MECHANICAL PROPERTIES OF LONGITUDINAL SUBMERGED ARC WELDED STEEL PIPES USED FOR GAS PIPELINE OF OFFSHORE OIL 被引量:10
1
作者 Z.Z. Yang W. Tian +5 位作者 Q.R. Ma Y.L. Li J.K. Li J.Z. Gao H.B. Zhang Y.H. Yang 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2008年第2期85-93,共9页
Since the development of offshore oil and gas, increased submarine oil and gas pipelines were installed. All the early steel pipes of submarine pipelines depended on importing because of the strict requirements of com... Since the development of offshore oil and gas, increased submarine oil and gas pipelines were installed. All the early steel pipes of submarine pipelines depended on importing because of the strict requirements of comprehensive properties, such as, anti-corrosion, resistance to pressure and so on. To research and develop domes- tic steel pipes used for the submarine pipeline, the Longitudinal-seam Submerged Arc Welded (LSAW) pipes were made of steel plates cut from leveled hot rolled coils by both the JCOE and UOE (the forming process in which the plate like the letter “J”, “C”, “0” or “U” shape, then expansion) forming processes. Furthermore, the mechanical properties of the pipe base metal and weld metal were tested, and the results were in accordance with the corresponding pipe specification API SPEC 5L or DNV- OS-FI01, which showed that domestic LSAW pipes could be used for submarine oil and gas pipelines. 展开更多
关键词 Mechanical properties Offshore oil and gas longitudinal-seamsubmerged arc welded pipe (LSA W) pipeline JCOE formingprocess UOE forming process
下载PDF
Three-roller continuous setting round process for longitudinally submerged arc welding pipes 被引量:4
2
作者 Xue-ying HUANG Jun ZHAO +3 位作者 Gao-chao YU Qing-dang MENG Zhen-kai MU Rui-xue ZHAI 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2021年第5期1411-1426,共16页
In order to solve the problems of excess ovality and cross-section distortion of longitudinally submerged arc welding pipes after forming,a new three-roller continuous setting round process was proposed.This process c... In order to solve the problems of excess ovality and cross-section distortion of longitudinally submerged arc welding pipes after forming,a new three-roller continuous setting round process was proposed.This process can be divided into three stages:loading stage,roll bending stage and unloading stage.Based on the discretization idea,the mechanical model of the primary statically indeterminate problem of the longitudinally submerged arc welding pipes at the roll bending stage was established,and the deformation response was obtained.The simulation and theoretical results show that there are three positive bending regions and three reverse bending regions along the circumference of the pipe.The loading force of each roller shows growth,stability and downward trend with time.The error between the theoretical fitting curve and the simulated data point is very small,and the simulation results verify the reliability of the theoretical calculation.The experimental results show that the residual ovality decreases with the increase of the reduction,and the reduction of the turning point is the optimum reduction.In addition,the residual ovality of the pipe is less than 0.7%without cross-section distortion,which verifies the feasibility of this process. 展开更多
关键词 longitudinally submerged arc welding pipes three-roller continuous setting round statically indeterminate problem mechanical model ovality optimum reduction
下载PDF
CONTRACTED EFFECT OF BELL-SHADE SHAPE WELDING ARC AND ACCOMPANIED MAGNETIC FIELD WITH SPIRAL PIPE SHAPE 被引量:4
3
作者 Yu Jianrong, Zhang Jiaying , Jiang Lipei, Jiao Xiangdong Beijing Institute of Petrochemical Technology, Beijing 102600 Department of Mechanical Engineering,Tsinghua University, Beijing 100084 Jia Changshen, Shi Yaowu Xi′an Jiaotong University, 《中国有色金属学会会刊:英文版》 CSCD 1997年第2期96-99,共4页
CONTRACTEDEFFECTOFBELLSHADESHAPEWELDINGARCANDACCOMPANIEDMAGNETICFIELDWITHSPIRALPIPESHAPE①YuJianrong,ZhangJi... CONTRACTEDEFFECTOFBELLSHADESHAPEWELDINGARCANDACCOMPANIEDMAGNETICFIELDWITHSPIRALPIPESHAPE①YuJianrong,ZhangJiaying,JiangLipei,... 展开更多
关键词 longitudinal magnetic field BELL SHADE SHAPE welding arc contracted effect ACCOMPANIED magnetic field SPIRAL pipe SHAPE
下载PDF
Comparative study of weld residual stress on steel pipes with different weld types
4
作者 Luo Yun Zhang Xiaolei +1 位作者 Jiang Wenchun Hao Muming 《China Welding》 EI CAS 2016年第4期52-60,共9页
This study developed a sequential coupling finite element procedure to predict residual stresses of steel pipes with longitudinal wela/ circumferential weld and spiral weld.The results show that the residual stress i... This study developed a sequential coupling finite element procedure to predict residual stresses of steel pipes with longitudinal wela/ circumferential weld and spiral weld.The results show that the residual stress in heat affected zone(HAZ)is higher than that in weld for spiral weld pipe.For the circumferential weld pipe and spiral weld pipe,the residual stress in inner surface is higher than that in outer surface.However,for the spiral weld pipe,the residual stress in inner surface is smaller than that in outer surface.The hoop residual stress of circumferential weld pipe is higher than that of longitudinal weld pipe,while the axial residual stress of circumferential weld pipe is smaller than that of longitudinal weld pipe.The hoop stresses for circumferential weld pipe and axial stress for longitudinal weld pipe have exceeded the yield strength of base metal.With the increase of helix angle,the hoop stress decreases while the axial stress increases.For the spiral pipe(α=30° to 50°),both the hoop stress and axial stress are relatively small.The spiral pipe(helix angle ranging from 30° to 50°) is helpful to reduce stress corrosion cracking(SCC) and it is recommended to manufacture the steel pipe. 展开更多
关键词 steel pipe residual stress longitudinal weld circumferential weld spiral weld
下载PDF
大直径直缝埋弧焊管矫形工艺研究进展
5
作者 于高潮 齐绍聪 +4 位作者 彭德平 赵非平 宋东涛 李森林 赵军 《焊管》 2024年第9期1-7,13,共8页
大直径直缝埋弧焊管特别适用于长输油气管线以及严寒地带或深海海底管线的敷设要求。矫形工艺是大直径直缝埋弧焊管生产中的精整工序,直接决定了其尺寸精度,同时对其服役性能也有重要影响。总结了大型直缝焊管矫圆、矫直及复合矫形工艺... 大直径直缝埋弧焊管特别适用于长输油气管线以及严寒地带或深海海底管线的敷设要求。矫形工艺是大直径直缝埋弧焊管生产中的精整工序,直接决定了其尺寸精度,同时对其服役性能也有重要影响。总结了大型直缝焊管矫圆、矫直及复合矫形工艺研究进展,指出了不同矫形工艺存在的问题和未来发展方向,以期为油气管道研究人员和制造商提供技术参考。 展开更多
关键词 直缝埋弧焊管 矫形 矫直 矫圆 直线度 椭圆度
下载PDF
高频直缝焊管FFX成型板边质量控制方法
6
作者 孙文奎 张慧明 《焊管》 2024年第4期63-68,共6页
为了改善FFX成型方式下高频直缝焊管的板边质量,针对小直径大壁厚钢管存在的板边成型不充分以及大直径薄壁管存在的板边成型波浪边的问题,提出了相应的调整措施。通过对粗成型辊(BD1)上辊的压下调整、BD1的成形曲率调整、精成型辊(FP)... 为了改善FFX成型方式下高频直缝焊管的板边质量,针对小直径大壁厚钢管存在的板边成型不充分以及大直径薄壁管存在的板边成型波浪边的问题,提出了相应的调整措施。通过对粗成型辊(BD1)上辊的压下调整、BD1的成形曲率调整、精成型辊(FP)的减径量调整,以及焊接挤压辊(SQ)上辊的压下调整,能够有效实现板边端面的“I”形对接;通过增加FP的减径量,合理调整BD、RVS和CL机架轧辊位置,减小材料在FFX成型过程产生的长度方向的伸长量,均匀分配整条生产线的拉力等措施,能够避免波浪边的产生。 展开更多
关键词 FFX成型 高频直缝焊管 板边质量 成型缺陷
下载PDF
Research & Development of Grade X70 LSAW Steel Pipes for West-East Gas Pipeline 被引量:1
7
作者 WangXiaoxiang SunQi 《工程科学(英文版)》 2004年第4期40-45,共6页
In this article the research and development of X70 large diameter longitudinal seam submerged arc welded (LSAW) steel pipes for West East Gas Transportation Pipeline project (WEGTP) in China are introduced, including... In this article the research and development of X70 large diameter longitudinal seam submerged arc welded (LSAW) steel pipes for West East Gas Transportation Pipeline project (WEGTP) in China are introduced, including the key technique, fabrication of pipe production line, mass production and the latest progress of LSAW steel pipe technique. 展开更多
关键词 WEGTP LSAW UOE管道 JCOE PFP X70 输气管道
下载PDF
海上风机基础用S355NL直缝焊管双丝埋弧焊工艺设计
8
作者 葛兰 彭静 +1 位作者 郑家胜 许峰 《焊管》 2023年第3期47-52,共6页
S355NL细晶粒结构钢以其优异的性能在海上风电、石油平台、焊接钢管等方面得到广泛应用。为进一步提高焊接钢管的生产效率,获得性能优良的海上风机基础用钢管焊接接头,开展S355NL直缝焊管的焊接工艺研究。采用双丝埋弧焊方式,选用低镍... S355NL细晶粒结构钢以其优异的性能在海上风电、石油平台、焊接钢管等方面得到广泛应用。为进一步提高焊接钢管的生产效率,获得性能优良的海上风机基础用钢管焊接接头,开展S355NL直缝焊管的焊接工艺研究。采用双丝埋弧焊方式,选用低镍合金焊材,不仅能够细化焊缝组织晶粒,同时降低淬硬倾向,提高S355NL直缝焊管焊缝的低温冲击韧性。在焊接过程中采用多层多道焊接,控制热输入≤5.0 kJ/mm,减少熔合区和热影响区在高温区域停留时间,保证熔合线和热影响区冲击性能。试验结果表明,该工艺所制试板及成品焊管各项力学性能试验合格,能够满足-40℃夏比冲击试验要求。生产应用表明,该焊接工艺制定及焊材选配正确恰当,能够提高焊接生产效率。 展开更多
关键词 S355NL 海上风机 直缝焊管 双丝埋弧焊 冲击性能
下载PDF
直缝焊管排辊成形中预成形段的动力显式仿真 被引量:8
9
作者 蒋劲茂 李大永 +2 位作者 彭颖红 李建新 李永宏 《上海交通大学学报》 EI CAS CSCD 北大核心 2008年第9期1443-1447,共5页
考虑到直缝焊管的排辊成形过程非常复杂,其间涉及明显的非线性,为了更好地了解板带的成形规律,针对406 mm焊管排辊成形机组的预成形段建立了弹塑性大变形有限元模型,采用动力显式算法进行了仿真计算,分别得到了预成形段管坯的等效塑性... 考虑到直缝焊管的排辊成形过程非常复杂,其间涉及明显的非线性,为了更好地了解板带的成形规律,针对406 mm焊管排辊成形机组的预成形段建立了弹塑性大变形有限元模型,采用动力显式算法进行了仿真计算,分别得到了预成形段管坯的等效塑性应变分布和几何变形,并通过开口度和板宽的测量验证了仿真的准确性.研究结果表明:在预成形段时最大塑性变形发生在带钢的边缘,其次是带钢中心以及带钢与粗成形轧辊端面接触的区域;弯边轧辊对带钢边缘的变形贡献最大. 展开更多
关键词 排辊成形 直缝焊管 开口度 等效塑性应变
下载PDF
国产X80管线钢的应变时效行为及预防措施 被引量:9
10
作者 高建忠 马秋荣 +3 位作者 王长安 李云龙 李记科 谢勇 《机械工程材料》 CAS CSCD 北大核心 2010年第1期5-8,共4页
针对管线钢存在的应变时效问题,对国产X80管线钢及其直缝埋弧焊管管体进行了不同时效后的拉伸试验,对其应变时效行为及预防措施进行了研究。结果表明:当时效温度达到210℃时,存在1%预应变的X80管线钢和经水压、冷扩径后的直缝埋弧焊管... 针对管线钢存在的应变时效问题,对国产X80管线钢及其直缝埋弧焊管管体进行了不同时效后的拉伸试验,对其应变时效行为及预防措施进行了研究。结果表明:当时效温度达到210℃时,存在1%预应变的X80管线钢和经水压、冷扩径后的直缝埋弧焊管均出现明显的应变时效,前者屈服强度和屈强比均上升6%,后者的分别上升9.5%和6.9%,且应力-应变曲线均出现明显的屈服平台;测定拉伸性能时要尽可能降低拉伸试样的温升,降低防腐前加热温度和缩短加热时间以及降低管线钢中的碳、氮含量,采用双相显微组织并在轧制工艺中用加速冷却后立即在线热处理等方法均是降低管线钢应变时效的有效措施。 展开更多
关键词 应变时效 管线钢 直缝埋弧焊管
下载PDF
应变时效对大口径X80管线钢拉伸性能的影响 被引量:8
11
作者 彭宁琦 史术华 +2 位作者 罗登 熊祥江 李中平 《机械工程材料》 CAS CSCD 北大核心 2018年第6期42-45,49,共5页
将大口径X80管线钢试样拉伸至应变为0.5%~3.5%,卸载后分别进行室温及200,230,250℃时效处理,研究了拉伸预应变和时效温度对试验钢拉伸性能的影响;采用直缝埋弧焊在制管扩径率为0.5%~0.8%下对试验钢进行制管,研究了制管扩径率对试验钢拉... 将大口径X80管线钢试样拉伸至应变为0.5%~3.5%,卸载后分别进行室温及200,230,250℃时效处理,研究了拉伸预应变和时效温度对试验钢拉伸性能的影响;采用直缝埋弧焊在制管扩径率为0.5%~0.8%下对试验钢进行制管,研究了制管扩径率对试验钢拉伸性能的影响。结果表明:进行一定应变预拉伸+时效处理或制管扩径后,试验钢发生应变时效,其屈服强度增大,抗拉强度变化较小,屈强比增大;制管扩径率对屈服强度增量和屈强比增量的影响比拉伸预应变的更大;室温应变时效后,拉伸预应变是影响屈服强度和屈强比提高的主要因素;200~250℃应变时效对试验钢拉伸性能的影响比室温应变时效的大,200~250℃时效温度的变化对拉伸性能影响不大。 展开更多
关键词 管线钢 应变时效 直缝埋弧焊管 扩径率
下载PDF
直缝埋弧焊钢管的成形方式及选择 被引量:3
12
作者 刘林 代以斌 +1 位作者 张洪洲 郝宪国 《油气储运》 CAS 北大核心 2004年第9期52-54,共3页
直缝埋弧焊钢管由于性能优良,在未来的输送流体管道中将占有很大的比例,长输油气管道用直缝埋弧焊钢管将逐渐代替螺旋埋弧焊管。分析总结了直缝埋弧焊钢管常见的成形方式,以及各种成形方式的优缺点,就实际工程设计中如何选择直缝埋弧焊... 直缝埋弧焊钢管由于性能优良,在未来的输送流体管道中将占有很大的比例,长输油气管道用直缝埋弧焊钢管将逐渐代替螺旋埋弧焊管。分析总结了直缝埋弧焊钢管常见的成形方式,以及各种成形方式的优缺点,就实际工程设计中如何选择直缝埋弧焊钢管提出了建议和意见。 展开更多
关键词 螺旋埋弧焊管 钢管 成形 性能 方式 选择 意见 未来 优缺点 比例
下载PDF
大型直缝焊管多点弯曲一次性矫直新工艺原理 被引量:6
13
作者 赵军 宋晓抗 +1 位作者 曹宏强 刘娟 《机械工程学报》 EI CAS CSCD 北大核心 2014年第2期92-97,共6页
由于大型直缝焊管的特殊性,多采用三点弯曲多次矫直的方法修正其直线度。基于平面弯曲弹复理论及过弯矫直等价原理,给出基于管件初始挠度曲线分布的理论矫直弯矩,施加该理论弯矩可将管件一次性完全矫直。为方便工业应用,将该弯矩离散线... 由于大型直缝焊管的特殊性,多采用三点弯曲多次矫直的方法修正其直线度。基于平面弯曲弹复理论及过弯矫直等价原理,给出基于管件初始挠度曲线分布的理论矫直弯矩,施加该理论弯矩可将管件一次性完全矫直。为方便工业应用,将该弯矩离散线性化,提出多点弯曲一次性矫直控制策略,并给出相应的工艺参数的确定方法。通过实测大型管件挠度分布,建立大型管件多点弯曲一次性矫直的数值仿真模型,并以小尺寸管件的物理模拟试验验证仿真模型的可靠性。对实际管件的仿真模拟结果验证多点弯曲一次性矫直控制策略的可行性,为全自动矫直机的设计和应用提供理论基础。 展开更多
关键词 大型直缝焊管 多点弯曲 压力矫直 弯矩 控制策略
下载PDF
X100直缝埋弧焊管断裂韧性的裂纹尖端张开位移试验研究 被引量:6
14
作者 熊庆人 刘俊 +2 位作者 张建勋 李云龙 谢勇 《西安交通大学学报》 EI CAS CSCD 北大核心 2011年第9期119-124,共6页
为了检验X100直缝埋弧焊管的断裂韧性,采用三点弯曲多试样法,在室温、-10℃和-30℃下对该焊管的母材、热影响区和焊缝部位进行了裂纹尖端张开位移(CTOD)试验.测试结果表明:在同一温度下,CTOD试验的表观启裂值δ0.05、条件启裂值δi和最... 为了检验X100直缝埋弧焊管的断裂韧性,采用三点弯曲多试样法,在室温、-10℃和-30℃下对该焊管的母材、热影响区和焊缝部位进行了裂纹尖端张开位移(CTOD)试验.测试结果表明:在同一温度下,CTOD试验的表观启裂值δ0.05、条件启裂值δi和最大载荷值δm的分布规律为母材最好,焊缝次之,热影响区最差;采用裂纹扩展阻力和撕裂模量表征的分布规律为母材最好,热影响区次之,焊缝最差;焊接热影响区组织中含有大量呈块状分布的铁素体,而粒状贝氏体等增强相的含量较少,这会造成其韧性下降,使焊管出现局部失稳现象. 展开更多
关键词 断裂韧性 裂纹尖端张开位移 直缝埋弧焊管 热影响区
下载PDF
大型直缝焊管三点单次矫直技术 被引量:3
15
作者 马瑞 展培培 +1 位作者 宋晓抗 赵军 《塑性工程学报》 CAS CSCD 北大核心 2012年第3期39-43,共5页
三点弯曲压力矫直,是目前规范大型直缝焊管直线度的主要手段。由于大型管件的特殊性,文章基于激光三角法建立了大型管件的挠度测量系统。通过实验,验证了直梁三点弯曲与曲梁三点压力矫直之间的等价关系;根据弹塑性小变形理论,解析了直... 三点弯曲压力矫直,是目前规范大型直缝焊管直线度的主要手段。由于大型管件的特殊性,文章基于激光三角法建立了大型管件的挠度测量系统。通过实验,验证了直梁三点弯曲与曲梁三点压力矫直之间的等价关系;根据弹塑性小变形理论,解析了直梁弯曲过程中压下量与管坯卸载弹复后最大挠度的关系曲线,并实验验证了其正确性。该文为大型直缝焊管压力矫直工艺参数制定,提供了理论基础,改变了目前大型直缝焊管生产厂家矫直工艺主要依赖操作人员经验的现状。挠度测量系统的实现,为大型管件智能化矫直,提供了理论指导。 展开更多
关键词 大型直缝焊管 矫直 塑性小变形 挠度测量
下载PDF
卷板制造JCOE直缝埋弧焊接钢管性能 被引量:4
16
作者 杨延华 杨专钊 +3 位作者 丁毅 李云龙 马秋荣 魏亚秋 《油气储运》 CAS 北大核心 2008年第6期27-31,共5页
简述了采用热轧卷板制造直缝埋弧焊接钢管的全过程。采用热轧卷板,经过卷板开平和切断,采用JCOE工艺制成直缝埋弧焊接钢管,分别进行成分、拉伸、冲击、硬度、DWTT等理化性能检测,结果符合相关技术规范DNV-OS-F101(2000)和API SPC 5L。
关键词 卷板 JCOE工艺 直缝埋弧焊接钢管 理化性能
下载PDF
高频直缝焊管焊接残余应力的三维有限元模拟研究 被引量:10
17
作者 于恩林 韩毅 +1 位作者 谷绪地 张洪亮 《燕山大学学报》 CAS 2012年第4期298-303,共6页
基于高频直缝焊管焊接热源的计算结果,综合考虑材料的物理属性随温度的高度非线性变化,以及高频加热的焊缝热影响区特有的温度分布规律,利用ANSYS有限元软件建立了高频直缝焊管焊接残余应力的三维有限元模型。获得了高频焊管温度场和残... 基于高频直缝焊管焊接热源的计算结果,综合考虑材料的物理属性随温度的高度非线性变化,以及高频加热的焊缝热影响区特有的温度分布规律,利用ANSYS有限元软件建立了高频直缝焊管焊接残余应力的三维有限元模型。获得了高频焊管温度场和残余应力场的分布规律,并对结果进行了分析。通过后处理模块,给出了焊缝部位残余应力的分布趋势,并分析了高频感应焊接残余应力的主要形成原因。发现焊缝附近的轴向残余应力较大,其中有些数值接近材料的屈服强度,而周向残余应力仅为材料屈服应力的1/3左右,径向残余应力数值较小,工程上可以忽略。 展开更多
关键词 高频直缝焊管 温度场 残余应力 有限元模拟 热影响区
下载PDF
JCO钢管成形仿真技术研究 被引量:5
18
作者 高颖 李强 孟宪昌 《铸造技术》 CAS 北大核心 2009年第1期77-79,共3页
多道次弯曲是大口径直缝埋弧焊管关键生产技术。由于弯曲成形中卸载后的弹性恢复影响焊管的最终成形尺寸,预测管坯在多道次成形后的最终形状成为本论文的研究目标。采用有限元分析方法,针对壁厚为14.6mm、直径为508mm的X-70管线钢的成... 多道次弯曲是大口径直缝埋弧焊管关键生产技术。由于弯曲成形中卸载后的弹性恢复影响焊管的最终成形尺寸,预测管坯在多道次成形后的最终形状成为本论文的研究目标。采用有限元分析方法,针对壁厚为14.6mm、直径为508mm的X-70管线钢的成形进行了仿真研究,找到了最佳的上模位移量,数值模拟结果与生产实际吻合较好。 展开更多
关键词 大口径直缝焊管 有限元仿真 UO/UOE JCO/JCOE RB/RBE
下载PDF
焊管去内毛刺方法与装置的研究 被引量:4
19
作者 于波 于影 于华艳 《佳木斯大学学报(自然科学版)》 CAS 2007年第5期637-640,共4页
内毛刺清除是焊管生产技术中的重要环节,它是生产石油专用管,其他高强度、高精度焊管的关键工序.本文对中小直缝焊管内毛刺清除中的问题进行了分析,介绍了一种新型的拉刀内毛刺清除装置,使残余毛刺高度降至0.05-1mm.
关键词 直缝焊管 毛刺 拉刀 液压系统
下载PDF
大口径直缝焊管机械扩径成形机理研究 被引量:8
20
作者 肖曙红 郑时雄 《锻压装备与制造技术》 北大核心 2004年第5期81-84,共4页
结合大口径直缝焊管机械扩径机组开发项目,分析了大口径直缝焊管机械扩径工艺的特点,利用有限元方法对机械扩径成形机理和成形过程进行了仿真,讨论了机械扩径对扩径设备的力能要求。在此基础上,对机械扩径的主要工艺参数及其对扩径质量... 结合大口径直缝焊管机械扩径机组开发项目,分析了大口径直缝焊管机械扩径工艺的特点,利用有限元方法对机械扩径成形机理和成形过程进行了仿真,讨论了机械扩径对扩径设备的力能要求。在此基础上,对机械扩径的主要工艺参数及其对扩径质量的影响进行了详细的论述,为扩径机组的开发提供理论依据。 展开更多
关键词 机械扩径 直缝焊管 成形机理 大口径 成形过程 工艺参数 开发项目 研究 有限元方法
下载PDF
上一页 1 2 11 下一页 到第
使用帮助 返回顶部