 被引量:4
14
作者 马保国 王信刚 +3 位作者 李相国 高小建 董荣珍 朱洪波 《哈尔滨工业大学学报》 EI CAS CSCD 北大核心 2006年第8期1288-1291,共4页
采用多通道椭圆环收缩开裂测试手段、自由收缩和强度试验综合评价了聚羧酸类、萘系和木质素系减水剂对水泥砂浆早期收缩开裂和强度的影响.结果表明,掺减水剂均延长了砂浆初始开裂时间,从而降低了砂浆的开裂敏感性.就减水剂降低砂浆开裂... 采用多通道椭圆环收缩开裂测试手段、自由收缩和强度试验综合评价了聚羧酸类、萘系和木质素系减水剂对水泥砂浆早期收缩开裂和强度的影响.结果表明,掺减水剂均延长了砂浆初始开裂时间,从而降低了砂浆的开裂敏感性.就减水剂降低砂浆开裂敏感性而言,聚羧酸类和高浓型萘系高效减水剂是行之有效的.掺聚羧酸类和掺木质素系减水剂都减小了砂浆的最大裂纹宽度,而掺萘系则加快了砂浆最大裂纹宽度的发展速度.掺高效减水剂均增大了砂浆自由收缩值,且萘系比聚羧酸类减水剂更能增大砂浆自由收缩值,而掺木质素系减水剂能稍微降低砂浆的自由收缩值.在干燥养护条件下,掺高效减水剂比掺木质素系减水剂更能有效地提高砂浆抗折和抗压强度,且掺聚羧酸类减水剂又比掺萘系高效减水剂更为有效. 展开更多
关键词 减水剂 收缩开裂 椭圆环试验 初始开裂时间
下载PDF
单轴压缩载荷作用下双裂隙扩展的CT扫描试验 被引量:23
15
作者 李廷春 吕海波 王辉 《岩土力学》 EI CAS CSCD 北大核心 2010年第1期9-14,共6页
由于精选后的陶瓷材料与岩石性质相似,因此选择陶瓷作为基本材料制作中部含2条圆币状裂隙的试件,进行单轴压缩荷载作用下的CT实时扫描试验,研究试件内双裂隙的扩展和损伤演化规律。采用3种不同区域划分方案,通过CT数、CT方差和CT图像的... 由于精选后的陶瓷材料与岩石性质相似,因此选择陶瓷作为基本材料制作中部含2条圆币状裂隙的试件,进行单轴压缩荷载作用下的CT实时扫描试验,研究试件内双裂隙的扩展和损伤演化规律。采用3种不同区域划分方案,通过CT数、CT方差和CT图像的对比,分析上、下裂隙及岩桥区域不同的扩展状况。分析表明,上裂隙区域一直以压密为主,扩展很小,对试件破坏影响较小;下裂隙区域扩展剧烈,最终形成了宏观裂纹,对试件的破坏影响较大;当上下裂隙之间的中心距离等于4倍的裂隙半径时,裂隙的扩展过程将与裂隙自身参数有关,几乎看不出裂隙之间的相互作用。 展开更多
关键词 单轴压缩 内置双裂隙 扩展规律 CT实时试验
下载PDF
用应变片法确定混凝土动态起裂时间的研究 被引量:17
16
作者 樊鸿 张盛 王启智 《振动与冲击》 EI CSCD 北大核心 2010年第1期153-156,共4页
在混凝土等准脆性材料的动态起裂韧度K_(1d)测试中,准确确定试件裂尖的起裂时间是测试工作的关键。采用分离式霍普金森压杆系统,对圆孔裂纹平台巴西圆盘混凝土试件进行动态径向冲击试验,通过在裂尖粘贴应变片的方法来确定起裂时间。讨... 在混凝土等准脆性材料的动态起裂韧度K_(1d)测试中,准确确定试件裂尖的起裂时间是测试工作的关键。采用分离式霍普金森压杆系统,对圆孔裂纹平台巴西圆盘混凝土试件进行动态径向冲击试验,通过在裂尖粘贴应变片的方法来确定起裂时间。讨论了应变片在裂纹尖端的粘贴位置、粘贴方向等因素对起裂时间测试值的影响,结果表明裂尖应变片的最佳粘贴方式是:在裂纹延长线上或在裂尖并与裂纹垂直的线上,都距离裂尖3 mm左右,且粘贴方向与裂纹延长线垂直。给出了考虑贴片位置和试件厚度的起裂时间计算公式。 展开更多
关键词 动态起裂韧度 起裂时间 应变片法 圆孔裂纹平台巴西圆盘 混凝土
下载PDF
30CrMnSiNi2A钢疲劳裂纹形成寿命表征与预测 被引量:2
17
作者 黄宏发 阎海 陶春虎 《材料工程》 EI CAS CSCD 北大核心 1997年第5期6-8,共3页
采用耐久性分析方法 ,由断口金相数据得到参考裂纹扩展时间 (TTCI)的概率分布函数 ,由 TTCI概率分布函数和约束条件得到了通用当量初始缺陷尺寸 (EIFS)的概率分布函数。
关键词 裂纹形成时间 初始缺陷尺寸 疲劳裂纹
下载PDF
面向残余应力检测的聚碳酸酯在溶剂环境下的初始应力-开裂时间关系 被引量:3
18
作者 韩健 闫辰光 +4 位作者 王一麦 张军利 张永亮 刘春太 申长雨 《材料科学与工程学报》 CAS CSCD 北大核心 2019年第1期47-50,共4页
本研究利用四点弯曲应力松弛实验装置,获得了聚碳酸酯(PC)材料在不同比例甲苯/正丁醇混合溶剂中的初始应力-开裂时间实验数据;依据离散数据的几何相似性,建立了一个指数关系模型,拟合得到了初始应力-开裂时间的连续分布,并基于对拟合曲... 本研究利用四点弯曲应力松弛实验装置,获得了聚碳酸酯(PC)材料在不同比例甲苯/正丁醇混合溶剂中的初始应力-开裂时间实验数据;依据离散数据的几何相似性,建立了一个指数关系模型,拟合得到了初始应力-开裂时间的连续分布,并基于对拟合曲线的抽样误差分析,建立了残余应力与初始应力之间的关系式,可用于提高PC制品残余应力的检测精度。 展开更多
关键词 聚碳酸酯 环境应力开裂 残余应力 初始应力-开裂时间
下载PDF
水泥基材料中高效减水剂应用效果的检测方法 被引量:6
19
作者 陈美祝 周明凯 李北星 《武汉理工大学学报》 EI CAS CSCD 北大核心 2007年第4期1-4,共4页
采用水泥浆体流动度、混凝土减水率、坍落度及强度增长率等指标确定了2种萘系高效减水剂的掺量,研究了二者在此掺量下对相同配比砂浆的流动度及经时损失、开裂敏感性及干湿变形的影响。结果表明:与水泥适应性均较好的2种萘系高效减水剂... 采用水泥浆体流动度、混凝土减水率、坍落度及强度增长率等指标确定了2种萘系高效减水剂的掺量,研究了二者在此掺量下对相同配比砂浆的流动度及经时损失、开裂敏感性及干湿变形的影响。结果表明:与水泥适应性均较好的2种萘系高效减水剂在各自掺量下,所配制的砂浆具有相同的初始流动度及流动度经时损失变化,但其初始开裂时间与干湿变形却存在差异,说明在评价高效减水剂的应用效果时除了检测与水泥的相容性外还应考虑其对水泥基材料收缩变形性能的影响;不同外加剂对水泥基材料体系碱度的适应能力不同,较高的碱度会增加材料的开裂敏感性。 展开更多
关键词 水泥基材料 高效减水剂 应用效果 初始开裂时间
下载PDF
全循环周期和保载时间对P91钢蠕变-疲劳裂纹扩展行为的影响 被引量:3
20
作者 刘长军 闫阿晨 +3 位作者 谈建平 秦敬芳 张静 王东辉 《动力工程学报》 CAS CSCD 北大核心 2019年第11期947-952,共6页
在620℃下对P91钢进行了蠕变-疲劳裂纹扩展试验,研究了全循环周期对裂纹起裂时间的影响,并讨论了不同保载时间下的裂纹扩展规律。结果表明:在单对数坐标下裂纹起裂时间与全循环周期呈线性关系;当全循环周期小于20 s时,裂纹起裂循环次数... 在620℃下对P91钢进行了蠕变-疲劳裂纹扩展试验,研究了全循环周期对裂纹起裂时间的影响,并讨论了不同保载时间下的裂纹扩展规律。结果表明:在单对数坐标下裂纹起裂时间与全循环周期呈线性关系;当全循环周期小于20 s时,裂纹起裂循环次数不随全循环周期变化;采用断裂参量ΔK表征裂纹扩展速率时,裂纹扩展速率随保载时间的增加而增大,但随ΔK的增大先减小后增大;断裂参量(Ct)avg可较好地关联不同保载时间的平均裂纹扩展速率。 展开更多
关键词 P91钢 蠕变 疲劳 全循环周期 保载时间 裂纹起裂时间 裂纹扩展性能
下载PDF