Aiming at the high temperature corrosion in a coal-fired boiler,the effect of H2S and SO2 on the corrosion of 12 CrlMoV under the water wall condition has been investigated by experiments.The results indicate that H2 ...Aiming at the high temperature corrosion in a coal-fired boiler,the effect of H2S and SO2 on the corrosion of 12 CrlMoV under the water wall condition has been investigated by experiments.The results indicate that H2 S can promote the corrosion significantly,and the coarse porous oxide film formed cannot stop the progress of corrosion.While SO2 presents little effect on the corrosion.The main composition of the surface of 12 CrlMoV corrosion products is Fe2 O3.With H2S in the atmosphere,the corrosion gradually develops into deeper layers by forming FeS,FeO and Fe2 O3 alternately.The corrosion rate is doubled for every 50℃ inerease in temperature at 400-500℃.展开更多
[Objectives]To determine the content of total saponins in Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S.kurita,fill the gap in the study of Paris daliensis H. Li et V. G. Soukoup and Paris du...[Objectives]To determine the content of total saponins in Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S.kurita,fill the gap in the study of Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita,and lay a foundation for searching new medicinal resources of Paris L. [Methods]The perchloric acid colorimetric method and UV spectrophotometer were used to determine the content of total saponins in Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita at 406 nm. [Results]The lowest content of total saponins in Paris daliensis H. Li et V. G. Soukoup was 2. 637%,while the highest content reached 5. 474%; the lowest content of total saponins in Paris dulongensis was 1. 806%,while the highest content reached 3. 532%. Through the methodological examination,it was found that this method was stable and reliable. [Conclusions] The content of total saponins was high in Paris daliensis H.Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita,and it was suggested to further study and find the medicinal resources of Paris L.展开更多
The effects of plastic deformation and H2 S on fracture toughness of high strength casing steel(C110 steel) were investigated. The studied casing specimens are as follows: original casing, plastic deformation(PD)...The effects of plastic deformation and H2 S on fracture toughness of high strength casing steel(C110 steel) were investigated. The studied casing specimens are as follows: original casing, plastic deformation(PD) casing and PD casing after being immersed in NACE A solution saturated with H2S(PD+H2S). Instrumented impact method was employed to evaluate the impact behaviors of the specimens, meanwhile, dynamic fracture toughness(JId) was calculated by using Rice model and Schindler model. The experimental results show that dynamic fracture toughness of the casing decreases after plastic deformation. Compared with that of the original casing and PD casing, the dynamic fracture toughness decreases further when the PD casing immersed in H2 S, moreover, there are ridge-shaped feature and many secondary cracks present on the fracture surface of the specimens. Impact fracture mechanism of the casing is proposed as follows: the plastic deformation results in the increase of defect density of materials where the atomic hydrogen can accumulate in reversible or irreversible traps and even recombine to form molecular hydrogen, subsequently, the casing material toughness decreases greatly.展开更多
E-learning platforms support education systems worldwide, transferring theoretical knowledge as well as soft skills. In the present study high-school pupils’, and adult students’ opinions were evaluated through a mo...E-learning platforms support education systems worldwide, transferring theoretical knowledge as well as soft skills. In the present study high-school pupils’, and adult students’ opinions were evaluated through a modern structured MOODLE interactive course, designed for the needs of the laboratory course “Automotive Systems”. The study concerns Greek secondary vocational education pupils aged 18 and vocational training adult students aged 20 to 50 years. The multistage, equal size simple random cluster sample was used as a sampling method. Pupils and adult students of each cluster completed structured 10-question questionnaires both before and after attending the course. A total of 120 questionnaires were collected. In general, our findings disclosed that the majority of pupils and adult students had significantly improved their knowledge and skills from using MOODLE. They reported strengthening conventional teaching, using the new MOODLE technology. The satisfaction indices improved quite, with the differences in their mean values being statistically significant.展开更多
An h-adaptive method is developed for high-order discontinuous Galerkin methods(DGM)to solve the laminar compressible Navier-Stokes(N-S)equations on unstructured mesh.The vorticity is regarded as the indicator of adap...An h-adaptive method is developed for high-order discontinuous Galerkin methods(DGM)to solve the laminar compressible Navier-Stokes(N-S)equations on unstructured mesh.The vorticity is regarded as the indicator of adaptivity.The elements where the vorticity is larger than a pre-defined upper limit are refined,and those where the vorticity is smaller than a pre-defined lower limit are coarsened if they have been refined.A high-order geometric approximation of curved boundaries is adopted to ensure the accuracy.Numerical results indicate that highly accurate numerical results can be obtained with the adaptive method at relatively low expense.展开更多
The corrosion behavior of the 110S tube steel in the environments of high H2 S and CO2 content was inves- tigated by using a high-temperature and high-pressure autoclave, and the corrosion products were characterized ...The corrosion behavior of the 110S tube steel in the environments of high H2 S and CO2 content was inves- tigated by using a high-temperature and high-pressure autoclave, and the corrosion products were characterized by scanning electron microscopy and X ray diffraction technique. The results showed that all of the corrosion products under the test conditions mainly consisted of different types of iron sulfides such as pyrrhotite of Fe0.95 S, mackinaw- ite of FeS0.9, Fe0. 985 S and FeS, and the absence of iron carbonate in the corrosion scales indicated that the corrosion process was controlled by H2S corrosion. The corrosion rate of the 110S steel decreased firstly and then increased with the rising of temperature. The minimum corrosion rate occurred at 110 ℃. When the H2 S partial pressure PH2s below 9 MPa, the corrosion rate declined with the increase of PH2s. While over 9 MPa, a higher PH2s resulted in a faster corrosion process. With the increasing of the CO2 partial pressure, the corrosion rate had an increasing trend. The morphologies of the corrosion scales had a good accordance with the corrosion rates.展开更多
基金supported by the National Key Research and Development Plan of China (No. 2018YFB0604203)
文摘Aiming at the high temperature corrosion in a coal-fired boiler,the effect of H2S and SO2 on the corrosion of 12 CrlMoV under the water wall condition has been investigated by experiments.The results indicate that H2 S can promote the corrosion significantly,and the coarse porous oxide film formed cannot stop the progress of corrosion.While SO2 presents little effect on the corrosion.The main composition of the surface of 12 CrlMoV corrosion products is Fe2 O3.With H2S in the atmosphere,the corrosion gradually develops into deeper layers by forming FeS,FeO and Fe2 O3 alternately.The corrosion rate is doubled for every 50℃ inerease in temperature at 400-500℃.
基金Supported by Sichuan Science and Technology Support Program(2016FZ-0045)Education and Teaching Research and Reform Project of Southwest University for Nationalities(2015)
文摘[Objectives]To determine the content of total saponins in Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S.kurita,fill the gap in the study of Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita,and lay a foundation for searching new medicinal resources of Paris L. [Methods]The perchloric acid colorimetric method and UV spectrophotometer were used to determine the content of total saponins in Paris daliensis H. Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita at 406 nm. [Results]The lowest content of total saponins in Paris daliensis H. Li et V. G. Soukoup was 2. 637%,while the highest content reached 5. 474%; the lowest content of total saponins in Paris dulongensis was 1. 806%,while the highest content reached 3. 532%. Through the methodological examination,it was found that this method was stable and reliable. [Conclusions] The content of total saponins was high in Paris daliensis H.Li et V. G. Soukoup and Paris dulongensis H. Li et S. kurita,and it was suggested to further study and find the medicinal resources of Paris L.
基金Funded by the Construction of Key Disciplines for Young Teacher Science Foundation of the Southwest Petroleum University(No.P209)the Research Fund for the Doctoral Program of Higher Education(No.20105121120002)the National Natural Science Foundation of China(Nos.51004084 and 51374177)
文摘The effects of plastic deformation and H2 S on fracture toughness of high strength casing steel(C110 steel) were investigated. The studied casing specimens are as follows: original casing, plastic deformation(PD) casing and PD casing after being immersed in NACE A solution saturated with H2S(PD+H2S). Instrumented impact method was employed to evaluate the impact behaviors of the specimens, meanwhile, dynamic fracture toughness(JId) was calculated by using Rice model and Schindler model. The experimental results show that dynamic fracture toughness of the casing decreases after plastic deformation. Compared with that of the original casing and PD casing, the dynamic fracture toughness decreases further when the PD casing immersed in H2 S, moreover, there are ridge-shaped feature and many secondary cracks present on the fracture surface of the specimens. Impact fracture mechanism of the casing is proposed as follows: the plastic deformation results in the increase of defect density of materials where the atomic hydrogen can accumulate in reversible or irreversible traps and even recombine to form molecular hydrogen, subsequently, the casing material toughness decreases greatly.
文摘E-learning platforms support education systems worldwide, transferring theoretical knowledge as well as soft skills. In the present study high-school pupils’, and adult students’ opinions were evaluated through a modern structured MOODLE interactive course, designed for the needs of the laboratory course “Automotive Systems”. The study concerns Greek secondary vocational education pupils aged 18 and vocational training adult students aged 20 to 50 years. The multistage, equal size simple random cluster sample was used as a sampling method. Pupils and adult students of each cluster completed structured 10-question questionnaires both before and after attending the course. A total of 120 questionnaires were collected. In general, our findings disclosed that the majority of pupils and adult students had significantly improved their knowledge and skills from using MOODLE. They reported strengthening conventional teaching, using the new MOODLE technology. The satisfaction indices improved quite, with the differences in their mean values being statistically significant.
基金supported by the National Natural Science Foundation of China(11272152)
文摘An h-adaptive method is developed for high-order discontinuous Galerkin methods(DGM)to solve the laminar compressible Navier-Stokes(N-S)equations on unstructured mesh.The vorticity is regarded as the indicator of adaptivity.The elements where the vorticity is larger than a pre-defined upper limit are refined,and those where the vorticity is smaller than a pre-defined lower limit are coarsened if they have been refined.A high-order geometric approximation of curved boundaries is adopted to ensure the accuracy.Numerical results indicate that highly accurate numerical results can be obtained with the adaptive method at relatively low expense.
基金Sponsored by Key National Science and Technology Specific Projects of China(2008ZX05017-002)
文摘The corrosion behavior of the 110S tube steel in the environments of high H2 S and CO2 content was inves- tigated by using a high-temperature and high-pressure autoclave, and the corrosion products were characterized by scanning electron microscopy and X ray diffraction technique. The results showed that all of the corrosion products under the test conditions mainly consisted of different types of iron sulfides such as pyrrhotite of Fe0.95 S, mackinaw- ite of FeS0.9, Fe0. 985 S and FeS, and the absence of iron carbonate in the corrosion scales indicated that the corrosion process was controlled by H2S corrosion. The corrosion rate of the 110S steel decreased firstly and then increased with the rising of temperature. The minimum corrosion rate occurred at 110 ℃. When the H2 S partial pressure PH2s below 9 MPa, the corrosion rate declined with the increase of PH2s. While over 9 MPa, a higher PH2s resulted in a faster corrosion process. With the increasing of the CO2 partial pressure, the corrosion rate had an increasing trend. The morphologies of the corrosion scales had a good accordance with the corrosion rates.