Understanding the anisotropic creep behaviors of shale under direct shearing is a challenging issue.In this context,we conducted shear-creep and steady-creep tests on shale with five bedding orientations (i.e.0°,...Understanding the anisotropic creep behaviors of shale under direct shearing is a challenging issue.In this context,we conducted shear-creep and steady-creep tests on shale with five bedding orientations (i.e.0°,30°,45°,60°,and 90°),under multiple levels of direct shearing for the first time.The results show that the anisotropic creep of shale exhibits a significant stress-dependent behavior.Under a low shear stress,the creep compliance of shale increases linearly with the logarithm of time at all bedding orientations,and the increase depends on the bedding orientation and creep time.Under high shear stress conditions,the creep compliance of shale is minimal when the bedding orientation is 0°,and the steady-creep rate of shale increases significantly with increasing bedding orientations of 30°,45°,60°,and 90°.The stress-strain values corresponding to the inception of the accelerated creep stage show an increasing and then decreasing trend with the bedding orientation.A semilogarithmic model that could reflect the stress dependence of the steady-creep rate while considering the hardening and damage process is proposed.The model minimizes the deviation of the calculated steady-state creep rate from the observed value and reveals the behavior of the bedding orientation's influence on the steady-creep rate.The applicability of the five classical empirical creep models is quantitatively evaluated.It shows that the logarithmic model can well explain the experimental creep strain and creep rate,and it can accurately predict long-term shear creep deformation.Based on an improved logarithmic model,the variations in creep parameters with shear stress and bedding orientations are discussed.With abovementioned findings,a mathematical method for constructing an anisotropic shear creep model of shale is proposed,which can characterize the nonlinear dependence of the anisotropic shear creep behavior of shale on the bedding orientation.展开更多
The shear mechanical behavior is regarded as an essential factor affecting the stability of the surrounding rocks in underground engineering.The shear strength and failure mechanisms of layered rock are significantly ...The shear mechanical behavior is regarded as an essential factor affecting the stability of the surrounding rocks in underground engineering.The shear strength and failure mechanisms of layered rock are significantly affected by the foliation angles.Direct shear tests were conducted on cubic slate samples with foliation angles of 0°,30°,45°,60°,and 90°.The effect of foliation angles on failure patterns,acoustic emission(AE)characteristics,and shear strength parameters was analyzed.Based on AE characteristics,the slate failure process could be divided into four stages:quiet period,step-like increasing period,dramatic increasing period,and remission period.A new empirical expression of cohesion for layered rock was proposed,which was compared with linear and sinusoidal cohesion expressions based on the results made by this paper and previous experiments.The comparative analysis demonstrated that the new expression has better prediction ability than other expressions.The proposed empirical equation was used for direct shear simulations with the combined finite-discrete element method(FDEM),and it was found to align well with the experimental results.Considering both computational efficiency and accuracy,it was recommended to use a shear rate of 0.01 m/s for FDEM to carry out direct shear simulations.To balance the relationship between the number of elements and the simulation results in the direct shear simulations,the recommended element size is 1 mm.展开更多
Shearing dislocation is a common failure type for rock–backfill interfaces because of backfill sedimentation and rock strata movement in backfill mining goaf.This paper designed a test method for rock–backfill shear...Shearing dislocation is a common failure type for rock–backfill interfaces because of backfill sedimentation and rock strata movement in backfill mining goaf.This paper designed a test method for rock–backfill shearing dislocation.Using digital image techno-logy and three-dimensional(3D)laser morphology scanning techniques,a set of 3D models with rough joint surfaces was established.Further,the mechanical behavior of rock–backfill shearing dislocation was investigated using a direct shear test.The effects of interface roughness on the shear–displacement curve and failure characteristics of rock–backfill specimens were considered.The 3D fractal dimen-sion,profile line joint roughness coefficient(JRC),profile line two-dimensional fractal dimension,and the surface curvature of the frac-tures were obtained.The correlation characterization of surface roughness was then analyzed,and the shear strength could be measured and calculated using JRC.The results showed the following:there were three failure threshold value points in rock–backfill shearing dis-location:30%–50%displacement before the peak,70%–90%displacement before the peak,and 100%displacement before the peak to post-peak,which could be a sign for rock–backfill shearing dislocation failure.The surface JRC could be used to judge the rock–backfill shearing dislocation failure,including post-peak sliding,uniform variations,and gradient change,corresponding to rock–backfill disloca-tion failure on the field site.The research reveals the damage mechanism for rock–backfill complexes based on the free joint surface,fills the gap of existing shearing theoretical systems for isomerism complexes,and provides a theoretical basis for the prevention and control of possible disasters in backfill mining.展开更多
Some rock joints exhibit significant brittleness,characterized by a sharp decrease in shear stress upon reaching the peak strength.However,existing models often fail to accurately represent this behavior and are encum...Some rock joints exhibit significant brittleness,characterized by a sharp decrease in shear stress upon reaching the peak strength.However,existing models often fail to accurately represent this behavior and are encumbered by numerous parameters lacking clear mechanical significance.This study presents a new statistical damage constitutive model rooted in both damage mechanics and statistics,containing only three model parameters.The proposed model encompasses all stages of joint shearing,including the compaction stage,linear stage,plastic yielding stage,drop stage,strain softening stage,and residual strength stage.To derive the analytical expression of the constitutive model,three boundary conditions are introduced.Experimental data from both natural and artificial rock joints is utilized to validate the model,resulting in average absolute relative errors ranging from 3%to 8%.Moreover,a comparative analysis with established models illustrates that the proposed model captures stress drop and post-peak strain softening more effectively,with model parameters possessing clearer mechanical interpretations.Furthermore,parameter analysis is conducted to investigate the impacts of model parameters on the curves and unveil the relationship between these parameters and the mechanical properties of rock joints.Importantly,the proposed model is straightforward in form,and all model parameters can be obtained from direct shear tests,thus facilitating the utilization in numerical simulations.展开更多
The deep cement mixing(DCM)is used to improve the capacity and reduce the settlement of the soft ground by forming cemented clay columns.The investigation on the mechanical behaviour of the DCM samples is limited to e...The deep cement mixing(DCM)is used to improve the capacity and reduce the settlement of the soft ground by forming cemented clay columns.The investigation on the mechanical behaviour of the DCM samples is limited to either laboratory-prepared samples or in-situ samples under unconfined compression.In this study,a series of drained and undrained triaxial shearing tests was performed on the in-situ cored DCM samples with high cement content to assess their mechanical behaviours.It is found that the drainage condition affects significantly the stiffness,peak and residual strengths of the DCM samples,which is mainly due to the state of excess pore water pressure at different strain levels,i.e.being positive before the peak deviatoric stress and negative after the peak deviatoric stress,in the undrained tests.The slope of the failure envelope changes obviously with the confining pressures,being steeper at lower stress levels and flatter at higher stress levels.The strength parameters,effective cohesion and friction angle obtained from lower stress levels(c′0 andφ′0)are 400 kPa and 58°,respectively,which are deemed to be true for design in most DCM applications where the in-situ stress levels are normally at lower values of 50-200 kPa.Additionally,the computed tomography(CT)scanning system was adopted to visualize the internal structures of DCM samples.It is found that the clay pockets existing inside the DCM samples due to uneven mixing affect markedly their stress-strain behaviour,which is one of the main reasons for the high variability of the DCM samples.展开更多
A Double Shear Model(DSM) was used in a numerical simulation on bolted rock joint shearing performance.An entire bolt deformed as the letter'U'under a shear load between two joints.Near the bolt-joint intersec...A Double Shear Model(DSM) was used in a numerical simulation on bolted rock joint shearing performance.An entire bolt deformed as the letter'U'under a shear load between two joints.Near the bolt-joint intersection,the bolt partly deformed as the letter'Z'.There were two critical points along the bolt:one was at the bolt-joint intersection with zero bending moment and the other at the maximum bending moment(plastic hinge) with zero shear stress.The blocks on two sides slid along the bolt as it deformed. A separation area was found between the two joint contact surfaces of the middle rock block and sided block.This area of separation was related to bolt diameter and external forces.We assume that this area is related to the work of external forces.Further research is needed.展开更多
The shearing/cooling roll (SCR) process was adopted to prepare semi-solid A2017 alloy. The formation and evolution of non-dendritic microstructures in semi-solid A2017 alloy were studied. It is shown that the micros...The shearing/cooling roll (SCR) process was adopted to prepare semi-solid A2017 alloy. The formation and evolution of non-dendritic microstructures in semi-solid A2017 alloy were studied. It is shown that the microstructures of semi-solid billets transform from coarse dendrites into fine equiaxed grains as the pouring temperature of molten alloy decreases o.r roll-shoe cavity height is reduced. From the inlet to the exit of roll-shoe cavity, microstructure of semi-solid slurry near the shoe surface is in the order of coarse dendrites, degenerated dendrites or equiaxed grains, but fine equiaxed grains are near the roll surface. Microstructural evolution of semi-solid slurry prepared by SCR process is that the molten alloy nucleates and grows into dendrite firstly on the roll and shoe's surface. Under the shearing and stirring given by the rotating roll, the dendrites crush off and disperse into the melt. Under the shearing and stirring on semi-solid slurry with high volume fraction of solid, the dendrite arms fracture and form equiaxed grain microstructures.展开更多
A self-designed setup of modified sloping cooling/shearing process was made to prepare the semisolid Al-3wt%Mg alloy. A three-dimensional simulation model was established for the analysis of preparing the semisolid Al...A self-designed setup of modified sloping cooling/shearing process was made to prepare the semisolid Al-3wt%Mg alloy. A three-dimensional simulation model was established for the analysis of preparing the semisolid Al-3wt%Mg alloy. Through simulation and experiment, it is shown that the sloping angle of the plate greatly affects temperature and velocity distributions, and the temperature and velocity of the alloy at the exit of the sloping plate increase with the increase of the sloping angle. The alloy temperature decreases linearly from the pouring mouth to the exit. The alloy temperature at the exit increases obviously with the increase of pouring temperature. To prepare the semisolid Al-3wt%Mg alloy with good quality, the sloping angle θ=45° is reasonable, and the pouring temperature is suggested to be designed above 650-660℃ but under 700℃.展开更多
The existing investigations on piezoelectric materials containing an elliptic hole mainly focus on remote uniform tensile loads. In order to have a better understanding of the fracture behavior of piezoelectric materi...The existing investigations on piezoelectric materials containing an elliptic hole mainly focus on remote uniform tensile loads. In order to have a better understanding of the fracture behavior of piezoelectric materials under different loading conditions, theoretical and numerical solutions are presented for an elliptic hole in transversely isotropic piezoelectric materials subjected to uniform internal shearing forces based on the complex potential approach. By solving ten variable linear equations, the analytical solutions inside and outside the hole satisfying the permeable electric boundary conditions are obtained. Taking PZT-4 ceramic into consideration, numerical results of electro-elastic fields along the edge of the hole and axes, and the electric displacements in the hole are presented. Comparison with stresses in transverse isotropic elastic materials shows that the hoop stress at the ends of major axis in two kinds of material equals zero for the various ratios of major to minor axis lengths; If the ratio is greater than 1, the hoop stress in piezoelectric materials is smaller than that in elastic materials, and if the ratio is smaller than 1, the hoop stress in piezoelectric materials is greater than that in elastic materials; When it is a circle hole, the shearing stress in two materials along axes is the same. The distribution of electric displacement components shows that the vertical electric displacement in the hole and along axes in the material is always zero though under the permeable electric boundary condition; The horizontal and vertical electric displacement components along the edge of the hole are symmetrical and antisymmetrical about horizontal axis, respectively. The stress and electric displacement distribution tends to zero at distances far from the elliptical hole, which conforms to the conclusion usually made on the basis of Saint-Venant’s principle. Unlike the existing work, uniform shearing forces acting on the edge of the hole, and the distribution of electro-elastic fields inside and outside the elliptic hole are considered.展开更多
Shearing behavior and failure mechanism of bolt-grout interface are of great significance for load transfer capacity and design of rock bolting system.In this paper,direct shear tests on bolt-grout interfaces under co...Shearing behavior and failure mechanism of bolt-grout interface are of great significance for load transfer capacity and design of rock bolting system.In this paper,direct shear tests on bolt-grout interfaces under constant normal load(CNL) conditions were conducted to investigate the effects of bolt profile(i.e.rib spacing and rib height) and grout mixture on the bolt-grout interface in terms of mechanical behaviors and failure modes.Test results showed that the peak shear strength and the deformation capacity of the bolt-grout interface are highly dependent on the bolt profile and grout mixture,suggesting that bolt performances can be optimized,which were unfortunately ignored in the previous studies.A new interface failure mode,i.e.'sheared-crush' mode,was proposed,which was characterized by progressive crush failure of the grout asperities between steel ribs during shearing.It was shown that the interface failure mode mainly depends on the normal stress level and rib spacing,compared with the rib height and grout mixture for the range of tested parameters in this study.展开更多
This paper studies some interesting features of two-dimensional granular shearing flow by using molecular dynamic approach for a specific granular system. The obtained results show that the probability distribution fu...This paper studies some interesting features of two-dimensional granular shearing flow by using molecular dynamic approach for a specific granular system. The obtained results show that the probability distribution function of velocities of particles is Gaussian at the central part, but diverts from Gaussian distribution nearby the wall. The macroscopic stress along the vertical direction has large fluctuation around a constant value, the non-zero average velocity occurs mainly near the moving wall, which forms a shearing zone.. In the shearing movement, the volume of the granular material behaves in a random manner. The equivalent fl'iction coefficient between moving slab and granular material correlates with the moving speed at low velocity, and approaches constant as the velocity is large enough.展开更多
A modified technique called compatible stress iterative procedure is proposed in finite element analysis,which has well improved the conventional weighted-residual method and was successful in dealing with the formati...A modified technique called compatible stress iterative procedure is proposed in finite element analysis,which has well improved the conventional weighted-residual method and was successful in dealing with the formation and localization process of shear banding.展开更多
The mechanical behavior of the joints inside a loess layer is greatly important in weak intercalation studies owing to its involvement in a wide range of landslides in the loess region in China.The shear behavior of t...The mechanical behavior of the joints inside a loess layer is greatly important in weak intercalation studies owing to its involvement in a wide range of landslides in the loess region in China.The shear behavior of the joints in the loess stratum during direct shear and cyclic loadings was investigated using the PFC2D discrete element software.Loess mudstone and mudstone with weak intercalated layer materials were subjected to direct testing,and cyclic shear tests were conducted with consideration to the influence of normal stress and shear velocity.The macroscopic properties and damage patterns were obtained for six numerical configurations;namely,loess-weathered mudstone with 0°,10°,and-10°joints and weathered mudstone with 0°,10°,and-10°weak intercalated layers.The numerical test results revealed that,in the direct shear tests,the shear stress and shear displacement of the samples increased with the normal stress.In the cyclic shear tests with a total cycle number N=20,the shear stress-shear strain curve of the six different configurations exhibited a hysteresis loop.The numerical tests also revealed that,under cyclic shear,the normal stress and shear velocity affected the shear strength.The degree of damage increased as the shear velocity decreased from 0.1 mm/s to 0.005 mm/s for all six numerical configurations.Compared with the damage pattern of the direct shear tests,the damage of the cyclic shear tests mainly comprised shear cracks and fractures,some shaking consolidation settlement and fewer shear strain occurred around the joints.In the direct shear tests,more compression cracks and fractures occurred in the samples.The damage mainly developed along the joints,and shearing-off damage occurred.The results obtained by this study further elucidate the failure mechanism and microscopic damage response of the joints in the loess stratum in Northwest China.展开更多
A hybrid finite-discrete element method was implemented to study the fracture process of rough rock joints under direct shearing. The hybrid method reproduced the joint shear resistance evolution process from asperity...A hybrid finite-discrete element method was implemented to study the fracture process of rough rock joints under direct shearing. The hybrid method reproduced the joint shear resistance evolution process from asperity sliding to degradation and from gouge formation to grinding. It is found that, in the direct shear test of rough rock joints under constant normal displacement loading conditions, higher shearing rate promotes the asperity degradation but constraints the volume dilation, which then results in higher peak shear resistance, more gouge formation and grinding, and smoother new joint surfaces. Moreover, it is found that the joint roughness affects the joint shear resistance evolution through influencing the joint fracture micro mechanism. The asperity degradation and gouge grinding are the main failure micro-mechanism in shearing rougher rock joints with deeper asperities while the asperity sliding is the main failure micro-mechanism in shearing smoother rock joints with shallower asperities. It is concluded that the hybrid finite-discrete element method is a valuable numerical tool better than traditional finite element method and discrete element method for modelling the joint sliding, asperity degradation, gouge formation, and gouge grinding occurred in the direct shear tests of rough rock joints.展开更多
The spores of Ganoderma lucidum were ground and broken to ultrafine particles by high speed centrifugal shearing(HSCS) pulverizer. The characteristics of Ganoderma lucidum spores were analyzed by scanning electron m...The spores of Ganoderma lucidum were ground and broken to ultrafine particles by high speed centrifugal shearing(HSCS) pulverizer. The characteristics of Ganoderma lucidum spores were analyzed by scanning electron microscope (SEM), Fourier transform infrared spectrophotometry (FTIR). Ultraviolet-visible pectrophotometer was used to determine the extraction ratio of aqueous solubility polysaccharide between the raw and broken spores. The immunological function on the mice before and after the breaking of spores wan investigated. The experimental results show that after being ground, the sporoderm-broken ratio reachs 100%, the original active ingredients of ganoderma lucidum spores do not change, and the extraction ratio of aqueous solubility polysaccharide is greatly increased by 40.08%. The broken spores show much higher immunological activity comparing with original spores of Ganoderma lucidum.展开更多
Excellent quality of shearing edge implies that a s mo oth cutting edge without tearing will be observed on the whole edge surface. Thi s is one of the most significant features of the Fine-blanking process. To achi e...Excellent quality of shearing edge implies that a s mo oth cutting edge without tearing will be observed on the whole edge surface. Thi s is one of the most significant features of the Fine-blanking process. To achi eve such a superb blanking edge quality in fine-blanking, there actually involv es quite a large number of factors, such as blanking speed, processing material, product shape, lubrication and tool geometry, to be considered simultaneously d uring the operation. Nevertheless, the thorough investigations on different effe cts of those critical factors for different kinds of popular and applicable mate rial are rare and limited. Thus, the objective of this paper is mainly focused o n the study of the quality influence of tool geometry change in fine-blanking f or non-homogeneous materials. However, the most obvious change of the tool geo metry during the operation will be the essential variation of the nose radius of the punch. This is because the nose radius usually seriously deteriorates with the increasing service period in mass production which eventually causes the ent irely lose of the specific features of the fine-blanking process. Therefore, a tailor-made experimental study was carried out to investigate the relationship between the punch nose radius and the shearing edge quality, such as blanked edg e finish, burr height and die-roll height, during fine-blanking for different types of material. Five punches with each specified nose radius (Rp), 0.00 mm, 0.25 mm, 0.50 mm, 0.75 mm and 1.00 mm, and four kinds of blanking material ( Mil d steel SS400, Stainless steel AISI316L, Copper alloy UNSC16200 and Aluminium al loy AA6063 ) were employed throughout the study. Subsequently, features of the s heared edge surfaces and data of each experiment were observed and captured for further analysis in this research. Consequently, findings show that an increase of punch nose radius would produce a higher percentage of fracture of blanked ed ge and increase the amount of burr height. In overall comparison, it is found th at mild steel and copper alloy do provide better surface edge finish with higher percentage of sheared area and less burr height than that of stainless steel an d aluminium alloy.展开更多
Intensive melt shearing has a significant grain refining effect on some light alloys.However,the persistence of the grain refining effect during isothermal holding and remelting is still unclear,although it is very im...Intensive melt shearing has a significant grain refining effect on some light alloys.However,the persistence of the grain refining effect during isothermal holding and remelting is still unclear,although it is very important for the practical application.In this study,intensive melt shearing was achieved in a twin-screw mechanism to investigate its grain refining effect on AZ91D magnesium alloy.The refinement mechanism was discussed and the persistence of grain refinement after remelting and isothermal holding was also studied.A Zeiss imaging system with polarized light was used for quantitative measurement of grain size.The results show that the intensive melt shearing has a significant grain refining effect on AZ91D magnesium alloy.With the application of intensive melt shearing,the grain size of AZ91D magnesium alloy can be reduced from 530 μm(for a typical as-cast microstructure) to 170 μm,which is about 70% size reduction.The grain refinement achieved by the intensive melt shearing can be partially kept after isothermal holding and remelting.It is believed that the refinement effect was mainly due to the finer and well dispersed oxide particles formed by high intensive shearing.The smaller size of oxide particles and their slow motion velocity in the sheared melt could make important contributions to the remained grain refinement.展开更多
Rock joints exhibit hysteresis shearing behavior and produce energy dissipation under shear cyclic loads,which however cannot be accurately depicted by existing constitutive models. This paper establishes a constituti...Rock joints exhibit hysteresis shearing behavior and produce energy dissipation under shear cyclic loads,which however cannot be accurately depicted by existing constitutive models. This paper establishes a constitutive model for hysteresis shearing and associated energy dissipation of rock joints. Analytical expressions of the model during cyclic shearing processes are derived. Derivation of the model indicates no energy dissipation in the elastic stage. When the shear load exceeds elastic boundary, nonlinear energy dissipation takes place. Validations with experiments show that the proposed model provides good conformities with direct shear curves and hysteresis loops, and can predict the energy dissipation characteristics of rock joints under different working conditions. Compared to the constitutive models using Weibull's distribution, the proposed one is smooth at the elastic boundary and can accurately capture the maximum shear stress. Unlike the existing incremental-type models, the proposed one provides clear and direct analytical expressions for both shear stress and energy dissipation during the whole displacement domain, which is more convenient in application.展开更多
Rock joints infilled with sediments can strongly influence the strength of rock mass. As infilled joints often exist under unsaturated condition, this study investigated the influence of matric suction of infill on th...Rock joints infilled with sediments can strongly influence the strength of rock mass. As infilled joints often exist under unsaturated condition, this study investigated the influence of matric suction of infill on the overall joint shear strength. A novel technique that allows direct measurement of matric suction of infill using high capacity tensiometers(HCTs) during direct shear of infilled joints under constant normal stiffness(CNS) is described. The CNS apparatus was modified to accommodate the HCT and the procedure is explained in detail. Joint specimens were simulated by gypsum plaster using threedimensional(3D) printed surface moulds, and filled with kaolin and sand mixture prepared at different water contents. Shear behaviours of both planar infilled joints and rough joints having joint roughness coefficients(JRCs) of 8-10 and 18-20 with the ratios of infill thickness to asperity height(t/a)equal to 0.5 were investigated. Matric suction shows predominantly unimodal behaviour during shearing of both planar and rough joints, which is closely associated with the variation of unloading rate and volumetric changes of the infill material. As expected, two-peak behaviour was observed for the rough joints and both peaks increased with the increase of infill matric suction. The results suggest that the contribution of matric suction of infill on the joint peak normalised shear stress is relatively independent of the joint roughness.展开更多
基金funded by the National Natural Science Foundation of China(Grant Nos.U22A20166 and 12172230)the Guangdong Basic and Applied Basic Research Foundation(Grant No.2023A1515012654)+1 种基金funded by the National Natural Science Foundation of China(Grant Nos.U22A20166 and 12172230)the Guangdong Basic and Applied Basic Research Foundation(Grant No.2023A1515012654)。
文摘Understanding the anisotropic creep behaviors of shale under direct shearing is a challenging issue.In this context,we conducted shear-creep and steady-creep tests on shale with five bedding orientations (i.e.0°,30°,45°,60°,and 90°),under multiple levels of direct shearing for the first time.The results show that the anisotropic creep of shale exhibits a significant stress-dependent behavior.Under a low shear stress,the creep compliance of shale increases linearly with the logarithm of time at all bedding orientations,and the increase depends on the bedding orientation and creep time.Under high shear stress conditions,the creep compliance of shale is minimal when the bedding orientation is 0°,and the steady-creep rate of shale increases significantly with increasing bedding orientations of 30°,45°,60°,and 90°.The stress-strain values corresponding to the inception of the accelerated creep stage show an increasing and then decreasing trend with the bedding orientation.A semilogarithmic model that could reflect the stress dependence of the steady-creep rate while considering the hardening and damage process is proposed.The model minimizes the deviation of the calculated steady-state creep rate from the observed value and reveals the behavior of the bedding orientation's influence on the steady-creep rate.The applicability of the five classical empirical creep models is quantitatively evaluated.It shows that the logarithmic model can well explain the experimental creep strain and creep rate,and it can accurately predict long-term shear creep deformation.Based on an improved logarithmic model,the variations in creep parameters with shear stress and bedding orientations are discussed.With abovementioned findings,a mathematical method for constructing an anisotropic shear creep model of shale is proposed,which can characterize the nonlinear dependence of the anisotropic shear creep behavior of shale on the bedding orientation.
基金support from the Natural Science Foundation of China(Grant Nos.41941018,U21A20153,42177140).
文摘The shear mechanical behavior is regarded as an essential factor affecting the stability of the surrounding rocks in underground engineering.The shear strength and failure mechanisms of layered rock are significantly affected by the foliation angles.Direct shear tests were conducted on cubic slate samples with foliation angles of 0°,30°,45°,60°,and 90°.The effect of foliation angles on failure patterns,acoustic emission(AE)characteristics,and shear strength parameters was analyzed.Based on AE characteristics,the slate failure process could be divided into four stages:quiet period,step-like increasing period,dramatic increasing period,and remission period.A new empirical expression of cohesion for layered rock was proposed,which was compared with linear and sinusoidal cohesion expressions based on the results made by this paper and previous experiments.The comparative analysis demonstrated that the new expression has better prediction ability than other expressions.The proposed empirical equation was used for direct shear simulations with the combined finite-discrete element method(FDEM),and it was found to align well with the experimental results.Considering both computational efficiency and accuracy,it was recommended to use a shear rate of 0.01 m/s for FDEM to carry out direct shear simulations.To balance the relationship between the number of elements and the simulation results in the direct shear simulations,the recommended element size is 1 mm.
基金supported by the National Key Research and Development Program of China(No.2021YFC3001302)the National Natural Science Foundation of China(No.52274072).
文摘Shearing dislocation is a common failure type for rock–backfill interfaces because of backfill sedimentation and rock strata movement in backfill mining goaf.This paper designed a test method for rock–backfill shearing dislocation.Using digital image techno-logy and three-dimensional(3D)laser morphology scanning techniques,a set of 3D models with rough joint surfaces was established.Further,the mechanical behavior of rock–backfill shearing dislocation was investigated using a direct shear test.The effects of interface roughness on the shear–displacement curve and failure characteristics of rock–backfill specimens were considered.The 3D fractal dimen-sion,profile line joint roughness coefficient(JRC),profile line two-dimensional fractal dimension,and the surface curvature of the frac-tures were obtained.The correlation characterization of surface roughness was then analyzed,and the shear strength could be measured and calculated using JRC.The results showed the following:there were three failure threshold value points in rock–backfill shearing dis-location:30%–50%displacement before the peak,70%–90%displacement before the peak,and 100%displacement before the peak to post-peak,which could be a sign for rock–backfill shearing dislocation failure.The surface JRC could be used to judge the rock–backfill shearing dislocation failure,including post-peak sliding,uniform variations,and gradient change,corresponding to rock–backfill disloca-tion failure on the field site.The research reveals the damage mechanism for rock–backfill complexes based on the free joint surface,fills the gap of existing shearing theoretical systems for isomerism complexes,and provides a theoretical basis for the prevention and control of possible disasters in backfill mining.
基金funded by the National Natural Science Foundation of China(No.41972266)Chongqing Natural Science Foundation(No.CSTB2024NSCQ-MSX0006).
文摘Some rock joints exhibit significant brittleness,characterized by a sharp decrease in shear stress upon reaching the peak strength.However,existing models often fail to accurately represent this behavior and are encumbered by numerous parameters lacking clear mechanical significance.This study presents a new statistical damage constitutive model rooted in both damage mechanics and statistics,containing only three model parameters.The proposed model encompasses all stages of joint shearing,including the compaction stage,linear stage,plastic yielding stage,drop stage,strain softening stage,and residual strength stage.To derive the analytical expression of the constitutive model,three boundary conditions are introduced.Experimental data from both natural and artificial rock joints is utilized to validate the model,resulting in average absolute relative errors ranging from 3%to 8%.Moreover,a comparative analysis with established models illustrates that the proposed model captures stress drop and post-peak strain softening more effectively,with model parameters possessing clearer mechanical interpretations.Furthermore,parameter analysis is conducted to investigate the impacts of model parameters on the curves and unveil the relationship between these parameters and the mechanical properties of rock joints.Importantly,the proposed model is straightforward in form,and all model parameters can be obtained from direct shear tests,thus facilitating the utilization in numerical simulations.
基金funded by the Environment and Conservation Fund(Grant Nos.2020-170 and 2021-156)the National Natural Science Foundation of China(Grant No.42102327).
文摘The deep cement mixing(DCM)is used to improve the capacity and reduce the settlement of the soft ground by forming cemented clay columns.The investigation on the mechanical behaviour of the DCM samples is limited to either laboratory-prepared samples or in-situ samples under unconfined compression.In this study,a series of drained and undrained triaxial shearing tests was performed on the in-situ cored DCM samples with high cement content to assess their mechanical behaviours.It is found that the drainage condition affects significantly the stiffness,peak and residual strengths of the DCM samples,which is mainly due to the state of excess pore water pressure at different strain levels,i.e.being positive before the peak deviatoric stress and negative after the peak deviatoric stress,in the undrained tests.The slope of the failure envelope changes obviously with the confining pressures,being steeper at lower stress levels and flatter at higher stress levels.The strength parameters,effective cohesion and friction angle obtained from lower stress levels(c′0 andφ′0)are 400 kPa and 58°,respectively,which are deemed to be true for design in most DCM applications where the in-situ stress levels are normally at lower values of 50-200 kPa.Additionally,the computed tomography(CT)scanning system was adopted to visualize the internal structures of DCM samples.It is found that the clay pockets existing inside the DCM samples due to uneven mixing affect markedly their stress-strain behaviour,which is one of the main reasons for the high variability of the DCM samples.
基金Financial support from the National Natural Science Foundation of China(No.50978251)the National Government Building High-Level University Graduate Programs of the China Scholarship Council
文摘A Double Shear Model(DSM) was used in a numerical simulation on bolted rock joint shearing performance.An entire bolt deformed as the letter'U'under a shear load between two joints.Near the bolt-joint intersection,the bolt partly deformed as the letter'Z'.There were two critical points along the bolt:one was at the bolt-joint intersection with zero bending moment and the other at the maximum bending moment(plastic hinge) with zero shear stress.The blocks on two sides slid along the bolt as it deformed. A separation area was found between the two joint contact surfaces of the middle rock block and sided block.This area of separation was related to bolt diameter and external forces.We assume that this area is related to the work of external forces.Further research is needed.
基金The authors would like to thank the National Natural Science Foundation of China and Baoshan Iron&Steel Co.of Shanghai for financial support under the grant No.50274020.
文摘The shearing/cooling roll (SCR) process was adopted to prepare semi-solid A2017 alloy. The formation and evolution of non-dendritic microstructures in semi-solid A2017 alloy were studied. It is shown that the microstructures of semi-solid billets transform from coarse dendrites into fine equiaxed grains as the pouring temperature of molten alloy decreases o.r roll-shoe cavity height is reduced. From the inlet to the exit of roll-shoe cavity, microstructure of semi-solid slurry near the shoe surface is in the order of coarse dendrites, degenerated dendrites or equiaxed grains, but fine equiaxed grains are near the roll surface. Microstructural evolution of semi-solid slurry prepared by SCR process is that the molten alloy nucleates and grows into dendrite firstly on the roll and shoe's surface. Under the shearing and stirring given by the rotating roll, the dendrites crush off and disperse into the melt. Under the shearing and stirring on semi-solid slurry with high volume fraction of solid, the dendrite arms fracture and form equiaxed grain microstructures.
基金This work was financially supported by the National Natural Science Foundation of China (No.50604007)the Natural ScienceFoundation of Liaoning Province, China (No.20062016)
文摘A self-designed setup of modified sloping cooling/shearing process was made to prepare the semisolid Al-3wt%Mg alloy. A three-dimensional simulation model was established for the analysis of preparing the semisolid Al-3wt%Mg alloy. Through simulation and experiment, it is shown that the sloping angle of the plate greatly affects temperature and velocity distributions, and the temperature and velocity of the alloy at the exit of the sloping plate increase with the increase of the sloping angle. The alloy temperature decreases linearly from the pouring mouth to the exit. The alloy temperature at the exit increases obviously with the increase of pouring temperature. To prepare the semisolid Al-3wt%Mg alloy with good quality, the sloping angle θ=45° is reasonable, and the pouring temperature is suggested to be designed above 650-660℃ but under 700℃.
基金supported by Hebei Provincial Natural Science Foundation of China (Grant No. A2011210033)Foundation of Hebei Provincial Education Department of China (Grant No. ZH2011116)Hebei Provincial Research Program for Higher Education and Teaching Reform of China (Grant No. 103024)
文摘The existing investigations on piezoelectric materials containing an elliptic hole mainly focus on remote uniform tensile loads. In order to have a better understanding of the fracture behavior of piezoelectric materials under different loading conditions, theoretical and numerical solutions are presented for an elliptic hole in transversely isotropic piezoelectric materials subjected to uniform internal shearing forces based on the complex potential approach. By solving ten variable linear equations, the analytical solutions inside and outside the hole satisfying the permeable electric boundary conditions are obtained. Taking PZT-4 ceramic into consideration, numerical results of electro-elastic fields along the edge of the hole and axes, and the electric displacements in the hole are presented. Comparison with stresses in transverse isotropic elastic materials shows that the hoop stress at the ends of major axis in two kinds of material equals zero for the various ratios of major to minor axis lengths; If the ratio is greater than 1, the hoop stress in piezoelectric materials is smaller than that in elastic materials, and if the ratio is smaller than 1, the hoop stress in piezoelectric materials is greater than that in elastic materials; When it is a circle hole, the shearing stress in two materials along axes is the same. The distribution of electric displacement components shows that the vertical electric displacement in the hole and along axes in the material is always zero though under the permeable electric boundary condition; The horizontal and vertical electric displacement components along the edge of the hole are symmetrical and antisymmetrical about horizontal axis, respectively. The stress and electric displacement distribution tends to zero at distances far from the elliptical hole, which conforms to the conclusion usually made on the basis of Saint-Venant’s principle. Unlike the existing work, uniform shearing forces acting on the edge of the hole, and the distribution of electro-elastic fields inside and outside the elliptic hole are considered.
基金supported by the Key Projects of the Yalong River Joint Fund of the National Natural Science Foundation of China(Grant No.U1865203)the National Natural Science Foundation of China(Grant No.51279201)+1 种基金Special project of the National Natural Science Foundation of China(Grant No.41941018)The partial support from the Youth Innovation Promotion Association,Chinese Academy of Sciences。
文摘Shearing behavior and failure mechanism of bolt-grout interface are of great significance for load transfer capacity and design of rock bolting system.In this paper,direct shear tests on bolt-grout interfaces under constant normal load(CNL) conditions were conducted to investigate the effects of bolt profile(i.e.rib spacing and rib height) and grout mixture on the bolt-grout interface in terms of mechanical behaviors and failure modes.Test results showed that the peak shear strength and the deformation capacity of the bolt-grout interface are highly dependent on the bolt profile and grout mixture,suggesting that bolt performances can be optimized,which were unfortunately ignored in the previous studies.A new interface failure mode,i.e.'sheared-crush' mode,was proposed,which was characterized by progressive crush failure of the grout asperities between steel ribs during shearing.It was shown that the interface failure mode mainly depends on the normal stress level and rib spacing,compared with the rib height and grout mixture for the range of tested parameters in this study.
基金supported by the National Natural Science Foundation of China (Grant Nos. 10872005 and 10128204)
文摘This paper studies some interesting features of two-dimensional granular shearing flow by using molecular dynamic approach for a specific granular system. The obtained results show that the probability distribution function of velocities of particles is Gaussian at the central part, but diverts from Gaussian distribution nearby the wall. The macroscopic stress along the vertical direction has large fluctuation around a constant value, the non-zero average velocity occurs mainly near the moving wall, which forms a shearing zone.. In the shearing movement, the volume of the granular material behaves in a random manner. The equivalent fl'iction coefficient between moving slab and granular material correlates with the moving speed at low velocity, and approaches constant as the velocity is large enough.
基金This research project was partly supported by NNSF of China.
文摘A modified technique called compatible stress iterative procedure is proposed in finite element analysis,which has well improved the conventional weighted-residual method and was successful in dealing with the formation and localization process of shear banding.
基金sponsored by National Natural Science Foundation of China(No.41902269)Chinese Universities Scientific Fund(2020TC095)。
文摘The mechanical behavior of the joints inside a loess layer is greatly important in weak intercalation studies owing to its involvement in a wide range of landslides in the loess region in China.The shear behavior of the joints in the loess stratum during direct shear and cyclic loadings was investigated using the PFC2D discrete element software.Loess mudstone and mudstone with weak intercalated layer materials were subjected to direct testing,and cyclic shear tests were conducted with consideration to the influence of normal stress and shear velocity.The macroscopic properties and damage patterns were obtained for six numerical configurations;namely,loess-weathered mudstone with 0°,10°,and-10°joints and weathered mudstone with 0°,10°,and-10°weak intercalated layers.The numerical test results revealed that,in the direct shear tests,the shear stress and shear displacement of the samples increased with the normal stress.In the cyclic shear tests with a total cycle number N=20,the shear stress-shear strain curve of the six different configurations exhibited a hysteresis loop.The numerical tests also revealed that,under cyclic shear,the normal stress and shear velocity affected the shear strength.The degree of damage increased as the shear velocity decreased from 0.1 mm/s to 0.005 mm/s for all six numerical configurations.Compared with the damage pattern of the direct shear tests,the damage of the cyclic shear tests mainly comprised shear cracks and fractures,some shaking consolidation settlement and fewer shear strain occurred around the joints.In the direct shear tests,more compression cracks and fractures occurred in the samples.The damage mainly developed along the joints,and shearing-off damage occurred.The results obtained by this study further elucidate the failure mechanism and microscopic damage response of the joints in the loess stratum in Northwest China.
基金The first author would like to thank the supports of the NARGS, IRGS and AAS grants of Australia, and the National Science Foundation grants (No. 51574060 and No. 51079017) of China, in which the first author is the intemational collaborator. The academic visits of the third and fourth authors to the University of Tasmania are partly supported by a PhD visiting scholarship and an academic visiting scholarship, respectively, provided by the China Scholarship Council, which are greatly appreciated.
文摘A hybrid finite-discrete element method was implemented to study the fracture process of rough rock joints under direct shearing. The hybrid method reproduced the joint shear resistance evolution process from asperity sliding to degradation and from gouge formation to grinding. It is found that, in the direct shear test of rough rock joints under constant normal displacement loading conditions, higher shearing rate promotes the asperity degradation but constraints the volume dilation, which then results in higher peak shear resistance, more gouge formation and grinding, and smoother new joint surfaces. Moreover, it is found that the joint roughness affects the joint shear resistance evolution through influencing the joint fracture micro mechanism. The asperity degradation and gouge grinding are the main failure micro-mechanism in shearing rougher rock joints with deeper asperities while the asperity sliding is the main failure micro-mechanism in shearing smoother rock joints with shallower asperities. It is concluded that the hybrid finite-discrete element method is a valuable numerical tool better than traditional finite element method and discrete element method for modelling the joint sliding, asperity degradation, gouge formation, and gouge grinding occurred in the direct shear tests of rough rock joints.
基金the National Natural Science Foundation of China(No.50272047)Ministry of Education of China(No.704034)
文摘The spores of Ganoderma lucidum were ground and broken to ultrafine particles by high speed centrifugal shearing(HSCS) pulverizer. The characteristics of Ganoderma lucidum spores were analyzed by scanning electron microscope (SEM), Fourier transform infrared spectrophotometry (FTIR). Ultraviolet-visible pectrophotometer was used to determine the extraction ratio of aqueous solubility polysaccharide between the raw and broken spores. The immunological function on the mice before and after the breaking of spores wan investigated. The experimental results show that after being ground, the sporoderm-broken ratio reachs 100%, the original active ingredients of ganoderma lucidum spores do not change, and the extraction ratio of aqueous solubility polysaccharide is greatly increased by 40.08%. The broken spores show much higher immunological activity comparing with original spores of Ganoderma lucidum.
文摘Excellent quality of shearing edge implies that a s mo oth cutting edge without tearing will be observed on the whole edge surface. Thi s is one of the most significant features of the Fine-blanking process. To achi eve such a superb blanking edge quality in fine-blanking, there actually involv es quite a large number of factors, such as blanking speed, processing material, product shape, lubrication and tool geometry, to be considered simultaneously d uring the operation. Nevertheless, the thorough investigations on different effe cts of those critical factors for different kinds of popular and applicable mate rial are rare and limited. Thus, the objective of this paper is mainly focused o n the study of the quality influence of tool geometry change in fine-blanking f or non-homogeneous materials. However, the most obvious change of the tool geo metry during the operation will be the essential variation of the nose radius of the punch. This is because the nose radius usually seriously deteriorates with the increasing service period in mass production which eventually causes the ent irely lose of the specific features of the fine-blanking process. Therefore, a tailor-made experimental study was carried out to investigate the relationship between the punch nose radius and the shearing edge quality, such as blanked edg e finish, burr height and die-roll height, during fine-blanking for different types of material. Five punches with each specified nose radius (Rp), 0.00 mm, 0.25 mm, 0.50 mm, 0.75 mm and 1.00 mm, and four kinds of blanking material ( Mil d steel SS400, Stainless steel AISI316L, Copper alloy UNSC16200 and Aluminium al loy AA6063 ) were employed throughout the study. Subsequently, features of the s heared edge surfaces and data of each experiment were observed and captured for further analysis in this research. Consequently, findings show that an increase of punch nose radius would produce a higher percentage of fracture of blanked ed ge and increase the amount of burr height. In overall comparison, it is found th at mild steel and copper alloy do provide better surface edge finish with higher percentage of sheared area and less burr height than that of stainless steel an d aluminium alloy.
基金supported by the Engineering and Physical Sciences Research Council(EPSRC) of the UK and the National Natural Science Foundation of China(Grant No.51104043)
文摘Intensive melt shearing has a significant grain refining effect on some light alloys.However,the persistence of the grain refining effect during isothermal holding and remelting is still unclear,although it is very important for the practical application.In this study,intensive melt shearing was achieved in a twin-screw mechanism to investigate its grain refining effect on AZ91D magnesium alloy.The refinement mechanism was discussed and the persistence of grain refinement after remelting and isothermal holding was also studied.A Zeiss imaging system with polarized light was used for quantitative measurement of grain size.The results show that the intensive melt shearing has a significant grain refining effect on AZ91D magnesium alloy.With the application of intensive melt shearing,the grain size of AZ91D magnesium alloy can be reduced from 530 μm(for a typical as-cast microstructure) to 170 μm,which is about 70% size reduction.The grain refinement achieved by the intensive melt shearing can be partially kept after isothermal holding and remelting.It is believed that the refinement effect was mainly due to the finer and well dispersed oxide particles formed by high intensive shearing.The smaller size of oxide particles and their slow motion velocity in the sheared melt could make important contributions to the remained grain refinement.
基金supported by the National Natural Science Foundation of China (No. 51974171)the Major Program of Shandong Provincial Natural Science Foundation (No. ZR2019ZD13)the Major Scientific and Technological Innovation Project of Shandong Provincial Key Research Development Program (No. 2019SDZY02)。
文摘Rock joints exhibit hysteresis shearing behavior and produce energy dissipation under shear cyclic loads,which however cannot be accurately depicted by existing constitutive models. This paper establishes a constitutive model for hysteresis shearing and associated energy dissipation of rock joints. Analytical expressions of the model during cyclic shearing processes are derived. Derivation of the model indicates no energy dissipation in the elastic stage. When the shear load exceeds elastic boundary, nonlinear energy dissipation takes place. Validations with experiments show that the proposed model provides good conformities with direct shear curves and hysteresis loops, and can predict the energy dissipation characteristics of rock joints under different working conditions. Compared to the constitutive models using Weibull's distribution, the proposed one is smooth at the elastic boundary and can accurately capture the maximum shear stress. Unlike the existing incremental-type models, the proposed one provides clear and direct analytical expressions for both shear stress and energy dissipation during the whole displacement domain, which is more convenient in application.
基金The financial support provided by the China Scholarship Council (Grant No. 201406420027)
文摘Rock joints infilled with sediments can strongly influence the strength of rock mass. As infilled joints often exist under unsaturated condition, this study investigated the influence of matric suction of infill on the overall joint shear strength. A novel technique that allows direct measurement of matric suction of infill using high capacity tensiometers(HCTs) during direct shear of infilled joints under constant normal stiffness(CNS) is described. The CNS apparatus was modified to accommodate the HCT and the procedure is explained in detail. Joint specimens were simulated by gypsum plaster using threedimensional(3D) printed surface moulds, and filled with kaolin and sand mixture prepared at different water contents. Shear behaviours of both planar infilled joints and rough joints having joint roughness coefficients(JRCs) of 8-10 and 18-20 with the ratios of infill thickness to asperity height(t/a)equal to 0.5 were investigated. Matric suction shows predominantly unimodal behaviour during shearing of both planar and rough joints, which is closely associated with the variation of unloading rate and volumetric changes of the infill material. As expected, two-peak behaviour was observed for the rough joints and both peaks increased with the increase of infill matric suction. The results suggest that the contribution of matric suction of infill on the joint peak normalised shear stress is relatively independent of the joint roughness.