期刊文献+
共找到4篇文章
< 1 >
每页显示 20 50 100
Investigation on a Sol-gel Coating Containing Inhibitors on 2024-T3 Aluminum Alloy
1
作者 SHI Hong-wei LIU Fu-chun HAN En-hou SUN Ming-cheng 《Chinese Journal of Aeronautics》 SCIE EI CAS CSCD 2006年第B12期106-112,共7页
For a long time, chromate incorporated conversion coatings have been drawn special attention in corrosion protection of aircraft-used aluminum alloys. However, ever-increasing environmental pressures requires that non... For a long time, chromate incorporated conversion coatings have been drawn special attention in corrosion protection of aircraft-used aluminum alloys. However, ever-increasing environmental pressures requires that non-chromate conversion coatings be developed because of the detrimental carcinogenic effects of the chromate compounds. In recent years, the sol-gel coatings doped with inhibitors were developed to replace chromate conversion coatings, and showed real promise; A sol-gel coating was prepared and its anti-corrosion behavior was investigated using the potentiodynamic scanning (PDS) and the electrochemical impedance spectroscopy (EIS). It is found that the sol-gel coating obtained by the hydrolysis and condensation of 3-glycidoxypropyltrimethoxysilane (GPTMS) and tetramethoxysilane (TMOS) is prone to form defects if cured at the room temperature, whereas if cured at a higher temperature (100℃), these flaws can be avoided. Furthermore, it can be seen that addition of anti-foam agents and surfactants will reduce the faults if cured at the room temperature. Effects of the corrosion inhibitors, CeCl3 and mercaptobenzothiazole (MBT), in the sol-gel coatings on 2024-T3 aluminum alloy were also investigated. Results show that the corrosion resistance of the sol-gel coatings containing CeCl3 proves to be better than that of the pure and MBT added sol-gel coatings by the electrochemical methods. 展开更多
关键词 corrosion protection sol-gel coating electrochemical impedance spectroscopy (EIS) inhibitor potentiodynamic scan (pds aluminum alloy
下载PDF
NaCl溶液中Al-Li合金腐蚀过程的电化学特征 被引量:16
2
作者 李劲风 张 昭 +4 位作者 程英亮 曹发和 王建明 张鉴清 曹楚南 《金属学报》 SCIE EI CAS CSCD 北大核心 2002年第7期760-764,共5页
采用电化学噪声技术,结合电化学阻抗谱及极化曲线测量,研究了峰时效AA2195-T8铝合金在3.0%NaCl溶液中的腐蚀电化学特征.结果表明,腐蚀初期,合金表面钝化膜上不断有孔核的形成与修复,并导致阻抗谱上感抗成分的存在.随腐蚀时间的延长,其... 采用电化学噪声技术,结合电化学阻抗谱及极化曲线测量,研究了峰时效AA2195-T8铝合金在3.0%NaCl溶液中的腐蚀电化学特征.结果表明,腐蚀初期,合金表面钝化膜上不断有孔核的形成与修复,并导致阻抗谱上感抗成分的存在.随腐蚀时间的延长,其感抗成分消失且阻抗模值降低.阳极极化时,由于其孔蚀电位与自腐蚀电位接近,钝化电位区间很小;随腐蚀时间的延长,极化电阻先增加而后减小,自腐蚀电流则呈相反趋势变化. 展开更多
关键词 AA2195-T8铝合金 NACL溶液 腐蚀 电化学噪声 阻抗谱 极化曲线
下载PDF
铝合金在NaCl溶液中的电化学腐蚀行为 被引量:17
3
作者 汪俊英 孔小东 刘信 《装备环境工程》 CAS 2010年第3期38-41,共4页
采用极化曲线法和交流阻抗法,分析了ZL102和LF6铝合金在不同pH的3%NaCl溶液中的腐蚀特性,并用金相显微镜观察了铝合金的微观组织。结果表明,2种铝合金的自腐蚀电位都随着pH的升高变得愈负;除pH=9.5的情形之外,ZL102铝合金的腐蚀速率均小... 采用极化曲线法和交流阻抗法,分析了ZL102和LF6铝合金在不同pH的3%NaCl溶液中的腐蚀特性,并用金相显微镜观察了铝合金的微观组织。结果表明,2种铝合金的自腐蚀电位都随着pH的升高变得愈负;除pH=9.5的情形之外,ZL102铝合金的腐蚀速率均小于LF6铝合金;LF6铝合金结构的不均匀性与其加入的合金化元素是导致其耐蚀性能较ZL102铝合金差的主要原因。 展开更多
关键词 铝合金 耐腐蚀性能 极化曲线 阻抗谱 微观组织
下载PDF
钨铝合金在不同NaCl溶液中的电化学腐蚀行为研究 被引量:13
4
作者 吴茂永 田继强 +3 位作者 曹立新 高荣杰 苏革 柳伟 《腐蚀科学与防护技术》 CAS CSCD 北大核心 2015年第1期25-30,共6页
采用极化曲线、电化学阻抗谱等电化学方法研究了钨铝合金在不同温度、盐度及p H值的Na Cl溶液中的腐蚀行为。实验结果表明:钨铝合金的腐蚀速率随盐度的增加而增加;耐腐蚀性能随温度的升高而下降;在中性Na Cl溶液中最耐腐蚀,且酸性越大,... 采用极化曲线、电化学阻抗谱等电化学方法研究了钨铝合金在不同温度、盐度及p H值的Na Cl溶液中的腐蚀行为。实验结果表明:钨铝合金的腐蚀速率随盐度的增加而增加;耐腐蚀性能随温度的升高而下降;在中性Na Cl溶液中最耐腐蚀,且酸性越大,腐蚀速率越快。 展开更多
关键词 钨铝合金 NACL溶液 腐蚀 阻抗图谱 极化曲线
原文传递
上一页 1 下一页 到第