FE SIMULATION OF CENTER CRACK OCCURRENCE IN TUBE ROUNDS DURING TWO-ROLL ROTARY ROLLING PROCESS 被引量:8
1
作者 S.Z. Li J. Xu +4 位作者 Y.D. Yin J.G. Xue F. Pan J.M. Zheng J.H. Yoon 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2007年第3期225-234,共10页
With the aid of FE (finite element) code MSC.Superform 2005, 2-D coupled thermo-mechanical simulation of center-crack occurrence in round billet during 2-roll rotary rolling process was presented using Oyane ductile... With the aid of FE (finite element) code MSC.Superform 2005, 2-D coupled thermo-mechanical simulation of center-crack occurrence in round billet during 2-roll rotary rolling process was presented using Oyane ductile fracture criteria. A simple modeling is put forward based on the spiral motion of the workpiece as an essential characteristic in movement. The influence of the feed angle and the entry cone angle of the main roll on the process was taken into account in the modeling. The soundness for simplifying the 3-D rotary rolling into a 2-D problem was discussed. By adopting the parameters of Diescher piercer in 140mm mandrel mill of Bao Steel, the distribution and development of strain/stress were analyzed, and the eigen value of ductile fracture as well. The critical percentage of diameter reduction was obtained from the simulation. The result showed a good agreement with the experimental value, and therefore was of widely guiding significance to the practical process for rationally formulating the deformation parameters of steel tube piercing. 展开更多
关键词 numerical simulation inside crack tube piercing rotary rolling seamless tube deformation
下载PDF
CFD Simulation of Propane Cracking Tube Using Detailed Radical Kinetic Mechanism 被引量:7
2
作者 张楠 邱彤 陈丙珍 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2013年第12期1319-1331,共13页
In the radiant section of cracking furnace,the thermal cracking process is highly coupled with turbulent flow,heat transfer and mass transfer.In this paper,a three-dimensional simulation of propane pyrolysis reactor t... In the radiant section of cracking furnace,the thermal cracking process is highly coupled with turbulent flow,heat transfer and mass transfer.In this paper,a three-dimensional simulation of propane pyrolysis reactor tube is performed based on a detailed kinetic radical cracking scheme,combined with a comprehensive rigorous computational fluid dynamics(CFD)model.The eddy-dissipation-concept(EDC)model is introduced to deal with turbulence-chemistry interaction of cracking gas,especially for the multi-step radical kinetics.Considering the high aspect ratio and severe gradient phenomenon,numerical strategies such as grid resolution and refinement,stepping method and relaxation technique at different levels are employed to accelerate convergence.Large scale of radial nonuniformity in the vicinity of the tube wall is investigated.Spatial distributions of each radical reaction rate are first studied,and made it possible to identify the dominant elementary reactions.Additionally,a series of operating conditions including the feedstock feed rate,wall temperature profile and heat flux profile towards the reactor tubes are investigated.The obtained results can be used as scientific guide for further technical retrofit and operation optimization aiming at high conversion and selectivity of pyrolysis process. 展开更多
关键词 numerical simulation cracking tube computational fluid dynamics(CFD) detailed radical kinetics
下载PDF
多炮孔岩体等离子体爆破定向致裂机理研究
3
作者 李雪 王传兵 +4 位作者 王雁冰 梅洪嘉 李琰庆 王兆阳 肖殿才 《工程科学学报》 EI 北大核心 2025年第2期259-270,共12页
为了研究等离子爆破技术结合切缝管和预切槽技术的定向致裂效果,开展等离子体电脉冲定向致裂试验,探究不同切缝管切缝形状和不同预切槽间距下等离子体爆破定向致裂机理和定向断裂效果,对比分析不同定向形式作用下等离子体爆破岩石定向... 为了研究等离子爆破技术结合切缝管和预切槽技术的定向致裂效果,开展等离子体电脉冲定向致裂试验,探究不同切缝管切缝形状和不同预切槽间距下等离子体爆破定向致裂机理和定向断裂效果,对比分析不同定向形式作用下等离子体爆破岩石定向断裂贯通效果.结果表明,与正楔形切缝管和平切形切缝管相比,切缝管岩石试件中倒楔形结构中产生的应力峰值最大,聚能效果最显著,其定向贯通岩石效果更显著.预切槽岩石的电爆聚能致裂效果随着钻孔切槽间距的增加而减小.切槽间距为40 mm时,预切槽岩石试件等离子体电脉冲的聚能效果优异,产生定向裂纹的效果明显优于切槽间距为50 mm和60 mm的预切槽岩石试件.同时,预切槽定向形式的等离子体爆破定向致裂效果相对于切缝管定向致裂效果更为显著. 展开更多
关键词 等离子体电脉冲爆破 定向致裂 切缝管 预切槽 数值模拟
下载PDF
催化裂化预提升管断裂原因分析与优化
4
作者 吴军 窦益华 《石油工业技术监督》 2025年第1期19-24,共6页
对某重油催化裂化装置的预提升管频繁失效问题进行了深入研究,开展了精细的检测与分析。结果表明,预提升管失效的主要原因是高温硫化氢等气体的腐蚀性开裂、高温环境下的持续冲蚀以及交变载荷下的疲劳应力。此外,还发现管材在高温条件... 对某重油催化裂化装置的预提升管频繁失效问题进行了深入研究,开展了精细的检测与分析。结果表明,预提升管失效的主要原因是高温硫化氢等气体的腐蚀性开裂、高温环境下的持续冲蚀以及交变载荷下的疲劳应力。此外,还发现管材在高温条件下发生了碳化现象。针对上述问题,提出了优化改进方案,旨在从根本上消除高温硫化氢的腐蚀影响,有效避免了非对称交变载荷引起的疲劳破坏。改进后的运行结果表明,预提升管的正常使用周期显著延长,同时优化了催化剂在提升管内的径向分布,实现了催化剂与原料的充分接触。 展开更多
关键词 预提升管 腐蚀开裂 疲劳破坏 冲刷磨损 高温碳化
下载PDF
CCUS注CO_(2)井管柱失效原因分析
5
作者 牛步青 郑振兴 +4 位作者 李丹杰 靳俊娅 史交齐 刘西西 任枭雄 《石油管材与仪器》 2025年第1期70-76,共7页
某油田现场CCUS注CO_(2)井油管和套管在使用过程中发生断裂失效。通过宏观观察、磁粉检测、化学成分分析、力学性能测试、金相分析、腐蚀产物(EDS和XRD)分析、断口微观形貌分析以及环空液样品检测,对失效原因进行分析。结果表明,在含有... 某油田现场CCUS注CO_(2)井油管和套管在使用过程中发生断裂失效。通过宏观观察、磁粉检测、化学成分分析、力学性能测试、金相分析、腐蚀产物(EDS和XRD)分析、断口微观形貌分析以及环空液样品检测,对失效原因进行分析。结果表明,在含有硫化物腐蚀介质的油套环空环境中,在局部应力作用下,普通碳钢(N80-1)油、套管发生了硫化物应力腐蚀开裂失效。 展开更多
关键词 碳捕获、利用和封存 油套管失效 失效分析 油套环空 硫化物应力腐蚀开裂
下载PDF
CFD Simulation on Ethylene Furnace Reactor Tubes 被引量:1
6
作者 Lan Xingying Xu Chunming +1 位作者 Gao Jinsen Zhang Hongmei 《Petroleum Science》 SCIE CAS CSCD 2006年第2期73-80,共8页
Different mathematical models for ethylene furnace reactor tubes were reviewed. On the basis of these models a new mathematical simulation approach for reactor tubes based on computational fluid dynamics (CFD) techn... Different mathematical models for ethylene furnace reactor tubes were reviewed. On the basis of these models a new mathematical simulation approach for reactor tubes based on computational fluid dynamics (CFD) technique was presented. This approach took the flow, heat transfer, mass transfer and thermal cracking reactions in the reactor tubes into consideration. The coupled reactor model was solved with the SIMPLE algorithm. Some detailed information about the flow field, temperature field and concentration distribution in the reactor tubes was obtained, revealing the basic characteristics of the hydrodynamic phenomena and reaction behavior in the reactor tubes. The CFD approach provides the necessary information for conclusive decisions regarding the production optimization, the design and improvement of reactor tubes, and the new techniques implementation. 展开更多
关键词 Reactor tube thermal cracking reaction FLOW mathematical simulation computational fluid dynamics
下载PDF
Torsional Behavior Design of UHPC Box Beams Based on Thin-Walled Tube Theory 被引量:7
7
作者 Imjong Kwahk Changbin Joh Jung Woo Lee 《Engineering(科研)》 2015年第3期101-114,共14页
This study proposed a prediction formula for the torsional strength enabling to reflect the tensile strength of ultra high performance concrete (UHPC) beams based upon the thin-walled tube theory. The remarkable ducti... This study proposed a prediction formula for the torsional strength enabling to reflect the tensile strength of ultra high performance concrete (UHPC) beams based upon the thin-walled tube theory. The remarkable ductile behavior of UHPC can also be attributed to the steel fiber reinforcement. This feature must be considered to provide rational explanation of the torsional behavior of UHPC structures. In this study, the proposed torsional design adopts a modified thin-walled tube theory so as to consider the tensile behavior of UHPC. And torsion test was conducted on thin-walled UHPC box beams to validate the proposed formula through comparison of the predicted torsional strength with the experimental results. The comparison of the predicted values of the cracking torque and torsional moment resistance with those observed in the torsional test of UHPC verified the validity of the design method. The contribution of the steel fibers to the torsional strength and cracking load was larger than that of the stirrups, but the stirrups appeared to contribute additionally to the torsional ductility. Accordingly, it is recommended that design should exploit effectively the contribution of the steel fiber rather than arrange a larger number of stirrups in UHPC structures subjected to torsion. 展开更多
关键词 TORSION Behavior Ultra High Performance Concrete (UHPC) THIN-WALLED tube Torsional Strength DIAGONAL crack
下载PDF
FAILURES AND THE LIFE OF FURNACE TUBES
8
作者 F.Z.Shen Y.Ding +4 位作者 D.M.Hou Z.P.Ning Y.Lü T.B.Dong A.R.Tuohuti 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2004年第4期419-425,共7页
It is showed after the furnace tubes serviced for 8-10 years that the density of damage in the HAZ (heat affected zone) of the weld has higher than in parent metals, though the depth of damage is not equal to. By the ... It is showed after the furnace tubes serviced for 8-10 years that the density of damage in the HAZ (heat affected zone) of the weld has higher than in parent metals, though the depth of damage is not equal to. By the test of creep crack growth, it is also acquired that under same mechanic parameter C* (t), the rate of creep crack growth in the HAZ is more than twice as fast as in parent metals. Two mechanisms (overheating and thermal shock) of failure occurred in an accident are presented. The stress of thermal shock is analyzed, in which the change of the elasticity modulus with the radius ET = /(r) is considered. Based on it, the safety region of the thermal shock is obtained. Finally, two sets of curves for the safe life are suggested which can facilitate to estimate the remaining life of HK-40 or HP-Nb tubes by their creep rupture data. 展开更多
关键词 FAILURE thermal stock creep crack growth remaining life furnace tube
下载PDF
裂解炉稀释蒸汽管道三通开裂原因分析
9
作者 陈静 孔范洋 +1 位作者 许铁群 陈怀宁 《压力容器》 北大核心 2024年第7期56-62,86,共8页
针对某乙烯裂解装置稀释蒸汽管道304H耐热不锈钢三通使用1年后发生开裂的情况,从材料成分、力学性能、金相组织、残余应力和断口特性等方面进行了分析。结果表明,裂纹分别启裂于三通的内壁和外壁,多数裂纹开裂处伴有晶间腐蚀特征,裂纹... 针对某乙烯裂解装置稀释蒸汽管道304H耐热不锈钢三通使用1年后发生开裂的情况,从材料成分、力学性能、金相组织、残余应力和断口特性等方面进行了分析。结果表明,裂纹分别启裂于三通的内壁和外壁,多数裂纹开裂处伴有晶间腐蚀特征,裂纹扩展特性以沿晶型为主;断口附近腐蚀产物存在O,S,Cl等酸性腐蚀介质。三通主管表面最大轴向应力达到147 MPa,三通相贯线附近距裂纹20 mm处的最大环向应力达到114 MPa,说明运行中的三通表面应力达到了材料屈服强度的1/2。分析认为,裂纹的产生是由于材料发生敏化后,在应力和腐蚀介质共同作用下形成的以沿晶为主的应力腐蚀开裂,更换三通材料或通过适当的固溶处理降低三通中的残余应力是避免三通开裂的重要途径。 展开更多
关键词 稀释蒸汽管道 三通 应力腐蚀开裂 304H不锈钢 敏化
下载PDF
P110S钢级油管管体断裂原因
10
作者 赵映辉 夏文斌 +1 位作者 周勇 赵建明 《理化检验(物理分册)》 CAS 2024年第4期68-71,共4页
某油井P110S钢级油管接箍下方8 m位置处发生断裂,采用宏观观察、化学成分分析、金相检验、扫描电镜和能谱分析、X射线衍射分析等方法对油管断裂原因进行分析。结果表明:该批油管力学性能不稳定,油管断口上的腐蚀产物主要为FeS;油管的强... 某油井P110S钢级油管接箍下方8 m位置处发生断裂,采用宏观观察、化学成分分析、金相检验、扫描电镜和能谱分析、X射线衍射分析等方法对油管断裂原因进行分析。结果表明:该批油管力学性能不稳定,油管断口上的腐蚀产物主要为FeS;油管的强度较高、使用温度较低且质量较大,导致油管内部形成硫化物应力腐蚀开裂。 展开更多
关键词 P110S钢级油管 硫化物 应力腐蚀开裂 力学性能 显微组织
下载PDF
PBL抗剪传力钢筋连接接头受拉力学性能试验
11
作者 龚超 梁梓豪 +4 位作者 张素梅 李孝忠 梁伟桥 闫贵海 姚志东 《哈尔滨工程大学学报》 EI CAS CSCD 北大核心 2024年第7期1391-1399,共9页
装配式混凝土构件间钢筋的连接是其适用性和经济性的关键环节,针对国内工程常用的灌浆套筒和约束浆锚钢筋连接技术存在施工难度大、效率低、质量不易检验等问题,本文提出了PBL-穿孔钢筋连接接头、PBL-穿孔钢管连接接头和PBL-U形钢筋连... 装配式混凝土构件间钢筋的连接是其适用性和经济性的关键环节,针对国内工程常用的灌浆套筒和约束浆锚钢筋连接技术存在施工难度大、效率低、质量不易检验等问题,本文提出了PBL-穿孔钢筋连接接头、PBL-穿孔钢管连接接头和PBL-U形钢筋连接接头3种钢筋连接接头,实现预制混凝土单元间钢筋应力的传递,具有施工简便、质量易保证、成本低等优势。对这3种钢筋接头进行了6组参数共18个钢筋接头试件的拉伸性能试验,研究了新型接头试件的破坏模式、承载力和变形能力等,得到各参数对新型接头拉伸强度的影响规律,并对不同接头的受拉力学性能进行对比分析。研究结果表明:3种钢筋连接接头能够实现钢筋应力的有效传递,验证了新型钢筋连接接头的可行性。 展开更多
关键词 装配式混凝土 钢筋连接接头 PBL剪力键 钢管混凝土 拉伸试验 裂缝发展 破坏模式 受拉承载力
下载PDF
120 ksi高强度小油管应力腐蚀性能研究 被引量:1
12
作者 李鸿斌 王涛 +3 位作者 张锦刚 余晗 苑清英 王晓波 《焊管》 2024年第4期39-44,共6页
对采用高强度卷板、高频焊焊接(HFW)工艺开发的120 ksi钢级小油管,开展了母材和焊缝的理化性能、氢致开裂、应力腐蚀等试验分析研究。结果表明:120 ksi小油管样品理化性能控制较好,但氢致开裂试验均出现大量裂纹,其裂纹敏感率、裂纹长... 对采用高强度卷板、高频焊焊接(HFW)工艺开发的120 ksi钢级小油管,开展了母材和焊缝的理化性能、氢致开裂、应力腐蚀等试验分析研究。结果表明:120 ksi小油管样品理化性能控制较好,但氢致开裂试验均出现大量裂纹,其裂纹敏感率、裂纹长度率、裂纹厚度率均较高,同时管材抗应力腐蚀性能较差,样管在66%σs应力加载下出现大量裂纹或断裂,表明普通120 ksi强度级别的油管无法满足抗硫化氢腐蚀要求。 展开更多
关键词 高强度 油管 氢致开裂 应力腐蚀
下载PDF
液氧相变气体膨胀技术在隧洞开挖中的应用研究 被引量:1
13
作者 方莹 李国良 +2 位作者 朱振海 刘杰 孔玉霞 《爆破》 CSCD 北大核心 2024年第2期232-237,共6页
为了实现在不许可使用炸药爆破条件下的隧洞快速开挖施工,应用新型氧气膨胀破岩技术,成功探索、研究、总结出一套适用于一般隧洞开挖的掏槽、扩槽、辅助、周边孔气体膨胀破岩施工方法,详细给出了适用于隧道开挖的优化钻爆参数。隧洞穿... 为了实现在不许可使用炸药爆破条件下的隧洞快速开挖施工,应用新型氧气膨胀破岩技术,成功探索、研究、总结出一套适用于一般隧洞开挖的掏槽、扩槽、辅助、周边孔气体膨胀破岩施工方法,详细给出了适用于隧道开挖的优化钻爆参数。隧洞穿越的山体为花岗岩,试验研究段属于Ⅳ~Ⅲ围岩,岩石的抗压强度为90~100 MPa,非常坚硬,解理裂隙比较发育,可爆性一般。采用现场试验研究方法,经过不断总结、改进、优化,对于面积约65 m^(2)的隧洞,实现了2 d一个循环,平均循环进尺约2.5 m,基本满足在不能使用炸药爆破情况下一般隧洞快速开挖施工的要求。研究表明:新型气体膨胀破岩技术可以在坚硬岩体中进行隧洞开挖,具有操作安全、破岩效率高、不涉及民爆物品和易制爆危险化学品、不产生爆炸冲击波、振动幅值较低等优点,可有效地解决复杂环境下不许可使用民爆物品及使用机械法开挖进度慢的问题。 展开更多
关键词 气体膨胀 致裂管 孔内充气 液氧 隧洞掘进
下载PDF
MS1180方管连续辊弯成形角部开裂机理
14
作者 张建邦 刘晓立 +4 位作者 黄素霞 李河宗 崔衍亮 闫宾 闻海强 《哈尔滨工业大学学报》 EI CAS CSCD 北大核心 2024年第8期153-162,共10页
方矩形管在辊弯成形中会产生角部开裂现象,这已成为严重制约方矩形管质量的关键问题,为解决其角部开裂缺陷展开深入研究,寻找控制开裂缺陷的方法。首先通过对MS1180进行单轴拉伸、缺口拉伸和平面应变实验得到了材料的力学特性,并分别利... 方矩形管在辊弯成形中会产生角部开裂现象,这已成为严重制约方矩形管质量的关键问题,为解决其角部开裂缺陷展开深入研究,寻找控制开裂缺陷的方法。首先通过对MS1180进行单轴拉伸、缺口拉伸和平面应变实验得到了材料的力学特性,并分别利用3种拉伸试验将Ayada、Rice-Tracey和标准化Cockroft-Latham准则进行校准,得到了预测误差最小的一种断裂准则,并以此构建了方矩管辊弯开裂模型。其次利用辊弯成形COPRA RF设计软件和有限元MARC仿真专业软件,结合生产实际条件建立了方矩形管连续辊弯成形三维有限元模型,并进行辊弯实验验证模型的准确性。最后采用扫描电镜和金相显微镜对方矩形管开裂件以及断口进行微观观察,针对性的利用有限元模型探究了方矩形管连续辊弯成形时应力-应变分布规律,并分析了道次数量、角部成形半径和机架间距对方矩管角部应力-应变分布的影响。结果表明:发现材料起裂点位于角部近外层,对开裂断口进行分析,得到其开裂方式为准解理开裂,角部剪切面上所受的主应力过大导致其开裂;增加辊弯道次数量、方矩形管角部成形半径以及机架之间的间距能有效减少开裂问题的出现,为以后解决方矩形管角部开裂问题提供了理论基础。 展开更多
关键词 辊弯成形 超高强钢 方矩形管 开裂 有限元分析
下载PDF
新型乙烷裂解炉辐射段炉管鼓包、开裂失效原因分析
15
作者 赵磊 王明明 +2 位作者 陈永伟 黄超 白涛涛 《化工管理》 2024年第34期129-133,共5页
某乙烯装置乙烷裂解炉为国内设计单位设计的HQF-G IV型裂解炉,辐射段炉管设计使用寿命10.0年,实际运行3.5年时发现10处鼓包,其中2处开裂失效,严重影响乙烯装置的安全运行。针对乙烷裂解炉辐射段炉管使用寿命严重低于设计值的情况,通过... 某乙烯装置乙烷裂解炉为国内设计单位设计的HQF-G IV型裂解炉,辐射段炉管设计使用寿命10.0年,实际运行3.5年时发现10处鼓包,其中2处开裂失效,严重影响乙烯装置的安全运行。针对乙烷裂解炉辐射段炉管使用寿命严重低于设计值的情况,通过宏观分析、化学成分分析、应力分析、硬度检测、CFD模拟分析、能谱分析、扫描电镜分析对炉管失效原因进行分析。结果表明:炉管失效由于长时间在不均匀温度场下服役,高温造成金属材料组织劣化,同时受到热应力、扭曲应力的共同作用,炉管局部区域发生塑形变形,产生高温蠕变,随着蠕变损伤的积累,导致炉管开裂。 展开更多
关键词 乙烷裂解炉 辐射段炉管 蠕变 开裂
下载PDF
电厂锅炉再热器管开裂原因 被引量:1
16
作者 刘永超 《理化检验(物理分册)》 CAS 2024年第2期28-30,共3页
某电厂锅炉前墙壁式再热器管、水冷壁管、分隔屏管发生蒸汽泄漏事故,采用宏观观察、金相检验、硬度测试等方法分析了锅炉管开裂的原因。结果表明:锅炉管开裂点位于壁式再热器管上,开裂原因不是管材过热或自身缺陷,而是安装施工过程中,... 某电厂锅炉前墙壁式再热器管、水冷壁管、分隔屏管发生蒸汽泄漏事故,采用宏观观察、金相检验、硬度测试等方法分析了锅炉管开裂的原因。结果表明:锅炉管开裂点位于壁式再热器管上,开裂原因不是管材过热或自身缺陷,而是安装施工过程中,前期滑动板与31根壁式再热器管的靠炉前侧发生误焊,产生了缺陷,导致管件开裂。 展开更多
关键词 锅炉壁再热器管 开裂 显微组织 残余应力
下载PDF
冷凝液汽提系统夹套管不锈钢内管开裂失效分析
17
作者 侯建琴 刘宝林 +2 位作者 白学刚 刘畅 宋策 《石油化工腐蚀与防护》 CAS 2024年第4期59-64,共6页
某化工企业甲醇中心净化装置冷凝液汽提系统夹套管不锈钢内管发生开裂泄漏,通过宏观观察、化学成分分析、力学性能测试、金相分析、硬度测试、能谱分析和断口扫描电镜分析等手段对失效原因进行了分析。结果显示:夹套管不锈钢内管力学性... 某化工企业甲醇中心净化装置冷凝液汽提系统夹套管不锈钢内管发生开裂泄漏,通过宏观观察、化学成分分析、力学性能测试、金相分析、硬度测试、能谱分析和断口扫描电镜分析等手段对失效原因进行了分析。结果显示:夹套管不锈钢内管力学性能不符合标准要求,且内部凹坑与裂纹均在酸洗前已存在,为原始制造缺陷。 展开更多
关键词 不锈钢内管 裂纹 失效分析
下载PDF
复杂服役工况下集箱管座的应力分析
18
作者 梁慧超 王硕 +1 位作者 张鹏宇 郝维勋 《失效分析与预防》 2024年第3期166-171,共6页
火力发电机组在灵活运行时,锅炉会频繁启停和升降负荷,此过程中伴随着温度和载荷的交替变化,由此带来集箱管座频繁开裂问题。本文以过热器集箱为模板,建立含有集箱、管座角焊缝和管接头的有限元模型,并对机组在升负荷和降负荷过程中管... 火力发电机组在灵活运行时,锅炉会频繁启停和升降负荷,此过程中伴随着温度和载荷的交替变化,由此带来集箱管座频繁开裂问题。本文以过热器集箱为模板,建立含有集箱、管座角焊缝和管接头的有限元模型,并对机组在升负荷和降负荷过程中管座的温度场和应力场进行分析。结果表明:升降负荷过程中,集箱的温度平衡速度相对缓慢,管接头则快速平衡;升降负荷过程中,管座区域最大热应力发生在焊缝熔合线处,而机械应力主要受管内压力波动的影响。 展开更多
关键词 集箱 管座开裂 有限元 热应力 机械应力
下载PDF
仪表风冷却器换热管开裂失效原因分析 被引量:1
19
作者 李广凯 王震 +2 位作者 于亚龙 刘志梅 王帅 《石油化工腐蚀与防护》 CAS 2024年第1期59-64,共6页
某炼化企业仪表风冷却器在运行中换热管发生了开裂失效,通过宏观形貌观察、微观形貌观察、能谱分析和金相组织分析等技术手段分析了该换热管发生开裂失效的原因,并提出了相应的解决方案。分析结果表明:该换热管材质为S31608奥氏体不锈钢... 某炼化企业仪表风冷却器在运行中换热管发生了开裂失效,通过宏观形貌观察、微观形貌观察、能谱分析和金相组织分析等技术手段分析了该换热管发生开裂失效的原因,并提出了相应的解决方案。分析结果表明:该换热管材质为S31608奥氏体不锈钢,该换热管发生开裂的主要原因是氯化物应力腐蚀开裂,其次为温差应力较大引发的腐蚀疲劳开裂。为了解决该换热管的开裂失效问题,应确保工艺操作平稳,对换热器结构进行优化设计,换热管应选用超低碳不锈钢材质。 展开更多
关键词 仪表风冷却器 换热管 开裂失效 氯离子 疲劳 应力腐蚀开裂
下载PDF
耶拿EA5000硫、氮分析仪技术参数优化探究
20
作者 李帆玉竹 《兰州石化职业技术大学学报》 2024年第4期8-11,共4页
耶拿EA5000仪器元素分析仪是化验室常用的元素分析仪器,它可对硫、氯、氮等元素进行准确的分析。其检测级别为PPB级,对化工分析中的生产可以提供准确的数据依据。对仪器技术参数以及个别含量较大、黏度较大易挥发样品进样方法进行了优化... 耶拿EA5000仪器元素分析仪是化验室常用的元素分析仪器,它可对硫、氯、氮等元素进行准确的分析。其检测级别为PPB级,对化工分析中的生产可以提供准确的数据依据。对仪器技术参数以及个别含量较大、黏度较大易挥发样品进样方法进行了优化,由原有的水平炉称量分析改为时间较短垂直炉方式进行分析,来延长仪器的使用寿命、减少仪器裂解管的更换频率、节省载气的用量和减少分析时长。优化后节约了分析成本,提高了分析效率。 展开更多
关键词 裂解管 气体流量 方法温度 参数优化
下载PDF
上一页 1 2 52 下一页 到第
使用帮助 返回顶部