Aqueous zinc ion batteries(AZIBs)are promising energy storage devices.However,the formation of dendrites,hydrogen evolution,and corrosion reaction seriously affect their electrochemical performance.Herein,the synergis...Aqueous zinc ion batteries(AZIBs)are promising energy storage devices.However,the formation of dendrites,hydrogen evolution,and corrosion reaction seriously affect their electrochemical performance.Herein,the synergistic effect of ion-migration regulation and interfacial engineering has been confirmed as the potential strategy by kaolin functionalized glass fiber separator(KL-GF)to alleviate these problems.The rapid and orderly Zn^(2+)migration was achieved to improve the transfer kinetics and induced uniform zinc deposition by more zinc-philic sites of KL-GF.Based on the interfacial engineering,the side reactions were effectively mitigated and crystal planes were regulated through KL-GF.The hydrophilicity of KL alleviated the corrosion and hydrogen evolution.Importantly,a preferential orientation of Zn(002)crystal plane by KL-GF was induced to further realize dendrite-free deposition by density functional theory(DFT)and X-ray diffraction(XRD)characterization.Hence,the Zn|KL-GF|MnO_(2)cell maintained a high discharge capacity of 96.8 mAh/g at 2 A/g after 1000 cycles.This work can provide guidance enabling high-performance zinc anode for AZIBs.展开更多
基金supported by the National Natural Science Foundation of China(Nos.51872090,51772097,82204604)the Hebei Natural Science Fund for Distinguished Young Scholar(No.E2019209433)+1 种基金the Youth Talent Program of Hebei Provincial Education Department(No.BJ2018020)the Natural Science Foundation of Hebei Province(Nos.E2020209151,E2022209158,H2022209012)。
文摘Aqueous zinc ion batteries(AZIBs)are promising energy storage devices.However,the formation of dendrites,hydrogen evolution,and corrosion reaction seriously affect their electrochemical performance.Herein,the synergistic effect of ion-migration regulation and interfacial engineering has been confirmed as the potential strategy by kaolin functionalized glass fiber separator(KL-GF)to alleviate these problems.The rapid and orderly Zn^(2+)migration was achieved to improve the transfer kinetics and induced uniform zinc deposition by more zinc-philic sites of KL-GF.Based on the interfacial engineering,the side reactions were effectively mitigated and crystal planes were regulated through KL-GF.The hydrophilicity of KL alleviated the corrosion and hydrogen evolution.Importantly,a preferential orientation of Zn(002)crystal plane by KL-GF was induced to further realize dendrite-free deposition by density functional theory(DFT)and X-ray diffraction(XRD)characterization.Hence,the Zn|KL-GF|MnO_(2)cell maintained a high discharge capacity of 96.8 mAh/g at 2 A/g after 1000 cycles.This work can provide guidance enabling high-performance zinc anode for AZIBs.