Superparamgnetic Fe_3O_4 and RE:Fe_3O_4(RE=Dy,Nd,La)nanoparticles with an average crystallite size in the range of 15–24 nm,were synthesized by co-precipitation method.The samples were characterized using X-ray diffr...Superparamgnetic Fe_3O_4 and RE:Fe_3O_4(RE=Dy,Nd,La)nanoparticles with an average crystallite size in the range of 15–24 nm,were synthesized by co-precipitation method.The samples were characterized using X-ray diffraction(XRD),scanning electron microscopy(SEM),vibrating sample magnetometer(VSM),UV–Vis spectroscopy,LCR bridge,and two-probe technique.X-ray diffraction patterns of all the investigated samples reveal the typical phase of magnetite structure,with a small contribution of orthoferrite(NdFeO_3)as a secondary phase in Nd:Fe_3O_4 sample.The saturation magnetization(M_s)of the samples has values in the range from 41.8 to 52.3 emu/g,and decreases with RE ion doping depending on the ionic radius.Negligible values of the coercivity H_c and remanenceM_r,indicate the superparamagnetic nature of the investigated samples.The calculated values of indirect optical band gap of Fe_3O_4 and RE:Fe_3O_4 nanoparticles are in the range of0.9–1.25 eV.The dielectric constant of the samples decreases,while their activation energy increases with the increasing of ionic radii of dopants.展开更多
基金the Deanship of Scientific Research at King Khalid University for funding this work through General Research Project under grant number G.R.P-310-38
文摘Superparamgnetic Fe_3O_4 and RE:Fe_3O_4(RE=Dy,Nd,La)nanoparticles with an average crystallite size in the range of 15–24 nm,were synthesized by co-precipitation method.The samples were characterized using X-ray diffraction(XRD),scanning electron microscopy(SEM),vibrating sample magnetometer(VSM),UV–Vis spectroscopy,LCR bridge,and two-probe technique.X-ray diffraction patterns of all the investigated samples reveal the typical phase of magnetite structure,with a small contribution of orthoferrite(NdFeO_3)as a secondary phase in Nd:Fe_3O_4 sample.The saturation magnetization(M_s)of the samples has values in the range from 41.8 to 52.3 emu/g,and decreases with RE ion doping depending on the ionic radius.Negligible values of the coercivity H_c and remanenceM_r,indicate the superparamagnetic nature of the investigated samples.The calculated values of indirect optical band gap of Fe_3O_4 and RE:Fe_3O_4 nanoparticles are in the range of0.9–1.25 eV.The dielectric constant of the samples decreases,while their activation energy increases with the increasing of ionic radii of dopants.