The molecular recyclability of poly (ethylene terephthalate) (PET) and three semi-aromatic polyesters poly (phloretic acid) (poly-H), poly (dihydroferulic acid) (poly-G), and poly (dihydrosinapinic acid) (poly-S) is e...The molecular recyclability of poly (ethylene terephthalate) (PET) and three semi-aromatic polyesters poly (phloretic acid) (poly-H), poly (dihydroferulic acid) (poly-G), and poly (dihydrosinapinic acid) (poly-S) is evaluated in this study. PET is an extensively used aromatic polyester, and poly-H, poly-G, and poly-S can be considered semi-aromatic poly (lactic acid) modifications. All these polyesters have been depolymerized at neutral pH and by acid- and base-catalyzed hydrolysis at two temperatures, i.e., 50˚C and 80˚C. Base-catalyzed depolymerization of virgin PET leads to an isolated yield of 38% after 48 hours of reaction at 80˚C. Contrary to these results for PET, almost all the monomers of the semi-aromatic polyesters poly-H, poly-G, and poly-S are recovered with isolated yields larger than 90% at the same temperature after 15 minutes in a facile manner. A shrinking particle model used to determine the global kinetics of the base-catalyzed depolymerization showed that the rate rises with increasing temperature. Using the shrinking particle model, the intrinsic reaction rate constants were determined. It has been demonstrated that the rate coefficients of the depolymerization of the semi-aromatic polyesters poly-H, poly-G, and poly-S are between 2 and 3 orders of magnitude higher than those for PET.展开更多
文摘The molecular recyclability of poly (ethylene terephthalate) (PET) and three semi-aromatic polyesters poly (phloretic acid) (poly-H), poly (dihydroferulic acid) (poly-G), and poly (dihydrosinapinic acid) (poly-S) is evaluated in this study. PET is an extensively used aromatic polyester, and poly-H, poly-G, and poly-S can be considered semi-aromatic poly (lactic acid) modifications. All these polyesters have been depolymerized at neutral pH and by acid- and base-catalyzed hydrolysis at two temperatures, i.e., 50˚C and 80˚C. Base-catalyzed depolymerization of virgin PET leads to an isolated yield of 38% after 48 hours of reaction at 80˚C. Contrary to these results for PET, almost all the monomers of the semi-aromatic polyesters poly-H, poly-G, and poly-S are recovered with isolated yields larger than 90% at the same temperature after 15 minutes in a facile manner. A shrinking particle model used to determine the global kinetics of the base-catalyzed depolymerization showed that the rate rises with increasing temperature. Using the shrinking particle model, the intrinsic reaction rate constants were determined. It has been demonstrated that the rate coefficients of the depolymerization of the semi-aromatic polyesters poly-H, poly-G, and poly-S are between 2 and 3 orders of magnitude higher than those for PET.