Effect of Melt Superheating on the Morphology of MC Carbide in a Cast Ni-base Superalloy M963 被引量:3
1
作者 殷凤仕 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2002年第3期42-45,共4页
The effect of the melt superheating temperature on the as cast microstructure of a cast nickel base superalloy M963 has been investigated. The results show that the as cast microstructure of the alloy consists of ... The effect of the melt superheating temperature on the as cast microstructure of a cast nickel base superalloy M963 has been investigated. The results show that the as cast microstructure of the alloy consists of γ solid solution matrix,γ′ precipitate in cubic shape, (γ+γ′) eutectic and MC carbide, and the morphology of MC carbide in the microstructure can be varied from coarse scriptlike, fine scriptlike to fine cubelike or discontinuous particles by increasing the melt superheating temperature. The mechanism of melt superheating is discussed by means of differential thermal analysis (DTA) technique. 展开更多
关键词 cast nickel base superalloy melt superheating MC carbide differential thermal analysis
下载PDF
R & D OF CAST SUPERALLOYS AND PROCESSING FOR GAS TURBINE BLADES IN BIAM 被引量:1
2
作者 Y.F. Han and R.Z. Chen(Institute of Aeronautical Materials, Beijing 100095,China ) 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1996年第6期457-463,共7页
Research and development of cast superalloys and processing for turbine blades in BIAM during the last 35 years have been reviewed briefly in this paper.
关键词 cast nickel base superalloy turbine blade ceramic core shell Mold
下载PDF