Three-dimensional(3D)porous absorbents have attracted significant attention in the oily wastewater treatment technology due to their high porosity and elasticity.Given their amphiphilic surface,they have a propensity ...Three-dimensional(3D)porous absorbents have attracted significant attention in the oily wastewater treatment technology due to their high porosity and elasticity.Given their amphiphilic surface,they have a propensity to simultaneously absorb water and oil,which restricts their range of applications.In this study,a reduced graphene oxide and titanium dioxide nanocomposite(rGO/TiO_(2))was used to fabricate an ultra-hydrophobic melamine sponge(MS)through interfacial modification using a solution immersion technique.To further modify it,poly-dimethylsiloxane(PDMS)was grafted onto its surface to establish stronger covalent bonds with the composite.The water contact angle of the sponge(rGO/TiO_(2)/PDMS/MS)was 164.2°,which satisfies the condition for ultrahydrophobicity.The evidence of its water repellency was demonstrated by the Cassie-Baxter theory and the lotus leaf effect.As a result of the increased density of rGO/TiO_(2)/PDMS/MS,it recorded an initial capacity that was 2 g/g lower than the raw MS for crude oil absorption.The raw MS retained 53% of its initial absorption capacity after 20 cycles of absorption,while rGO/TiO_(2)/PDMS/MS retained 97%,suggesting good recyclability.Excellent oil and organic solvent recovery(90%-96%)was demonstrated by rGO/TiO_(2)/PDMS/MS in oil-water combinations.In a continuous separation system,it achieved a remarkable separation efficiency of 2.4×10^(6)L/(m^(3)·h),and in turbulent emulsion separation,it achieved a demulsification efficiency of 90%-91%.This study provides a practical substitute for massive oil spill cleaning.展开更多
A compound varifocal lens based on electromagnetic drive technology is designed and fabricated, where the polydimethylsiloxane(PDMS) film acts as a driving component, while the PDMS biconvex lens and the plane-concave...A compound varifocal lens based on electromagnetic drive technology is designed and fabricated, where the polydimethylsiloxane(PDMS) film acts as a driving component, while the PDMS biconvex lens and the plane-concave lens form a coaxial compound lens system. The plane-concave lens equipped with driving coils is installed directly above the PDMS lens surrounded by the annular magnet. When different currents are applied, the annular magnet moves up and down, driving the PDMS film to undergo elastic deformation, and then resulting in longitudinal movement of the PDMS lens. The position change of the PDMS lens changes the focal length of the compound lens system. To verify the feasibility and practicability of this design, a prototype of our compound lens system is fabricated in experiment. Our proposed compound lens shows that its zoom ability reaches 9.28 mm when the current ranges from -0.20 A to 0.21 A.展开更多
Polydimethylsiloxane (PDMS) rubber latex with two sorts of sensitizers, trimethylol propane tri-methacrylate (TMPTMA) and diethylene glycol di-acrylate (DEGDA), was irradiated with γ-rays and electron beams in variou...Polydimethylsiloxane (PDMS) rubber latex with two sorts of sensitizers, trimethylol propane tri-methacrylate (TMPTMA) and diethylene glycol di-acrylate (DEGDA), was irradiated with γ-rays and electron beams in various conditions. The radiation crosslinking reaction of PDMS occurs in the inner phase of the latex and is relatively isolated from the water phase. Therefore the oxygen and the radicals produced by the radiolysis reaction of water almost have no effect on the crosslinking reaction of polymer. The experimental data correspond with the Charlesby-Pinner relationship in the main. The gelation doses, degree of crosslinking and degradation as well as G values of crosslinking were calculated. From them, the sensitization coefficients were derived to offer a quantitative measurement of the enhancing effect of sensitizer on the radiation crosslinking.展开更多
A novel hydroxypolyether blocked polydimethylsiloxane, poly(ethylene oxide) propyl-b-polydimethylsiloxane-b-propyl poly(ethylene oxide) (PEO-b-PDMS-b-PEO) was synthesized by simple hydrosilation reaction of poly...A novel hydroxypolyether blocked polydimethylsiloxane, poly(ethylene oxide) propyl-b-polydimethylsiloxane-b-propyl poly(ethylene oxide) (PEO-b-PDMS-b-PEO) was synthesized by simple hydrosilation reaction of poly(ethylene glycol) monoallyl ether with α,ω-dihydrogen terminated PDMS (HPDMS). Fourier transform infrared spectroscopy (FTIR) and IH NMR were used to identify the structure of PEO-b-PDMS-b-PEO and intermediate product HPDMS. Based on the effect investigations of temperature, reactant molar ratio, catalyst and time on the hydrosilation, it was found that the conversion of Si-H bond to SiC bond increased with the increase of catalyst and time, and the reaction completed when the content of catalyst was 22μg/g and the time was 5 h, respectively. Urethane reaction of OH and NCO group confirms that PEO-b-PDMS-b-PEO is more reactive toward to diisocyanate than α,ω-dihydroxylbutyl terminated PDMS.展开更多
Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile...Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile) (PPEN) in the presence of chlorobenzcne/N-methyl pyrrolidone (NMP) as solvents. The products were characterized by FTIR, ^1H NMR and gel permeation chromatography. Differential scanning calorimetry analysis indicated that the block copolymers showed separated microphase.展开更多
基金supported by the Universiti Brunei Darussalam Research Funding(Grant No.UBD/OAVCRI/CRGWG(022)/171001).
文摘Three-dimensional(3D)porous absorbents have attracted significant attention in the oily wastewater treatment technology due to their high porosity and elasticity.Given their amphiphilic surface,they have a propensity to simultaneously absorb water and oil,which restricts their range of applications.In this study,a reduced graphene oxide and titanium dioxide nanocomposite(rGO/TiO_(2))was used to fabricate an ultra-hydrophobic melamine sponge(MS)through interfacial modification using a solution immersion technique.To further modify it,poly-dimethylsiloxane(PDMS)was grafted onto its surface to establish stronger covalent bonds with the composite.The water contact angle of the sponge(rGO/TiO_(2)/PDMS/MS)was 164.2°,which satisfies the condition for ultrahydrophobicity.The evidence of its water repellency was demonstrated by the Cassie-Baxter theory and the lotus leaf effect.As a result of the increased density of rGO/TiO_(2)/PDMS/MS,it recorded an initial capacity that was 2 g/g lower than the raw MS for crude oil absorption.The raw MS retained 53% of its initial absorption capacity after 20 cycles of absorption,while rGO/TiO_(2)/PDMS/MS retained 97%,suggesting good recyclability.Excellent oil and organic solvent recovery(90%-96%)was demonstrated by rGO/TiO_(2)/PDMS/MS in oil-water combinations.In a continuous separation system,it achieved a remarkable separation efficiency of 2.4×10^(6)L/(m^(3)·h),and in turbulent emulsion separation,it achieved a demulsification efficiency of 90%-91%.This study provides a practical substitute for massive oil spill cleaning.
文摘A compound varifocal lens based on electromagnetic drive technology is designed and fabricated, where the polydimethylsiloxane(PDMS) film acts as a driving component, while the PDMS biconvex lens and the plane-concave lens form a coaxial compound lens system. The plane-concave lens equipped with driving coils is installed directly above the PDMS lens surrounded by the annular magnet. When different currents are applied, the annular magnet moves up and down, driving the PDMS film to undergo elastic deformation, and then resulting in longitudinal movement of the PDMS lens. The position change of the PDMS lens changes the focal length of the compound lens system. To verify the feasibility and practicability of this design, a prototype of our compound lens system is fabricated in experiment. Our proposed compound lens shows that its zoom ability reaches 9.28 mm when the current ranges from -0.20 A to 0.21 A.
基金Contract grant sponsors: Major State Basic Research Projects of China (G1999064800)
文摘Polydimethylsiloxane (PDMS) rubber latex with two sorts of sensitizers, trimethylol propane tri-methacrylate (TMPTMA) and diethylene glycol di-acrylate (DEGDA), was irradiated with γ-rays and electron beams in various conditions. The radiation crosslinking reaction of PDMS occurs in the inner phase of the latex and is relatively isolated from the water phase. Therefore the oxygen and the radicals produced by the radiolysis reaction of water almost have no effect on the crosslinking reaction of polymer. The experimental data correspond with the Charlesby-Pinner relationship in the main. The gelation doses, degree of crosslinking and degradation as well as G values of crosslinking were calculated. From them, the sensitization coefficients were derived to offer a quantitative measurement of the enhancing effect of sensitizer on the radiation crosslinking.
基金the National Natural Science Foundation of China(No.50273035)Anhui Provincial Education Department(No.2004kj362zd)are acknowledged.
文摘A novel hydroxypolyether blocked polydimethylsiloxane, poly(ethylene oxide) propyl-b-polydimethylsiloxane-b-propyl poly(ethylene oxide) (PEO-b-PDMS-b-PEO) was synthesized by simple hydrosilation reaction of poly(ethylene glycol) monoallyl ether with α,ω-dihydrogen terminated PDMS (HPDMS). Fourier transform infrared spectroscopy (FTIR) and IH NMR were used to identify the structure of PEO-b-PDMS-b-PEO and intermediate product HPDMS. Based on the effect investigations of temperature, reactant molar ratio, catalyst and time on the hydrosilation, it was found that the conversion of Si-H bond to SiC bond increased with the increase of catalyst and time, and the reaction completed when the content of catalyst was 22μg/g and the time was 5 h, respectively. Urethane reaction of OH and NCO group confirms that PEO-b-PDMS-b-PEO is more reactive toward to diisocyanate than α,ω-dihydroxylbutyl terminated PDMS.
文摘Block copolymers with different backbone compositions have been prepared by the condensation of dimethylamino terminated poly(dimethylsiloxane) (PDMS) and hydroquinone terminated poly(phthalazinone ether nitrile) (PPEN) in the presence of chlorobenzcne/N-methyl pyrrolidone (NMP) as solvents. The products were characterized by FTIR, ^1H NMR and gel permeation chromatography. Differential scanning calorimetry analysis indicated that the block copolymers showed separated microphase.