Effect of rare-earth oxides on properties of silicon nitride obtained by normal sintering and sinter-HIP 被引量:4
1
作者 Cecilia C.Guedes-Silva Flávio Machado de Souza Carvalho José Carlos Bressiani 《Journal of Rare Earths》 SCIE EI CAS CSCD 2012年第11期1177-1183,共7页
This paper presented the microstructure, mechanical properties and oxidation behavior of silicon nitride obtained by both conventional sintering and sintering followed by hot isostatic pressing (HIP). Silicon nitrid... This paper presented the microstructure, mechanical properties and oxidation behavior of silicon nitride obtained by both conventional sintering and sintering followed by hot isostatic pressing (HIP). Silicon nitride with additives such as 5 wt.% Al2O3 and 5 wt.% Ln203 (Ln= La, La concentrate, Gd or La+Gd) were studied. The results revealed that Gd203 additions increased the formation of elongated grains of β-Si3N4, the fracture toughness and oxidation resistance. La2O3 additions led to higher densification and hardness values, while addition of La2O3 concentrate promoted the formation of materials with intermediate properties, compared to the other studied compositions. Hot isostatic pressing increased the hardness but decreased the fracture toughness of the material, mainly because it allowed residual pores to close and also reduced the average aspect ratio of β-Si3N4 grains. 展开更多
关键词 rare earths silicon nitride properties normal sintering sinter-HIP
原文传递
无铅压电陶瓷铌酸钾钠的常压烧结及其电学性能 被引量:17
2
作者 张利民 张波萍 +2 位作者 李敬锋 王轲 张海龙 《硅酸盐学报》 EI CAS CSCD 北大核心 2007年第1期1-5,共5页
用常压烧结方法制备了Na0.5K0.5NbO3(NKN)无铅压电陶瓷。研究了烧结温度与NKN陶瓷的密度、结构以及电学性能的关系。结果表明:NKN陶瓷与KNbO3相似为正交结构,烧结温度超过1080℃时,出现无压电性第二相。在很小的温度范围内(1020~1100℃... 用常压烧结方法制备了Na0.5K0.5NbO3(NKN)无铅压电陶瓷。研究了烧结温度与NKN陶瓷的密度、结构以及电学性能的关系。结果表明:NKN陶瓷与KNbO3相似为正交结构,烧结温度超过1080℃时,出现无压电性第二相。在很小的温度范围内(1020~1100℃)烧结体密度有显著不同,当烧结温度为1080℃时,NKN陶瓷烧结密度达到最大值(4.22g/cm3,相对密度为92%)。经1060℃烧结的NKN陶瓷其压电常数最高,达到122pC/N;Curie温度为409℃;矫顽场为9kV/cm;剩余极化强度为15μC/cm2。 展开更多
关键词 铌酸钾钠陶瓷 无铅压电陶瓷 常压烧结
下载PDF
常压烧结制备Al_2O_3/TiCN复合陶瓷材料 被引量:12
3
作者 李喜坤 修稚萌 +1 位作者 孙旭东 郑龙熙 《硅酸盐学报》 EI CAS CSCD 北大核心 2003年第11期1069-1074,共6页
采用常压烧结的方法制备Al_2O_3/TiCN复合陶瓷,研究了试样成分、烧结温度对试样相对密度、抗弯强度、断裂韧性、Vickers硬度等力学性能的影响。结果表明:采用Al_2O_3+TiCN作为埋粉、氩气保护、在烧结温度低于1650℃,保温时间为1h时,烧... 采用常压烧结的方法制备Al_2O_3/TiCN复合陶瓷,研究了试样成分、烧结温度对试样相对密度、抗弯强度、断裂韧性、Vickers硬度等力学性能的影响。结果表明:采用Al_2O_3+TiCN作为埋粉、氩气保护、在烧结温度低于1650℃,保温时间为1h时,烧结试样的相对密度最高为98.0%,其抗弯强度、断裂韧性、及硬度分别达到最大值,为851 MPa,5.94 MPa·m^(1/2),21.12 MPa。显微结构分析表明:TiCN颗粒弥散在Al_2O_3晶界处,晶粒细小,多在1 μm左右,分布均匀,TiCN与Al_2O_3颗粒相互交织在一起,抑制晶粒生长,从而起到了增韧补强作用,有利于材料力学性能的提高。从压痕裂纹尖端的扩展的扫描电镜照片可以看出:基体与增强相多个晶粒构成的裂纹桥联行为;而有的则在其初始或(和)末端与其他次主裂纹相互作用,形成裂纹偏转、分支与桥联的共存区,主要起作用的是TiCN颗粒弥散增韧机制,它将纯Al_2O_3陶瓷的断裂韧度从3.59 MPa·m^(1/2)提高到5.94 MPa·m^(1/2)。 展开更多
关键词 碳氮化钛 氧化铝 复合陶瓷材料 常压烧结 相对密度 力学性能
下载PDF
高纯超细氧化铝粉的常压烧结与高压烧结 被引量:7
4
作者 孙致平 滕元成 +2 位作者 齐晓敏 陈堃 鲁伟员 《化工学报》 EI CAS CSCD 北大核心 2007年第11期2932-2936,共5页
以高纯超细α-Al2O3粉为原料,采用常压、高压烧结制备了高纯Al2O3陶瓷。研究表明,在乙醇溶剂中高速球磨可显著降低Al2O3粉料的平均颗粒尺寸,提高粉料的比表面积与烧结活性;在4.5GPa、1230℃高压烧结30min,制备了相对密度达98.71%的无烧... 以高纯超细α-Al2O3粉为原料,采用常压、高压烧结制备了高纯Al2O3陶瓷。研究表明,在乙醇溶剂中高速球磨可显著降低Al2O3粉料的平均颗粒尺寸,提高粉料的比表面积与烧结活性;在4.5GPa、1230℃高压烧结30min,制备了相对密度达98.71%的无烧结助剂掺杂的Al2O3陶瓷;与常压烧结相比,高压烧结可显著降低烧结温度,提高传质速率,大幅度缩短烧结时间,达到快速、低温烧结的效果;由于相对较低的烧结温度,掺杂微量MgO的Al2O3陶瓷在高压烧结中未出现液相,MgO对烧结致密化及Al2O3晶粒生长抑制几乎无影响。 展开更多
关键词 氧化铝 常压烧结 高压烧结 氧化镁 液相
下载PDF
双相Sialon材料的研究 被引量:3
5
作者 傅博 颜丰 王永兰 《耐火材料》 CAS 北大核心 1997年第5期249-252,共4页
研究了工艺条件、化学组成、显微结构与材料性能的关系,制备了双相Sialon材料。该材料室温抗折强度、断裂韧性分别达到624MPa、4MPa·m1/2,硬度达到Hv2000左右。其最佳烧结温度为1550℃,1.5h。添加剂Y2O3、Al2O3和AlN的最佳含... 研究了工艺条件、化学组成、显微结构与材料性能的关系,制备了双相Sialon材料。该材料室温抗折强度、断裂韧性分别达到624MPa、4MPa·m1/2,硬度达到Hv2000左右。其最佳烧结温度为1550℃,1.5h。添加剂Y2O3、Al2O3和AlN的最佳含量分别为10%、5%、5%。 展开更多
关键词 常压烧结 相变 烧结 陶瓷材料 SIALON材料
下载PDF
制备工艺对(ZrO_2)_(0.90)(Y_2O_3)_(0.04)(CaO)_(0.06)电解质材料电性能的影响 被引量:1
6
作者 李英 谢裕生 +2 位作者 龚江宏 唐子龙 张中太 《电源技术》 CAS CSCD 北大核心 2001年第5期330-332,336,共4页
目前ZrO2 基三元系材料的研究是固体电解质材料领域的一个热点。在关于ZrO2 Y2 O3 CaO系统电解质材料电性能研究的前期工作的基础上 ,探讨了不同的制备工艺对 (ZrO2 ) 0 .90 (Y2 O3) 0 .0 4 (CaO) 0 .0 6材料的电导率的影响问题 ,发... 目前ZrO2 基三元系材料的研究是固体电解质材料领域的一个热点。在关于ZrO2 Y2 O3 CaO系统电解质材料电性能研究的前期工作的基础上 ,探讨了不同的制备工艺对 (ZrO2 ) 0 .90 (Y2 O3) 0 .0 4 (CaO) 0 .0 6材料的电导率的影响问题 ,发现 :对于常规烧结的试样 ,其电导率随相对密度的提高而增大 ;与常规烧结相比 ,微波烧结能使材料具有更均匀的微观结构 ,更小的晶粒平均尺寸。较小的晶粒尺寸导致的较为显著的晶界效应是微波烧结试样的电导率有所降低的主要原因。由于微波烧结可以改善材料的力学性能 ,因此认为微波烧结是制备ZrO2 Y2 O3 展开更多
关键词 燃料电池 电解质材料 电性能 制备工艺 (ZrO2)0.90-(Y2O3)0.04-(CaO)0.06
下载PDF
影响碳化硼陶瓷致密化的因素 被引量:4
7
作者 张辉 穆柏春 唐立丹 《辽宁工学院学报》 2005年第6期378-381,共4页
从纯碳化硼的无压烧结、添加烧结助剂、烧结时加压等方面介绍了碳化硼陶瓷活化烧结致密化的方法,综述了国内外在不同的烧结工艺下制备的碳化硼陶瓷材料的性能,进而分析了各种方法提高碳化硼陶瓷致密度的机制,比较了各种烧结方法的优缺... 从纯碳化硼的无压烧结、添加烧结助剂、烧结时加压等方面介绍了碳化硼陶瓷活化烧结致密化的方法,综述了国内外在不同的烧结工艺下制备的碳化硼陶瓷材料的性能,进而分析了各种方法提高碳化硼陶瓷致密度的机制,比较了各种烧结方法的优缺点。结果表明:通过综合各种措施可以提高碳化硼陶瓷的致密度。 展开更多
关键词 碳化硼 致密化 热压烧结 常压烧结
下载PDF
Microstructure and electrical properties of Ti-modified (Na_(0.5)K_(0.5))(Ti_xNb_(1-x))O_3 lead-free piezoelectric ceramics 被引量:1
8
作者 Zhang, Qian Zhang, Boping +2 位作者 Zhao, Pei Li, Haitao Zhang, Limin 《Rare Metals》 SCIE EI CAS CSCD 2009年第2期142-146,共5页
Ti-Modified (Na0.5K0.5)(TixNb1-x)O3 (NKNT) piezoelectric ceramics were fabricated by double-layer buried powder process at 1020°C for 2 h. The microstructures,and piezoelectric and dielectric properties of the le... Ti-Modified (Na0.5K0.5)(TixNb1-x)O3 (NKNT) piezoelectric ceramics were fabricated by double-layer buried powder process at 1020°C for 2 h. The microstructures,and piezoelectric and dielectric properties of the lead-free NKNT ceramics were investigated. X-ray diffraction re-sults indicated that Ti4+ had diffused into the (Na0.5K0.5)NbO3 lattices to form a solid solution with a perovskite structure. The introducing of Ti into the (Na0.5K0.5)NbO3 solid solution effectively reduced the sintering temperature and... 展开更多
关键词 lead-free piezoelectric ceramics TI-DOPED piezoelectric property dielectric property normal sintering oxygen vacancies
下载PDF
Preparation and characteristic of NASICON ceramics 被引量:1
9
作者 ZHU Dongmei LUO Fa XIE Zhanglong ZHOU Wancheng 《Rare Metals》 SCIE EI CAS CSCD 2006年第z1期39-42,共4页
Hot-pressed sintering was employed to prepare the sodium super ionic conductor (Na1+xZr2SixP3-xO12, 1.8≤x≤2.2) ceramics and compare with the sample obtained from normal-press sintering. The phase formation, density,... Hot-pressed sintering was employed to prepare the sodium super ionic conductor (Na1+xZr2SixP3-xO12, 1.8≤x≤2.2) ceramics and compare with the sample obtained from normal-press sintering. The phase formation, density, and conductivity of the hot-press sintered and the normal-press sintered samples were investigated in detail. Results show that the density of NASICON ceramics and the degree of crystallization can be improved by hot-press process efficiently. The density of the sample sintered by normal sintering is obviously lower than that sintered by hot press. XRD analysis indicates all the hot press sintered samples contain mainly monoclinic NASICON and no ZrO2 phase was found. The ionic conductivity of normal-press sintered sample is much lower than that of hot-press sintered sample. When the composition is close to Na3Zr2Si2PO12, the dc conductivities of the hot press sintered samples were in the order of 10-3 S·cm-1. The variation of the ac conductivity with frequency in the high frequency region agrees with the power law feature of σ(ω)∝ωn(0<n<1). 展开更多
关键词 NASICON normal sintering hot pressed sintering electronic conductivity
下载PDF
ZrO_2(3Y)增韧增强WC-20%Co金属陶瓷复合材料 被引量:1
10
作者 安林 韩静涛 陈军 《北京科技大学学报》 EI CAS CSCD 北大核心 2006年第10期959-963,共5页
采用热等静压真空烧结工艺制备了不同含量ZrO2(3Y)/WC-20%Co金属陶瓷复合材料.对复合材料进行了硬度、抗弯强度和冲击韧性等力学性能测试,用扫描电子显微镜(SEM)分析了微观组织及冲击断口成分,用X射线衍射定量分析计算了力学性能试验前... 采用热等静压真空烧结工艺制备了不同含量ZrO2(3Y)/WC-20%Co金属陶瓷复合材料.对复合材料进行了硬度、抗弯强度和冲击韧性等力学性能测试,用扫描电子显微镜(SEM)分析了微观组织及冲击断口成分,用X射线衍射定量分析计算了力学性能试验前后t→m相变量.实验表明ZrO2(3Y)在WC-20%Co基体中呈球形,均匀分布在Co相和WC相中,该复合材料抗弯强度和冲击韧性明显提高,硬度指标提高不明显. 展开更多
关键词 金属陶瓷复合材料 ZrO2(3Y) 力学性能 热等静压 真空烧结 扫描电子显微镜 X射线衍射分析
下载PDF
利用粉煤灰反应烧结合成ZrO_2-莫来石复合材料 被引量:7
11
作者 马北越 厉英 翟玉春 《东北大学学报(自然科学版)》 EI CAS CSCD 北大核心 2010年第6期852-855,共4页
以粉煤灰、锆英石和氧化铝为原料,通过反应烧结法合成ZrO2-莫来石复合材料.研究了烧结温度对合成材料线收缩率、密度、吸水率、常温耐压强度和抗热震性的影响.采用XRD和SEM表征材料的相组成和显微结构.研究结果表明,在1600℃下烧结4h可... 以粉煤灰、锆英石和氧化铝为原料,通过反应烧结法合成ZrO2-莫来石复合材料.研究了烧结温度对合成材料线收缩率、密度、吸水率、常温耐压强度和抗热震性的影响.采用XRD和SEM表征材料的相组成和显微结构.研究结果表明,在1600℃下烧结4h可以合成常温耐压强度高、烧结性和抗热震性优异的ZrO2-莫来石复合材料;合成材料中ZrO2多以粒状形式存在,平均粒径约为5~10μm,能较均匀地分布于莫来石基质中. 展开更多
关键词 复合材料 ZrO2-莫来石 粉煤灰 烧结性能 常温耐压强度 抗热震性
下载PDF
常温固化免烧结泡沫陶瓷复合材料的制备及性能 被引量:1
12
作者 冯胜山 刘庆丰 《陶瓷》 CAS 2009年第12期17-21,共5页
利用自制的粘结剂,选用合适的填料、悬浮剂和减水剂、表面活性剂等附加剂,采用聚氨酯泡沫塑料先驱体挂浆成形法和常温固化工艺,制备出具有均匀、相互贯通孔结构的免烧结泡沫陶瓷复合材料,其生产工序简单,生产成本低,同时由于聚氨酯泡沫... 利用自制的粘结剂,选用合适的填料、悬浮剂和减水剂、表面活性剂等附加剂,采用聚氨酯泡沫塑料先驱体挂浆成形法和常温固化工艺,制备出具有均匀、相互贯通孔结构的免烧结泡沫陶瓷复合材料,其生产工序简单,生产成本低,同时由于聚氨酯泡沫塑料载体保留其中,所以产品韧性好,不易脆断。研究结果表明:随着粘结剂加入量的提高和泡沫塑料载体孔径的减小,泡沫陶瓷复合材料的抗压强度显著增大,但通孔率明显降低;采用适当浓度的碱液对泡沫塑料进行表面改性处理,可显著降低其表面张力,提高表面粗糙度,还能溶解残留的封孔薄膜,从而可增加挂浆量,提高其力学性能;但随着泡沫塑料载体表面改性处理时间的延长,泡沫陶瓷复合材料的通孔率下降;随着常温固化时间的延长,泡沫陶瓷复合材料的抗压强度逐步上升;常温固化28 d时,其抗压强度基本上达到最大值。 展开更多
关键词 常温固化 免烧结 泡沫陶瓷 复合材料 制备 性能
下载PDF
硅渣循环常压脱硅的老化周期及脱硅效率研究
13
作者 王红伟 马科友 龙建华 《湿法冶金》 CAS 北大核心 2012年第6期380-382,共3页
研究了烧结法脱硅中,常压下用硅渣作晶种,其循环使用周期及周期内脱硅效率。结果表明:常压下,硅渣循环使用老化周期为28h;前20h内,硅量指数在215以上,脱硅效率保持在88%左右;同一周期内,随时间延长,硅量指数和脱硅效率都呈上升趋势。
关键词 烧结法 常压 脱硅 硅渣 循环 老化周期 脱硅效率
下载PDF
硅渣常压脱硅效果研究
14
作者 马科友 王红伟 +1 位作者 龙建华 秦凤婷 《有色金属(冶炼部分)》 CAS 北大核心 2012年第9期31-33,37,共4页
在烧结法脱硅工序中,采用硅渣做晶种进行常压脱硅,研究在不同的Al2O3浓度、种子添加量和原液αk条件下的脱硅效果,并与拜耳赤泥的脱硅效果进行比较。结果表明,控制原液Al2O3浓度110~125g/L,αk=1.40~1.50,脱硅温度100℃,脱硅时间4h,... 在烧结法脱硅工序中,采用硅渣做晶种进行常压脱硅,研究在不同的Al2O3浓度、种子添加量和原液αk条件下的脱硅效果,并与拜耳赤泥的脱硅效果进行比较。结果表明,控制原液Al2O3浓度110~125g/L,αk=1.40~1.50,脱硅温度100℃,脱硅时间4h,种子添加量50g/L时,硅量指数可达到300以上。 展开更多
关键词 氧化铝 硅量指数 硅渣 常压脱硅 晶种 烧结法
下载PDF
粉煤灰陶粒混凝土与普通混凝土抗海水侵蚀试验研究 被引量:1
15
作者 籍凤秋 郝相雨 《石家庄铁道学院学报》 1994年第4期15-21,共7页
在试验室的条件下,采用加速循环的试验方法,将粉煤灰陶粒混凝土与普通混凝土的抗海水侵蚀性能进行了对比试验。 试验结果表明,粉煤灰陶粒混凝土比普通混凝土的抗海水侵蚀性能好。在有化学侵蚀性的海洋环境中。用粉煤灰陶粒混凝土代替普... 在试验室的条件下,采用加速循环的试验方法,将粉煤灰陶粒混凝土与普通混凝土的抗海水侵蚀性能进行了对比试验。 试验结果表明,粉煤灰陶粒混凝土比普通混凝土的抗海水侵蚀性能好。在有化学侵蚀性的海洋环境中。用粉煤灰陶粒混凝土代替普通混凝土,具有明显的技术经济效益。 展开更多
关键词 粉煤灰 陶粒混凝土 混凝土 抗侵蚀性
下载PDF
热压烧结制备晶须补强复合材料 被引量:4
16
作者 高桂英 陈立富 严勇军 《厦门大学学报(自然科学版)》 CAS CSCD 北大核心 1998年第6期880-884,共5页
通过热压烧结成功地制备了高致密度的SiCw晶须补强CMAS玻璃陶瓷基复合材料.SiCw晶须经超声波分散以后,加入到已球磨好的CMAS粉末与有机添加剂的浆料中,搅拌得到SiCw分散均匀的混合浆料.含有机添加剂的浆料在较... 通过热压烧结成功地制备了高致密度的SiCw晶须补强CMAS玻璃陶瓷基复合材料.SiCw晶须经超声波分散以后,加入到已球磨好的CMAS粉末与有机添加剂的浆料中,搅拌得到SiCw分散均匀的混合浆料.含有机添加剂的浆料在较低的压力下(2.37kPa)挤压通过微孔(=250μm),获得SiCw晶须分散均匀并高度取向的纤维状生坯.含晶须20%的CMAS通过无压烧结,烧结后样品相对密度仅达80%.但是通过热压烧结就可制备出相对密度达94.2%的复合材料. 展开更多
关键词 CMAS玻璃陶瓷 热压烧结 复合材料 晶须补强
下载PDF
ZBO(ZnO∶B)靶材烧结机理与特征的研究 被引量:1
17
作者 侯天雅 张弓 庄大明 《真空科学与技术学报》 EI CAS CSCD 北大核心 2006年第6期504-507,共4页
用常压烧结方法,在1200℃-1350℃烧结不同含B量的掺硼氧化锌(ZBO)靶材。研究了掺杂量、烧结温度对ZBO靶材微观结构的影响。实验表明,随着烧结温度的增加。ZBO陶瓷的晶粒大小和密度逐渐增大。指出了由于B2O3的挥发,造成ZBO靶材的剩... 用常压烧结方法,在1200℃-1350℃烧结不同含B量的掺硼氧化锌(ZBO)靶材。研究了掺杂量、烧结温度对ZBO靶材微观结构的影响。实验表明,随着烧结温度的增加。ZBO陶瓷的晶粒大小和密度逐渐增大。指出了由于B2O3的挥发,造成ZBO靶材的剩余含B量与掺B量的不符,要获得含定量B的ZBO就必须掺入大约2倍所需量的B2O3。 展开更多
关键词 常压烧结 ZBO SEM XRD
下载PDF
镁铝尖晶石质铸造砂的制备探究
18
作者 陈战考 田玉明 +3 位作者 周少鹏 李秋书 李占刚 黄麒 《中国陶瓷》 CAS CSCD 北大核心 2014年第2期25-29,共5页
利用铝矾土、轻质氧化镁粉,采用固相烧结工艺制备尖晶石质铸造砂。首先,研究球磨时间对原料粒径与表面形貌的影响;其次研究了烧结温度与保温时间对试样晶相组成、显微结构及物理性能的影响。结果表明:随着球磨时间的延长,原料发生二次... 利用铝矾土、轻质氧化镁粉,采用固相烧结工艺制备尖晶石质铸造砂。首先,研究球磨时间对原料粒径与表面形貌的影响;其次研究了烧结温度与保温时间对试样晶相组成、显微结构及物理性能的影响。结果表明:随着球磨时间的延长,原料发生二次细化与团聚,粉末形貌变化明显,球磨4 h与12 h均可将原料中位径降低至4μm;1450℃保温4 h烧结,得到发育完整清晰,外形呈八面体形貌,晶粒排列致密主晶相为MgAl2O4,体积密度约为3.0 g/cm3、显气孔约为3.3%;随着烧结温度的升高试样常温抗折强度得到提高,超过1500℃后变化不大。 展开更多
关键词 镁铝尖晶石质 球磨 烧结温度 保温时间 常温抗折强度
下载PDF
Microstructure and mechanical properties of WC-20wt% Co/ZrO_2(3Y)cermet composites 被引量:4
19
作者 Lin An Jingtao Han Jan Chen 《Journal of University of Science and Technology Beijing》 CSCD 2006年第2期174-177,共4页
The cermet composites WC-20wt%Co/ZrO2(E6)with four different comtents of ZrO2(3Y)were prepared by normal vacuum sinter processing;the optical microscope and SEMwere used to characterize their microstructures.The h... The cermet composites WC-20wt%Co/ZrO2(E6)with four different comtents of ZrO2(3Y)were prepared by normal vacuum sinter processing;the optical microscope and SEMwere used to characterize their microstructures.The hardness.bending strength and impact toughness of the specimens were determined.The experimental results show that ZrO2(3Y) particles in WC-20wt%Co matrix are sphcrical particles in different sizes which are distributed uniformly in Co phases and WC phases,the bending strength and impact toughness of the WC-20wt%Co cermet composites added ZrO2(3Y)improve remarkably.but the hardness values have little change. 展开更多
关键词 ZrO2(3Y) cermet composites mechanical properties microstructure normal vacuum sinter
下载PDF
微波热效应陶瓷材料性能研究
20
作者 王彬彬 刘秉国 +2 位作者 彭金辉 许磊 张世敏 《材料导报(纳米与新材料专辑)》 EI CAS 2012年第2期245-247,251,共4页
采用常压烧结法合成了Fe2O3-莫来石微波热效应陶瓷材料,并对材料的抗弯强度、抗热震性能及介电性能进行了研究。结果表明,随烧结温度由1250℃升高至1350℃,烧结样品中残留的刚玉相减少,微波热效应陶瓷材料的体积密度、抗弯强度显著增大... 采用常压烧结法合成了Fe2O3-莫来石微波热效应陶瓷材料,并对材料的抗弯强度、抗热震性能及介电性能进行了研究。结果表明,随烧结温度由1250℃升高至1350℃,烧结样品中残留的刚玉相减少,微波热效应陶瓷材料的体积密度、抗弯强度显著增大,相对介电常数随Fe2O3含量增加而增大,气孔率适中。在最佳烧结温度1350℃,氧化铁含量为30%,莫来石理论含量为70%条件下,制备的微波热效应陶瓷材料的体积密度为2.185g/cm3,抗压强度为77MPa,相对介电常数适中,满足微波热效应陶瓷性能要求。 展开更多
关键词 陶瓷 微波热效应 常压烧结 微波吸波 蓄热