期刊文献+
共找到18,663篇文章
< 1 2 250 >
每页显示 20 50 100
Selective leaching of lithium from spent lithium-ion batteries using sulfuric acid and oxalic acid 被引量:1
1
作者 Haijun Yu Dongxing Wang +6 位作者 Shuai Rao Lijuan Duan Cairu Shao Xiaohui Tu Zhiyuan Ma Hongyang Cao Zhiqiang Liu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第4期688-696,共9页
Traditional hydrometallurgical methods for recovering spent lithium-ion batteries(LIBs)involve acid leaching to simultaneously extract all valuable metals into the leachate.These methods usually are followed by a seri... Traditional hydrometallurgical methods for recovering spent lithium-ion batteries(LIBs)involve acid leaching to simultaneously extract all valuable metals into the leachate.These methods usually are followed by a series of separation steps such as precipitation,extraction,and stripping to separate the individual valuable metals.In this study,we present a process for selectively leaching lithium through the synergistic effect of sulfuric and oxalic acids.Under optimal leaching conditions(leaching time of 1.5 h,leaching temperature of 70°C,liquid-solid ratio of 4 mL/g,oxalic acid ratio of 1.3,and sulfuric acid ratio of 1.3),the lithium leaching efficiency reached89.6%,and the leaching efficiencies of Ni,Co,and Mn were 12.8%,6.5%,and 21.7%.X-ray diffraction(XRD)and inductively coupled plasma optical emission spectrometer(ICP-OES)analyses showed that most of the Ni,Co,and Mn in the raw material remained as solid residue oxides and oxalates.This study offers a new approach to enriching the relevant theory for selectively recovering lithium from spent LIBs. 展开更多
关键词 selective leaching oxalic acid sulfuric acid spent lithium-ion batteries
下载PDF
Recovery of Li, Ni, Co and Mn from spent lithium-ion batteries assisted by organic acids: Process optimization and leaching mechanism 被引量:1
2
作者 Liuyi Ren Bo Liu +5 位作者 Shenxu Bao Wei Ding Yimin Zhang Xiaochuan Hou Chao Lin Bo Chen 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第3期518-530,共13页
The proper recycling of spent lithium-ion batteries(LIBs)can promote the recovery and utilization of valuable resources,while also negative environmental effects resulting from the presence of toxic and hazardous subs... The proper recycling of spent lithium-ion batteries(LIBs)can promote the recovery and utilization of valuable resources,while also negative environmental effects resulting from the presence of toxic and hazardous substances.In this study,a new environmentally friendly hydro-metallurgical process was proposed for leaching lithium(Li),nickel(Ni),cobalt(Co),and manganese(Mn)from spent LIBs using sulfuric acid with citric acid as a reductant.The effects of the concentration of sulfuric acid,the leaching temperature,the leaching time,the solid-liquid ratio,and the reducing agent dosage on the leaching behavior of the above elements were investigated.Key parameters were optimized using response surface methodology(RSM)to maximize the recovery of metals from spent LIBs.The maxim-um recovery efficiencies of Li,Ni,Co,and Mn can reach 99.08%,98.76%,98.33%,and 97.63%.under the optimized conditions(the sulfuric acid concentration was 1.16 mol/L,the citric acid dosage was 15wt%,the solid-liquid ratio was 40 g/L,and the temperature was 83℃ for 120 min),respectively.It was found that in the collaborative leaching process of sulfuric acid and citric acid,the citric acid initially provided strong reducing CO_(2)^(-),and the transition metal ions in the high state underwent a reduction reaction to produce transition metal ions in the low state.Additionally,citric acid can also act as a proton donor and chelate with lower-priced transition metal ions,thus speeding up the dissolution process. 展开更多
关键词 spent lithium-ion batteries leaching response surface methodology sulfuric acid citric acid
下载PDF
Effect of Na_(2)CO_(3)Roasting Activation on Acid Leaching Property of Fly Ash
3
作者 LIU Chenjia ZHAO Aichun +4 位作者 YE Xin ZHAO Zi ZHANG Tingan YANG Xiaorong QIN Yanmei 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2024年第6期1613-1620,共8页
By using high-alumina fly ash as raw material,a process was proposed for activating the fly ash with Na_(2)CO_(3)calcination and extracting aluminum from activated clinker with sulfuric acid leaching.The feasibility o... By using high-alumina fly ash as raw material,a process was proposed for activating the fly ash with Na_(2)CO_(3)calcination and extracting aluminum from activated clinker with sulfuric acid leaching.The feasibility of roasting process of activated fly ash by Na_(2)CO_(3)was discussed based on thermodynamic analysis.The experimental results showed that Na_(2)CO_(3)gradually reactes with mullite over 700 K to produce NaAlSiO_(4).The optimal process conditions for the activation stage are:a material ratio of 1:1 between sodium carbonate and fly ash,a calcination temperature of 900℃,and a calcination time of 2.5 hours.Under these conditions,the leaching rate of aluminum is 90.3%.By comparing the SEM and XRD analysis of raw and clinker materials,it could be concluded that the mullite phase of fly ash is almost completely destroyed and transformed into sodium aluminosilicate with good acid solubility. 展开更多
关键词 fly ash calcination activation acid leaching ALUMINUM
下载PDF
Hydrometallurgical processing of chalcopyrite:A review of leaching techniques
4
作者 Darwin Michell Cheje Machaca Amilton Barbosa Botelho Junior +2 位作者 Thamyres Cardoso de Carvalho Jorge Alberto Soares Tenório Denise Crocce Romano Espinosa 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第12期2537-2555,共19页
Copper,an essential metal for the energy transition,is primarily obtained from chalcopyrite through hydrometallurgical and pyrometallurgical methods.The risks and harmful impacts of these processes pose significant co... Copper,an essential metal for the energy transition,is primarily obtained from chalcopyrite through hydrometallurgical and pyrometallurgical methods.The risks and harmful impacts of these processes pose significant concerns for environmental and human safety,highlighting the need for more efficient and eco-friendly hydrometallurgical methods.This review article emphasizes current pro-cesses such as oxidative leaching,bioleaching,and pressure leaching that have demonstrated efficiency in overcoming the complicated chalcopyrite network.Oxidative leaching operates under benign conditions within the leaching media;nevertheless,the introduction of oxidizing agents provides benefits and advantages.Bioleaching,a non-aggressive method,has shown a gradual increase in copper extrac-tion efficiency and has been explored using both primary and secondary sources.Pressure leaching,known for its effectiveness and se-lectivity in copper extraction,is becoming commercially more viable with increased research investments.This research also provides im-portant data for advancing future research in the field. 展开更多
关键词 chalcopyrite leaching BIOleaching ionic liquids CHLORIDE hydrogen peroxide
下载PDF
Study on synergistic leaching of potassium and phosphorus from potassium feldspar and solid waste phosphogypsum via coupling reactions
5
作者 Chao Li Shizhao Wang +3 位作者 Yunshan Wang Xuebin An Gang Yang Yong Sun 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2024年第1期117-129,共13页
To achieve the resource utilization of solid waste phosphogypsum(PG)and tackle the problem of utilizing potassium feldspar(PF),a coupled synergistic process between PG and PF is proposed in this paper.The study invest... To achieve the resource utilization of solid waste phosphogypsum(PG)and tackle the problem of utilizing potassium feldspar(PF),a coupled synergistic process between PG and PF is proposed in this paper.The study investigates the features of P and F in PG,and explores the decomposition of PF using hydrofluoric acid(HF)in the sulfuric acid system for K leaching and leaching of P and F in PG.The impact factors such as sulfuric acid concentration,reaction temperature,reaction time,material ratio(PG/PF),liquid–solid ratio,PF particle size,and PF calcination temperature on the leaching of P and K is systematically investigated in this paper.The results show that under optimal conditions,the leaching rate of K and P reach more than 93%and 96%,respectively.Kinetics study using shrinking core model(SCM)indicates two significant stages with internal diffusion predominantly controlling the leaching of K.The apparent activation energies of these two stages are 11.92 kJ·mol^(-1)and 11.55 kJ·mol^(-1),respectively. 展开更多
关键词 PHOSPHOGYPSUM Potassium feldspar Coupling reaction leaching Waste treatment Kinetics
下载PDF
Effect of Saline Water on Soil Acidity, Alkalinity and Nutrients Leaching in Sandy Loamy Soil in Rwamagana Bella Flower Farm, Rwanda
6
作者 Abel Mwubahaman Wali Umaru Garba +3 位作者 Hussein Bizimana Jean de Dieu Bazimenyera Eric Derrick Bugenimana Jean Nepomuscene Nsengiyumva 《Agricultural Sciences》 2024年第1期15-35,共21页
The necessity to saline and sodic waters is sometimes used for irrigating agricultural activities under certain circumstances, but it is important to note that the use of these waters comes with specific consideration... The necessity to saline and sodic waters is sometimes used for irrigating agricultural activities under certain circumstances, but it is important to note that the use of these waters comes with specific considerations and limitations. One way to decrease undesirable effects of sodic waters on the physical and chemical properties of soils is to apply organic and chemical amendments within the soil. This study aimed to assess the effectiveness of saline water on soil acidity, alkalinity and nutrients leaching in sandy loamy soil at Bella flower farm, in Rwamagana District, Rwanda. The water used was from the Muhazi Lake which is classified as Class I (Saline water quality). Column leaching experiments using treated soils were then conducted under saturated conditions. The soil under experimental was first analyzed for its textural classification, soil properties and is classified as sandy loamy soil. The t-test was taken at 1%, 5% and 10% levels of statistical significance compared to control soil. The results indicated that the application of saline water to soils caused an increase in some soil nutrients like increase of Phosphorus (P), Potassium (K<sup>+</sup>), Magnesium (Mg2<sup>+</sup>), Sulphur (S), CN ratio and Sodium (Na<sup>+</sup>) and decreased soil texture, physical and chemical properties and remained soil nutrients. Consequently, the intensive addition of saline water leachates to soil in PVC pipes led to decreased of soil EC through leaching and a raiser Soluble Sodium Percentage (SSP). The rate of saline water application affected the increase accumulation of SAR and Na% in the top soil layers. The study indicated that saline water is an inefficient amendment for sandy soil with saline water irrigation. The study recommends further studies with similar topic with saline water irrigation, as it accentuated the alkalinity levels. 展开更多
关键词 NUTRIENTS leaching Saline Water Soil Acidity Soil Alkalinity
下载PDF
Experimental investigation of dynamic characteristics of leaching tubing for solution mining of salt cavern carbon and energy storage
7
作者 Yin-Ping Li Xin-Bo Ge +1 位作者 Xi-Lin Shi Hong-Ling Ma 《Petroleum Science》 SCIE EI CAS CSCD 2024年第4期2703-2722,共20页
Salt caverns are extensively utilized for storing various substances such as fossil energy,hydrogen,compressed air,nuclear waste,and industrial solid waste.In China,when the salt cavern is leached through single-well ... Salt caverns are extensively utilized for storing various substances such as fossil energy,hydrogen,compressed air,nuclear waste,and industrial solid waste.In China,when the salt cavern is leached through single-well water solution mining with oil as a cushion,engineering challenges arise with the leaching tubing,leading to issues like damage and instability.These problems significantly hinder the progress of cavern construction and the control of cavern shape.The primary cause of this is the flowinduced vibration instability of leaching tubing within a confined space,which results in severe bending or damage to the tubing.This study presents a model experimental investigation on the dynamic characteristics of leaching tubing using a self-developed liquid-solid coupling physical model experiment apparatus.The experiment utilizes a silicone-rubber pipe(SRP)and a polycarbonate pipe(PCP)to examine the effects of various factors on the dynamic stability of cantilevered pipes conveying fluid.These factors include external space constraint,flexural rigidity,medium outside the pipe,overhanging length,and end conditions.The experiments reveal four dynamic response phenomena:water hammer,static buckling,chaotic motion,and flutter instability.The study further demonstrates that the length of the external space constraint has a direct impact on the flutter critical flow velocity of the cantilevered pipe conveying fluid.Additionally,the flutter critical flow velocity is influenced by the end conditions and different external media. 展开更多
关键词 Salt cavern storage Solution mining leaching tubing Experimental investigation Flutter instability
下载PDF
Extraction of Valuable Metals from Titanium-bearing Blast Furnace Slag by Acid Leaching
8
作者 刘燕 CHEN Xuegui +2 位作者 MAO Shuaidong XIAO Yadong LI Jiacong 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2024年第2期376-385,共10页
To realize the resource utilization of the valuable metals in the titanium-containing blast furnace slag,the process route of “hydrochloric acid leaching-electrolysis-carbonization and carbon dioxide capture-preparat... To realize the resource utilization of the valuable metals in the titanium-containing blast furnace slag,the process route of “hydrochloric acid leaching-electrolysis-carbonization and carbon dioxide capture-preparation of calcium carbonate” was proposed.In this study,the influences of process conditions on the leaching rates of calcium,magnesium,aluminum,and iron and the phases of the leaching residue were investigated for the leaching process.The experimental results show that the HCl solution could selectively leach the elements from the titanium-containing blast furnace slag.The better leaching conditions are the HCl solution concentration of 4 mol/L,the leaching time of 30 min,the ratio of liquid volume to solid gas of 10 mL/g,and the stirring paddle speed of 300 r/min.Under the conditions,the leaching rates of calcium,magnesium,aluminum,and iron can reach 85.87%,73.41%,81.35%,and 59.08%,and the leaching rate of titanium is 10.71%.The iron and the aluminum are removed from the leachate to obtain iron-aluminum water purification agents,and the magnesium is removed from the leachate to obtain magnesium hydroxide.The leaching residue phase is dominated by perovskite,followed by magnesium silicate and tricalcium aluminate,and the titaniumrich material could be obtained from the leaching residue by desiliconization. 展开更多
关键词 titanium-containing blast furnace slag acid leaching valuable metals comprehensive utilization
下载PDF
Preparation of sodium molybdate from molybdenum concentrate by microwave roasting and alkali leaching
9
作者 Fengjuan Zhang Chenhui Liu +2 位作者 Srinivasakannan Chandrasekar Yingwei Li Fuchang Xu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CSCD 2024年第1期91-105,共15页
The preparation process of sodium molybdate has the disadvantages of high energy consumption,low thermal efficiency,and high raw material requirement of molybdenum trioxide,in order to realize the green and efficient ... The preparation process of sodium molybdate has the disadvantages of high energy consumption,low thermal efficiency,and high raw material requirement of molybdenum trioxide,in order to realize the green and efficient development of molybdenum concentrate resources,this paper proposes a new process for efficient recovery of molybdenum from molybdenum concentrate and preparation of sodium molybdate by microwave-enhanced roasting and alkali leaching.Thermodynamic analysis indicated the feasibility of oxidation roasting of molybdenum concentrate.The effects of roasting temperature,holding time,and power-to-mass ratio on the oxidation product and leaching product sodium molybdate (Na_(2)MoO_(4)·2H_(2)O) were investigated.Under the optimal process conditions:roasting temperature of 700℃,holding time of 110 min,and power-to-mass ratio of 110 W/g,the molybdenum state of existence was converted from MoS_(2) to Mo O3.The process of preparing sodium molybdate by alkali leaching of molybdenum calcine was investigated,the optimal leaching conditions include a solution concentration of 2.5 mol/L,a liquid-to-solid ratio of 2 mL/g,a leaching temperature of 60℃,and leaching solution termination at pH 8.The optimum conditions result in a leaching rate of sodium molybdate of 96.24%.Meanwhile,the content of sodium molybdate reaches 94.08wt%after leaching and removing impurities.Iron and aluminum impurities can be effectively separated by adjusting the pH of the leaching solution with sodium carbonate solution.This research avoids the shortcomings of the traditional process and utilizes the advantages of microwave metallurgy to prepare high-quality sodium molybdate,which provides a new idea for the highvalue utilization of molybdenum concentrate. 展开更多
关键词 molybdenum metallurgy microwave oxidation roasting removing impurities sodium hydroxide leaching
下载PDF
Process engineering of demineralisation of moderate to high ash Indian coals through NaOH‑HCl leaching and HF leaching
10
作者 Heena Dhawan D.K.Sharma 《International Journal of Coal Science & Technology》 EI CAS CSCD 2024年第2期111-122,共12页
Chemical leaching of coals would be required to produce cleaner coals for some special applications where physical benefi-ciation may not be effective enough.This would also help in recovering Li and rare earth metals... Chemical leaching of coals would be required to produce cleaner coals for some special applications where physical benefi-ciation may not be effective enough.This would also help in recovering Li and rare earth metals besides in the sequestration of CO_(2).About 20 Indian coals having complexly distributed moderate to high ash contents were sequentially treated with various alkali–acid such as NaOH-HCl,HF,HCl,HCl-HF,and NaOH-HCl-HF leaching.This aimed to establish and design the best stepwise sequential process for the highest degree of demineralisation through a chemical leaching process.Kinetics and process intensification studies were carried out.More than 80%demineralisation of Madhaipur and Neemcha coals was observed using the best sequential treatment designed presently.The repeated stepwise treatment of the alkali and the acid was also studied,which was found to significantly enhance the degree of demineralisation of coals.The integrated process of alkali–acid leaching followed by solvent extraction(Organo-refining)and vice versa of the treated coal was also studied for producing cleaner coals. 展开更多
关键词 Alkali–acid leaching DEMINERALISATION Integrated process Rare earth elements
下载PDF
Study on metal recovery process and kinetics of oxidative leaching from spent LiFePO_(4)Li-batteries
11
作者 Xiaoming Zhang Wen Xie +5 位作者 Xiaolei Zhou Wenjie Zhang Jiawei Wen Xin Wang Guoyong Huang Shengming Xu 《Chinese Journal of Chemical Engineering》 SCIE EI CAS CSCD 2024年第4期94-102,共9页
A green environmental protection and enhanced leaching process was proposed to recover all elements from spent lithium iron phosphate(LiFePO_(4)) lithium batteries.In order to reduce the influence of Al impurity in th... A green environmental protection and enhanced leaching process was proposed to recover all elements from spent lithium iron phosphate(LiFePO_(4)) lithium batteries.In order to reduce the influence of Al impurity in the recovery process,NaOH was used to remove impurity.After impurity removal,the spent LiFePO_(4) cathode material was used as raw material under the H_(2)SO_(4) system,and the pressure oxidation leaching process was adopted to achieve the preferential leaching of lithium.The E-pH diagram of the Fe-P-Al-H_(2)O system can determine the stable region of each element in the recovery process of spent LiFePO_(4)Li-batteries.Under the optimal conditions(500 r·min^(-1),15 h,363.15 K,0.4 MPa,the liquid-solid ratio was 4:1 ml·g^(-1)and the acid-material ratio was 0.29),the leaching rate of Li was 99.24%,Fe,Al,and Ti were 0.10%,2.07%,and 0.03%,respectively.The Fe and P were precipitated and recovered as FePO_(4)·2H_(2)O.The kinetic analysis shows that the process of high-pressure acid leaching of spent LiFePO_(4) materials depends on the surface chemical reaction.Through the life cycle assessment(LCA)of the spent LiFePO_(4) whole recovery process,eight midpoint impact categories were selected to assess the impact of recovery process.The results can provide basic environmental information on production process for recycling industry. 展开更多
关键词 Spent LiFePO_(4)Li-batteries Oxidative leaching Kinetic study Life cycle assessment
下载PDF
Environmental availability and ecological risk assessment of heavy metals in zinc leaching residue 被引量:26
12
作者 闵小波 谢先德 +3 位作者 柴立元 梁彦杰 李密 柯勇 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第1期208-218,共11页
Four different methods,namely mineralogical analysis,three-stage BCR sequential extraction procedure,dynamic leaching test and Hakanson Potential Ecological Risk Index Method were used to access the environmental acti... Four different methods,namely mineralogical analysis,three-stage BCR sequential extraction procedure,dynamic leaching test and Hakanson Potential Ecological Risk Index Method were used to access the environmental activity and potential ecological risks of heavy metals in zinc leaching residue.The results demonstrate that the environmental activity of heavy metals declines in the following order:CdZnCuAsPb.Potential ecological risk indices for single heavy metal are CdZnCuAsPb.Cd has serious potential ecological risk to the ecological environment and contributes most to the potential toxicity response indices for various heavy metals in the residue. 展开更多
关键词 heavy metals BCR sequential extraction environmental availability leaching toxicity dynamic leaching potential ecological risk index method zinc leaching residue
下载PDF
Leaching behavior of metals from high-arsenic dust by NaOH-Na_2S alkaline leaching 被引量:23
13
作者 郭学益 易宇 +1 位作者 石靖 田庆华 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2016年第2期575-580,共6页
Arsenic is selectively extracted from high-arsenic dust by NaOH-Na2S alkaline leaching process. In the leaching arsenic process, the effects of alkali-to-dust ratio, sodium sulfide addition, leaching temperature, leac... Arsenic is selectively extracted from high-arsenic dust by NaOH-Na2S alkaline leaching process. In the leaching arsenic process, the effects of alkali-to-dust ratio, sodium sulfide addition, leaching temperature, leaching time and liquid-to-solid ratio on metals leaching efficiencies were investigated. The results show that the arsenic can be effectively separated from other metals under the optimum conditions of alkali/dust mass ratio of 0.5, sodium sulfide addition of 0.25 g/g, leaching temperature of 90 ℃, leaching time of 2 h, and liquid-to-solid ratio of 5:1 (mL/g). Under these conditions, the average leaching efficiencies of arsenic, antimony, lead, tin and zinc are 92.75%, 11.68%, 0.31%, 29.75% and 36.85%, respectively. The NaOH-Na2S alkaline leaching process provides a simple and highly efficient way to remove arsenic from high-arsenic dust, leaving residue as a suitable lead resource. 展开更多
关键词 high arsenic dust alkaline leaching leaching behavior ARSENIC
下载PDF
Technological mineralogy and environmental activity of zinc leaching residue from zinc hydrometallurgical process 被引量:19
14
作者 李密 彭兵 +3 位作者 柴立元 彭宁 谢先德 闫缓 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第5期1480-1488,共9页
Chemical, physical, structural and morphological properties of zinc leaching residue were examined by the combination of various detection means such as AAS, XRF, XRD, M?ssbauer spectrometry, SEM-EDS, TG-DSC, XPS and... Chemical, physical, structural and morphological properties of zinc leaching residue were examined by the combination of various detection means such as AAS, XRF, XRD, M?ssbauer spectrometry, SEM-EDS, TG-DSC, XPS and FTIR. The toxicity characteristic leaching procedure (TCLP) was used to investigate the environmental activity of zinc leaching residue for a short contact time. The phase composition analysis indicated that the zinc leaching residue mainly consists of super refined flocculent particles including zinc ferrite, sulfate and silicate. The physical structural analysis showed that it has a thermal instability and strong water absorption properties. The results of TCLP indicated that the amounts of Zn and Cd in the leaching solution exceed 40 and 90 times of limit, respectively, which demonstrate that this residue is unstable in weak acidic environment for a short contact time. 展开更多
关键词 zinc leaching residue phase composition microstructure technological mineralogy leaching toxicity
下载PDF
Leaching of heavy metals from Dexing copper mine tailings pond 被引量:25
15
作者 郭耀广 黄鹏 +5 位作者 张武刚 袁学武 范凤霞 王焕丽 柳建设 王兆慧 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第10期3068-3075,共8页
AThe wastewater source of 4# tailing pond in Dexing copper mine consists of alkaline flotation pulp and acid mine drainage (AMD) from the nearby opencast mine. Therefore, the heavy metals in tailing ore are very lik... AThe wastewater source of 4# tailing pond in Dexing copper mine consists of alkaline flotation pulp and acid mine drainage (AMD) from the nearby opencast mine. Therefore, the heavy metals in tailing ore are very likely to be released due to acidification from AMD. The leaching behaviors ofZn, Cu, Fe and Mn in mine tailings from Dexing copper mine were investigated by a series of laboratory batch experiments. The effectcs ofpH, temperature, particle size and contact time on the leachability of such heavy metals were examined. It was evident that Zn, Cu, Fe and Mn were major heavy metals in the tailings while gangue minerals like quartz were major constituents in examined tailings. The tailing dissolution reaction was controlled by the acid, whose kinetics could be expressed according to the heterogeneous reaction models and explained by a shrinking core model with the surface chemical reaction as the rate-controlling step. The leachability of all metals examined depended on pH and contact time. The batch studies indicated that the maximum leaching ratios ofZn, Cu, Fe and Mn at pH 2.0 were 5.4%, 5.8%, l 1.1% and 34.1%, respectively. The dissolubility of all metals examined was positively correlated to the temperatures. The particle size would not change dissolution tendency of those heavy metals, but decrease the concentrations of leached heavy metals. 展开更多
关键词 leaching TAILINGS heavy metals dissolution rate
下载PDF
Leaching behavior of metals from limonitic laterite ore by high pressure acid leaching 被引量:14
16
作者 郭学益 石文堂 +1 位作者 李栋 田庆华 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第1期191-195,共5页
The leaching behavior of metals from a nickeliferous limonitic laterite ore was investigated by high pressure acid leaching process for the extraction of nickel and cobalt.The effects of sulfuric acid added,leaching t... The leaching behavior of metals from a nickeliferous limonitic laterite ore was investigated by high pressure acid leaching process for the extraction of nickel and cobalt.The effects of sulfuric acid added,leaching temperature,leaching time and liquid/solid(L/S) ratio on metals extraction were examined.More than 97% Ni,96% Co,93% Mn,95% Mg and less than 1% Fe are extracted under optimum conditions.Analysis of the high pressure acid leaching residue by chemical and XRD analysis indicates that the residual iron and sulfur are mainly present in phases of hematite and alunite,respectively.The high pressure leaching process provides a simple and efficient way for the high recovery of nickel and cobalt from laterite ore,leaving residue as a suitable iron resource. 展开更多
关键词 high pressure acid leaching limonitic laterite leaching behavior NICKEL
下载PDF
Extraction of molybdenum and nickel from Ni-Mo ore by pressure acid leaching 被引量:10
17
作者 王私富 魏昶 +5 位作者 邓志敢 李存兄 李兴彬 吴钧 王明双 张帆 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第10期3083-3088,共6页
A direct hydrometallurgical route for nickel and molybdenum extraction from a nickel-molybdenum (Ni-Mo) ore using pressure acid leaching was studied. The nickel and molybdenum were extracted by acid leaching under o... A direct hydrometallurgical route for nickel and molybdenum extraction from a nickel-molybdenum (Ni-Mo) ore using pressure acid leaching was studied. The nickel and molybdenum were extracted by acid leaching under oxygen pressure. Compared with traditional roasting methods, this hydrometallurgical method eliminates SO2 and As203 emission (the Ni-Mo ore containing 15%-25% S). Compared with existing alkali leaching recovery of molybdenum process, almost all the nickel and considerable molybdenum were extracted in the acid leaching process. Under oxygen pressure conditions, almost all the nickel and a substantial part of the molybdenum were dissolved into the acid leaching liquor and the other part of the molybdenum was left in the acid leach residue. The acid leach residue was further leached under alkaline (NaOH) conditions. Under optimal experimental conditions, the extraction rates nickel and molybdenum reached 97% and 96%, respectively. 展开更多
关键词 nickel-molybdenum ore pressure leaching alkaline leaching NICKEL MOLYBDENUM
下载PDF
Recovery of Co and Li from spent lithium-ion batteries by combination method of acid leaching and chemical precipitation 被引量:23
18
作者 朱曙光 贺文智 +3 位作者 李光明 周旭 张骁君 黄菊文 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2012年第9期2274-2281,共8页
Cathode material of spent lithium-ion batteries was refined to obtain high value-added cobalt and lithium products based on the chemical behaviors of metal in different oxidation states. The active substances separate... Cathode material of spent lithium-ion batteries was refined to obtain high value-added cobalt and lithium products based on the chemical behaviors of metal in different oxidation states. The active substances separated from the cathode of spent lithium-ion batteries were dissolved in H2SO4 and H2O2 solution, and precipitated as CoC2O4·2H2O microparticles by addition of (NH4)2C2O4. After collection of the CoC2O4·2H2O product by filtration, the Li2CO3 precipitates were obtained by addition of Na2CO3 in the left filtrate. The experimental study shows that 96.3% of Co (mass fraction) and 87.5% of Li can be dissolved in the solution of 2 mol/L H2SO4 and 2.0% H2O2 (volume fraction), and 94.7% of Co and 71.0% of Li can be recovered respectively in the form of CoC2O4·2H2O and Li2CO3. 展开更多
关键词 spent lithium-ion batteries RECOVERY leaching PRECIPITATION
下载PDF
Extraction of lithium from lepidolite using chlorination roasting-water leaching process 被引量:24
19
作者 颜群轩 李新海 +5 位作者 王志兴 王接喜 郭华军 胡启扬 彭文杰 伍习飞 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2012年第7期1753-1759,共7页
Chlorination roasting followed by water leaching process was used to extract lithium from lepidolite.The microstructure of the lepidolite and roasted materials were characterized by X-ray diffraction(XRD).Various pa... Chlorination roasting followed by water leaching process was used to extract lithium from lepidolite.The microstructure of the lepidolite and roasted materials were characterized by X-ray diffraction(XRD).Various parameters including chlorination roasting temperature,time,type and amount of chlorinating agents were optimized.The conditional experiments indicate that the best mass ratio of lepidolite to NaCl to CaCl2 is 1:0.6:0.4 during the roasting process.The extraction of lithium reaches peak value of 92.86% at 880 °C,potassium,rubidium,and cesium 88.49%,93.60% and 93.01%,respectively.The XRD result indicates that the major phases of the product after roasting lepidolite with mixture of chlorinating agents(CaCl2 and NaCl) are SiO2,CaF2,KCl,CaSiO3,CaAl2Si2O8,NaCl and NaAlSi3O8. 展开更多
关键词 LEPIDOLITE LITHIUM chlorination roasting water leaching
下载PDF
Atmospheric oxygen-rich direct leaching behavior of zinc sulphide concentrate 被引量:9
20
作者 徐志峰 江庆政 王成彦 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第12期3780-3787,共8页
The leaching behavior of main metallic sulphides in zinc concentrate under atmospheric oxygen-rich direct leaching conditions was studied through mineralogical analysis. The results show that the sulphides dissolve ob... The leaching behavior of main metallic sulphides in zinc concentrate under atmospheric oxygen-rich direct leaching conditions was studied through mineralogical analysis. The results show that the sulphides dissolve obviously except pyrite. Based on the relationship between elemental sulfur and the residual sulphides in the leaching residue, the dissolution of sphalerite, chalcopyrite, covellite and galena is assumed to follow the indirect oxidation reactions, where the acidic dissolution takes place firstly and then the released H2S transfers from the mineral surface into bulk solution and is further oxidized into elemental sulfur. The interface chemical reaction is further supposed as the controlling step in the leaching of these sulphides. The direct electrochemical oxidation reactions are assumed to contribute to the dissolution of pyrrhotite, which is controlled by the diffusion through elemental sulfur layer. 展开更多
关键词 zinc sulphide concentrate atmospheric direct leaching oxygen-rich leaching leaching behavior MINERALOGY
下载PDF
上一页 1 2 250 下一页 到第
使用帮助 返回顶部