The effect of frequency and sample shape on fatigue behaviors of DZ125 superalloy
1
作者 Yuli Gu Chunhu Tao +1 位作者 Yuhuai He Changkui Liu 《Theoretical & Applied Mechanics Letters》 2012年第3期31-35,共5页
The effect of frequency and sample shape on fatigue behaviors of DZ125 superalloy are systematically studied.The results show that fatigue fracture still occurs above the cycle of 10~8 for tests carried out at the fre... The effect of frequency and sample shape on fatigue behaviors of DZ125 superalloy are systematically studied.The results show that fatigue fracture still occurs above the cycle of 10~8 for tests carried out at the frequency of f=20 kHz and stress ratio R =-1,so the traditional fatigue limit at cycle of 10~7 is not appropriate for fatigue design.Fatigue fracture surfaces are perpendicular to stress axis for cylindrical and plate specimens,and the fatigue cracks originate from the extra surface of the specimens.Fatigue crack is apt to propagate from cutting direction to forward direction,which occurs mainly in the second propagation stage at higher stress amplitude. There is an obvious frequency effect for DZ125 superalloy.The higher the test frequency is,the more serious the effect of frequency on fatigue behaviors of the alloy.After the frequency correction,the ultra-high cycle fatigue S-N curve well coincide with the traditional fatigue S-N curve. 展开更多
关键词 directionally solidification superalloy ultra-high cycle fatigue FREQUENCY sample shape
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部