It is generally accepted that carbonates can be subducted to the mantle depths,where they are reduced with iron metal to produce a diamond.In this work,we found that this is not always the case.The mantle carbonates f...It is generally accepted that carbonates can be subducted to the mantle depths,where they are reduced with iron metal to produce a diamond.In this work,we found that this is not always the case.The mantle carbonates from inclusions in diamonds show a wide range of cation compositions(Mg,Fe,Ca,Na,and K).Here we studied the reaction kinetics of these carbonates with iron metal at 6-6.5 GPa and 1000-1500℃.We found that the reduction of carbonate with Fe produces C-bearing species(Fe,Fe-C melt,Fe_(3)C,F e_(7)C_(3),C)and wüistite containing Na_(2)O,CaO,and MgO.The reaction rate constants(k=△x^(2)/2t)are log-linear relative to 1/T and their temperature dependences are determined to be k_(MgcO_(3))(m^(2)/s)=4.37×10^(-3)exp[-251(kJ/mol)/RT]k_(caMg(CO_(3))2)(m^(2)/s)=1.48×10^(-3)exp[-264(kJ/mol)/RT]k_(cacO_(3))(m^(2)/s)=3.06×10^(-5)exp[-245(kJ/mol)/RT]and k_(Na_(2)cO_(3))(m^(2)/s)=1.88×10^(-10)exp[-155(kJ/mol)/RT].According to obtained results at least,45-70 vol%of carbonates preserve during subduction down to the 660-km discontinuity if no melting occurs.The slab stagnation and warming,subsequent carbonate melting,and infiltration into the mantle saturated with iron metal are accompanied by a reduction of carbonate melt with Fe.The established sequence of reactivity of carbonates:FeCO_(3)≥MgCO_(3)>CaMg(CO_(3))2>CaCO_(3)>>Na_(2)CO_(3),where K_(2)CO_(3)does not react at all with iron metal,implies that during reduction carbonate melt with Fe evolves toward alkali-rich.The above conclusions are consistent with the findings of carbonates in inclusions in diamonds from the lower mantle and high concentrations of alkalis,particularly K,in mantle carbonatite melts entrapped by diamonds from kimberlites and placers worldwide.展开更多
基金Russian Science Foundation(project No 21-17-00024).
文摘It is generally accepted that carbonates can be subducted to the mantle depths,where they are reduced with iron metal to produce a diamond.In this work,we found that this is not always the case.The mantle carbonates from inclusions in diamonds show a wide range of cation compositions(Mg,Fe,Ca,Na,and K).Here we studied the reaction kinetics of these carbonates with iron metal at 6-6.5 GPa and 1000-1500℃.We found that the reduction of carbonate with Fe produces C-bearing species(Fe,Fe-C melt,Fe_(3)C,F e_(7)C_(3),C)and wüistite containing Na_(2)O,CaO,and MgO.The reaction rate constants(k=△x^(2)/2t)are log-linear relative to 1/T and their temperature dependences are determined to be k_(MgcO_(3))(m^(2)/s)=4.37×10^(-3)exp[-251(kJ/mol)/RT]k_(caMg(CO_(3))2)(m^(2)/s)=1.48×10^(-3)exp[-264(kJ/mol)/RT]k_(cacO_(3))(m^(2)/s)=3.06×10^(-5)exp[-245(kJ/mol)/RT]and k_(Na_(2)cO_(3))(m^(2)/s)=1.88×10^(-10)exp[-155(kJ/mol)/RT].According to obtained results at least,45-70 vol%of carbonates preserve during subduction down to the 660-km discontinuity if no melting occurs.The slab stagnation and warming,subsequent carbonate melting,and infiltration into the mantle saturated with iron metal are accompanied by a reduction of carbonate melt with Fe.The established sequence of reactivity of carbonates:FeCO_(3)≥MgCO_(3)>CaMg(CO_(3))2>CaCO_(3)>>Na_(2)CO_(3),where K_(2)CO_(3)does not react at all with iron metal,implies that during reduction carbonate melt with Fe evolves toward alkali-rich.The above conclusions are consistent with the findings of carbonates in inclusions in diamonds from the lower mantle and high concentrations of alkalis,particularly K,in mantle carbonatite melts entrapped by diamonds from kimberlites and placers worldwide.