Phase-field-lattice Boltzmann study for lamellar eutectic growth in a natural convection melt 被引量:6
1
作者 Ang Zhang Zhi-peng Guo Shou-mei Xiong 《China Foundry》 SCIE 2017年第5期373-378,共6页
In the present study, the influence of natural convection on the lamellar eutectic growth is determined by a phase-field-lattice Boltzmann study for Al-Cu eutectic alloy. The mass difference resulting from concentrati... In the present study, the influence of natural convection on the lamellar eutectic growth is determined by a phase-field-lattice Boltzmann study for Al-Cu eutectic alloy. The mass difference resulting from concentration difference led to the fluid flow, and a robust parallel and adaptive mesh refinement algorithm was employed to improve the computational efficiency without any compromising accuracy. Results show that the existence of natural convection would affect the growth undercooling and thus control the interface shape by adjusting the lamellar width. In particular, by alternating the magnitude of the solute expansion coefficient, the strength of the natural convection is changed. Corresponding microstructure patterns are discussed and compared with those under no-convection conditions. 展开更多
关键词 自然传送对流 薄片状的宽度 阶段地模型 格子 Boltzmann 方法 TP391.99
下载PDF
Achieving exceptionally high strength and rapid degradation rate of Mg-Er-Ni alloy by strengthening with lamellar γ' and bulk LPSO phases
2
作者 Chaoneng Dai Jingfeng Wang +7 位作者 Yuanlang Pan Kai Ma Yinhong Peng Ye Wang Danqian Wang Chunhua Ran Jinxing Wang Yanlong Ma 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2024年第1期88-102,共15页
As-extruded Mg-Er-Ni alloys with different volume fractions of long-period stacking ordered(LPSO)phase and density of lamellar γ' phase were prepared,and the microstructure,mechanical,and degradation properties w... As-extruded Mg-Er-Ni alloys with different volume fractions of long-period stacking ordered(LPSO)phase and density of lamellar γ' phase were prepared,and the microstructure,mechanical,and degradation properties were investigated.Coupling the bulk LPSO phase and the lamellar γ' phase,and controlling the dynamic recrystallization processes during deformation by adjusting the volume fraction of LPSO and the density of the γ' phase,a synergistic increase in strength and degradation rate can be achieved.On the one hand,the increase in corrosion rate was related to the increased volume fraction of the bulk LPSO phase and the densities of the lamellar γ' phase,which provide more galvanic corrosion.Moreover,high densities of the lamellar γ' phase can provide more corrosion interface by inhibiting the recrystallization process to refine dynamic recrystallized(DRXed)grains during the hot extrusion.On the other hand,the ultimate tensile strength(UTS)and tensile yield strength(TYS)of the Mg-Er-Ni alloy increased from 345 and 265 MPa to 514 MPa and 358 MPa,respectively,which was mainly attributed to grain boundary and texture strengthening,bulk LPSO phase and lamellar γ' phase strengthening.Overall,Mg^(-1)4Er-4Ni alloy,which contains the highest volume fraction bulk LPSO phase and the densities of lamellar γ' phase,re-alized a synergistic enhancement of strength and degradation rate.The UTS,TYS,and degradation rate of Mg^(-1)4Er-4Ni were 514 MPa,358 MPa,and 142.5 mg cm^(-2)h^(-1)(3 wt%KCl solution at 93◦C),respectively.This research provides new insight into developing Mg alloys with high strength and degradation rates for fracturing tool materials in the application of oil and gas exploitation in harsh environments. 展开更多
关键词 Mg-Er-Ni alloy lamellarγ'and bulk LPSO phases Rapid degradation rate High strength Mechanical and corrosion mechanism
原文传递
Effect of the glyceryl monooleate-based lyotropic phases on skin permeation using in vitro diffusion and skin imaging
3
作者 Dae Gon Lim Won-Wook Jeong +5 位作者 Nam Ah Kim Jun Yeul Lim Seol-Hoon Lee Woo Sun Shim Nae-Gyu Kang Seong Hoon Jeong 《Asian Journal of Pharmaceutical Sciences》 SCIE CAS 2014年第6期324-329,共6页
Glyceryl monooleate(GMO)is a polar lipid that can exist in various liquid crystalline phases in the presence of different amounts of water.It is regarded as a permeation enhancer due to its amphiphilic property.Variou... Glyceryl monooleate(GMO)is a polar lipid that can exist in various liquid crystalline phases in the presence of different amounts of water.It is regarded as a permeation enhancer due to its amphiphilic property.Various phases of GMO/solvent system containing sodium fluorescein were prepared to compare permeability using confocal laser scanning microscopy(CLSM).GMO was melted in a vial in a water bath heated to 45℃.Propylene glycol and hexanediol were homogeneously dissolved in the melted GMO.Sodium fluorescein in aqueous solution was diluted to various ratios and thoroughly mixed by an ultrasonic homogenizer.Each GMO/Solvent system with fluorescein was applied onto the epidermal side of excised pig skin and incubated overnight.CLSM was performed to observe how the GMO/solvent system in its different phases affect skin permeability.Cubic and lamellar phase formulations enhanced the fluorescein permeation through the stratum corneum.A solution system had the weakest permeability compared to the other two phases.Due to the amphiphilic nature of GMO,cubic and lamellar phases might reduce the barrier function of stratum corneum which was observed by CLSM as fluorescein accumulated in the dermis.Based on the results,the glyceryl monooleate lyotropic mixtures could be applied to enhance skin permeation in various topical and transdermal formulations. 展开更多
关键词 Confocal microscopy IMAGING Glyceryl monooleate Skin permeation Cubic phase lamellar phase
下载PDF
新型多相TiAl合金的β/B2相含量变化及其对拉伸性能的影响
4
作者 冯像征 高帆 +1 位作者 刘宏武 李臻熙 《航空材料学报》 CAS CSCD 北大核心 2024年第4期96-108,共13页
以新型多相TiAl合金(Ti-43.5Al-6(Nb、Cr、Ta))的挤压态组织为研究对象,先通过热处理分析该合金中β/B2相、α/α2相和γ相平均含量随固溶温度和保温时间的演变规律,然后测试合金在三相区内不同β/B2相含量时的室温和高温(750℃和800℃... 以新型多相TiAl合金(Ti-43.5Al-6(Nb、Cr、Ta))的挤压态组织为研究对象,先通过热处理分析该合金中β/B2相、α/α2相和γ相平均含量随固溶温度和保温时间的演变规律,然后测试合金在三相区内不同β/B2相含量时的室温和高温(750℃和800℃)拉伸性能。结果表明:在1190~1350℃范围内,γ相含量随固溶温度的升高和保温时间的延长逐渐减少,在1270℃时,γ相完全消失;在1190~1350℃范围内,β/B2相含量随固溶温度的升高先减少后增加,随保温时间的延长逐渐减少,而层片团的含量和尺寸与β/B2相的含量变化负相关;在1230~1280℃范围内,β/B2相平均含量可控制在10%以下;在1250~1270℃范围内,延长保温时间可将β/B2相平均含量控制在0.5%以下;当合金处于三相区时,控制β/B2相平均含量约6%,可得到综合拉伸性能优异的均匀细小近层片组织,且该组织的室温抗拉强度超过1050 MPa、室温伸长率1.5%~2%,750℃抗拉强度超过950 MPa,800℃抗拉强度超过850 MPa。 展开更多
关键词 多相TiAl合金 β/B2相 变形TiAl合金 细小近层片组织 拉伸性能
下载PDF
A phase-field model for simulating various spherulite morphologies of semi-crystalline polymers 被引量:5
5
作者 王晓东 欧阳洁 +1 位作者 苏进 周文 《Chinese Physics B》 SCIE EI CAS CSCD 2013年第10期387-393,共7页
A modified phase-field model is proposed for simulating the isothermal crystallization of polymer melts. The model consists of a second-order phase-field equation and a heat conduction equation. It obtains its model p... A modified phase-field model is proposed for simulating the isothermal crystallization of polymer melts. The model consists of a second-order phase-field equation and a heat conduction equation. It obtains its model parameters from the real material parameters and is easy to use with tolerable computational cost. Due to the use of a new free energy functional form, the model can reproduce various single crystal morphologies of polymer melts under quiescent conditions, including dendritic, lamellar branching, ring-banded, breakup of ring-banded, faceted hexagonal, and spherulitic structures. Simulation results of isotactic polystyrene crystals demonstrate that the present phase-field model has the ability to give qualitative predictions of polymer crystallization under isothermal and quiescent conditions. 展开更多
关键词 phase-FIELD crystallization polymer DENDRITIC lamellar ring-banded
下载PDF
Application of cold drawn lamellar microstructure for developing ultra-high strength wires 被引量:15
6
作者 S. Goto R. Kirchheim +1 位作者 T . Al-Kassab C. Borchers 《中国有色金属学会会刊:英文版》 EI CSCD 2007年第6期1129-1138,共10页
Composite materials having lamellar structure are known to have a good combination of high strength and ductility. They are widely used in the fields of automobiles, civil engineering and construction, machines and ma... Composite materials having lamellar structure are known to have a good combination of high strength and ductility. They are widely used in the fields of automobiles, civil engineering and construction, machines and many other industries. An application of lamellar microstructure for developing ultra-high strength steel wires was studied and discussed. Based on the experimental results, the relationships between the strength increase and microstructure development during the cold wire drawing were studied to reveal the strengthening mechanism. As cold drawing proceeds, the wire strength extremely increases, the microstructure changes from large single crystal lamellar structure to very fine polycrystalline lamellar one which has nano-sized grains, high dislocation density and amorphous regions. From the results obtained, it is concluded that heavy cold drawing technique is an effective method for lamellar composite to get high strength wires. Furthermore, formation process of the best microstructure for producing the ultra-high strength wires was also discussed. 展开更多
关键词 薄片复合物 金属丝 加固装置 机械性质
下载PDF
A MICROSTRUCTURE-BASED ANALYSIS FOR CYCLIC PLASTICITY OF DUAL-PHASE PEARLITIC RAIL STEELS
7
作者 Peng Xianghe Chang Jian 《Acta Mechanica Solida Sinica》 SCIE EI 2001年第4期334-343,共10页
Based on the assumption that a representative element of apearlitic steel is an aggregate of numerous spherical pearliticcolonies with randomly distributed orientations, and that each colonyis com- posed of many paral... Based on the assumption that a representative element of apearlitic steel is an aggregate of numerous spherical pearliticcolonies with randomly distributed orientations, and that each colonyis com- posed of many parallel fine lamellas of ferrite andcementite, a description for the dual-phase pearlitic steel isobtained by making use of a microstructure-based constitutiveequation for a single dual-phase pearlitic colony and the Hill'sself-consistent scheme. The elastoplastic response of dual-phasepearlitic steel BS11 subjected to asymmetrically cyclic loading isanalyzed, and a comparison with the experimental results showssatisfacto- ry agreement. The non-proportional cyclic plasticity ofBS11 is also analyzed, in which stress develops along a semi-circlein a biaxial tension/compression and shear stress plane, as istypically experienced by the sur- face elements in rolling andsliding contact. 展开更多
关键词 pearlitic steel lamellar dual-phase material Hill's self-consistent scheme cyclic plasticity
下载PDF
MECHANISMS OF α_2→α_2/γ PHASE TRANSFORMATION IN A TiAL ALLOY
8
作者 XU Qiang LEI Changhui (BeiJing Laboratory of Electron Microscopy. Chinese Academy of Sciences, P. O. Box 2724.100080 )Beijing, China.ZHANG Yonggang (Department of Materials Science and Engineering, BeiJing University of Aeronautics and Astronautics, 1000 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 1995年第Z1期597-602,共6页
A Ti-45at.%Al alloy which was solution-treated at 1350℃ for 30 minutes and quenched in water is employed to explore mechanisms of α_2→γphase transformation. The ageing process of the quenched alloy has been in si... A Ti-45at.%Al alloy which was solution-treated at 1350℃ for 30 minutes and quenched in water is employed to explore mechanisms of α_2→γphase transformation. The ageing process of the quenched alloy has been in situ studied it has been found that the γ lamellae can precipitate in the α_2 matrix by two mechanisms. When The alloy is aged at 700℃, the stacking faults pre-existing in the α_2 matrix start to grow and more are generated.With the increase of ageing time and ageing temperature the density of stacking faults is increased and the γ lamellae then precipitate. This isα diffusion-controlled process. Alternatively, the γ lamellae may be formed from the α_2 matrix by 1/3(1100) shearing on the (0001) plane. The latter mechanism implies that the strain-induced transformation may occur, which is confirmed by deformation of the quenched alloy. 展开更多
关键词 TIAL phase transformation lamellar structure
下载PDF
Phase field study on crystal orientation effects in eutectoid phase transformation
9
作者 Dong-qiao Zhang Ya-jun Yin +1 位作者 Jian-xin Zhou Zhi-xin Tu 《China Foundry》 SCIE 2017年第5期435-442,共8页
In this present work, a multi-phase field model was used to simulate the eutectoid transformation process, and on the basis of the nucleation model that was previously proposed by our research team, anisotropic and or... In this present work, a multi-phase field model was used to simulate the eutectoid transformation process, and on the basis of the nucleation model that was previously proposed by our research team, anisotropic and orientation relationship models were introduced to study the growth mechanism of the pearlite lamellae with anisotropy. It was found that the growth direction of the pearlite lamellae is related to its orientation and spacing. In the process of lamellar growth, deflection growth of pearlite will appear along with the adjustment of lamellar spacing, and the deflection angle is equal to the orientation difference between the austenite and the pearlite. Comparison between experimental and numerical results indicates a good consistency in pearlite morphology. 展开更多
关键词 模拟 阶段地 薄片状的生长 珠泽铁形态学 生长方向 TP391.99
下载PDF
双相钛合金材料疲劳问题研究进展
10
作者 汤可可 蔡肖 +2 位作者 赵银盾 吴昊 仲政 《力学季刊》 CAS CSCD 北大核心 2023年第3期491-511,共21页
双相钛合金材料多样的微观组织结构特征,以及不可避免的内在缺陷,对材料疲劳裂纹萌生、扩展以及失效等多个阶段有着重要的影响.本文针对双相钛合金材料的疲劳问题,聚焦微观组织与几何缺陷效应,从试验和数值模拟两个角度,系统综述了双相... 双相钛合金材料多样的微观组织结构特征,以及不可避免的内在缺陷,对材料疲劳裂纹萌生、扩展以及失效等多个阶段有着重要的影响.本文针对双相钛合金材料的疲劳问题,聚焦微观组织与几何缺陷效应,从试验和数值模拟两个角度,系统综述了双相钛合金材料在裂纹萌生以及扩展阶段的疲劳性能评估与寿命预测方面的最新研究成果.同时,针对微观细节丰富的片层组织,重点总结了片层组织与微观缺陷协同效应下的双态合金疲劳裂纹萌生问题,并对后续研究中的机遇与挑战进行了展望. 展开更多
关键词 双相钛合金 微观组织 几何缺陷 片层组织 疲劳
下载PDF
固溶时效对Ti-5Al-3V-1Mo-1Zr钛合金钻杆组织演变及力学性能的影响 被引量:1
11
作者 冯春 宋文文 +5 位作者 张凯 刘洪涛 赵密锋 朱丽娟 刘会群 刘乐 《中国有色金属学报》 EI CAS CSCD 北大核心 2023年第6期1795-1803,共9页
利用激光共聚焦显微镜(CLSM)、电子扫描显微镜(SEM)、透射电子显微镜(TEM)和力学性能测试等手段分析相变点上两阶段固溶时效(TSSA)对Ti-5Al-3V-1Mo-1Zr钛合金钻杆片层组织演变规律及力学性能的影响。结果表明:通过采用相变点上TSSA工艺... 利用激光共聚焦显微镜(CLSM)、电子扫描显微镜(SEM)、透射电子显微镜(TEM)和力学性能测试等手段分析相变点上两阶段固溶时效(TSSA)对Ti-5Al-3V-1Mo-1Zr钛合金钻杆片层组织演变规律及力学性能的影响。结果表明:通过采用相变点上TSSA工艺获得了全片层转变组织,随时效温度的升高,全片层转变组织的晶界α相平均宽度由5.5μm增至9.0μm,集束内的α片层平均宽度由2.75μm增至3.95μm,材料抗拉和屈服强度变化幅度均小于0.15 MPa/℃;与原始挤压态相比,钛合金的冲击功增加74.07%,材料冲击功与α片宽度满足Hall-Petch关系;经(1000℃, 1 h,炉冷(FC))→(600℃, 1 h,空冷(AC))+(550℃, 6 h,AC)热处理后钛合金具有良好的综合性能匹配,其屈服强度为894 MPa,夏比V型缺口冲击功(-20℃)为46 J,伸长率为7.5%。 展开更多
关键词 Ti-5Al-3V-1Mo-1Zr 钛合金钻杆 相变点 固溶时效 片层组织 力学性能
下载PDF
钛合金片层α相在热加工过程中演变规律的定量研究(英文) 被引量:9
12
作者 王凯旋 曾卫东 +4 位作者 赵永庆 邵一涛 周建华 王晓英 周义刚 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2010年第4期565-569,共5页
对具有片层α相的Ti-17合金圆饼在两相区进行5种变形程度的等温锻造及固溶时效处理,用定量金相学方法研究了片层α相在热加工过程中的演变规律。研究发现:α相的厚度随着应变量的增大而增大;变形程度及圆饼的变形区域对α相形态的变化... 对具有片层α相的Ti-17合金圆饼在两相区进行5种变形程度的等温锻造及固溶时效处理,用定量金相学方法研究了片层α相在热加工过程中的演变规律。研究发现:α相的厚度随着应变量的增大而增大;变形程度及圆饼的变形区域对α相形态的变化有很大影响。随变形程度的增大,α相的形态参数FeretRatio(Feretmax/Feretmin)的分布曲线在FeretRatio介于1.5~2.5区间出现单峰,且峰值不断增大,大FeretRatio的α相比例逐渐减小。圆饼中心位置的FeretRatio分布曲线具有较大的峰值。大变形使片层α相的等轴化程度提高,改善了圆饼的组织均匀性。等效应变对组织中不同形态α相分布的影响曲线表明:球化α相比例随着等效应变的增大呈单调增大,增大速率表现为慢—快—极慢的分阶段特征;近等轴状的α相比例先快速增长后不断减少;片层状和大片层状α相比例随着等效应变增大呈单调减少。片层α相的临界球化与完全球化的等效应变分别约为0.4与1.0。 展开更多
关键词 TI-17合金 片层α相 组织演变 定量研究
下载PDF
片状组织TA15钛合金动态球化行为 被引量:5
13
作者 董显娟 鲁世强 +2 位作者 王克鲁 郑海忠 李鑫 《特种铸造及有色合金》 CAS CSCD 北大核心 2009年第11期987-990,共4页
利用热模拟试验机对片状TA15钛合金进行等温恒应变速率压缩试验,研究了应变速率为10-3~1s-1、真应变为0.22~0.92、变形温度为900℃和950℃时片状组织的动态球化行为。结果表明,真应变对动态球化有较大影响,真应变从0.22增加到0.92时,... 利用热模拟试验机对片状TA15钛合金进行等温恒应变速率压缩试验,研究了应变速率为10-3~1s-1、真应变为0.22~0.92、变形温度为900℃和950℃时片状组织的动态球化行为。结果表明,真应变对动态球化有较大影响,真应变从0.22增加到0.92时,α相的球化率最大增幅为40%;900℃和950℃变形时α相的球化率差别不大;当应变速率为10-3~10-1s-1时,降低应变速率能够显著提高片状α相的球化率,但当应变速率大于10-1s-1后,球化率随应变速率的变化并不明显。TA15钛合金的真应力-真应变曲线均呈"应变软化"型,这种软化行为主要是由片状α相的动态球化和弯折引起的。 展开更多
关键词 TA15钛合金 片状α相 动态球化 热变形参数
下载PDF
亚硫酸钙对水泥水化性能的影响 被引量:21
14
作者 姚建可 杨利群 +1 位作者 蒋年平 徐先宇 《水泥》 CAS 2001年第11期1-3,共3页
采用XRD、SEM等测试方法研究了亚硫酸钙(CaSO3·1/2H2O)对水泥水化性能的影响,并与石膏(CaSO4·2H2O)进行了对比。结果表明:在水泥中CaSO3·1/2H2O不具有石膏那样的调节水泥凝结时间的作用。掺CaSO3·1/2H2O的水泥试样1... 采用XRD、SEM等测试方法研究了亚硫酸钙(CaSO3·1/2H2O)对水泥水化性能的影响,并与石膏(CaSO4·2H2O)进行了对比。结果表明:在水泥中CaSO3·1/2H2O不具有石膏那样的调节水泥凝结时间的作用。掺CaSO3·1/2H2O的水泥试样1d强度比掺CaSO4·2H2O试样显著降低,3d后两者强度相近。60d的抗折、抗压强度与28d相比,增幅很小,有的甚至倒缩。CaSO3·1/2H2O和铝酸盐矿物反应,主要生成片状的C3A·CaSO3·11H2O。 展开更多
关键词 亚硫酸钙 水泥 水化 片状相
下载PDF
溶致液晶中金属纳米粒子的掺杂及其作用机制研究 被引量:2
15
作者 隋震鸣 陈晓 +2 位作者 王庐岩 许丽梅 杨春杰 《物理化学学报》 SCIE CAS CSCD 北大核心 2006年第6期737-743,共7页
在用琥珀酸二异辛酯磺酸钠(AOT)构建的具有长程有序结构的层状溶致液晶内,用不同方式导入预制的亲油或亲水贵金属纳米粒子,可得到纳米粒子分布在不同介观空间内的无机/有机杂合体.依据小角X射线散射和偏光显微镜结果,通过分析掺杂纳米... 在用琥珀酸二异辛酯磺酸钠(AOT)构建的具有长程有序结构的层状溶致液晶内,用不同方式导入预制的亲油或亲水贵金属纳米粒子,可得到纳米粒子分布在不同介观空间内的无机/有机杂合体.依据小角X射线散射和偏光显微镜结果,通过分析掺杂纳米粒子与液晶模板的相互作用,对掺杂前后体系结构的变化及制得杂合体的稳定性进行了表征.结果表明,除考虑掺杂粒子与层状模板空间的匹配外,体系中静电斥力、范德华引力和Helfrich涨落力之间的平衡是维持液晶结构稳定的基本条件. 展开更多
关键词 溶致液晶 层状相 纳米粒子 小角X射线散射
下载PDF
溶致液晶模板电化学沉积束状铂纳米材料 被引量:2
16
作者 柴永存 陈晓 +1 位作者 隋震鸣 庄文昌 《物理化学学报》 SCIE CAS CSCD 北大核心 2006年第12期1506-1510,共5页
以非离子型三嵌段共聚物EO106PO70EO106(F127)/正丁醇/氯铂酸水溶液构建的溶致液晶层状相为模板,电化学沉积制备铂纳米材料.透射电镜和扫描电镜显示,产物为具有高长径比的纳米线形成的束状结构,能量弥散谱与电极电势分析证实产物为铂单... 以非离子型三嵌段共聚物EO106PO70EO106(F127)/正丁醇/氯铂酸水溶液构建的溶致液晶层状相为模板,电化学沉积制备铂纳米材料.透射电镜和扫描电镜显示,产物为具有高长径比的纳米线形成的束状结构,能量弥散谱与电极电势分析证实产物为铂单质,而循环伏安测量表明产物的比表面积约为53m2·g-1.对影响产物形貌的因素和产物生成的可能机理进行了分析. 展开更多
关键词 嵌段共聚物 溶致液晶 层状相 纳米材料
下载PDF
小角X射线散射表征AOT/水层状溶致液晶的有序性(英文) 被引量:1
17
作者 庄文昌 陈晓 +2 位作者 杨春杰 王庐岩 柴永存 《物理化学学报》 SCIE CAS CSCD 北大核心 2005年第9期1055-1058,共4页
用小角X射线散射研究了AOT/水层状溶致液晶的有序性. 通过对散射曲线的解析, 讨论了表面活性剂浓度、温度和助表面活性剂等三个方面对溶致液晶层状相结构有序性的影响. 在一定的范围内, 提高温度,改变表面活性剂浓度和加入少量助表面活... 用小角X射线散射研究了AOT/水层状溶致液晶的有序性. 通过对散射曲线的解析, 讨论了表面活性剂浓度、温度和助表面活性剂等三个方面对溶致液晶层状相结构有序性的影响. 在一定的范围内, 提高温度,改变表面活性剂浓度和加入少量助表面活性剂可使碳氢链排列由稀疏转变为密实, 层状相也相应地由“柔性双层”过渡到更加有序化的“平面双层”. 基于形状因子和体系内分子间作用力, 提出了层状相形成与有序化的机理, 同时采用分子模拟的方法展现了不同浓度下的液晶结构. 展开更多
关键词 小角X射线散射 分子模拟 层状相
下载PDF
表面活性剂体系中电荷诱导的层状相向囊泡相的转化 被引量:2
18
作者 穆念孔 赵红军 +2 位作者 王鸿雁 宋爱新 郝京诚 《化学研究》 CAS 2007年第4期68-71,共4页
向一种非离子表面活性剂LA070(英文名AlcoholC12-C16Poly(1-6)Ethoxylate)复配体系LA070/C8H17OH/H2O形成的层状相中加入离子型表面活性剂使其电荷化,在电荷诱导下,双分子层的曲率发生变化,闭合形成具有黏弹性的囊泡相.离子型表面活性... 向一种非离子表面活性剂LA070(英文名AlcoholC12-C16Poly(1-6)Ethoxylate)复配体系LA070/C8H17OH/H2O形成的层状相中加入离子型表面活性剂使其电荷化,在电荷诱导下,双分子层的曲率发生变化,闭合形成具有黏弹性的囊泡相.离子型表面活性剂的加入量增大到一定程度时,由于反离子的屏蔽作用,囊泡结构被破坏,溶液的黏弹性消失,澄清的溶液逐渐变混浊,然后分为两相. 展开更多
关键词 层状相 离子型表面活性剂 曲率 黏弹性 囊泡相
下载PDF
层状溶致液晶中磁性纳米粒子掺杂的研究 被引量:1
19
作者 靖波 陈晓 +3 位作者 隋震鸣 王庐岩 柴永存 邱化玉 《化学学报》 SCIE CAS CSCD 北大核心 2006年第13期1319-1323,共5页
选择非离子表面活性剂十二烷基(4)聚氧乙烯醚(C12E4)与H2O构成的溶致液晶(LLC)层状模板,掺杂油酸铵包覆的Fe3O4亲水性磁性纳米粒子,构建稳定的有机/无机杂合体.用透射电镜(TEM),X射线粉末衍射(XRD),偏光显微镜(POM),小角X射线散射(SAXS... 选择非离子表面活性剂十二烷基(4)聚氧乙烯醚(C12E4)与H2O构成的溶致液晶(LLC)层状模板,掺杂油酸铵包覆的Fe3O4亲水性磁性纳米粒子,构建稳定的有机/无机杂合体.用透射电镜(TEM),X射线粉末衍射(XRD),偏光显微镜(POM),小角X射线散射(SAXS)和振动探针式磁强计(VSM)等对粒子及掺杂前后的层状液晶相结构变化进行表征.结果表明,粒子掺入使LLC模板的层间距产生了改变,同时增强了体系有序性.通过对杂合体表征结果的分析,阐述了模板与粒子间相互作用的机理. 展开更多
关键词 十二烷基(4)聚氧乙烯醚 溶致层状液晶 掺杂 磁性纳米粒子 小角X射线散射
下载PDF
层片状珠光体生长形貌的相场法模拟 被引量:3
20
作者 冯力 高亚龙 +3 位作者 朱昶胜 安国升 肖荣振 路妮妮 《兰州理工大学学报》 CAS 北大核心 2018年第1期11-16,共6页
采用相场法,以共析钢为例,模拟研究了不同初始共析层片间距及不同初始过冷度条件下层片状珠光体微观组织的生长形貌,探讨了不同初始层片间距及不同初始过冷度条件下层片状珠光体微观组织生长的规律.模拟结果表明:过冷度不变时,随着初始... 采用相场法,以共析钢为例,模拟研究了不同初始共析层片间距及不同初始过冷度条件下层片状珠光体微观组织的生长形貌,探讨了不同初始层片间距及不同初始过冷度条件下层片状珠光体微观组织生长的规律.模拟结果表明:过冷度不变时,随着初始层片间距的增大,共析层片振幅增大,共析层片生长形貌的变化是规则对称的层片状→非规则非对称形状→棒状;层片间距不变,初始过冷度在19.6~20K时,随着初始过冷度的减小,共析钢中碳原子扩散能力增大,层片间距的失稳,致使共析层片由规则状向非规则形状变化;初始过冷度在20~22K时,随着初始过冷度的增大,共析钢中碳原子的扩散能力减弱,渗碳体相前沿碳原子浓度无法使其规则对称地生长,渗碳体相向碳原子浓度高的地方生长,从而产生倾斜生长以及层片合并现象. 展开更多
关键词 层片状珠光体 相场法 初始层片间距 初始过冷度 组织形貌
下载PDF