Through the comparison of calcination conditions between cement preclinkering technology and cement precalcining technology,we studied the characteristics of temperature field distribution of cement preclinkering tech...Through the comparison of calcination conditions between cement preclinkering technology and cement precalcining technology,we studied the characteristics of temperature field distribution of cement preclinkering technology systems including cyclone preheater,preclinkering furnace,and rotary kiln.We used numericalsimulation method to obtain data of temperature field distribution.Some results are found by system study.The ratio of tailcoalof cement preclinkering technology is about 70%,and raw mealtemperature can reach 1070 ℃.Shorter L/D kiln type of preclinkering technology can obtain more stable calcining zone temperature.The highest solid temperature of cement preclinkering technology is higher than 80 ℃,and high temperature region(〉1450 ℃)length is 2 times,which is beneficialfor calcining clinker and higher clinker quality.So cement preclinkering technology can obtain more performance temperature filed,which improves both the solid-phase reaction and liquid-phase reaction.展开更多
基金Funded by the Major State Basic Research Perelopment Program of China(973 Program)(No.2009CB623102)the Key Fund Project of Sichuan Provincial Department of Education(No.14ZA0086)the Key Fund Project of Professional Scientific Research Innovation Team of Southwest University of Science and Technology(No.14tdfk01)
文摘Through the comparison of calcination conditions between cement preclinkering technology and cement precalcining technology,we studied the characteristics of temperature field distribution of cement preclinkering technology systems including cyclone preheater,preclinkering furnace,and rotary kiln.We used numericalsimulation method to obtain data of temperature field distribution.Some results are found by system study.The ratio of tailcoalof cement preclinkering technology is about 70%,and raw mealtemperature can reach 1070 ℃.Shorter L/D kiln type of preclinkering technology can obtain more stable calcining zone temperature.The highest solid temperature of cement preclinkering technology is higher than 80 ℃,and high temperature region(〉1450 ℃)length is 2 times,which is beneficialfor calcining clinker and higher clinker quality.So cement preclinkering technology can obtain more performance temperature filed,which improves both the solid-phase reaction and liquid-phase reaction.