The depth adjustment factor for bending strength stated in Eurocode 5(EC5)is only applicable to timbers having a characteristic density below 700 kg/m^(3).However,most Malaysian timbers are hardwood,some with a charac...The depth adjustment factor for bending strength stated in Eurocode 5(EC5)is only applicable to timbers having a characteristic density below 700 kg/m^(3).However,most Malaysian timbers are hardwood,some with a characteristic density reaching above 700 kg/m^(3).Therefore,the objective of this study was to examine whether the depth adjustment factor stipulated in EC5 is valid for Malaysian hardwood timbers.Six timber species were selected for this study,namely Kapur(Dryobalanops C.F.Gaertn.),Kempas(Koompassia Maingay ex Benth.),Keruing(Dipterocarpus C.F.Gaertn.),Light red meranti(Shorea Roxb.ex C.F.Gaertn.),Geronggang(Cratoxylum Blume)and Balau(Shorea Roxb.ex C.F.Gaertn.).The determination of bending strength and characteristic density was conducted according to BS EN 408:2010 and BS EN 384:2016,respectively.A graph for mean bending strength vs.(150/h)was plotted for each timber species.The power function was selected to analyze the relationship between the two variables.The power of the regression equations varied depending on the characteristic density of the timber species.For species with a characteristic density below 700 kg/m^(3),such as Kapur,Keruing,and Light red meranti,the power was between 0.16 to 0.17.In contrast,for species having a characteristic density above 700 kg/m^(3),namely Kempas and Balau,the power was higher at 0.23 and 0.24,respectively.Geronggang was an exception to this pattern.These values are close to the depth adjustment factor given in EC5,which is 0.2.Based on the results,it can be suggested that the adjustment factor of 0.2 is also applicable to Malaysian hardwood timbers with a characteristic density above 700 kg/m^(3).展开更多
基金funded by Geran Penyelidikan Khas(GPK),(600-RMC/GPK 5/3(071/2020)).
文摘The depth adjustment factor for bending strength stated in Eurocode 5(EC5)is only applicable to timbers having a characteristic density below 700 kg/m^(3).However,most Malaysian timbers are hardwood,some with a characteristic density reaching above 700 kg/m^(3).Therefore,the objective of this study was to examine whether the depth adjustment factor stipulated in EC5 is valid for Malaysian hardwood timbers.Six timber species were selected for this study,namely Kapur(Dryobalanops C.F.Gaertn.),Kempas(Koompassia Maingay ex Benth.),Keruing(Dipterocarpus C.F.Gaertn.),Light red meranti(Shorea Roxb.ex C.F.Gaertn.),Geronggang(Cratoxylum Blume)and Balau(Shorea Roxb.ex C.F.Gaertn.).The determination of bending strength and characteristic density was conducted according to BS EN 408:2010 and BS EN 384:2016,respectively.A graph for mean bending strength vs.(150/h)was plotted for each timber species.The power function was selected to analyze the relationship between the two variables.The power of the regression equations varied depending on the characteristic density of the timber species.For species with a characteristic density below 700 kg/m^(3),such as Kapur,Keruing,and Light red meranti,the power was between 0.16 to 0.17.In contrast,for species having a characteristic density above 700 kg/m^(3),namely Kempas and Balau,the power was higher at 0.23 and 0.24,respectively.Geronggang was an exception to this pattern.These values are close to the depth adjustment factor given in EC5,which is 0.2.Based on the results,it can be suggested that the adjustment factor of 0.2 is also applicable to Malaysian hardwood timbers with a characteristic density above 700 kg/m^(3).