共找到3篇文章
< 1 >
每页显示 20 50 100
Production of carbon anodes by high-temperature mould pressing 被引量:3
1
作者 王耀武 彭建平 +1 位作者 狄跃忠 冯乃祥 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第10期3119-3124,共6页
Laboratory-scale carbon anodes were produced by a new method of high temperature mould pressing, and their physico-chemical properties were studied. The influence of mould pressing conditions and coal pitch addition o... Laboratory-scale carbon anodes were produced by a new method of high temperature mould pressing, and their physico-chemical properties were studied. The influence of mould pressing conditions and coal pitch addition on the bulk density, crushing strength, and oxidation resistance was analyzed. The mierostructure of carbon anodes was investigated by scanning electron microscopy (SEM), and the mechanism of producing carbon anodes by high-temperature mould pressing was analyzed. The results show that when the anodes are produced by high-temperature mould pressing, coal pitch can expand into the coke particles and fill the pores inside the particles, which is beneficial for improving the quality of prebaked anodes. The bulk density of carbon anodes is 1.64-1.66 g/cm3, which is 0.08-0.12 g/cm3 higher than that of industrial anodes, and the oxidation resistance of carbon anodes is also significantly improved. 展开更多
关键词 carbon anodes high temperature mould pressing aluminum electrolysis high bulk density
下载PDF
Fabrication of pure copper rods containing continuous columnar crystals by continuous unidirectional solidification technology 被引量:9
2
作者 Hong zhang Jianxin Xie Zidong Wang Materials Science and Engineering School, University of Science and Technology Beijing, Beijing 100083, China 《Journal of University of Science and Technology Beijing》 CSCD 2004年第3期240-244,共5页
Pure copper rods containing continuous columnar crystals were fabricatedusing the downward CUS (Continuous Unidirectional Solidification) equipment. When the technologicalparameters were set as the ranges of mould tem... Pure copper rods containing continuous columnar crystals were fabricatedusing the downward CUS (Continuous Unidirectional Solidification) equipment. When the technologicalparameters were set as the ranges of mould temperature 1100-1300℃, cooling distance (the distancefrom the exit of the cast mould to the start point of cooling) 10-20 mm, casting speed 0.2-2.5 mm/s,cooling water (20-25℃) volume 1000-1320 L/h, and when these parameters matched reasonably, the CUSprocess was performed stably, and pure copper rods containing continuous columnar crystals withbright and smooth surface were produced. The dendritic arm spacing of the crystals in copper rodsdecreased with increasing the casting speed. The results of the texture by X-ray diffractionanalysis showed that the rods has strong <100> fiber texture. 展开更多
关键词 COPPER continuous unidirectional solidification mould temperature castingspeed microstructure TEXTURE
下载PDF
Thermo-elasto-visco-plastic finite element analysis on formation and propagation of off-corner subsurface cracks in bloom continuous casting 被引量:2
3
作者 Yu-jun Li Huan Li +2 位作者 Peng Lan Hai-yan Tang Jia-quan Zhang 《Journal of Iron and Steel Research International》 SCIE EI CAS CSCD 2017年第11期1159-1168,共10页
The formation and propagation of the popular off-corner subsurface cracks in bloom continuous casting were investigated through thermo-mechanical analysis using three coupled thermo-mechanical models. A two-dimensiona... The formation and propagation of the popular off-corner subsurface cracks in bloom continuous casting were investigated through thermo-mechanical analysis using three coupled thermo-mechanical models. A two-dimensional thermo-elasto-visco-plastic finite element model was developed to predict the mould gap evolution, temperature profiles and deformation behavior of the solidified shell in the mould region. Then, a three-dimensional model was adopted to calculate the shell growth, tempera- ture history and the development of stresses and strains of the shell in the following secondary cooling zones. Finally, another three-dimensional model was used to analyze the stress distributions in the straightening region, The results showed that the off-corner cracks in the shell originated from the mould owing to the tensile strain developed in the crack sensitive regions of the solidification front, and they could be driven deeper by the possible severe surface temperature rebound and the extensive tensile stress in the secondary cooling zone, especially upon the straightening operation of the bloom casting. It is revealed that more homogenous shell temperature and thickness can be obtained through optimization of mould corner radius, casting speed and secondary cooling scheme, which help to decrease stress and strain concentration and therefore prevent the initiation of the cracks. 展开更多
关键词 Thermo elasto-visco-plastic finite element model Off-corner subsurface crack Mould corner radius temperature rebound Straightening operation Bloom continuous casting
原文传递