Effects of heat treatment on the microstructure and mechanical properties of ZA84 magnesium alloy 被引量:5
1
作者 Mingbo Yang Liang Bai +1 位作者 Fusheng Pan Hongjun Hu 《Journal of University of Science and Technology Beijing》 CSCD 2008年第6期747-752,共6页
The effects of heat treatment on the microstructure and mechanical properties of ZA84 (Mg-8Zn-4Al-0.25Mn) alloy were investigated. The results indicate that the as-cast microstructure of the alloy is mainly composed... The effects of heat treatment on the microstructure and mechanical properties of ZA84 (Mg-8Zn-4Al-0.25Mn) alloy were investigated. The results indicate that the as-cast microstructure of the alloy is mainly composed of α-Mg matrix and two different morphologies of precipitates (continuous and quasi-continuous Mg32(Al,Zn)49 phases and isolated Mg5Al2Zn2 phases). After solid solution treatment at 345℃, the Mg32(Al,Zn)49 phases change from continuous and quasi-continuous net to disconnected acute angle shape, and parts of second phases sphericize. The optimum heat treatment condition for the alloy is solution treatment at 345℃ for 48 h and water quenching, then aging treatment at 200℃ for 12 h and atmosphere cooling. Under the optimum condition, the ulti- mate tensile strength and yield strength of the alloy can be imoroved, but the elongation is not effected much bv heat treatment. 展开更多
关键词 za84 magnesium alloy heat treatment MICROSTRUCTURE mechanical properties PRECIPITATES
下载PDF
Effects of minor Sr, Sn and Sc addition on as-cast microstructure and mechanical properties of ZA84 magnesium alloy 被引量:2
2
作者 杨明波 朱翊 +1 位作者 潘复生 杨惠 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2010年第B07期306-310,共5页
The effects of minor Sr, Sn and Sc addition on the as-cast microstructure and mechanical properties of the ZA84 magnesium alloy were compared. The results indicate that addition of 0.1%Sr, 0.5%Sn or 0.3%Sc (mass fract... The effects of minor Sr, Sn and Sc addition on the as-cast microstructure and mechanical properties of the ZA84 magnesium alloy were compared. The results indicate that addition of 0.1%Sr, 0.5%Sn or 0.3%Sc (mass fraction) to the ZA84 alloy can refine the grains of the alloy. Furthermore, addition of 0.1%Sr to the ZA84 alloy does not obviously change the morphology and distribution of Mg32(Al,Zn)49 phase. However, addition of 0.5%Sn or 0.3%Sc not only refines and modifies the Mg32(Al,Zn)49 phase but also suppresses the formation of Mg32(Al,Zn)49 phase, especially with the addition of 0.3%Sc. Furthermore, addition of 0.1%Sr, 0.5%Sn or 0.3%Sc to the ZA84 alloy improves the tensile properties at room temperature and 150℃, especially with the addition of 0.1%Sr and 0.3%Sc. However, addition of 0.1%Sr is not beneficial to the creep properties, and addition of 0.5%Sn has no obvious influence on the creep properties. Oppositely, addition of 0.3%Sc to the ZA84 alloy greatly improves the creep properties. 展开更多
关键词 magnesium alloy za84 magnesium alloy SR SN SC
下载PDF
As-cast Microstructure,Mechanical Properties and Casting Fluidity of ZA84 Magnesium Alloy Containing TiC
3
作者 杨明波 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2008年第6期854-858,共5页
The as-cast microstructure, mechanical properties and casting fluidity of ZA84 alloy containing TiC were investigated. The experimental results indicate that adding 0.5wt%TiC to ZA84 alloy can refine the as-cast micro... The as-cast microstructure, mechanical properties and casting fluidity of ZA84 alloy containing TiC were investigated. The experimental results indicate that adding 0.5wt%TiC to ZA84 alloy can refine the as-cast microstructure, and do not cause the formation of any new phase. After 0.5wt%TiC was added to the ZA84 alloy, the morphology of ternary phases on the grain boundaries changed from coarse quasi-continuous net to fine disconnected net, and the distribution of ternary phases became dispersive and homogeneous. At the same time, the tensile properties of ZA84+0.5TiC alloy at room temperature were comparable to those of AZ91D alloy, and were higher than those of ZA84 alloy. At 150 ℃, the tensile and creep properties of ZA84+0.5TiC alloy were also higher than those of ZA84 and AZ91D alloys. In addition, compared with the AZ91D alloy, the casting fluidity of ZA84+0.5TiC alloy was slightly poor, but better than that of ZA84 alloy. The reason could be related to the effect of TiC on the solidification temperature range of ZA84 alloy. 展开更多
关键词 elevated temperature magnesium alloy Mg-Zn-Al alloys za84 magnesium alloy TIC