In order to produce the hear-resistant inner layer of hot-forging die, the plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% tungst...In order to produce the hear-resistant inner layer of hot-forging die, the plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% tungsten carbide (WC) ceramic powder used as coating material to obtain different Nickel-based WC alloys coating. Micro-structure and micro-hardness analysis of the coating layer are conducted, as well as thermophysical properties for the coating layer were measured. The experimental results show that the coating prepared with 70%Ni60, 30%WC powder has the best properties with plasma spray welding, in which the micro-hardness can achieve 900HV, meanwhile it can improve the thermal property of hot-forging die dramatically.展开更多
The finite element analysis (FEA) software Ansys was employed to study the stress state of the dies of both plane and non-plane parting face structures with uniform interference and the die of plane parting face str...The finite element analysis (FEA) software Ansys was employed to study the stress state of the dies of both plane and non-plane parting face structures with uniform interference and the die of plane parting face structure with non-uniform interference. Considering the symmetry of the die, a half gear tooth model of the two-ring assembled die with 2.5 GPa inner pressure was constructed. Four paths were defined to investigate the stress state at the bottom comer of the die where stress concentration was serious. FEA results show that the change of parting face from non-plane to plane can greatly reduce the stress at the teeth tips of the die so that the tip fracture is avoided. The interference structure of the die is the most important influencing factor for the stress concentration at the bottom comer. When non-uniform interference is adopted the first principal stress at the comer on the defined paths of the die is much lower than that with uniform interference. The bottom hole radius is another important influencing factor for the comer stress concentration. The first principal stress at the comer of the plane parting face die with non-uniform interference is reduced from 2.3 to 1.9 GPa when the hole radius increases from 12.5 to 16.0 mm. The optimization of the die structure increases the life of the die from 100 to 6 000 hits.展开更多
A new design technique for the long life hot forging die has been proposed. By finite element analysis, the reason .for the failure of hot forging die was analyzed and it was concluded that thermal stress is the main ...A new design technique for the long life hot forging die has been proposed. By finite element analysis, the reason .for the failure of hot forging die was analyzed and it was concluded that thermal stress is the main reason for the failure of hot forging die. Based on this conclusion, the whole hot forging die was divided into the substrate part and the heat-resistant part according to the thermal stress distribution. Moreover, the heat-resistant part was further subdivided into more zones and the material of each zone was reasonably selected to ensure that the hot forging die can work in an elastic state. When compared with the existing techniques, this design can greatly increase the service life because the use of multi-materials can alleviate the thermal stress in hot forging die.展开更多
The tempering stability of three Fe–Cr–Mo–W–V hot forging die steels(DM, H21, and H13) was investigated through hardness measurements and transmission electron microscopy(TEM) observations. Both dilatometer tests ...The tempering stability of three Fe–Cr–Mo–W–V hot forging die steels(DM, H21, and H13) was investigated through hardness measurements and transmission electron microscopy(TEM) observations. Both dilatometer tests and TEM observations revealed that DM steel has a higher tempering stability than H21 and H13 steels because of its substantial amount of M_2C(M represents metallic element) carbide precipitations. The activation energies of the M_2C carbide precipitation processes in DM, H21, and H13 steels are 236.4, 212.0, and 228.9 kJ/mol, respectively. Furthermore, the results indicated that vanadium atoms both increase the activation energy and affect the evolution of M_2C carbides, resulting in gradual dissolution rather than over-aging during tempering.展开更多
Al/Mg/Al sheet with good bonding quality and mechanical properties was fabricated based on the proposed porthole die co-extrusion and forging(PCE-F)process.There were no voids,cracks or other defects on the Al/Mg inte...Al/Mg/Al sheet with good bonding quality and mechanical properties was fabricated based on the proposed porthole die co-extrusion and forging(PCE-F)process.There were no voids,cracks or other defects on the Al/Mg interface.A continuous diffusion zone with two-sub-layer structure was formed across the Al/Mg interface,and its width increased with higher temperature or reduction ratio.The sub-layers formed at low and high temperature were identified to be solid solutions and intermetallic compounds(IMCs)including y-MgpAl^and^-Al3Mg.In Al layer,the welding zone mainly consisted of fine equiaxed grains with several coarse elongated grains,while the majority of matrix zone is coarse elongated grains.The rolling textures were dominated in both welding and matrix zones.In Mg layer,the welding zone exhibited complete DRXed grain structure,while several unDRXed coarse grains were observed in the matrix zone.With the increasing temperature,the grain size of Al and Mg layer firstly decreased and then increased.High reduction ratio strongly refined the grain structure of Al layer,while slightly affected the Mg layer.The Al/Mg/AI sheet experienced stress-drops twice during the tensile test.The first stress-drop was determined by the IMCs and microstructure of Mg layer,while the second stress-drop was closely related to the microstructure of Al layer.Al/Mg/Al sheet forged at the lowest temperature without the formation IMCs exhibited the highest stress for the first stress-drop,and that forged under the highest reduction ratio with the smallest grain size in Al layer had the highest stress for the second stress-drop.展开更多
In order to produce the hear-resistant inner layer of hot-forging die, plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% SiC cerami...In order to produce the hear-resistant inner layer of hot-forging die, plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% SiC ceramic powder used as coating material to obtain different Ni-based SiC alloys coating. Micro-structure and micro-hardness analysis of the coating layer were followed, as well as thermophysical properties for the coating layer were measured. The experimental results show that the coating prepared with 70% Ni60, 30% SiC powder has best properties with plasma spray welding, in which the micro-hardness can achieve 1100 HV, meanwhile can improve the thermal property of hot-forging die dramatically.展开更多
A process parameter optimization method for mold wear during die forging process is proposed and a mold life prediction method based on polynomial fitting is presented,by combining the variance analysis method in the ...A process parameter optimization method for mold wear during die forging process is proposed and a mold life prediction method based on polynomial fitting is presented,by combining the variance analysis method in the orthogonal test with the finite element simulation test in the forging process.The process parameters with the greatest influence on the mold wear during the die forging process and the optimal solution of the process parameters to minimize the wear depth of the mold are derived.The hot die forging process is taken as an example,and a mold wear correction model for hot forging processes is derived based on the Archard wear model.Finite element simulation analysis of die wear process in hot die forging based on deform software is performed to study the relationship between the wear depth of the mold working surface and the die forging process parameters during hot forging process.The optimized process parameters suitable for hot forging are derived by orthogonal experimental design and analysis of variance.The average wear amount of the mold during the die forging process is derived by calculating the wear depth of a plurality of key nodes on the mold surface.Mold life for the entire production process is predicted based on average mold wear depth and polynomial fitting.展开更多
The closed die forging(or fully-enclosed die forging) method was employed to form a rotor instead of the conventional machining method. A combined female die was designed so that the rotor could be released easily fro...The closed die forging(or fully-enclosed die forging) method was employed to form a rotor instead of the conventional machining method. A combined female die was designed so that the rotor could be released easily from the female die after forging. In order to improve the metal flow ability, the isothermal forming technique was introduced to the closed die forging process. On the basis of the rigid-viscoplastic FEM principle, the DEFORM 3D software package was employed to simulate the forming process. The simulation results illustrate that the deformation of different part of the billet is not the same. The material near the entrance of the die cavity is deformed greatly whose strain rate and strain are both large, while the deformation of the material at the billet center is much smaller.展开更多
To meet the performance requirements of hot forging die heat resistant layer, the Ni60-SiC coating, Ni60-Cr3C2 coating, and Ni60-WC coating were prepared using W6Mo5Cr4V2 as substrate material with 30%SiC, 10%Cr3C2, 3...To meet the performance requirements of hot forging die heat resistant layer, the Ni60-SiC coating, Ni60-Cr3C2 coating, and Ni60-WC coating were prepared using W6Mo5Cr4V2 as substrate material with 30%SiC, 10%Cr3C2, 30%WC powder by means of plasma spraying and plasma spray re-melting and plasma spray welding, respectively. Microstructure of each carbide coating was analyzed, micro-hardness was tested, and mainly thermal parameters of coating were detected. The experimental results show that using plasma spray welding, the performance of 70%Ni60/30%SiC powder is the best, and its micro-hardness can achieved 1100HV, showing good thermal-physical property.展开更多
The effect of main alloying elements on thermal wear of cast hot-forging die steels was studied. The wear mechanism was discussed. The results show that alloying elements have significant influences on the thermal wea...The effect of main alloying elements on thermal wear of cast hot-forging die steels was studied. The wear mechanism was discussed. The results show that alloying elements have significant influences on the thermal wear of cast hot-forging die steels. The wear rates decrease with an increase in chromium content from 3% to 4% and molybdenum content from 2% to 3%, respectively. With further increase of chromium and molybdenum contents, chromium slightly reduces the wear resistance and molybdenum severely deteriorates the wear resistance with high wear rate. Lower vanadium/carbon ratio (1.5-2.5) leads to a lower wear resistance with higher wear rate. With an increase in vanadium/carbon ratio, the wear resistance of the cast steel substantially increases. When vanadium/carbon ratio is 3, the wear rate reaches the lowest value. The predominant mechanism of thermal wear of cast hot-forging die steels are oxidation wear and fatigue delamination. The Fe2O3 and Fe3O4 or lumps of brittle wear debris are formed on the wear surface.展开更多
Thermal wear of cast hot-forging die steel modified by rare earths(RE) was studied and compared with commercially used die steels. The function of RE and the mechanism of thermal wear of cast steel modified by RE we...Thermal wear of cast hot-forging die steel modified by rare earths(RE) was studied and compared with commercially used die steels. The function of RE and the mechanism of thermal wear of cast steel modified by RE were discussed. The results showed that with increasing content of RE, the wear rate of cast steel reduced at first and then increased. By adding 0.05% (mass fraction) RE, the cast hot-forging die steel with optimum thermal wear resistance was obtained, which was better than that of H13 and 3Cr2WSV. The large amount of coarse inclusions, (RE)2O2S, resulted from excessive RE, which obviously deteriorated thermal wear resistance. The mechanism of thermal wear of the modified cast die steel is oxidation wear and oxide fatigue delamination. The wear debris are lumps of Fe2O3 and Fe3O4.展开更多
The closed-died cold forging technology of the bevel gears used in Jada car was investigated. With the analysis of the strain field and velocity field of the plastic deformation and the endured forces of the dies, the...The closed-died cold forging technology of the bevel gears used in Jada car was investigated. With the analysis of the strain field and velocity field of the plastic deformation and the endured forces of the dies, the filling rules for the metal were analyzed by the elastic-plastic finite element method (FEM). The results show that there is a great difference among closed-die cold forging, extrusion and forging, as far as the metal flowing is concerned. The outer addendum cannot be filled completely in the closed-die cold forging of the bevel gears, and the round angle will be formed. But it does not influence the application of the bevel gears. At the beginning, the rigid area is formed in the cavity of the lower die. And then it will move upwards to supply the metal for the gear filling. For the closed-die cold forging of the bevel gears, the force acting on the upper die and the lower die is significantly different.展开更多
The fatigue behavior of cemented carbide die under service load in the multistage cold forging of steel was investigated. It was found that the fatigue cracks do not initiate at the stress concentration position and t...The fatigue behavior of cemented carbide die under service load in the multistage cold forging of steel was investigated. It was found that the fatigue cracks do not initiate at the stress concentration position and the crack initiation position can be classified to three types. The crack initiation position can be predicted by FEM only when the plastic deformation of the die is considered.展开更多
Forging die design is heavily dependent on engineers’ experiences.But traditional AI technologies can barely pro- vide a standard knowledge representation style for knowledge transferring.This paper introduces ontolo...Forging die design is heavily dependent on engineers’ experiences.But traditional AI technologies can barely pro- vide a standard knowledge representation style for knowledge transferring.This paper introduces ontology into forging die design. 3-layer forging die design ontology is built,which includes Meta-ontology,Domain-ontology and Bottom ontology.Further,by conceptualization,the concepts and their relations are formally addressed by primitives such as Term,Relation and Function etc, which are explicitly expressed by concept tree.Bottom ontology uses Knowledge Item and Prototype to represent and capture general knowledge for knowledge reuse and share.Forging die design ontology building approach is discussed for standard knowledge repre- sentation,knowledge mine and knowledge driven CAD design etc.And OWL language is employed for integration among different domain ontologies integration.Finally a locomotive forging die KBE system is presented to demonstrate this approach.展开更多
A new forging technique short-hollow--rapid die forging, used in Ti-Al alloys was studied.Compared with conventional method, the new method can improve the crystalline structure properties of theforged piece, reduce t...A new forging technique short-hollow--rapid die forging, used in Ti-Al alloys was studied.Compared with conventional method, the new method can improve the crystalline structure properties of theforged piece, reduce the average forging pressure by 20% to 30%, lessen the thickness deviation by 5 mm,and prolong the service life of the dies by 2 to 4 times.展开更多
Traditionally a rotary forging process is a kind of metal forming method where a conic upper die, whose axis is deviated an angle from the axis of machine, forges a billet continuously and partially to finish the whol...Traditionally a rotary forging process is a kind of metal forming method where a conic upper die, whose axis is deviated an angle from the axis of machine, forges a billet continuously and partially to finish the whole deformation. For the rotary forging process simulation, more researches were focused on simulating the simple stage forming process with axisymmetric part geometry. Whereas in this paper, the upper die is not cone-shaped, and the billet is non-axisymmetric. So the movement of the punch is much more complicated than ever. The 3D FEM simulation models for the preforming & final forming processes are set up aider carefully studying the complicated movement pattern. Deform-3D is used to simulate the material flow, and the boundary nodal resisting forces calculated by the final stage process simulation is used to analyze the final forming die strength. The CAE analysis of the die shows that the design of the final forming die is not reasonable with lower pre-stress which is easy to crack at the critical corners. An optimum die design is also provided with higher pre-stress, and verified by CAE analysis.展开更多
The alteration of the strength, hardness and impact ductility of 5CrNiMo steel using three different additions of RE La element is studied in this paper. The mechanical properties of 5CrNiMo steel with RE La additions...The alteration of the strength, hardness and impact ductility of 5CrNiMo steel using three different additions of RE La element is studied in this paper. The mechanical properties of 5CrNiMo steel with RE La additions are be compared with that of the 5CrNiMo steel on the same heat-treatment condition without RE La element addition. The results show that the strength, hardness and impact ductility of 5CrNiMo steel will be improved obviously when the content of RE La element is proper, and as the content of RE La element is 0.033%(mass fraction), the 5CrNiMo steel has the best mechanical properties.展开更多
Based on the car front-wheel-hub forging forming process of numerical simulation, the temperature gradient expression of forging model cavity near the surface layer was got ten, which illustrates that the forging temp...Based on the car front-wheel-hub forging forming process of numerical simulation, the temperature gradient expression of forging model cavity near the surface layer was got ten, which illustrates that the forging temperature gradient is related to forging die materials thermal conductivity, specific heat and impact speed, and the correlation coefficient is 0.97. Under the different thermal conductivity, heat capacity and forging speed, the temperature gradient was compared with each other. The paper obtained the relevant laws, which illustrates the temperature gradient relates to these three parameters in a sequence of thermal conductivity 〉 impact speed〉 specific heat capacity. To reduce thermal stress in the near-surface layer of hot forging cavity, the material with greater thermal conductivity coefficient and specific heat capacity should be used.展开更多
In the process of riveting an MB15 forging die,cracks were discovered emerging along the longitudinal direction and near the riveting hole.Through fracture analysis,microscopic observation,energy spectrum analysis,met...In the process of riveting an MB15 forging die,cracks were discovered emerging along the longitudinal direction and near the riveting hole.Through fracture analysis,microscopic observation,energy spectrum analysis,metallographic examination,and hardness test,the properties and causes of the cracks are discussed.The results indicate that the cracking type is intergranular brittle cracking,occurring during the forging stage.Furthermore,the recrystallization at the crack site is found to be incomplete,which is attributed to the low deformation temperature.展开更多
基金Funded by the National Natural Science Foundation of China(No.50675165)the National Key Technology R&D Program(No.2006BAF02A29)
文摘In order to produce the hear-resistant inner layer of hot-forging die, the plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% tungsten carbide (WC) ceramic powder used as coating material to obtain different Nickel-based WC alloys coating. Micro-structure and micro-hardness analysis of the coating layer are conducted, as well as thermophysical properties for the coating layer were measured. The experimental results show that the coating prepared with 70%Ni60, 30%WC powder has the best properties with plasma spray welding, in which the micro-hardness can achieve 900HV, meanwhile it can improve the thermal property of hot-forging die dramatically.
基金Project(2006BAF04B06) supported by the National Key Technology R & D Program of ChinaProject(2005AA101B19) supported by the Key Technology R & D Program of Hubei Province, China
文摘The finite element analysis (FEA) software Ansys was employed to study the stress state of the dies of both plane and non-plane parting face structures with uniform interference and the die of plane parting face structure with non-uniform interference. Considering the symmetry of the die, a half gear tooth model of the two-ring assembled die with 2.5 GPa inner pressure was constructed. Four paths were defined to investigate the stress state at the bottom comer of the die where stress concentration was serious. FEA results show that the change of parting face from non-plane to plane can greatly reduce the stress at the teeth tips of the die so that the tip fracture is avoided. The interference structure of the die is the most important influencing factor for the stress concentration at the bottom comer. When non-uniform interference is adopted the first principal stress at the comer on the defined paths of the die is much lower than that with uniform interference. The bottom hole radius is another important influencing factor for the comer stress concentration. The first principal stress at the comer of the plane parting face die with non-uniform interference is reduced from 2.3 to 1.9 GPa when the hole radius increases from 12.5 to 16.0 mm. The optimization of the die structure increases the life of the die from 100 to 6 000 hits.
基金the National Natural Science Foundation of China (No. 50675165).
文摘A new design technique for the long life hot forging die has been proposed. By finite element analysis, the reason .for the failure of hot forging die was analyzed and it was concluded that thermal stress is the main reason for the failure of hot forging die. Based on this conclusion, the whole hot forging die was divided into the substrate part and the heat-resistant part according to the thermal stress distribution. Moreover, the heat-resistant part was further subdivided into more zones and the material of each zone was reasonably selected to ensure that the hot forging die can work in an elastic state. When compared with the existing techniques, this design can greatly increase the service life because the use of multi-materials can alleviate the thermal stress in hot forging die.
基金financially supported by the National Key Technologies R & D Program of China (Nos.2016YFB0300400 and 2016YFB0300402)
文摘The tempering stability of three Fe–Cr–Mo–W–V hot forging die steels(DM, H21, and H13) was investigated through hardness measurements and transmission electron microscopy(TEM) observations. Both dilatometer tests and TEM observations revealed that DM steel has a higher tempering stability than H21 and H13 steels because of its substantial amount of M_2C(M represents metallic element) carbide precipitations. The activation energies of the M_2C carbide precipitation processes in DM, H21, and H13 steels are 236.4, 212.0, and 228.9 kJ/mol, respectively. Furthermore, the results indicated that vanadium atoms both increase the activation energy and affect the evolution of M_2C carbides, resulting in gradual dissolution rather than over-aging during tempering.
基金the National Natural Science Foundation of China(51875317)Key Research and Development Program of Shandong Province(2019GGX104087)Natural Science Foundation of Shandong Province(ZR2019QEE030).
文摘Al/Mg/Al sheet with good bonding quality and mechanical properties was fabricated based on the proposed porthole die co-extrusion and forging(PCE-F)process.There were no voids,cracks or other defects on the Al/Mg interface.A continuous diffusion zone with two-sub-layer structure was formed across the Al/Mg interface,and its width increased with higher temperature or reduction ratio.The sub-layers formed at low and high temperature were identified to be solid solutions and intermetallic compounds(IMCs)including y-MgpAl^and^-Al3Mg.In Al layer,the welding zone mainly consisted of fine equiaxed grains with several coarse elongated grains,while the majority of matrix zone is coarse elongated grains.The rolling textures were dominated in both welding and matrix zones.In Mg layer,the welding zone exhibited complete DRXed grain structure,while several unDRXed coarse grains were observed in the matrix zone.With the increasing temperature,the grain size of Al and Mg layer firstly decreased and then increased.High reduction ratio strongly refined the grain structure of Al layer,while slightly affected the Mg layer.The Al/Mg/AI sheet experienced stress-drops twice during the tensile test.The first stress-drop was determined by the IMCs and microstructure of Mg layer,while the second stress-drop was closely related to the microstructure of Al layer.Al/Mg/Al sheet forged at the lowest temperature without the formation IMCs exhibited the highest stress for the first stress-drop,and that forged under the highest reduction ratio with the smallest grain size in Al layer had the highest stress for the second stress-drop.
基金Funded by the National Natural Science Foundation of China (No. 50675165)
文摘In order to produce the hear-resistant inner layer of hot-forging die, plasma spraying and plasma re-melting and plasma spray welding were adopted. Substrate material was W6Mo5Cr4V2, including 10%, 20%, 30% SiC ceramic powder used as coating material to obtain different Ni-based SiC alloys coating. Micro-structure and micro-hardness analysis of the coating layer were followed, as well as thermophysical properties for the coating layer were measured. The experimental results show that the coating prepared with 70% Ni60, 30% SiC powder has best properties with plasma spray welding, in which the micro-hardness can achieve 1100 HV, meanwhile can improve the thermal property of hot-forging die dramatically.
基金This work was supported in part by the National Natural Science Foundation of China(No.51575008).
文摘A process parameter optimization method for mold wear during die forging process is proposed and a mold life prediction method based on polynomial fitting is presented,by combining the variance analysis method in the orthogonal test with the finite element simulation test in the forging process.The process parameters with the greatest influence on the mold wear during the die forging process and the optimal solution of the process parameters to minimize the wear depth of the mold are derived.The hot die forging process is taken as an example,and a mold wear correction model for hot forging processes is derived based on the Archard wear model.Finite element simulation analysis of die wear process in hot die forging based on deform software is performed to study the relationship between the wear depth of the mold working surface and the die forging process parameters during hot forging process.The optimized process parameters suitable for hot forging are derived by orthogonal experimental design and analysis of variance.The average wear amount of the mold during the die forging process is derived by calculating the wear depth of a plurality of key nodes on the mold surface.Mold life for the entire production process is predicted based on average mold wear depth and polynomial fitting.
文摘The closed die forging(or fully-enclosed die forging) method was employed to form a rotor instead of the conventional machining method. A combined female die was designed so that the rotor could be released easily from the female die after forging. In order to improve the metal flow ability, the isothermal forming technique was introduced to the closed die forging process. On the basis of the rigid-viscoplastic FEM principle, the DEFORM 3D software package was employed to simulate the forming process. The simulation results illustrate that the deformation of different part of the billet is not the same. The material near the entrance of the die cavity is deformed greatly whose strain rate and strain are both large, while the deformation of the material at the billet center is much smaller.
文摘To meet the performance requirements of hot forging die heat resistant layer, the Ni60-SiC coating, Ni60-Cr3C2 coating, and Ni60-WC coating were prepared using W6Mo5Cr4V2 as substrate material with 30%SiC, 10%Cr3C2, 30%WC powder by means of plasma spraying and plasma spray re-melting and plasma spray welding, respectively. Microstructure of each carbide coating was analyzed, micro-hardness was tested, and mainly thermal parameters of coating were detected. The experimental results show that using plasma spray welding, the performance of 70%Ni60/30%SiC powder is the best, and its micro-hardness can achieved 1100HV, showing good thermal-physical property.
基金Item Sponsored by Early-Term Key Technology of Industrialization and Whole Set Equipment From Plan Committee of China(1999317) ,863 Project of China (2002AA331180) ,and Project of Key Lab of Universities in Jiangsu Province of China(Kjsmcx04004)
文摘The effect of main alloying elements on thermal wear of cast hot-forging die steels was studied. The wear mechanism was discussed. The results show that alloying elements have significant influences on the thermal wear of cast hot-forging die steels. The wear rates decrease with an increase in chromium content from 3% to 4% and molybdenum content from 2% to 3%, respectively. With further increase of chromium and molybdenum contents, chromium slightly reduces the wear resistance and molybdenum severely deteriorates the wear resistance with high wear rate. Lower vanadium/carbon ratio (1.5-2.5) leads to a lower wear resistance with higher wear rate. With an increase in vanadium/carbon ratio, the wear resistance of the cast steel substantially increases. When vanadium/carbon ratio is 3, the wear rate reaches the lowest value. The predominant mechanism of thermal wear of cast hot-forging die steels are oxidation wear and fatigue delamination. The Fe2O3 and Fe3O4 or lumps of brittle wear debris are formed on the wear surface.
基金Project supported by the Itemof Early-TermKey Technology of Industrialization ,Plan Committee of China (1999317) 863project of China (2002AA331180)
文摘Thermal wear of cast hot-forging die steel modified by rare earths(RE) was studied and compared with commercially used die steels. The function of RE and the mechanism of thermal wear of cast steel modified by RE were discussed. The results showed that with increasing content of RE, the wear rate of cast steel reduced at first and then increased. By adding 0.05% (mass fraction) RE, the cast hot-forging die steel with optimum thermal wear resistance was obtained, which was better than that of H13 and 3Cr2WSV. The large amount of coarse inclusions, (RE)2O2S, resulted from excessive RE, which obviously deteriorated thermal wear resistance. The mechanism of thermal wear of the modified cast die steel is oxidation wear and oxide fatigue delamination. The wear debris are lumps of Fe2O3 and Fe3O4.
文摘The closed-died cold forging technology of the bevel gears used in Jada car was investigated. With the analysis of the strain field and velocity field of the plastic deformation and the endured forces of the dies, the filling rules for the metal were analyzed by the elastic-plastic finite element method (FEM). The results show that there is a great difference among closed-die cold forging, extrusion and forging, as far as the metal flowing is concerned. The outer addendum cannot be filled completely in the closed-die cold forging of the bevel gears, and the round angle will be formed. But it does not influence the application of the bevel gears. At the beginning, the rigid area is formed in the cavity of the lower die. And then it will move upwards to supply the metal for the gear filling. For the closed-die cold forging of the bevel gears, the force acting on the upper die and the lower die is significantly different.
文摘The fatigue behavior of cemented carbide die under service load in the multistage cold forging of steel was investigated. It was found that the fatigue cracks do not initiate at the stress concentration position and the crack initiation position can be classified to three types. The crack initiation position can be predicted by FEM only when the plastic deformation of the die is considered.
文摘Forging die design is heavily dependent on engineers’ experiences.But traditional AI technologies can barely pro- vide a standard knowledge representation style for knowledge transferring.This paper introduces ontology into forging die design. 3-layer forging die design ontology is built,which includes Meta-ontology,Domain-ontology and Bottom ontology.Further,by conceptualization,the concepts and their relations are formally addressed by primitives such as Term,Relation and Function etc, which are explicitly expressed by concept tree.Bottom ontology uses Knowledge Item and Prototype to represent and capture general knowledge for knowledge reuse and share.Forging die design ontology building approach is discussed for standard knowledge repre- sentation,knowledge mine and knowledge driven CAD design etc.And OWL language is employed for integration among different domain ontologies integration.Finally a locomotive forging die KBE system is presented to demonstrate this approach.
文摘A new forging technique short-hollow--rapid die forging, used in Ti-Al alloys was studied.Compared with conventional method, the new method can improve the crystalline structure properties of theforged piece, reduce the average forging pressure by 20% to 30%, lessen the thickness deviation by 5 mm,and prolong the service life of the dies by 2 to 4 times.
文摘Traditionally a rotary forging process is a kind of metal forming method where a conic upper die, whose axis is deviated an angle from the axis of machine, forges a billet continuously and partially to finish the whole deformation. For the rotary forging process simulation, more researches were focused on simulating the simple stage forming process with axisymmetric part geometry. Whereas in this paper, the upper die is not cone-shaped, and the billet is non-axisymmetric. So the movement of the punch is much more complicated than ever. The 3D FEM simulation models for the preforming & final forming processes are set up aider carefully studying the complicated movement pattern. Deform-3D is used to simulate the material flow, and the boundary nodal resisting forces calculated by the final stage process simulation is used to analyze the final forming die strength. The CAE analysis of the die shows that the design of the final forming die is not reasonable with lower pre-stress which is easy to crack at the critical corners. An optimum die design is also provided with higher pre-stress, and verified by CAE analysis.
文摘The alteration of the strength, hardness and impact ductility of 5CrNiMo steel using three different additions of RE La element is studied in this paper. The mechanical properties of 5CrNiMo steel with RE La additions are be compared with that of the 5CrNiMo steel on the same heat-treatment condition without RE La element addition. The results show that the strength, hardness and impact ductility of 5CrNiMo steel will be improved obviously when the content of RE La element is proper, and as the content of RE La element is 0.033%(mass fraction), the 5CrNiMo steel has the best mechanical properties.
基金Funded by the Fundamental Research Funds for the Central University (No.2010-II-025)the National Natural Science Foundation of China(No.50675165)
文摘Based on the car front-wheel-hub forging forming process of numerical simulation, the temperature gradient expression of forging model cavity near the surface layer was got ten, which illustrates that the forging temperature gradient is related to forging die materials thermal conductivity, specific heat and impact speed, and the correlation coefficient is 0.97. Under the different thermal conductivity, heat capacity and forging speed, the temperature gradient was compared with each other. The paper obtained the relevant laws, which illustrates the temperature gradient relates to these three parameters in a sequence of thermal conductivity 〉 impact speed〉 specific heat capacity. To reduce thermal stress in the near-surface layer of hot forging cavity, the material with greater thermal conductivity coefficient and specific heat capacity should be used.
基金Key R&D Plan Projects in Hubei Province(Grant No.2021BID001)the Research on Multiple Regression and Fitting Technology of Simulation Data for Dynamic Umbrella Opening of Lifesaving Umbrella(Grant No.HX2021157)。
文摘In the process of riveting an MB15 forging die,cracks were discovered emerging along the longitudinal direction and near the riveting hole.Through fracture analysis,microscopic observation,energy spectrum analysis,metallographic examination,and hardness test,the properties and causes of the cracks are discussed.The results indicate that the cracking type is intergranular brittle cracking,occurring during the forging stage.Furthermore,the recrystallization at the crack site is found to be incomplete,which is attributed to the low deformation temperature.