期刊文献+
共找到108篇文章
< 1 2 6 >
每页显示 20 50 100
Effect of Fast Cooling Rate on the Microstructure and Mechanical Properties of Low-Carbon High-Strength Steel Annealed in the Intercritical Region 被引量:3
1
作者 李壮 田勇 +2 位作者 KANG Shaopu ZHENG Zhen LIU Ming 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2014年第3期572-577,共6页
The effect of fast cooling rate on the microstructure and mechanical properties of low-carbon high-strength steel annealed in the intercritical region was investigated using a Gleeble 1500 thermomechanical simulator a... The effect of fast cooling rate on the microstructure and mechanical properties of low-carbon high-strength steel annealed in the intercritical region was investigated using a Gleeble 1500 thermomechanical simulator and a continuous annealing thermomeehanical simulator. The results showed that the microstructure consisted of ferrite and bainite as the main phases with a small amount of retained austenite and martensite islands at cooling rate of 5 and 50 ℃/s, respectively. Fast cooling after continuous annealing affected all constituents of the microstructure. The mechanical properties were improved considerably. Ultimate tensile strength (U-TS) increased and total elongation (TEL) decreased with increasing cooling rate in all specimens. The specimen 1 at a cooling rate of 5 ℃/s exhibited the maximum TEL and UTSxTEL (20% and 27 200 MPa%, respectively) because of the competition between weakening by presence of the retained austenite plus the carbon indigence by carbide precipitation, and strengthening by martensitic islands and precipitation. The maximum UTS and YS (1 450 and 951 MPa, respectively) were obtained for specimen 2 at a cooling rate of 50 ℃/s. This is attributed to the effect of dispersion strengthening of finer martensite islands and the effect of precipitation strengthening of carbide precipitates. 展开更多
关键词 cooling rate low-carbon high-strength steel intercritical annealing MICROSTRUCTURE mechanical properties
下载PDF
回火温度对低碳Fe-Mn-Si-Al高强钢组织和力学性能影响
2
作者 徐飞越 李兵 +2 位作者 张鹏 张红霞 邢俊峰 《精密成形工程》 北大核心 2024年第10期190-198,共9页
目的对低碳Fe-Mn-Si-Al高强钢进行不同回火温度研究,以探究适宜的回火温度,避免产生第一类、第二类回火脆性的问题,从而获得性能优良的低碳高强钢。方法首先设计一种合适的热处理工艺对试样进行淬火处理,随后采用光学显微镜、扫描电镜... 目的对低碳Fe-Mn-Si-Al高强钢进行不同回火温度研究,以探究适宜的回火温度,避免产生第一类、第二类回火脆性的问题,从而获得性能优良的低碳高强钢。方法首先设计一种合适的热处理工艺对试样进行淬火处理,随后采用光学显微镜、扫描电镜以及拉伸试验及硬度测试等方法,系统研究低碳Fe-Mn-Si-Al高强钢在200~600℃下的组织转变和力学性能。结果与初始试样相比,试验钢在200~400℃范围内回火时,微观组织类型没有明显变化,随着回火温度上升,铁素体晶界逐渐清晰,并在400℃时在铁素体晶界上析出θ-碳化物(Fe_(3)C);当回火温度在500~600℃时,铁素体发生再结晶现象,晶粒过度长大,导致晶界轮廓模糊。随着回火温度的增加,其试样的抗拉强度逐渐下降,初始试样的抗拉强度为1206.0 MPa,回火600℃时,试样抗拉强度为878.8 MPa。材料的强塑积在回火300、400和600℃时较高,分别为32.8、32.5和33.5 GPa%,而200℃和500℃时较低,分别仅为27.3 GPa%和26.9 GPa%,且200℃是试验钢的第一类回火脆性温度,500℃是试验钢的第二类回火脆性温度。试样的硬度在500℃达到最高,为271.3HV。试样的回火拉伸断口断裂方式为韧性断裂,且都存有明显的韧窝状花样。结论系统分析了不同回火温度对低碳Fe-Mn-Si-Al高强钢组织演变规律和力学性能的影响,得出适宜的回火工艺和不同回火温度下的力学性能。对于此类钢,应避免在200℃和500℃的工作环境下使用。 展开更多
关键词 低碳高强钢 回火温度 微观组织 力学性能 回火脆性
下载PDF
Q235和Q345材料的异型管弯曲成型质量的仿真研究
3
作者 王翠竹 潘发兴 《模具技术》 2024年第1期71-79,共9页
由于管坯不同材料的力学特性的差异、热硬化指数、厚向异性系数以及延伸率都不同,使得不同强度钢材在弯曲成型过程中出现各种质量问题。为判断不同材料下不同截面大小的异型管弯曲不同角度成型时对管坯质量的影响,建立了Q235和Q345两种... 由于管坯不同材料的力学特性的差异、热硬化指数、厚向异性系数以及延伸率都不同,使得不同强度钢材在弯曲成型过程中出现各种质量问题。为判断不同材料下不同截面大小的异型管弯曲不同角度成型时对管坯质量的影响,建立了Q235和Q345两种材料弯曲30°~90°的12种工况下的有限元模型。研究结果表明:同一截面尺寸的不同材料,对管坯中面高度缩减率和壁厚减薄率影响规律一致;不同截面尺寸大小的同一材料,其最大中面高度缩减率和最大壁厚减薄率数据相差甚大;临界弯曲角度为60°,超出临界弯曲角度,管坯截面尺寸小且大角度弯曲时,其最大壁厚减薄率呈急速加大趋势,此时严重影响管坯成型质量。 展开更多
关键词 普通碳素结构钢 低合金高强钢 绕弯成型 异型管 有限元模拟
下载PDF
Cu Partitioning Behavior and Its Effect on Microstructure and Mechanical Properties of 0.12C-1.33Mn-0.55Cu Q&P Steel 被引量:6
4
作者 陈连生 HU Baojia +4 位作者 XU Jinghui 田亚强 ZHENG Xiaoping SONG Jinying XU Yong 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2017年第5期1179-1185,共7页
Cu, as an austenitic stable element, is added to steel in order to suppress the adverse effects of high content of C and Mn on welding. Based on C partitioning, Cu and Mn partitioning can further improve the stability... Cu, as an austenitic stable element, is added to steel in order to suppress the adverse effects of high content of C and Mn on welding. Based on C partitioning, Cu and Mn partitioning can further improve the stability of retained austenite in the intercritical annealing process. A sample of low carbon steel containing Cu was treated by the intercritical annealing, then quenching process(I&Q). Subsequently, another sample was treated by the intercritical annealing, subsequent austenitizing, then quenching and partitioning process(I&Q&P). The effects of element partitioning behavior in intercritical region on the microstructure and mechanical properties of the steel were studied. The results showed that after the I&Q process ferrite and martensite could be obtained, with C, Cu and Mn enriched in the martensite. When intercritically heated at 800 ℃, Cu and Mn were partitioned from ferrite to austenite, which was enhanced gradually as the heating time was increased. This partitioning effect was the most obvious when the sample was heated at 800 ℃ for 40 min. At the early stage of α→γ transformation, the formation of γ was controlled by the partitioning of carbon, while at the later stage, it was mainly affected by the partitioning of Cu and Mn. After the I&Q&P process, the partitioning effect of Cu and Mn element could be retained. C was assembled in retained austenite during the quenching and partitioning process. The strength and elongation of I&Q&P steel was increased by 5 305 MPa% compared with that subjected to Q&P process. The volume fraction of retained autensite was increased from 8.5% to 11.2%. Hence, the content of retained austenite could be improved significantly by Mn and Cu partitioning, which increased the elongation of steel. 展开更多
关键词 low carbon high strength steel intercritical annealing element partitioning behavior retained austenite mechanical properties
下载PDF
Evolution of Microstructures of a Low Carbon Bainitic Steel Held at High Service Temperature
5
作者 Chao Sun Shanwu Yang Guoliang Liu 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2014年第3期436-443,共8页
Low carbon bainitic steel derives the high strength mainly from high density of dislocations rather than carbon and alloy element content, so it tends to evolve into equilibrium microstructure with low density of disl... Low carbon bainitic steel derives the high strength mainly from high density of dislocations rather than carbon and alloy element content, so it tends to evolve into equilibrium microstructure with low density of dislocations under thermal disturbance. In the present investigation, granular bainite and lath-like bainitic ferrite were produced respectively in Mo-free low-carbon steels by changing cooling rate;. It has been found that granular bainite possesses a lower strength at room temperature than bainitic ferrite, but it exhibits a slower decrease of strength with temperature increasing. Dislocation density in both granular bainite and bainitic ferrite decreases via recovery and recrystallization at high temperature. However, when reheating of bainite is carded out at temperature below 600 ℃, a long time will be needed for incubation of recrystallization, during which the hardness of bainite maintains stable. The property makes bainite, especially granular bainite, become a potential microstructure for matrix of high strength fire-resistant steel. 展开更多
关键词 low carbon bainitic steel high temperature strength Microstructure evolution RECRYSTALLIZATION BAINITE
原文传递
临界区退火温度对舰船用低碳高强钢组织和性能的影响
6
作者 李子赟 董欣欣 +5 位作者 徐海卫 张露友 刘秋彤 王怡含 李红斌 田亚强 《机械工程材料》 CAS CSCD 北大核心 2023年第6期48-52,85,共6页
对舰船用低碳高强钢进行900℃奥氏体化淬火+不同温度(770,790,810,830℃)临界区退火+500℃回火处理,研究了临界区退火温度对试验钢显微组织和力学性能的影响。结果表明:随着临界区退火温度的升高,退火后形成的板条马氏体和贝氏体发生回... 对舰船用低碳高强钢进行900℃奥氏体化淬火+不同温度(770,790,810,830℃)临界区退火+500℃回火处理,研究了临界区退火温度对试验钢显微组织和力学性能的影响。结果表明:随着临界区退火温度的升高,退火后形成的板条马氏体和贝氏体发生回复,趋于合并而呈块状特征;在770℃退火条件下,试验钢的强度较低,-20℃冲击功较高,冲击断裂模式为韧性断裂;当退火温度升高到790℃及以上时,试验钢的强度增大,冲击功下降,断裂模式转变为准解理断裂,并且冲击功随温度升高进一步下降,拉伸性能则变化不大。 展开更多
关键词 低碳高强钢 临界区退火温度 显微组织 力学性能
下载PDF
热处理对特种设备用高强钢激光–电弧复合焊接头氢脆断裂行为的影响研究 被引量:3
7
作者 张明鲲 王新辉 +1 位作者 张云动 梁治国 《精密成形工程》 北大核心 2023年第5期115-122,共8页
目的提高800 MPa级特种设备用低碳贝氏体高强钢激光–电弧复合焊接头的抗氢脆性能。方法采用预充氢后慢应变速率拉伸试样的方法,定量评估焊态、焊后直接高温回火和焊后调质3种状态下800 MPa级低碳贝氏体高强钢激光–电弧复合焊接头的氢... 目的提高800 MPa级特种设备用低碳贝氏体高强钢激光–电弧复合焊接头的抗氢脆性能。方法采用预充氢后慢应变速率拉伸试样的方法,定量评估焊态、焊后直接高温回火和焊后调质3种状态下800 MPa级低碳贝氏体高强钢激光–电弧复合焊接头的氢脆敏感性,结合扫描电镜下的初始微观组织和断裂特征,讨论抗氢脆性能的改善机理。结果焊后调质处理有效消除了焊接热循环形成的马氏体组织,使接头各区域的微观组织趋于一致,接头的抗氢脆性能较焊态和直接焊后高温回火态的显著提高,断裂特征也从沿晶和穿晶的混合断裂转变为穿晶解理断裂。结论焊后调质处理可以有效提高800 MPa级低碳贝氏体高强钢激光–电弧复合焊接头的抗氢脆性能。 展开更多
关键词 激光-电弧复合焊 低碳贝氏体高强钢 焊后热处理 氢脆 马氏体
下载PDF
Microstructure and Mechanical Properties of 1,000 MPa Ultra-High Strength Hot-Rolled Plate Steel for Coal Mine Refuge Chamber 被引量:2
8
作者 Changsheng Li Biao Ma +1 位作者 Tao Li Tao Zhu 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2014年第3期422-429,共8页
The 1,000 MPa ultra-high strength hot-rolled plate steel with low-carbon bainitic microstructure was developed in the laboratory for coal mine refuge chamber. The static recrystallization behavior, microstructure evol... The 1,000 MPa ultra-high strength hot-rolled plate steel with low-carbon bainitic microstructure was developed in the laboratory for coal mine refuge chamber. The static recrystallization behavior, microstructure evolution, and mechanical properties of this hot-rolled plate steel were investigated by the hot compression, continuous cooling trans- formation, and tensile deformation test. The results show that the developed steel has excellent mechanical properties at both room and elevated temperature, and its microstructure mainly consists of lath bainite, granular bainite, and ferrite after thermal-mechanical control process (TMCP). The ultra-high strength plate steel is obtained by the TMCP process in hot rolling, strengthened by bainitic transformation, microstructure refinement, and precipitation of alloying elements such as Nb, Ti, Mo, and Cu. The experimental steel has relatively low welding crack sensitivity index and high atmospheric corrosion resistance index. Therefore, the developed steel has a good balance of strength and ductility both at room and elevated temperature, weldability and corrosion resistance, and it can suffice for the basic demands for materials in the manufacture of coal mine refuge chamber. 展开更多
关键词 Ultra-high strength steel low-carbon bainite Coal mine refuge chamber MICROSTRUCTURE Mechanical property
原文传递
不同冷轧状态的ELC-BH钢板连续退火再结晶规律 被引量:26
9
作者 关小军 周家娟 +2 位作者 陈晓闽 李阳 马景 《金属热处理》 CAS CSCD 北大核心 2003年第2期31-33,共3页
对不同压下率的ELC BH钢板进行了连续退火试验。研究结果发现 ,随着冷轧压下率增加和冷轧板厚度减薄 ,ELC BH钢板的连续退火再结晶过程提前并缩短 ,晶粒长大过程相对延长 。
关键词 冷轧 ELC-BH钢板 连续退火 再结晶 超低碳钢 烘烤硬化
下载PDF
Q690CFD低碳贝氏体高强钢的焊接性能 被引量:8
10
作者 董现春 张熹 +2 位作者 张立英 陈延清 许良红 《机械工程材料》 CAS CSCD 北大核心 2010年第8期68-71,共4页
用药芯焊丝和实心焊丝对Q690CFD低碳贝氏体高强钢进行了CO_2气体保护焊焊接,采用斜Y裂纹敏感性试验、焊接热影响区最高硬度试验对该钢进行了冷裂敏感性评价,通过冲击试验探讨了从800℃冷却到500℃(t_(8/5))时焊接粗晶区的韧性;通过光学... 用药芯焊丝和实心焊丝对Q690CFD低碳贝氏体高强钢进行了CO_2气体保护焊焊接,采用斜Y裂纹敏感性试验、焊接热影响区最高硬度试验对该钢进行了冷裂敏感性评价,通过冲击试验探讨了从800℃冷却到500℃(t_(8/5))时焊接粗晶区的韧性;通过光学显微镜、拉伸试验机、硬度试验机、冲击试验机等评价了该钢的焊接工艺性。结果表明:该钢板在14℃、不预热条件下焊接将有一定的淬硬倾向;t_(8/5)大于40 s后,粗晶区韧性显著降低;用药芯焊丝当预热温度为80℃(厚25 mm)和100℃(厚30 mm)时或者采用实心焊丝不预热时均可避免裂纹出现,焊接粗晶区组织为板条马氏体和少量贝氏体,焊接接头性能良好,焊后550℃×2 h消除应力热处理对热影响区和母材的拉伸性能没有明显影响。 展开更多
关键词 Q690CFD钢 低碳贝氏体高强钢板 焊接性
下载PDF
铜含量对超高强度低碳贝氏体钢力学性能的影响 被引量:4
11
作者 宋新莉 郭爱民 +2 位作者 袁泽喜 唐金权 董汉雄 《特殊钢》 北大核心 2007年第1期19-20,共2页
实验用低碳贝氏体钢(%:0.042~0.045C、1.43~1.47Mn、1.0~2.5Cu、0.29~0.30Mo、0.025~0.029Nb、0.011~0.018Ti、0.0013~0.0023B)由50kg真空感应炉冶炼。实验结果表明,随铜含量由1.0%增加至2.5%,8.Cu在... 实验用低碳贝氏体钢(%:0.042~0.045C、1.43~1.47Mn、1.0~2.5Cu、0.29~0.30Mo、0.025~0.029Nb、0.011~0.018Ti、0.0013~0.0023B)由50kg真空感应炉冶炼。实验结果表明,随铜含量由1.0%增加至2.5%,8.Cu在钢中沉淀速度加快,峰值硬度增大;随Cu%的增加,轧后直接淬火(DQ)钢的屈服强度由865MPa增至918MPa。DQ+500℃回火钢的屈服强度由935MPa增至1140MPa,但1.0%~2.5%CuDQ+500℃回火钢的抗拉强度和冲击韧性均比DQ态钢有所降低。 展开更多
关键词 超高强度 低碳贝氏体 ε-Cu沉淀 力学性能
下载PDF
新一代低碳钢——HSLC钢 被引量:9
12
作者 傅杰 《中国有色金属学报》 EI CAS CSCD 北大核心 2004年第F01期82-90,共9页
在整个钢生产过程中,综合考虑了钢的冶金质量控制和轧制工艺控制,实现了低碳钢晶粒细化和第二相析出综合强化,使普通成分的低碳钢或不添加微合金元素V,Nb的低C Mn钢的屈服强度达到了400~500MPa,开发了新一代低碳钢———HSLC钢。介绍了... 在整个钢生产过程中,综合考虑了钢的冶金质量控制和轧制工艺控制,实现了低碳钢晶粒细化和第二相析出综合强化,使普通成分的低碳钢或不添加微合金元素V,Nb的低C Mn钢的屈服强度达到了400~500MPa,开发了新一代低碳钢———HSLC钢。介绍了HSLC钢的力学性能及其冶金质量控制,主要为HSLC钢与HSLA钢的力学性能对比;CSP条件下低碳钢中碳的控制;电炉钢低氮控制理论与控制技术;夹杂物超细化—纳米硫化物和氧化物固态析出的成分设计原则和控制技术以及钢中铝的作用与控制。并对低碳钢中纳米铁碳化物的析出及其对钢的强化作用、转炉薄板坯连铸连轧生产HSLC钢以及HSLC钢用于建筑钢筋生产的可能性进行了分析讨论,指出HSLC钢具有广阔的发展前景。 展开更多
关键词 HSLC钢 低碳钢 低碳高强度钢 成分控制 纯洁度控制 析出强化 综合强化
下载PDF
超高强度平头圆柱形弹体对低碳合金钢板的高速撞击实验 被引量:11
13
作者 任杰 徐豫新 王树山 《爆炸与冲击》 EI CAS CSCD 北大核心 2017年第4期629-636,共8页
为分析不同组分低碳合金钢板抗超高强度低碳合金钢弹体的高速撞击性能及破坏模式,以两种典型防弹特种钢SS、AS以及常见的Q235A钢为研究对象,通过静态拉伸、静态压缩及动态压缩测试,获得静态拉伸和压缩性能参数以及1 000~6 000s^(-1)应... 为分析不同组分低碳合金钢板抗超高强度低碳合金钢弹体的高速撞击性能及破坏模式,以两种典型防弹特种钢SS、AS以及常见的Q235A钢为研究对象,通过静态拉伸、静态压缩及动态压缩测试,获得静态拉伸和压缩性能参数以及1 000~6 000s^(-1)应变率范围内的力学行为,分析了材料组分与力学性能的相关性。采用弹道枪加载撞击方法,获得了两种超高强度合金钢平头圆柱形弹体对3种钢板(14.5~15.9mm厚)的弹道极限速度,通过分析获得了不同工况下的极限比吸收能,讨论了合金钢板在弹体高速撞击下破坏模式的差异,分析了材料力学性能与破坏模式的相关性。研究表明:3种合金钢板抗弹体撞击性能与材料屈服强度正相关,但其性能间的差异远小于屈服强度间的差异;在超高强度合金钢平头圆柱形弹体的高速撞击下,3种钢板的失效机制与其力学性能密切相关,Si和Mn含量高的AS钢呈硬脆性特征,其断裂失效主要取决于材料的剪切强度,而Si和Mn含量较低的SS钢和Q235A钢具有良好的塑性,其断裂失效主要取决于材料的压缩强度和剪切强度。 展开更多
关键词 破坏模式 高速撞击 低碳合金钢 超高强度弹体
下载PDF
一种新型700 MPa级低碳高强度钢的研制 被引量:4
14
作者 衣海龙 杜林秀 +2 位作者 李晓强 王国栋 刘相华 《机械工程材料》 CAS CSCD 北大核心 2006年第11期43-44,55,共3页
通过控制轧制与控制冷却,研制出下屈服强度为700 MPa级的低碳高强度钢,并对其组织及强化机制进行了分析。结果表明:该高强度钢的组织为铁素体,其强化相为细晶铁素体及在铁素体基体上分布的细小析出相,且析出强化量为250MPa,这是过去热... 通过控制轧制与控制冷却,研制出下屈服强度为700 MPa级的低碳高强度钢,并对其组织及强化机制进行了分析。结果表明:该高强度钢的组织为铁素体,其强化相为细晶铁素体及在铁素体基体上分布的细小析出相,且析出强化量为250MPa,这是过去热轧微合金钢板的2~4倍。铁素体基体中较高的位错密度和分布细小的析出物改善了钢材的塑性,使材料具有良好的伸长率。 展开更多
关键词 控制轧制 控制冷却 低碳高强度钢
下载PDF
含磷高强IF钢中心偏析研究 被引量:3
15
作者 闫永其 崔衡 +2 位作者 王征 刘柏松 陈斌 《铸造技术》 CAS 北大核心 2015年第7期1627-1630,共4页
通过热酸侵蚀、原位分析和化学分析,研究含磷高强IF钢铸坯中P、S和Mn元素的中心偏析情况。结果表明,铸坯宽度1/4处存在明显的中心偏析情况,伴随有中心疏松和缩孔等缺陷。铸坯宽度1/2处S元素的最大偏析度为1.08,偏析带较宽,Mn和P元素不... 通过热酸侵蚀、原位分析和化学分析,研究含磷高强IF钢铸坯中P、S和Mn元素的中心偏析情况。结果表明,铸坯宽度1/4处存在明显的中心偏析情况,伴随有中心疏松和缩孔等缺陷。铸坯宽度1/2处S元素的最大偏析度为1.08,偏析带较宽,Mn和P元素不存在明显中心偏析。 展开更多
关键词 中心偏析 高强IF钢 超低碳
下载PDF
过热度和轻压下量对高强IF钢中心偏析的影响 被引量:1
16
作者 闫永其 崔衡 +3 位作者 王征 刘柏松 刘国梁 青靓 《铸造技术》 CAS 北大核心 2017年第1期43-45,53,共4页
通过热酸侵蚀、化学分析等方法,对不同浇注过热度、不同凝固末端轻压下量条件下生产的高强IF钢铸坯中心偏析情况进行研究,分析浇注过热度及轻压下量对铸坯中心偏析的影响。结果表明:试验条件下轻压下量为2.9 mm或3.9 mm对铸坯中心偏析... 通过热酸侵蚀、化学分析等方法,对不同浇注过热度、不同凝固末端轻压下量条件下生产的高强IF钢铸坯中心偏析情况进行研究,分析浇注过热度及轻压下量对铸坯中心偏析的影响。结果表明:试验条件下轻压下量为2.9 mm或3.9 mm对铸坯中心偏析没有影响,而浇注过热度为33℃或29℃对铸坯中心偏析影响较大,过热度越高,铸坯中心偏析越严重。浇注过热度为33℃时,P元素中心偏析度在0.95~1.08之间,S元素中心偏析度在0.91~1.12之间;浇注过热度为29℃时,P元素中心偏析度控制在0.95~1.03之间,S元素中心偏析度控制在0.93~1.07之间。在浇注条件允许的情况下,应该尽量降低浇注过热度。 展开更多
关键词 中心偏析 高强IF钢 超低碳钢
下载PDF
超低碳高强度BH钢板的织构发展 被引量:6
17
作者 关小军 王先进 +1 位作者 凤佩华 朱学刚 《钢铁研究》 CAS 1995年第5期22-25,共4页
采用三维取向分布函数—ODF对实验室所研制的一种超低碳高强度烘烤硬化钢板不同工艺过程的织构进行了研究。结果表明,它的热轧、冷轧和退火织构之间存在一定的联系,以至于织构的发展具有遗传性。
关键词 超低碳钢 高强度 烘烤 硬化 织构 钢板
下载PDF
390MPa级Ti+Nb超低碳高强度BH钢组织性能研究 被引量:4
18
作者 刘光明 康永林 +3 位作者 陈继平 冯月雪 周建 滕华湘 《材料工程》 EI CAS CSCD 北大核心 2010年第4期5-9,共5页
对Ti+Nb+B复合处理超低碳高强度BH钢的热轧、冷轧和连续退火进行实验。结果表明:试制的超低碳高强度BH钢退火板的屈强比为0.536,烘烤硬化值为44MPa,具有较为优良的成形性能和烘烤硬化性能,抗拉强度为394MPa,达到了390MPa级超低碳高强度B... 对Ti+Nb+B复合处理超低碳高强度BH钢的热轧、冷轧和连续退火进行实验。结果表明:试制的超低碳高强度BH钢退火板的屈强比为0.536,烘烤硬化值为44MPa,具有较为优良的成形性能和烘烤硬化性能,抗拉强度为394MPa,达到了390MPa级超低碳高强度BH钢板的强度要求。物理化学相分析表明:添加在超低碳高强度BH钢中的B除了析出了2mg/kg的BN,大部分的B在钢中以间隙固溶的形式存在,对超低碳高强度BH钢基体起到了固溶强化的作用。 展开更多
关键词 超低碳 高强度BH钢 Ti+Nb+B 第二相析出 固溶强化
下载PDF
超高强低碳Si-Mn冷轧双相钢的回火组织和力学性能研究 被引量:11
19
作者 蒋俊华 李俊 胡文彬 《金属热处理》 EI CAS CSCD 北大核心 2007年第9期14-18,共5页
将Fe-0.12C-0.45Si-1.80Mn-0.25Cr钢轧硬材在临界区加热保温后水冷,获得抗拉强度超过1100 MPa的铁素体+马氏体双相钢.研究了不同温度回火后,该双相钢组织和力学性能的变化.结果表明,低碳Si-Mn冷轧双相钢随着回火温度的提高,强度逐渐下... 将Fe-0.12C-0.45Si-1.80Mn-0.25Cr钢轧硬材在临界区加热保温后水冷,获得抗拉强度超过1100 MPa的铁素体+马氏体双相钢.研究了不同温度回火后,该双相钢组织和力学性能的变化.结果表明,低碳Si-Mn冷轧双相钢随着回火温度的提高,强度逐渐下降而伸长率增加.在200~300 ℃回火,强度性能下降不多但伸长率大大提高,而且屈强比低,有利于获得较好的综合性能(抗拉强度大于1000 MPa,总伸长率接近14%).在回火温度超过300 ℃时,马氏体岛内孪晶晶界变得模糊,回火温度达到600 ℃时,马氏体岛分解比较完全,分解为粗大渗碳体球化颗粒.超过300 ℃回火后,应力应变曲线出现不连续屈服,而且随着回火温度增加屈服平台逐渐伸长. 展开更多
关键词 超高强低碳Si-Mn双相钢 回火组织 力学性能
下载PDF
低碳贝氏体高强钢Q690CFD焊接粗晶区组织韧性 被引量:11
20
作者 董现春 张熹 陈延清 《钢铁钒钛》 CAS 北大核心 2011年第1期62-66,共5页
利用Gleeble-2000热模拟试验机对低碳贝氏体高强钢Q690CFD进行不同焊接工艺下的热模拟试验,研究焊接条件下热影响区粗晶区(CGHAZ)组织、韧性及其变化规律。结果表明:CGHAZ组织为板条马氏体;CGHAZ韧性在800~500℃随冷却时间增大而降低;... 利用Gleeble-2000热模拟试验机对低碳贝氏体高强钢Q690CFD进行不同焊接工艺下的热模拟试验,研究焊接条件下热影响区粗晶区(CGHAZ)组织、韧性及其变化规律。结果表明:CGHAZ组织为板条马氏体;CGHAZ韧性在800~500℃随冷却时间增大而降低;在合适的条件下焊接,CGHAZ可获得很好低温韧性。同时对粗晶区进行了不同温度的焊后处理,研究焊后热处理后组织、韧性变化规律。随着热处理温度的提高,粗晶区冲击韧性呈降低趋势。在250~500℃范围内进行焊后热处理,可以获得优异的冲击韧性。应尽量避免在500℃以上长时间保温处理。 展开更多
关键词 Q690CFD 低碳贝氏体 高强钢 粗晶区组织韧性 消除应力热处理
下载PDF
上一页 1 2 6 下一页 到第