Direct and Simultaneous Determination of Several Impurity Elements in Manganese Tetroxide using ICP-AES 被引量:2
1
作者 姚俊 Atakora Djak Ladislau Kékedy-Nagy 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2006年第1期4-8,共5页
A rapid method for the determination of impurity elements, such as Zn, Ni, Co, Cr, Cu, Cd and Pb in manganese tetroxide was developed, using inductively coupled plasma atomic emission spectrometry (ICP-AES). The cri... A rapid method for the determination of impurity elements, such as Zn, Ni, Co, Cr, Cu, Cd and Pb in manganese tetroxide was developed, using inductively coupled plasma atomic emission spectrometry (ICP-AES). The critical instrumental parameters such as sample flow rate and radio frequency incident were thoroughly optimized. The effect of matrix was also examined. The sensitivity was investigated using calibration curves obtained in presence of the matrix. The obtained recoveries for Ni, Co, Cr, Cu, and Cd at the μg· g^ -1 level were satisfactory and practically independent of the matrix used for the calibration standards. The recoveries of Pb and Zn were less suffwient. The method can be applied for routine analysis and quality control purposes at μg· g^-1 level of concentration. 展开更多
关键词 manganese tetroxide impurity elements inductively coupled plasma-atomic emission spectrometry
下载PDF
Synthesis and characterization of manganese tetroxide(Mn_(3)O_(4))nanofibers by electrospinning technique 被引量:2
2
作者 Benudhar SAHOO Prasanta Kumar PANDA 《Journal of Advanced Ceramics》 SCIE CAS 2013年第1期26-30,共5页
Manganese tetroxide(Mn_(3)O_(4))nanofibers were prepared by electrospinning homogeneous viscous solution of 20 wt%,28 wt%and 36 wt%manganese acetate in poly vinyl alcohol(PVA)and calcining the nanofibers at 1000℃for ... Manganese tetroxide(Mn_(3)O_(4))nanofibers were prepared by electrospinning homogeneous viscous solution of 20 wt%,28 wt%and 36 wt%manganese acetate in poly vinyl alcohol(PVA)and calcining the nanofibers at 1000℃for 2 h.Electrospinning was carried out at 9 kV DC with tip to collector distance(TCD)of 7 cm.Thermo gravimetric analysis(TGA)of the fibers indicates the pure phase of manganese oxide above 500℃.XRD analysis of calcined(at 1000℃)nanofibers indicates the formation of phase-pure tetragonal Mn_(3)O_(4).Scanning electron microscopy(SEM)studies show the fibers cylindrical with the diameters in the range of 100-600 nm and aspect ratio>1000.In general,the average diameter of the green fibers decreases with the increase in manganese acetate concentration.The diameter of calcined nanofibers is reduced by 34%. 展开更多
关键词 ELECTROSPINNING manganese tetroxide poly vinyl alcohol NANOFIBER
原文传递