Fabrication of Isotropic Pyrocarbon at 1400 ℃ by Thermal Gradient Chemical Vapor Deposition Apparatus
1
作者 郭领军 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2009年第5期728-731,共4页
An experiment was designed to prepare isotropic pyrocarbon by thermal gradient chemical vapor deposition apparatus. The deposition was performed under ambient atmosphere at 1400 ℃, with natural gas volume flow of 3.5... An experiment was designed to prepare isotropic pyrocarbon by thermal gradient chemical vapor deposition apparatus. The deposition was performed under ambient atmosphere at 1400 ℃, with natural gas volume flow of 3.5 m^3/h for 80 h. The results show that the thickness and the bulk density of the deposit are about 1.95 g/cm^3 and 10 mm, respectively. The microstructure of the deposit was examined by polarized light microscopy and scanning electron microscopy, which shows that the deposit is constituted of sphere isotropic pyrocarbon, pebble pyrocarbon and laminar pyrocarbon. 展开更多
关键词 isotropic pyrocarbon chemical vapor deposition laminar pyrocarbon pebble pyrocarbon
下载PDF
纳米压痕技术测试纤维束内沥青炭和粗糙层热解炭的力学性能
2
作者 陈智勇 张东生 +4 位作者 齐乐华 李妙玲 吴恒 刘建寿 程广伟 《炭素技术》 CAS 北大核心 2018年第6期11-13,34,共4页
为了研究纤维束内沥青炭和粗糙层热解炭的力学性能,以2.5D针刺炭毡为增强体,分别通过中温煤沥青浸渍炭化和化学气相沉积制备得到C/C复合材料。使用G200型纳米压痕仪对C/C复合材料纤维束内基体进行纳米压痕测试,采用连续刚度测试方法,利... 为了研究纤维束内沥青炭和粗糙层热解炭的力学性能,以2.5D针刺炭毡为增强体,分别通过中温煤沥青浸渍炭化和化学气相沉积制备得到C/C复合材料。使用G200型纳米压痕仪对C/C复合材料纤维束内基体进行纳米压痕测试,采用连续刚度测试方法,利用Oliver和Pharr模型获得试样弹性模量随测试深度的变化,利用弹性模量和硬度两参数Weibull分布函数对纳米压痕测试结果进行统计分析。结果表明,沥青炭和粗糙层热解炭的弹性模量平均值分别为(14.92±2.02) GPa和(12.87±1.35)GPa;硬度的平均值分别为(0.64±0.14) GPa和(0.67±0.17) GPa。沥青炭和粗糙层热解炭的弹性模量的Weibull分布模数分别为8.60和9.18,弹性模量的特征值分别为15.63 GPa和13.40 GPa。 展开更多
关键词 C/C复合材料 纳米压痕技术 沥青炭 粗糙层热解炭 力学性能
原文传递