The aging-hardening kinetics of powder metallurgy processed 2014Al alloy and its composite have been studied. The existence of n-SiC particulates leads to the increase of peak hardness. Interestingly, the aginghardeni... The aging-hardening kinetics of powder metallurgy processed 2014Al alloy and its composite have been studied. The existence of n-SiC particulates leads to the increase of peak hardness. Interestingly, the aginghardening peak of the composite takes place at earlier time than that of the unreinforced alloy. Transmission electron microscopy(TEM) studies indicated that the major precipitation phases are Al_5Cu_2Mn_3 and θ′(Al_2Cu). Besides, Ω phase appeared in both specimens at peak hardening condition, which has been rarely observed previously in aluminum metal matrix composites without Ag. Accelerated aging kinetics and increased peak hardness may be attributed to the higher dislocation density resulted from the mismatch of coefficients of thermal expansion between n-SiC and 2014Al matrix. The results are beneficial to fabricating high performance composites for the application in automobile field such as pistons, driveshaft tubes, brake rotors, bicycle frames, railroad brakes. 展开更多
关键词 Metal matrix composites Nano-SiC Powder metallurgy hot extrusion aging hardening
原文传递
Comparison effects of lanthanum stearate and antioxidants in epoxidized natural rubber 被引量:2
2
作者 杨昌金 罗勇悦 +2 位作者 彭政 许逵 钟杰平 《Journal of Rare Earths》 SCIE EI CAS CSCD 2015年第11期1236-1240,共5页
This work studied possibilities of using lanthanum stearate(LaS t) as an antioxidant in epoxidized natural rubber containing 25 mol.% expoxidation(ENR25) compounds. For comparison purposes, two commercial antioxid... This work studied possibilities of using lanthanum stearate(LaS t) as an antioxidant in epoxidized natural rubber containing 25 mol.% expoxidation(ENR25) compounds. For comparison purposes, two commercial antioxidant 4010 NA and MB were also used. The influence of LaS t, antioxidant 4010 NA and MB on cure characteristics, mechanical properties, crosslink density, hot air aging and thermo-oxidative degradation were studied. The results indicated that the incorporation of LaS t and antioxidants could accelerate the vulcanization of ENR. The ENR vulcanizates with antioxidant MB had better mechanical properties than 4010 NA and LaS t. Compared with antioxidant 4010 NA and MB, the ENR25 vulcanizates with the addition of LaS t exhibited the best hot air aging resistance and thermo-oxidative stability. 展开更多
关键词 lanthanum stearate antioxidants ENR25 thermal degradation hot air aging resistance rare earths