La2/3Sr1/3MnO3/La1.4Sr1.6Mn2O7 composites with arbitrary weight percentage were prepared using a one-step solid-state reaction method. The experimental results demonstrated that addition of K2CO3 during preparation fa...La2/3Sr1/3MnO3/La1.4Sr1.6Mn2O7 composites with arbitrary weight percentage were prepared using a one-step solid-state reaction method. The experimental results demonstrated that addition of K2CO3 during preparation favored the formation of the composites even though the K+ ions were volatilized under the high temperatures of sintering. Full quantitative analysis with the Rietveld method showed that the content of La1.4Sr1.6Mn2O7 phase decreased and the fraction of the La2/3Sr1/3MnO3 phase increased as the a...展开更多
基金Project supported by the High Technology Research and Development Program of China (2007AA03Z116)Natural Science Foundation of He-bei Province (E2008000194) Science Foundation of Hebei Education Department (2009133)
文摘La2/3Sr1/3MnO3/La1.4Sr1.6Mn2O7 composites with arbitrary weight percentage were prepared using a one-step solid-state reaction method. The experimental results demonstrated that addition of K2CO3 during preparation favored the formation of the composites even though the K+ ions were volatilized under the high temperatures of sintering. Full quantitative analysis with the Rietveld method showed that the content of La1.4Sr1.6Mn2O7 phase decreased and the fraction of the La2/3Sr1/3MnO3 phase increased as the a...