Online application of automatic surface quality inspection system to finishing line of cold rolled strips 被引量:4
1
作者 Hao Sun, Ke Xu, and Jinwu XuNational Engineering Research Center of Advanced Rolling, University of Science and Technology Beijing, Beijing 100083, China 《Journal of University of Science and Technology Beijing》 CSCD 2003年第4期38-41,共4页
An automatic surface quality inspection system installed on a finishing lineof cold rolled strips is introduced. The system is able to detect surface defects on cold rolledstrips, such as scratches, coil breaks, rusts... An automatic surface quality inspection system installed on a finishing lineof cold rolled strips is introduced. The system is able to detect surface defects on cold rolledstrips, such as scratches, coil breaks, rusts, roll imprints, and so on. Multiple CCD area scancameras were equipped to capture images of strip surface simultaneously. Defects were detectedthrough 'Dark-field illumination' which is generated by LED illuminators. Parallel computationtechnique and fast processing algorithms were developed for real-time data processing. Theapplication to the production line shows that the system is able to detect defects effectively. 展开更多
关键词 surface inspection cold rolled strip finishing line CCD cameras IMAGEPROCESSING
下载PDF
An in Vitro Analysis to Evaluate Coronal Residual Dentine Thickness after Different Anterior Crown Preparations
2
作者 Nana Frimpomah Adu-Ampomah Patrick Caldicock Ampofo +5 位作者 Anno Nyako Sandra Hewlett Alexander Oti Acheampong Gladia Toledo Mayari Yabang Stephen Ankoh Ruby Goka 《Open Journal of Stomatology》 2023年第12期442-449,共8页
Background: Knife edge, chamfer, and shoulder are the three distinct finishing lines utilized in crown preparations. Each finishing line has relative benefits and drawbacks. However, not much scientific data exists re... Background: Knife edge, chamfer, and shoulder are the three distinct finishing lines utilized in crown preparations. Each finishing line has relative benefits and drawbacks. However, not much scientific data exists regarding which of these finishing lines will leave the most amount of residual dentine coronally on maxillary lateral incisors and mandibular incisors. Objective: To assess the coronal residual dentine thickness after different cervical finishing lines for anterior crown preparations. Materials and Methods: A prospective comparative study was conducted including mandibular incisors and maxillary laterals that were taken from subjects from 18 to 30 years old. Teeth in each of the three groups were randomly separated into three cervical margin preparation groups: knife edge, chamfer and shoulder. The teeth were then prepared for single crown coverage using these finishing lines. The teeth were sectioned halfway through the crown preparation, and a digital caliper was used to determine the residual dentine thickness at the buccal, lingual, mesial and distal areas. The Tukey test was used for mean comparison, and ANOVA analysis was used to evaluate the variation in mean residual dentine thickness. Results: For upper lateral incisors, knife edge finishing lines showed the highest amount of remaining dentine thickness—1.5 mm. lingually, while the upper lateral incisors mesially had the least amount of 0.53 mm for shoulder finishing lines. The least residual dentine (0.53 mm for the shoulder and 0.70 mm for the chamfer finishing line) was found in the interproximal portions of all the teeth that were selected. Lower central incisors had the least amount of residual dentine 0.61 mm for shoulder preparations mesially whiles lower lateral incisors had the least amount of residual dentine for shoulder preparations 0.58 mm distally. There was a statistically significant difference of 0.001 across the groups. Conclusion: The thickness of residual dentine seen coronally after the three finishing line preparations showed a statistically significant difference and the knife edge finishing line provided enough coronal protection within the scope of this study. 展开更多
关键词 CORONAL finishing lines Residual Dentine Thickness
下载PDF
A GREEN FINISH LINE
3
《Beijing Review》 2018年第35期16-17,共2页
In China’s unremitting efforts to fight against desertification,Elion Resources Group,a private enterprise in north China’s Inner Mongolia Autonomous Region,is playing an exemplary role.Wang Wenbiao,Chairman of the ... In China’s unremitting efforts to fight against desertification,Elion Resources Group,a private enterprise in north China’s Inner Mongolia Autonomous Region,is playing an exemplary role.Wang Wenbiao,Chairman of the company,received the Champions of the Earth Award from the United Nations 展开更多
关键词 A GREEN FINISH line
原文传递