A Mathematical Model for Predicting Shrinkage Defect of Ductile Iron Castings
1
作者 ZhiqiangHan Junyi Su Kaike Cai Metallurgy School, University of Science and Technology Beijing, Beijing 100083, China Xi’an Jiaotong University, Xi’an 710049, China 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2000年第1期24-29,共6页
The shrinkage defect of a ductile iron casting is attributed to the volume variations occurring in solidification, which consist of liquid contraction, solidification shrinkage, graphitization expansion, and mold cavi... The shrinkage defect of a ductile iron casting is attributed to the volume variations occurring in solidification, which consist of liquid contraction, solidification shrinkage, graphitization expansion, and mold cavity enlargement. Based on this understanding, a mathematical model for predicting the shrinkage defect of the casting is developed, in which the volume variations of the casting in soli- dification are numerically simulated, especially, the mold cavity enlargement is quantitatively calculated. Moreover, the reliability of the model is verified in production and experiment. 展开更多
关键词 ductile iron casting shrinkage defect mold cavity enlargement mathematical model
下载PDF
Active Air Venting of Mold Cavity to Improve Performance of Injection Molded Direct Joining
2
作者 Fuminobu Kimura Shotaro Kadoya Yusuke Kajihara 《Nanomanufacturing and Metrology》 2021年第2期109-117,共9页
A surface micro-/nano-structured metal plate can be joined with an injection molded plastic piece in a mold,which has been named injection molded direct joining(IMDJ).The injected plastic melt infiltrates the micro-/n... A surface micro-/nano-structured metal plate can be joined with an injection molded plastic piece in a mold,which has been named injection molded direct joining(IMDJ).The injected plastic melt infiltrates the micro-/nano-structure,e.g.,a porous structure with micro/nano pores,on the metal plate while flowing in the mold cavity where the metal plate is inserted.After solidification of the plastic,the metal and plastic materials are directly joined via the micro-/nano-structured metal surface.Since air is trapped by the plastic melt,it is easily imagined that the air in the mold cavity prevents the melt plastic from contacting the metal surface and infiltrating the micro-/nano-structure,which could result in poorer joining performance.To avoid the prevention of the air for the better joining performance,the present study proposes a system actively venting the mold cavity during injection molding.To apply the active venting to IMDJ,venting and sealing systems were newly developed.In addition,a system measuring air pressure of the mold cavity was developed.The proposed system was evaluated by a measurement of joining strengths of IMDJ specimens that were produced under various conditions.From the results,it is concluded that the active venting does not necessarily have a positive effect in any cases:the effect depends on the type of surface micro-/nano-structure. 展开更多
关键词 Metal-plastic direct joining Micro-/nano-structured surface Injection molding Active venting mold cavity pressure measurement